CN202463004U - Kneading roll and embossed moist towelette manufactured by using same - Google Patents

Kneading roll and embossed moist towelette manufactured by using same Download PDF

Info

Publication number
CN202463004U
CN202463004U CN2012200817216U CN201220081721U CN202463004U CN 202463004 U CN202463004 U CN 202463004U CN 2012200817216 U CN2012200817216 U CN 2012200817216U CN 201220081721 U CN201220081721 U CN 201220081721U CN 202463004 U CN202463004 U CN 202463004U
Authority
CN
China
Prior art keywords
embossing
roller
rubbing roller
towel
wet
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn - After Issue
Application number
CN2012200817216U
Other languages
Chinese (zh)
Inventor
何林燕
陈善樑
俞慧丽
张东丽
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Gold HongYe Paper Group Co Ltd
Original Assignee
Gold HongYe Paper Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Gold HongYe Paper Group Co Ltd filed Critical Gold HongYe Paper Group Co Ltd
Priority to CN2012200817216U priority Critical patent/CN202463004U/en
Application granted granted Critical
Publication of CN202463004U publication Critical patent/CN202463004U/en
Anticipated expiration legal-status Critical
Withdrawn - After Issue legal-status Critical Current

Abstract

A kneading roll comprises an upper kneading roll and a lower kneading roll. A plurality of bumps are arranged on the upper kneading roll, a plurality of grooves are formed on the lower kneading roll, the bumps of the upper kneading roll are matched with the grooves of the lower kneading roll so that the bumps extend into the grooves, the distance between two center points of each two adjacent bumps is 5-10mm, the areas of transverse sections of the bumps are gradually reduced in a direction from a position close to the center of the upper kneading roll to a position far away from the center of the upper kneading roll, the longitudinal section of each bump is trapezoidal, each bump is provided with a top end surface, the area of each top end surface is 1-20mm<2>, and the height of each bump is 0.05-5mm. The utility model also provides embossed moist towelette manufactured by using the kneading roll.

Description

Crumple roller and use the wet towel of embossing that this rubbing roller makes
Technical field
The utility model relates to a kind ofly to be crumpled roller and uses the wet towel of embossing that this rubbing roller makes.
Background technology
The base material of wet towel is nonwoven mostly on the market at present.Nonwoven is claimed non-weaving cloth again; Be meant without traditional spinning; Woven or knitting made cloth, it generally is to become net through means such as air-flow or machineries after utilizing carding machine that the fibrous raw material combing is the single fiber state, the modes such as water thorn, acupuncture or hot rolling of passing through then are fixed; The cloth of the last nothing braiding that forms through arrangement later is the tencel goods of a kind of ventilative, light weight and environmental protection.
Yet; In actual production process; The fibrous raw material that is carded to single fiber through carding machine is in the lapping process, and the influence owing to the reasons such as size, kind and antistatic property of lapping mode and fiber itself can reassemble into fibre bundle or fiber block between the fiber; These highdensity fiber blocks and fibre bundle cause the pliability of wet towel relatively poor, during wiping and the sense of touch of skin not good.Though existing jacquard non-woven fabrics can improve the outward appearance and the wiping efficient of nonwoven, the complex manufacturing of jacquard non-woven fabrics, price are high, and its outward appearance with the raising of wiping efficient the time to the pliability of jacquard non-woven fabrics and contain fluid power power negative effect is all arranged.
In addition; Because the fiber in the nonwoven has certain orientation; Usually differentiate anti-the tear performance of nonwoven product on all directions with vertical (MD) and horizontal (CD) powerful ratio of fiber; The ratio of MD/CD is more little, and it is more little that anti-on all directions that the nonwoven product is described tears performance difference.And in existing non-woven fabrics craft; In the fleece behind carding; Fiber is most can arrange along vertical (being the MD direction), and the fiber of on horizontal (CD direction) direction, arranging is less relatively, thereby causes the ratio of MD/CD big (promptly; Vertical transverse strength is bigger), make the nonwoven product to tear performance difference vertically and transversely anti-bigger.
The utility model content
In view of this, a kind of rubbing roller that can make wet towel have good appearance, highly-flexible degree and high wiping efficient is provided.
In addition, also be necessary to provide a kind of wet towel of embossing that above-mentioned rubbing roller makes of using.
A kind of rubbing roller; Comprise rubbing roller and following rubbing roller, on crumple roller and have a plurality of convexities, following rubbing roller has a plurality of grooves; And the convexity of last rubbing roller is mated so that convexity stretches in the groove with the groove of crumpling roller down; Spacing between adjacent two protruding two central points is 5-10mm, and the area in the cross section that each is protruding is from reducing near the direction of mind-set the last rubbing roller away from said center gradually, and each protruding vertical section is trapezoidal; Each convexity has a top end face, the area 1-20mm of this top end face 2, each protruding height is 0.05-5mm.
The density of crumpling the convexity on the roller preferably, is 1-30/cm 2
The density of crumpling the convexity on the roller preferably, is 3-10/cm 2
Preferably, when this top end face was circle, its diameter was 1-5mm.
Preferably, the spacing between the two adjacent grooves is identical with spacing between adjacent two convexities, the opening of each groove near crumple down roller mind-set increase gradually away from the direction at said center, the vertical section of this groove is trapezoidal.
Preferably, said each groove has a bottom face, and the area of this bottom face is 1-50mm 2
Preferably, when this bottom face was circle, its diameter was 1-8mm.
Preferably, when the vertical section of convexity or groove was isosceles trapezoid, the angle between trapezoidal two waists of these isosceles was 35-85o.
Preferably, the long-pending 30%-70% that accounts for the total surface area of rubbing roller of said a plurality of raised surface.
A kind ofly use the wet towel of embossing that above-mentioned rubbing roller makes; The wet towel surface of this embossing is formed with a plurality of embossing salient points and a plurality of recess; Spacing between two central points of two adjacent salient points is 5-10mm; The vertical section of each embossing salient point is trapezoidal, and the area in the cross section of each embossing salient point is from reduce near the direction of mind-set the wet towel of embossing away from said center gradually; Each embossing salient point has an end face, and the area of this end face is 1-20mm 2The height of this embossing salient point is 0.05-5mm.
Preferably, the density of said embossing salient point is 1-30/cm 2
Preferably, when the vertical section of embossing salient point was isosceles trapezoid, the angle between trapezoidal two waists of these isosceles was 35-85o.
Preferably, the aspect intensity ratio of the wet towel of this embossing is 0.8-10.
Preferably, the surface area of said a plurality of embossing salient points accounts for the 30%-70% of the total surface area of the wet towel of this embossing.
Preferably, be nonwoven in order to the base material that forms the wet towel of this embossing.
Compare prior art; The utility model rubbing roller is at last rubbing roller and following convexity and the groove that designs specific dimensions on the roller respectively of crumpling; Following advantage is arranged: (1) is used this and is rubbed roller; Can effectively reduce fiber block and fibre bundle on the nonwoven, improve the fiber uniformity and the bulk of the wet towel of this embossing; (2) use this and rub roller; Fiber in this nonwoven is turned to towards the CD direction; Thereby increase the arrange quantity of the fiber of the wet towel of this embossing in the CD direction; Effectively reduce the aspect intensity ratio of this nonwoven, reduced anti-the tear performance difference of the wet towel of made embossing in all directions; (3) make the fiber of this nonwoven occur bending and deformation, form predetermined floral designs thereby make on the wet towel of the embossing that makes according to predetermined design.
Description of drawings
Fig. 1 is the sketch map of the rubbing roller of the utility model one preferred embodiment;
Fig. 2 is the partial cutaway schematic of the rubbing roller of the utility model one preferred embodiment;
Fig. 3 is the sketch map of the wet towel of embossing of the utility model one preferred embodiment;
Fig. 4 is the sketch map of the wet towel of embossing of another preferred embodiment of the utility model;
Fig. 5 is the sketch map of the wet towel of embossing of another preferred embodiment of the utility model;
Fig. 6 is the profile of the embossing salient point of the wet towel of embossing shown in Figure 3.
The main element symbol description
The rubbing roller 100
Last rubbing roller 10
Under crumple roller 20
Protruding 11
Groove 21
Top end face 111
Bottom face 211
Nonwoven 30
The embossing towel that wets 200,200a,200b
The embossing salient point 210
End face 220
Recess 230
The following specific embodiment will combine above-mentioned accompanying drawing to further specify the utility model.
The specific embodiment
Please consult Fig. 1 and Fig. 2 in the lump, the rubbing roller 100 of the utility model comprises going up rubbing roller 10 and crumpling roller 20 down of coupling setting.Should go up rubbing roller 10 and all be cylindrical tube shape with following rubbing roller 20.Last rubbing roller 10 has outward extending a plurality of protruding 11; Crumple roller 20 down and have a plurality of grooves 21 that are arranged with inwardly; And the convexity 11 of last rubbing roller 10 is provided with for mating one to one with the groove 21 of crumpling roller 20 down; When last rubbing roller 10 when rubbing roller 20 rotates each other down, on crumple roller 10 convexity 11 stretch into down in the groove 21 of crumpling roller 20.Said go up rubbing roller 10 and down rubbing roller 20 be steel rider, one of maybe should go up in rubbing roller 10 and the rubbing roller 20 down is the wool roller, another is a steel rider.
A plurality of protruding 11 pattern effects of last rubbing roller 10 according to certain arrangement mode formation needs.Each cross section of protruding 11 can be regular shapes such as circle, ellipse, square and rectangle, can be also that other are irregularly shaped.The area in each cross section of protruding 11 is from reduce near the direction of mind-set the last rubbing roller 10 away from said center gradually.Each top end face 111 of protruding 11 can be regular shapes such as circle, ellipse, square and rectangle, can be also that other are irregularly shaped.Be illustrated in figure 2 as protruding 11 profilograph, the area 1-20mm of this top end face 2When this top end face 111 was circle, its diameter D1 was 1-5mm.The height H 1 of this convexity 11 is 0.05-5mm.Each vertical section of protruding 11 is trapezoidal.When protruding 11 vertical section was isosceles trapezoid, the angle C1 between trapezoidal two waists of these isosceles was 35-85o.Spacing between every adjacent two protruding 11 can equate also can not wait, and the spacing that goes up between two protruding 11 adjacent two central points of rubbing roller 10 is 5-10mm.Said protruding 11 is 1-30/cm in last rubbing roller 10 distribution densities 2, be preferably 3-10/cm 2Said a plurality of surface area of protruding 11 accounts for the 30%-70% of the total surface area of rubbing roller 10, is preferably 50%; So, can improve the wiping effect of the wet towel of embossing that adopts these rubbing roller 100 preparations.
Mostly be long fibre, the equal 5mm of this long stapled average length owing to be used to prepare the discontinuous long fibre that nonwoven adopts; Keeping the said spacing that goes up between two protruding 11 adjacent two central points of rubbing roller 10 is 5-10mm; Can guarantee that the contact point between every long fibre, the long fibre can be crumpled and make the part fiber to turn to uniformly, improve the fibroreticulate uniformity and the bulk of the wet towel of embossing.
A plurality of protruding 11 the arrangement mode of arrangement mode and last rubbing roller 10 of a plurality of grooves 21 of crumpling roller 20 down is corresponding, and is corresponding one by one with convexity 11 to guarantee groove 21.Promptly the spacing between the two adjacent grooves 21 is identical with spacing between the two adjacent convexities 11; The distribution density of groove 21 is identical with the distribution density of convexity 11.The cross section of said groove 21 is identical with protruding 11 cross section shape, and the cross section of said groove 21 can be regular shapes such as circle, ellipse, square and rectangle, can be also that other are irregularly shaped.The opening of each groove 21 near crumple down roller 20 mind-set increase gradually away from the direction at said center.Each groove 21 has a bottom face 211.This bottom face 211 demonstrates the shape identical with top end face 111, and this bottom face 211 can be regular shapes such as circle, ellipse, square and rectangle, can be also that other are irregularly shaped.The area 1-50mm of this bottom face 2When this bottom face 211 was circle, its diameter D2 was 1-8mm.The depth H 2 of this groove 21 equates with the height H 1 of convexity 11, and the depth H 2 of groove 21 is 0.05-5mm.The vertical section of groove 21 forms trapezoidal.When this vertical section was isosceles trapezoid, the angle C2 between trapezoidal two waists of these isosceles equated with angle C1, and angle C2 is 35-85o.
Please further consult Fig. 2; A kind of embossed technology; Use above-mentioned rubbing roller 100; The required rubbing roller 10 and the gap of rubbing roller 20 down of going up is set, with nonwoven 30 send into rubbing roller 10 and down between the rubbing roller 20 and make nonwoven 30 with certain speed through rubbing roller 100, make nonwoven 30 in groove 21 and protruding 11 extruding generation plastic deformation and appear and crumple the identical ridge design of roller 100 roll surfaces down.Said nonwoven 30 can be the nonwoven of spunlace non-woven cloth, dustless nonwoven, hot-wind nonwoven cloth, needle punched non-woven fabrics or other kinds.
Before embossing was handled, said nonwoven 30 was pre-soaked and/or apply suitable composition, and said composition can be oil-in-water (O/W) the type emulsion that water-based is dissolved.The main component of said composition comprises surfactant, skin conditioner, also can add an amount of anticorrisive agent, pH conditioning agent and essence as required.Wherein, the quality percentage composition of surfactant is 0.1-20.0%; The quality percentage composition of skin conditioner is 0.1-10.0%.The shared mass ratio of oiliness composition is 0.01%-5% in the said composition.
Said surfactant is mainly used in solubilising, emulsification and strengthens the clean-up performance of emulsion.This surfactant main component is emulsifying agent and cleaning additive, and this emulsifying agent can be ionic emulsifying agent or nonionic emulsifier.The hydrophilic lipophilic balance of nonionic emulsifier (being the HLB value) is between 5-18.
This emulsifying agent can be polyethylene glycol series, sapn series, tween is serial, rilanit special is serial or fatty glyceride is serial emulsifying agent, specifically can be emulsifying agents such as span-40 type emulsifying agent, PEG-7 rilanit special, PEG-40 rilanit special, tween-20 type emulsifying agent, tween-80 type emulsifying agent, tristerin, monoolein or lauric acid amide of ethanol.
Said cleaning additive can be betaines (like Cocoamidopropyl betaine; Octyl group/decyl amido propyl betaine; Ricinoleic acid amide CAB etc.); Both sexes acetate salt is (like cocounut oil both sexes sodium acetate; Cocounut oil both sexes diacetic acid disodium); Propionate compound (like cocounut oil both sexes sodium propionate etc.); The sulfosuccinic acid salt is (like polyethylene glycol-5 lauryl citric acid disodium sulfosuccinate; The lauryl alcohol disodium sulfosuccinate; Ricinoleic acid amide MEA disodium sulfosuccinate; Lauryl disodium sulfosuccinate etc.) and cleaning additive such as APG class.
Said skin conditioner has cleaning efficacy, or also can have effects such as moist, anti-irritated, anti-tight, Sage Extract or the obstruction of mediation pore.This skin conditioner can be natural or synthetic skin conditioners such as alcohols skin conditioner, ester class skin conditioner, oils skin conditioner, macromolecule skin conditioner or other complementary skin conditioner.This alcohols skin conditioner can comprise at least a in the alcohols materials such as propane diols, pentanediol and hexadecanol; Ester class skin conditioner can comprise at least a in carbonic acid dioctyl ester, caprylic/capric triglyceride, isobutyl palmitate, isopropyl myristate (IPM) and the isopropyl palmitate Esters such as (IPP); The oils skin conditioner can comprise olive oil, lanolin and have at least a in the vegetable oil of cleaning, the Sage Extract effect oily substances such as (smart like lavender oil, jojoba oil, tea oil, lemon, fish pelargonium essential oil and cypress); The macromolecule skin conditioner can comprise hyaluronic acid and/or collagen; Other complementary skin conditioner can comprise at least a in anti-inflammation agent, NMF and other skin-care effect auxiliary agents.This anti-inflammation agent can be bisabolol, witch hazel extract and chamomile extract etc.This NMF can be the aloe NMF.
Please consult Fig. 3 and Fig. 6 in the lump; A kind of by the wet towel 200 of the prepared embossing of above-mentioned embossed technology; The wet towel 200 of this embossing has upper surface and the lower surface that is oppositely arranged, and is formed with a plurality of embossing salient points 210 and recess 230 on the upper surface, and lower surface is formed with the embossing concave point corresponding with embossing salient point 210.The pattern effect that said a plurality of embossing salient point 210 needs according to certain arrangement mode formation.Spacing between the two whenever adjacent embossing salient points 210 can equate also can not wait, and the spacing between two central points of two adjacent embossing salient points 210 is 5-10mm.The distribution density of this embossing salient point 210 on the wet towel 200 of embossing is 1-30/cm 2, be preferably 3-10/cm 2The surface area of said a plurality of embossing salient points 210 accounts for the 30%-70% of the total surface area of the wet towel 200 of this embossing, is preferably 50%; So can improve the wiping intensity of the wet towel 200 of embossing and retain the ability of dirt, thereby improve wiping efficient.
The cross section of each embossing salient point 210 is circular, and the area in the cross section of each embossing salient point 210 is from reduce near the direction of mind-set the wet towel 200 of embossing away from said center gradually.Each embossing salient point 210 has an end face 220, and this end face 220 is circular, and the area of this end face 220 is 1-20mm 2, its diameter D3 is 1-5mm.The height H 3 of this embossing salient point 210 is 0.05-5mm.The vertical section of each embossing salient point 210 is trapezoidal, and when this vertical section was isosceles trapezoid, the angle C3 between trapezoidal two waists of these isosceles equated with angle C1, C2, and angle C3 is 35-85o.
The wet towel 200 of this embossing contains oil-in-water (O/W) the type emulsion compositions that water-based is dissolved.The main component of said composition comprises surfactant, skin conditioner, also can add an amount of anticorrisive agent, pH conditioning agent and essence as required.Wherein, the quality percentage composition of surfactant is 0.1-20.0%; The quality percentage composition of skin conditioner is 0.1-10.0%.The shared mass ratio of oiliness composition is 0.01%-5% in the said composition.
Said surfactant is mainly used in solubilising, emulsification and strengthens the clean-up performance of emulsion.This surfactant main component is emulsifying agent and cleaning additive, and this emulsifying agent can be ionic emulsifying agent or nonionic emulsifier.The HLB value of nonionic emulsifier is between 5-18.
This emulsifying agent can be polyethylene glycol series, sapn series, tween is serial, rilanit special is serial or fatty glyceride is serial emulsifying agent, specifically can be emulsifying agents such as span-40 type emulsifying agent, PEG-7 rilanit special, PEG-40 rilanit special, tween-20 type emulsifying agent, tween-80 type emulsifying agent, tristerin, monoolein or lauric acid amide of ethanol.
Said cleaning additive can be betaines (like Cocoamidopropyl betaine; Octyl group/decyl amido propyl betaine; Ricinoleic acid amide CAB etc.); Both sexes acetate salt is (like cocounut oil both sexes sodium acetate; Cocounut oil both sexes diacetic acid disodium); Propionate compound (like cocounut oil both sexes sodium propionate etc.); The sulfosuccinic acid salt is (like polyethylene glycol-5 lauryl citric acid disodium sulfosuccinate; The lauryl alcohol disodium sulfosuccinate; Ricinoleic acid amide MEA disodium sulfosuccinate; Lauryl disodium sulfosuccinate etc.) and cleaning additive such as APG class.
Said skin conditioner has cleaning efficacy, or also can have at least a in the effects such as moist, anti-irritated, anti-tight, Sage Extract and the obstruction of mediation pore.This skin conditioner can be natural or synthetic skin conditioners such as alcohols skin conditioner, ester class skin conditioner, oils skin conditioner, macromolecule skin conditioner or other complementary skin conditioner.This alcohols skin conditioner can comprise at least a in the alcohols materials such as propane diols, pentanediol and hexadecanol; Ester class skin conditioner can comprise at least a in carbonic acid dioctyl ester, caprylic/capric triglyceride, isobutyl palmitate, isopropyl myristate (IPM) and the isopropyl palmitate Esters such as (IPP); The oils skin conditioner can comprise olive oil, lanolin and have at least a in the vegetable oil of cleaning, the Sage Extract effect oily substances such as (smart like lavender oil, jojoba oil, tea oil, lemon, fish pelargonium essential oil and cypress); The macromolecule skin conditioner can comprise hyaluronic acid and/or collagen; Other complementary skin conditioner can comprise at least a in anti-inflammation agent, NMF and other skin-care effect auxiliary agents.This anti-inflammation agent can be bisabolol, witch hazel extract and chamomile extract etc.This NMF can be the aloe NMF.
The humidity of the wet towel 200 of the embossing that makes through said method is 20%-90%, and its aspect intensity ratio is 0.8-10.The embossing salient point 210 of the wet towel 200 of this embossing is basic identical with the fibre density of recess 230.
In conjunction with consulting Fig. 4, the embossing of another preferred embodiment of the utility model towel 200a that wets, the cross section and the end face of different with the wet towel of embossing 200 is each embossing salient point 210 of the wet towel 200a of this embossing are square.
In conjunction with consulting Fig. 5, the embossing of another preferred embodiment of the utility model towel 200b that wets, the cross section and the end face of different with the wet towel of embossing 200 is each embossing salient point 210 of the wet towel 200b of this embossing are rectangle.
Understandable, cross section, the end face of the embossing salient point 210 of the wet towel 200 of said embossing also can be ellipse, other regular shapes or irregularly shaped.
Understandable; Because the wet towel 200 of embossing itself is a kind ofly to have certain flexible material, so the embossing salient point 210 that after embossing, produces has the bounce that part is recovered original shape, a spot of recovery deformation will take place; The sharp keen corner angle of embossing salient point 210 can flatten, and become slick and sly.
Compare prior art; The utility model rubbing roller 100 is in last rubbing roller 10 and the following convexity 11 and groove 21 that designs specific dimensions on the roller 20 respectively of crumpling; Following advantage is arranged: (1) is used this and is rubbed roller 100; Can effectively reduce fiber block and fibre bundle on this nonwoven 30, improve the fiber uniformity and the bulk of the wet towel 200 of this embossing; (2) use this and rub roller 100; Fiber in this nonwoven 30 is turned to towards the CD direction; Thereby increase fiber in this nonwoven 30 in the quantity of arranging of CD direction; Effectively reduce the aspect intensity ratio of the wet towel 200 of this embossing, reduced anti-the tear performance difference of the wet towel 200 of made embossing in all directions; (3) make the fiber of this nonwoven 30 occur bending and deformation, thereby form predetermined floral designs at the wet towel 200 of the embossing that makes according to predetermined design.(4) make the surface area of embossing salient point 210 on the wet towel 200 of the embossing that makes account for the 30%-70% of the total surface area of the wet towel 200 of this embossing; Can guarantee that the wet towel 200 of this embossing has enough wiping areas; Guarantee that simultaneously said recess 230 can provide enough volume in order to retain the dirt of emulsion and dissolving; Avoid fouling products to be back to wipe surfaces again, thereby improve the wiped clean performance of the wet towel 200 of embossing.
See also following table; Be to adopt the resulting elementary nonwoven sample 1 of cross lapping mode and sample 2, the employing resulting elementary nonwoven sample 3 of parallel laid net mode and sample 4 passing through the above-mentioned situation of change that roller 100 is rubbed the rerum natura of front and back of rubbing; Wherein, To be elementary nonwoven rubbed before adding wet process the physical data of sample 1 and sample 3 that to handle the back measured, and the physical data of sample 2 and sample 4 is that elementary nonwoven is rubbed after handling measured adding wet process after.
By the data in the last table, can find out obviously that through all increases to some extent of thickness of elementary nonwoven sample 1, sample 2, sample 3 and sample 4 after rubbing, MD/CD ratio all decreases.Experimental verification through is repeatedly learnt; Aspect thickness; The scope that nonwoven thickness after rubbing increases on original basis is between 1% ~ 30%, and aspect MD/CD ratio, the scope that the nonwoven MD/CD ratio after rubbing reduces on original basis is between 1% ~ 25%.
In addition, those skilled in the art also can make various modifications, interpolation and the replacement on other form and the details in the utility model claim scope of disclosure and spirit.Certainly, these all should be included within the utility model scope required for protection according to the variations such as various modifications, interpolation and replacement that the utility model spirit is made.

Claims (15)

1. crumple roller for one kind; Comprise rubbing roller and following rubbing roller, on crumple roller and have a plurality of convexities, following rubbing roller has a plurality of grooves; And the convexity of last rubbing roller is mated so that convexity stretches in the groove with the groove of crumpling roller down; It is characterized in that: the spacing between adjacent two protruding two central points is 5-10mm, and the area in the cross section that each is protruding is from reducing near the direction of mind-set the last rubbing roller away from said center gradually, and each protruding vertical section is trapezoidal; Each convexity has a top end face, the area 1-20mm of this top end face 2, each protruding height is 0.05-5mm.
2. rubbing roller as claimed in claim 1 is characterized in that: on crumple the convexity on the roller density be 1-30/cm 2
3. rubbing roller as claimed in claim 1 is characterized in that: on crumple the convexity on the roller density be 3-10/cm 2
4. rubbing roller as claimed in claim 1 is characterized in that: when this top end face was circle, its diameter was 1-5mm.
5. rubbing roller as claimed in claim 1; It is characterized in that: the spacing between the two adjacent grooves is identical with spacing between adjacent two convexities; The opening of each groove near crumple down roller mind-set increase gradually away from the direction at said center, the vertical section of this groove is trapezoidal.
6. like claim 1 or 5 described rubbing rollers, it is characterized in that: said each groove has a bottom face, and the area of this bottom face is 1-50mm 2
7. rubbing roller as claimed in claim 6 is characterized in that: when this bottom face was circle, its diameter was 1-8mm.
8. rubbing roller as claimed in claim 1 is characterized in that: when the vertical section of convexity or groove was isosceles trapezoid, the angle between trapezoidal two waists of these isosceles was 35-85o.
9. rubbing roller as claimed in claim 1 is characterized in that: the long-pending 30%-70% that accounts for the total surface area of rubbing roller of said a plurality of raised surface.
10. one kind is used the wet towel of embossing that any described rubbing roller makes in the claim 1-9 item; The wet towel surface of this embossing is formed with a plurality of embossing salient points and a plurality of recess; It is characterized in that: the spacing between two central points of two adjacent salient points is 5-10mm; The vertical section of each embossing salient point is trapezoidal, and the area in the cross section of each embossing salient point is from reduce near the direction of mind-set the wet towel of embossing away from said center gradually; Each embossing salient point has an end face, and the area of this end face is 1-20mm 2The height of this embossing salient point is 0.05-5mm.
The towel 11. embossing as claimed in claim 10 is wet is characterized in that: the density of said embossing salient point is 1-30/cm 2
The towel 12. embossing as claimed in claim 10 is wet is characterized in that: when the vertical section of embossing salient point was isosceles trapezoid, the angle between trapezoidal two waists of these isosceles was 35-85o.
The towel 13. embossing as claimed in claim 10 is wet is characterized in that: the aspect intensity ratio of the wet towel of this embossing is 0.8-10.
The towel 14. embossing as claimed in claim 10 is wet is characterized in that: the surface area of said a plurality of embossing salient points accounts for the 30%-70% of the total surface area of the wet towel of this embossing.
The towel 15. embossing as claimed in claim 10 is wet is characterized in that: the base material in order to form the wet towel of this embossing is a nonwoven.
CN2012200817216U 2012-03-07 2012-03-07 Kneading roll and embossed moist towelette manufactured by using same Withdrawn - After Issue CN202463004U (en)