CN202132652U - 牺牲套 - Google Patents
牺牲套 Download PDFInfo
- Publication number
- CN202132652U CN202132652U CN201120237397U CN201120237397U CN202132652U CN 202132652 U CN202132652 U CN 202132652U CN 201120237397 U CN201120237397 U CN 201120237397U CN 201120237397 U CN201120237397 U CN 201120237397U CN 202132652 U CN202132652 U CN 202132652U
- Authority
- CN
- China
- Prior art keywords
- layer
- cover
- sacrificial sleeve
- sleeve
- crosslinked polyethylene
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种穿越管防护件,尤其是一种牺牲套。本实用新型提供了一种便于穿越的牺牲套,包括呈两端开口套状的主体以及两个端部,至少一个端部处的壁厚逐渐减小形成倾斜端面。由于倾斜端面的存在,因此牺牲套的前端就形成一个锥面,在穿越的过程中,前端就形成过渡端部,在遇到阻挡时也能前进,牺牲套也不会由于端部被卡住而划破或脱落。通过增强纤维层的作用,可以极大的提高增强牺牲套的强度,其耐磨性和撕裂强度都大幅度的提高,因此在使用时不易损坏,能够更好的保护穿越管道。
Description
技术领域
本实用新型涉及一种穿越管防护件,尤其是一种牺牲套。
背景技术
输油,输气钢管道在铺设施工过程中,会遇到不能开挖施工的情况,比如建筑物下,河流,桥梁下等,这种情况就需要采取定向钻穿越的方式来施工。在定向钻穿越施工的过程中,会遇到较坚硬的岩层,砂土等,对钢管道接头防腐结构造成破坏,因此,目前普遍采用牺牲套,安装于主补口套拖行方向前端,以保护主补口套。而牺牲套的厚度一般都有3MM以上,这样就会和钢管主体防腐之间形成一个台阶,牺牲套在穿越过程中易被坚硬的岩层,砂土等划破或顶腹,起不到保护主补口套的目的。即便牺牲套不被破坏,其与主体防腐之间的台阶也会对穿越形成阻力,阻碍穿越的进行。
实用新型内容
本实用新型所要解决的技术问题是提供一种便于穿越的牺牲套。
本实用新型解决其技术问题所采用的牺牲套,包括呈两端开口套状的主体以及两个端部,至少一个端部处的壁厚逐渐减小形成倾斜端面。
进一步的是,形成倾斜端面的端部由环氧底漆制成。
进一步的是,主体由辐射交联聚乙烯层与增强纤维层组成,所述增强纤维层设置在辐射交联聚乙烯层之中。
进一步的是,增强纤维层为辐射交联聚乙烯丝与玻璃纤维的编织物。
进一步的是,主体还包括热熔胶层,所述热熔胶层复合在辐射交联聚乙烯层的内层。
本实用新型的有益效果是:由于倾斜端面的存在,因此牺牲套的前端就形成一个锥面,在穿越的过程中,前端就形成过渡端部,在遇到阻挡时也能前进,牺牲套也不会由于端部被卡住而划破或脱落。通过增强纤维层的作用,可以极大的提高增强牺牲套的强度,其耐磨性和撕裂强度都大幅度的提高,因此在使用时不易损坏,能够更好的保护穿越管道。增强纤维层可以由玻璃纤维与辐射交联聚乙烯纤丝编织而成,这样既保证了增强纤维层在受热时能够收缩,也保证了增强纤维层具有足够的强度。热熔胶层能够使得增强牺牲套更容易粘合在穿越管道上。
附图说明
图1是本实用新型的示意图;
图2是主体各层的示意图;
图中零部件、部位及编号:主体1、端部2、辐射交联聚乙烯层11、增强纤维层12、热熔胶层13。
具体实施方式
下面结合附图对本实用新型作进一步说明。
如图1所示,本实用新型包括呈两端开口套状的主体1以及两个端部2,至少一个端部2处的壁厚逐渐减小形成倾斜端面。主体1即呈圆柱形的套状,在储存运输时可以压平,在使用时与管道形状相匹配。在将本实用新型安装到穿越管时,首先通过加热使得主体1收缩到穿越管上,至少在用于穿越的一端部2设置倾斜端面,因此,此处的端部2就呈锥形,这样在穿越过程中,端部2就不易被阻挡物卡住,受到的阻力也就较小,牺牲套也不会因为被剥离而失效。这样就很好的保护的穿越管。
具体的,形成倾斜端面的端部2由环氧底漆制成。这样,牺牲套可以先收缩到穿越管上后,再在回拖端涂抹环氧底漆以形成具有倾斜端面的端部2。这样就方便加工牺牲套,在施工时也是分步骤,能够达到更好的工艺。
为了增加强度,如图2所示,主体1包括辐射交联聚乙烯层11和增强纤维层12,所述增强纤维层12设置在所述辐射交联聚乙烯层11中。增强纤维层12可以由一些高强度的纤维编织而成,例如尼龙、玻璃纤维等。将增强纤维层12设置在辐射交联聚乙烯层11中,就可以增强牺牲套的强度以及耐磨性,牺牲套通过热缩的工艺安装到穿越管上,在穿越的过程中,由于牺牲套的高强度保护,即可保护穿越管上的防腐处理不受到损坏。
为了使增强纤维层12具有一定的热收缩性,增强纤维层12为辐射交联聚乙烯丝与玻璃纤维的编织物。交联聚乙烯丝在受热时便可以收缩,而玻璃纤维具有较高的强度并且成本较低,因此,在进行热收缩工艺的过程中,增强纤维层12也可以适应性地热收缩,与交联聚乙烯层1密切贴合。
为了便于安装牺牲套,如图1、图2所示,还包括热熔胶层13,所述热熔胶层13复合在辐射交联聚乙烯层11的内层。辐射交联聚乙烯层11的内层即位于牺牲套内环的一面,在进行热收缩工艺时,热熔胶层13会熔化,从而使得牺牲套能够更好地粘接到穿越管上。
Claims (5)
1.牺牲套,包括呈两端开口套状的主体(1)以及两个端部(2),其特征在于:至少一个端部(2)处的壁厚逐渐减小形成倾斜端面。
2.如权利要求1所述的牺牲套,其特征在于:所述形成倾斜端面的端部(2)由环氧底漆制成。
3.如权利要求1所述的牺牲套,其特征在于:所述主体(1)包括辐射交联聚乙烯层(11)与增强纤维层(12),所述增强纤维层(12)设置在辐射交联聚乙烯层(11)之中。
4.如权利要求3所述的增强牺牲套,其特征在于:所述增强纤维层(12)为辐射交联聚乙烯丝与玻璃纤维的编织物。
5.如权利要求3或4所述的增强牺牲套,其特征在于:所述主体(1)还包括热熔胶层(13),所述热熔胶层(13)复合在辐射交联聚乙烯层(11)的内层。