CN202465907U - 万安培稀土熔盐电解槽坩埚 - Google Patents

万安培稀土熔盐电解槽坩埚 Download PDF

Info

Publication number
CN202465907U
CN202465907U CN2012200941162U CN201220094116U CN202465907U CN 202465907 U CN202465907 U CN 202465907U CN 2012200941162 U CN2012200941162 U CN 2012200941162U CN 201220094116 U CN201220094116 U CN 201220094116U CN 202465907 U CN202465907 U CN 202465907U
Authority
CN
China
Prior art keywords
rare earth
crucible
container body
earth molten
molten salt
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2012200941162U
Other languages
English (en)
Inventor
邝国春
毛建辉
张旭熙
潘艳芳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANXI NANFANG RARE EARTH HIGH TECHNOLOGY Co Ltd
Original Assignee
JIANXI NANFANG RARE EARTH HIGH TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANXI NANFANG RARE EARTH HIGH TECHNOLOGY Co Ltd filed Critical JIANXI NANFANG RARE EARTH HIGH TECHNOLOGY Co Ltd
Priority to CN2012200941162U priority Critical patent/CN202465907U/zh
Application granted granted Critical
Publication of CN202465907U publication Critical patent/CN202465907U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型公开了一种万安培稀土熔盐电解槽坩埚,包括容器体,其特征在于:所述容器体内壁及底面铺设一层耐高温液流冲刷的金属层。本实用新型与现有技术相比的优点是:避免电解出的金属液体与筑炉材料的接触,降低电解出的稀土金属中非稀土元素含量,可局部更换坩埚拼接材料,提高坩埚使用寿命,结构简单。

Description

万安培稀土熔盐电解槽坩埚
技术领域
[0001] 本实用新型涉及一种电解电流为万安培以上稀土熔盐电解槽用盛装金属液的容器,此容器隔离电解过程获得的金属液与筑炉材料的接触,避免杂质污染,并能耐高温。
背景技术
目前,公知的万安培电流以上上挂阴阳极稀土熔盐电解槽坩埚均采用钨或钼材料制成的整体圆形平底坩埚或单层材料拼接的半圆弧形底面、端面为平面的坩埚。但整体坩埚当有局部损坏时,影响整体使用,使用寿命短,使用成本高,而单层材料拼接的坩埚由于接缝的影响,金属液易渗透与筑炉材料发生化学反应,造成金属液非稀土金属元素含量偏高,影响电解金属产品质量。
发明内容
为了克服现有的万安培稀土熔盐电解槽坩埚寿命短,易被非稀土元素污染的不足,本实用新型提供一种万安培稀土熔盐电解槽坩埚以提高坩埚使用寿命和隔离非稀土元素的污染。
本实用新型的上述目的通过以下的技术方案来实现:一种万安培稀土熔盐电解槽坩埚,包括容器体,其特征在于:所述容器体内壁及底面铺设一层耐高温液流冲刷的金属层。
所述金属层为钨板层。
所述金属层为钼板层。
本实用新型与现有技术相比的优点是:避免电解出的金属液体与筑炉材料的接触,降低电解出的稀土金属中非稀土元素含量,可局部更换坩埚拼接材料,提高坩埚使用寿命,结构简单。
附图说明
图1是本实用新型实施例的纵剖面构造图。
图2是本实用新型的俯视图。
图中:1—容器体;2—金属层。
【具体实施方式】
下面结合附图对本实用新型进一步详述:
如图1、图2所示,在方形耐高温及熔盐腐蚀的盛装液态金属的容器体1的内壁及底面铺设一层耐高温液流冲刷的金属层2,该金属层2可以是钨板层,也可以是钼板层,并固定在容器体1上。由于盛装金属的容器隔离了与筑炉材料的接触,且上面铺设了一层耐高温液流冲刷的钨板或钼板,因而隔离了非稀土元素对电解出的金属液体的污染,提高了坩埚使用寿命。

Claims (3)

1.一种万安培稀土熔盐电解槽坩埚,包括容器体,其特征在于:所述容器体内壁及底面铺设一层耐高温液流冲刷的金属层。
2.根据权利要求1所述的一种万安培稀土熔盐电解槽坩埚,其特征在于:所述金属层为钨板层。
3.根据权利要求1所述的一种万安培稀土熔盐电解槽坩埚,其特征在于:所述金属层为钼板层。
CN2012200941162U 2012-03-14 2012-03-14 万安培稀土熔盐电解槽坩埚 Expired - Fee Related CN202465907U (zh)