CN202734569U - 一种闪速炉冷却水套 - Google Patents

一种闪速炉冷却水套 Download PDF

Info

Publication number
CN202734569U
CN202734569U CN 201220289361 CN201220289361U CN202734569U CN 202734569 U CN202734569 U CN 202734569U CN 201220289361 CN201220289361 CN 201220289361 CN 201220289361 U CN201220289361 U CN 201220289361U CN 202734569 U CN202734569 U CN 202734569U
Authority
CN
China
Prior art keywords
water jacket
cooling water
jacket
furnace cooling
flash furnace
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201220289361
Other languages
English (en)
Inventor
刘铸
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jinchuan Group Co Ltd
Original Assignee
Jinchuan Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jinchuan Group Co Ltd filed Critical Jinchuan Group Co Ltd
Priority to CN 201220289361 priority Critical patent/CN202734569U/zh
Application granted granted Critical
Publication of CN202734569U publication Critical patent/CN202734569U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

一种闪速炉冷却水套,涉及一种用于闪速炉连接部的冷却水套,适用于各种炉窑连接部。其特征在于其结构包括冷却套本体和位于冷却水套本体内部的、为预埋铜冷却水管的冷却水通道。本实用新型采用镍闪速炉连接部齿形水套,消除了水套漏水隐患,增强了水套底部的耐磨损程度。

Description

一种闪速炉冷却水套
技术领域
一种闪速炉冷却水套,涉及一种用于镍闪速炉连接部的冷却水套,适用于各种炉窑连接部。
背景技术
目前,镍闪速炉一直采用轧制钻孔铜水套工艺作为炉体的冷却方式,水套采用三道密封技术。三道密封包括涂抹高温密封胶的过盈配合铜塞子、双面抹高温胶的金属石墨缠绕垫和抹高温胶的管螺纹丝堵,对水套加工工艺孔进行密封。但是在镍闪速炉上的反应塔和沉淀池的连接部用倒F水套连接,钻孔水套的工艺孔在高速气流的冲刷、高温烟气的冲刷和高温熔体的直接腐蚀下存在漏水的安全隐患。
发明内容
本实用新型的目的是针对上述已有技术存在的不足,提供一种能有效消了水套漏水隐患,增强了水套底部的耐磨损度的闪速炉冷却水套
本实用新型的目的是通过以下技术方案实现的。
一种闪速炉冷却水套,其特征在于其结构包括冷却套本体和位于冷却水套本体内部的、为预埋铜冷却水管的冷却水通道。
本实用新型的一种闪速炉冷却水套,其特征在于所述的冷却套本体外壁一体地设有直齿形凸状体。
本实用新型的一种闪速炉冷却水套,其特征在于所述的冷却套本体底部设有堆焊联接的耐高温耐磨合金材料层。
本实用新型的一种闪速炉冷却水套,采用预埋铜管铸造铜水套替代轧制紫铜钻孔倒F水套,铜管铸造铜水套耐高速气流的冲刷、耐高温烟气的冲刷和高温熔体的直接腐蚀,避免了工艺孔的漏水等特点。倒F水套改造成齿形水套,齿型水套底部堆焊耐高温耐磨合金材料,可防止底部烟气冲刷造成的磨损。
附图说明
图1为本实用新型的结构示意图。
具体实施方式
一种闪速炉冷却水套,其结构包括冷却套本体1和位于冷却水套本体内部的、为预埋铜冷却水管的冷却水通道2;所述的冷却套本体外壁一体地设有直齿形凸状体3;所述的冷却套本体底部设有堆焊联接的耐高温耐磨合金材料层4。
实施例
在镍闪速炉反应塔和沉淀池连接部的镍闪速炉连接部采用本实用新型的水套。采用埋管式铸铜,浇铸材料为紫铜,埋管为铜管,需要整根弯制,无焊接接头,铸造完毕后母材含铜量为99.7%。铜管无熔穿,铜管于母材融合率为93%;齿型水套底部堆焊耐高温耐磨合金材料,写具体是什么材料,水套无漏水现象出现。

Claims (3)

1.一种闪速炉冷却水套,其特征在于其结构包括冷却套本体和位于冷却水套本体内部的、为预埋铜冷却水管的冷却水通道。
2.根据权利要求1所述的一种闪速炉冷却水套,其特征在于所述的冷却套本体外壁一体地设有直齿形凸状体。
3.根据权利要求1所述的一种闪速炉冷却水套,其特征在于所述的冷却套本体底部设有堆焊联接的耐高温耐磨合金材料层。
CN 201220289361 2012-06-20 2012-06-20 一种闪速炉冷却水套 Expired - Fee Related CN202734569U (zh)