CN202443772U - 一种杜美丝线材 - Google Patents
一种杜美丝线材 Download PDFInfo
- Publication number
- CN202443772U CN202443772U CN2011204574670U CN201120457467U CN202443772U CN 202443772 U CN202443772 U CN 202443772U CN 2011204574670 U CN2011204574670 U CN 2011204574670U CN 201120457467 U CN201120457467 U CN 201120457467U CN 202443772 U CN202443772 U CN 202443772U
- Authority
- CN
- China
- Prior art keywords
- copper layer
- cuprous oxide
- dumet wire
- oxide film
- utility
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种杜美丝线材,包括芯棒(1)和包覆铜层(2),所述包覆铜层(2)包覆芯材(1),包覆铜层(2)外有一层氧化亚铜膜(3),所述芯棒(1)为含有锰、硅、硫和碳元素的铁镍合金;所述氧化亚铜膜(2)外涂有一层硼酸盐(4)。本实用新型具有调整膨胀系数的优点,且不易漏气。
Description
技术领域
本实用新型涉及封装技术领域,尤其是涉及一种杜美丝线材。
背景技术
杜美丝线材是半导体器件、真空电子器件(如电子管、显像管)和电光源灯丝引出线的材料,由于它在使用时位于半导体器件、真空电子器件和电光源的封接部位,这就要求它的膨胀系数与上述封接部位的软玻璃大体一致,否则就会造成封接部位漏气或炸裂。而杜美丝与软玻璃封接后的急冷应力易使氧化亚铜-铜界面分离等因素会导致慢性漏气,因此需要在氧化亚铜层上增设一层使氧化亚铜对急冷应力不敏感的物质。
实用新型内容
本实用新型是为了解决目前杜美丝线材易慢性漏气,膨胀系数和软玻璃不一致的问题,为此提供了一种杜美丝线材,包括芯棒1和包覆铜层2,所述包覆铜层2包覆芯材1,包覆铜层2外有一层氧化亚铜膜3,所述氧化亚铜膜2外涂有一层硼酸盐4。
本实用新型杜美丝线材,所述铁镍合金的芯棒1,化学成分:Si≤0.3%、S≤0.02%、C≤0.05%、Mn:0.7-1.2%、Ni:41-43%,余量为铁。
本实用新型杜美丝线材,
本实用新型的有益效果是:
由于芯棒材质为含有锰、硅、硫、磷和碳元素的铁镍合金,具有便于调整径向和轴向膨胀系数的优点;而在氧化亚铜上涂有的四硼酸钠,减少了杜美丝与软玻璃封接后的急冷应力使氧化亚铜-铜界面分离导致的慢性漏气。
附图说明
本实用新型将通过例子并参照附图的方式说明,其中:
图1是本实用新型示意图。
具体实施方式
本说明书中公开的所有特征,或公开的所有方法或过程中的步骤,除了互相排斥的特征和/或步骤以外,均可以以任何方式组合。
本说明书(包括任何附加权利要求、摘要和附图)中公开的任一特征,除非特别叙述,均可被其他等效或具有类似目的的替代特征加以替换。即,除非特别叙述,每个特征只是一系列等效或类似特征中的一个例子而已。
如图1所示的杜美丝线材,包括芯棒1和包覆铜层2,所述包覆铜层2包覆芯材1,包覆铜层2外有一层氧化亚铜膜3,所述芯棒1为含有锰、硅、硫和碳元素的铁镍合金,所述铁镍合金的芯棒1,具有便于调整径向和轴向膨胀系数的优点;所述氧化亚铜膜2外涂有一层硼酸盐4,所述硼酸盐4为四硼酸钠,减少了杜美丝与软玻璃封接后的急冷应力使氧化亚铜-铜界面分离导致的慢性漏气。
本实用新型并不局限于前述的具体实施方式。本实用新型扩展到任何在本说明书中披露的新特征或任何新的组合,以及披露的任一新的方法或过程的步骤或任何新的组合。
Claims (2)
1.一种杜美丝线材,包括芯棒(1)和包覆铜层(2),所述包覆铜层(2)包覆芯材(1),包覆铜层(2)外有一层氧化亚铜膜(3),其特征是:所述氧化亚铜膜(2)外涂有一层硼酸盐(4)。
2.根据权利要求1所述的杜美丝线材,其特征是:所述硼酸盐(4)为四硼酸钠。