CN202242271U - 无版缝版辊 - Google Patents
无版缝版辊 Download PDFInfo
- Publication number
- CN202242271U CN202242271U CN201120297659XU CN201120297659U CN202242271U CN 202242271 U CN202242271 U CN 202242271U CN 201120297659X U CN201120297659X U CN 201120297659XU CN 201120297659 U CN201120297659 U CN 201120297659U CN 202242271 U CN202242271 U CN 202242271U
- Authority
- CN
- China
- Prior art keywords
- groove
- metal tube
- heat carrier
- plate
- roller
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
本实用新型提供一种无版缝版辊,属于印刷机械领域,包括一根金属管,所述金属管管壁内设有电加热装置;所述金属管外表面沿轴向开设一道凹槽,该凹槽内由非导热体填充,且所述非导热体的外表面与所述金属管的外表面形成完整的光滑圆柱面。该版辊在压印镭射膜时,可使激光图文压印至镭射基材,并使镭射膜表面不留版缝。
Description
所属技术领域
本实用新型涉及印刷机械行业领域,特别地,一种用于压印镭射膜的版辊。
背景技术
在印刷行业中,经常需要印刷一种表面具有镭射效果的印刷品,在生产该种印刷品时,需要使用到一种镭射膜,因此,首先需要印制镭射膜。在镭射膜的印制过程中,需要使用版辊,版辊上卷有一层模压工作版,且版辊上具有加热装置,当版辊表面温度达到工作温度时,使模压工作版压向压辊上的镭射膜基材,即可获得镭射膜。然而,由于工作版是包卷在版辊上的,因此工作版在版辊上将形成一道接缝,在压印过程中,若不采取措施,该拼缝将在镭射膜上留下一道痕迹,亦即版缝,这将对镭射膜的外观效果造成严重破坏,导致镭射膜报废。鉴于该问题,目前普遍采用的方案是,使版缝压印于镭射膜表面的各光柱中央,使光柱的强光掩盖住版缝,但即便如此,在仔细辨别之时,仍能看出版缝痕迹,因此采用目前的版辊进行镭射膜压印,其压印效果十分有限。
实用新型内容
为了解决上述问题,本实用新型的目的在于提供一种无版缝版辊,该版辊在压印镭射膜时,可使激光图文压印至镭射基材,并使镭射膜表面不留版缝。
本实用新型解决其技术问题所采用的技术方案是:该无版缝版辊包括一根金属管,所述金属管管壁内设有电加热装置;所述金属管外表面沿轴向开设一道凹槽,该凹槽内由非导热体填充,且所述非导热体的外表面与所述金属管的外表面形成完整的光滑圆柱面。
作为优选,所述电加热装置为设于所述金属管管壁孔道内的电热管或电热丝。
作为优选,所述非导热体由绝热陶瓷体构成。
作为优选,所述凹槽的横截面呈外宽内窄的等腰梯形状,所述非导热体的横截面与所述凹槽相配合,从而使所述非导热体可以沿轴向塞入所述凹槽,在径向上被所述凹槽卡住,而无需使用胶体固定。
本实用新型的有益效果在于:该无版缝版辊在工作时,使模压工作版的接缝处于所述非导热体的中央,所述电加热装置给所述金属管加热,将使所述金属管的表面达到压印工作温度,一般在120℃以上,而所述非导热体由于不导热,故所述模压工作版接缝处温度较低,难以达到工作温度,因此在压印时,所述模压工作版包含激光图文信息的部分将压印至镭射基材,而接缝部分由于温度过低,无法压印至镭射基材,因此,镭射基材上只留下激光图文信息,而无版缝,具有优越的压印效果。
附图说明
图1是本无版缝版辊的横截面示意图。
图2是本无版缝版辊的前向示意图。
图3是本无版缝版辊包卷了模压工作版后的横截面示意图。
具体实施方式
下面结合附图和实施例对本实用新型进一步说明:
在图1-图3所示实施例中,该无版缝版辊包括一根金属管1,所述金属管1管壁内设有电加热装置2;所述金属管1外表面沿轴向开设一道凹槽,该凹槽内由非导热体11填充,且所述非导热体11的外表面与所述金属管1的外表面形成完整的光滑圆柱面。
上述的无版缝版辊,所述电加热装置2为设于所述金属管1管壁孔道内的电热管或电热丝,它们沿着所述金属管1管壁的周向均匀分布,在所述非导热体11正对的管壁处则不设置电加热装置2。
上述的无版缝版辊,所述非导热体11由绝热陶瓷体构成,不仅具有较高的耐热能力、较小的导热系数,且具有光滑表面。
上述的无版缝版辊,所述凹槽的横截面呈外宽内窄的等腰梯形状,所述非导热体11的横截面与所述凹槽相配合,从而使所述非导热体11可以沿轴向塞入所述凹槽,在径向上被所述凹槽卡住,而无需使用胶体固定。
上述无版缝版辊在工作时,如图3所示,使模压工作版3的接缝30处于所述非导热体11的中央,所述电加热装置2给所述金属管1加热,将使所述金属管1的表面达到压印工作温度,一般在120℃以上,而所述非导热体11由于不导热,故所述模压工作版3接缝30处温度较低,难以达到工作温度,因此在压印时,所述模压工作版3包含激光图文信息的部分将压印至镭射基材,而接缝30部分由于温度过低,无法压印至镭射基材,因此,镭射基材上只留下激光图文信息,而无版缝,具有优越的压印效果。
以上所述仅为本实用新型的较佳实施例,并不用以限制本实用新型,凡在本实用新型的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本实用新型的保护范围之内。
Claims (4)
1.一种无版缝版辊,包括一根金属管(1),所述金属管(1)管壁内设有电加热装置(2),其特征在于:所述金属管(1)外表面沿轴向开设一道凹槽,该凹槽内由非导热体(11)填充,且所述非导热体(11)的外表面与所述金属管(1)的外表面形成完整的光滑圆柱面。
2.根据权利要求1所述的无版缝版辊,其特征在于:所述电加热装置(2)为设于所述金属管(1)管壁孔道内的电热管或电热丝。
3.根据权利要求1所述的无版缝版辊,其特征在于:所述非导热体(11)由绝热陶瓷体构成。
4.根据权利要求1所述的无版缝版辊,其特征在于:所述凹槽的横截面呈外宽内窄的等腰梯形状,所述非导热体(11)的横截面与所述凹槽相配合。