CN202928917U - 一种评价碱性电池无汞锌粉性能的装置 - Google Patents
一种评价碱性电池无汞锌粉性能的装置 Download PDFInfo
- Publication number
- CN202928917U CN202928917U CN 201220571619 CN201220571619U CN202928917U CN 202928917 U CN202928917 U CN 202928917U CN 201220571619 CN201220571619 CN 201220571619 CN 201220571619 U CN201220571619 U CN 201220571619U CN 202928917 U CN202928917 U CN 202928917U
- Authority
- CN
- China
- Prior art keywords
- zinc powder
- shaped pipe
- mercury
- alkaline battery
- performance
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型一种评价碱性电池无汞锌粉性能的装置,其特征在于包括带密封盖的塑料容器、水浴锅、带刻度的U型管,塑料容器放在水浴锅内,水浴锅内装有水溶液,塑料容器内装有锌膏,锌膏上方用液体石蜡封住,U型管两端开口,U型管的其中一端与塑料容器相通,U型管的另一端与大气相通,U型管中间段灌有液体石蜡,扩大了取样量,避免了气体产生却无法准确读取析气量的问题,利用了金属锌粉的表面自由能,以及对气泡上升的内部阻力。通过测试材料的体积膨胀体积来评价锌粉气体产生的大小,有效的评估无汞锌粉的性能。这种方法能结合实际生产,通过无汞电池的锌膏配方更直观的评价锌粉在制备成锌膏后的性能。
Description
技术领域
本实用新型涉及一种碱性电池检性能测装置,尤其是涉及一种评价碱性电池无汞锌粉性能的装置。
背景技术
无汞锌粉作为碱性电池无汞化的最重要材料,它的性能直接影响了电池的性能。无汞锌粉性能是物理化学综合因素的表现,单从杂质含量、添加元素含量、或者从颗粒度分布、还是氧化锌含量都无法准确表述锌粉性能,这些条件是构成锌粉优良性能的必要条件而不是充分条件。因而我们需要一种锌粉性能参数,能够直观快速的评价锌粉性能,用来指导生产。锌粉作为碱性电池负极材料,存在于碱性环境中。目前通过锌粉析气量来综合评价锌粉的性能,锌粉析气量主要有下列几个原因产生:
1)锌的氧化电位高于水的还原电位,因而锌容易在电解液中发生析氢反应,活性物质会被消耗;
2)锌粉中的微量杂质,如铁、铜、镍等杂质的析氢电位较锌更低,因而形成锌腐蚀微电池加速锌腐蚀放出氢气。
综上所述,析气量是一个评价锌粉质量的综合性指标,从电池安全性能上而言,析气量越小,电池漏液气胀的概率就越低,电池安全性能就越好。目前国内,最常用的析气量测试方法是根据行业推荐的集气法测定锌粉析气量。
用该方法存在如下缺点:锌粉在碱液中产生自腐蚀,在金属表面产生气泡,但是由于金属的表面自由能的存在,使产生的气体有吸附在金属表面的趋向,同时由于锌粉和碱液之间存在内部阻力,导致产生的气泡吸附在金属表面,无法顺利析出。而恰恰是产生的气体就是我们需要测试的析气量,当部分析气量通过气泡的形式吸附在金属表面时,导致了我们的测试方法只能收集到部分析出的气体,所收集到的气体无法直观的表达出锌粉析气量的大小,这样就导致了析气量的实际测试值偏低,气泡的产生很大程度上受到操作的干扰。
发明内容
本实用新型所要解决的技术问题是提供一种受干扰小、客观准确地评价碱性电池无汞锌粉性能的装置。
本实用新型解决上述技术问题所采用的技术方案为:一种评价碱性电池无汞锌粉性能的装置,其特征在于包括带密封盖的塑料容器、水浴锅、带刻度的U型管,所述的塑料容器放在所述的水浴锅内,所述的水浴锅内装有水溶液,所述的塑料容器内装有锌膏,锌膏上方用液体石蜡封住,所述的U型管两端开口,U型管的其中一端与塑料容器相通,所述的U型管的另一端与大气相通,所述的U型管中间段灌有液体石蜡。
还包括支撑架,所述的支撑架上设置有挂架,所述的U型管的另一端固定在所述的挂架上。
所述的U型管一端连接有橡胶管,所述的橡胶管一端穿过所述的密封盖伸进所述的塑料容器内。
所述的密封盖由橡胶材料制成。
与现有技术相比,本实用新型的优点是首先得到初始状态下锌膏的体积V2和型管内的初始刻度为V0,恒温加热装置将水溶液加热到60度并保持三天,再读取U型管内的最终刻度为V1,利用析气量=V1—V0)/ V2*100%即得,本实用新型扩大了取样量,避免了气体产生却无法准确读取析气量的问题,利用了金属锌粉的表面自由能,以及对气泡上升的内部阻力。通过测试材料的体积膨胀体积来评价锌粉气体产生的大小,有效的评估无汞锌粉的性能。这种方法能结合实际生产,通过无汞电池的锌膏配方更直观的评价锌粉在制备成锌膏后的性能。
附图说明
图1为本实用新型的结构图。
具体实施方式
以下结合附图实施例对本实用新型作进一步详细描述。
一种评价碱性电池无汞锌粉性能的装置,包括带密封盖1的塑料容器2、水浴锅3、带刻度的U型管4,塑料容器带有刻度,塑料容器2放在水浴锅3内,水浴锅3内装有水溶液,塑料容器2内装有锌膏5,锌膏5上方用液体石蜡6封住,U型管4两端开口,U型管4的其中一端与塑料容器2相通,U型管4的另一端与大气相通,U型管4中间段灌有液体石蜡6。 还包括支撑架7,支撑架7上设置有挂架8,U型管4的另一端固定在挂架8上。U型管4一端连接有橡胶管9,橡胶管9一端穿过密封盖1伸进塑料容器2内。密封盖1由橡胶材料制成。
Claims (4)
1.一种评价碱性电池无汞锌粉性能的装置,其特征在于包括带密封盖的塑料容器、水浴锅、带刻度的U型管,所述的塑料容器放在所述的水浴锅内,所述的水浴锅内装有水溶液,所述的塑料容器内装有锌膏,锌膏上方用液体石蜡封住,所述的U型管两端开口,U型管的其中一端与塑料容器相通,所述的U型管的另一端与大气相通,所述的U型管中间段灌有液体石蜡。
2.根据权利要求1所述的一种评价碱性电池无汞锌粉性能的装置,其特征在于还包括支撑架,所述的支撑架上设置有挂架,所述的U型管的另一端固定在所述的挂架上。
3.根据权利要求2所述的一种评价碱性电池无汞锌粉性能的装置,其特征在于所述的U型管一端连接有橡胶管,所述的橡胶管一端穿过所述的密封盖伸进所述的塑料容器内。
4.根据权利要求3所述的一种评价碱性电池无汞锌粉性能的装置,其特征在于所述的密封盖由橡胶材料制成。