CN202123749U - Light metal or light metal alloy material - Google Patents

Light metal or light metal alloy material Download PDF

Info

Publication number
CN202123749U
CN202123749U CN2011202371351U CN201120237135U CN202123749U CN 202123749 U CN202123749 U CN 202123749U CN 2011202371351 U CN2011202371351 U CN 2011202371351U CN 201120237135 U CN201120237135 U CN 201120237135U CN 202123749 U CN202123749 U CN 202123749U
Authority
CN
China
Prior art keywords
light metal
alloy material
metal alloy
plastic layer
ceramic membrane
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN2011202371351U
Other languages
Chinese (zh)
Inventor
高谊恬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kunshan Fengshi Electronic Appearance Technology Co., Ltd.
Original Assignee
KUNSHAN JINLI SURFACE MATERIALS APPLICATION TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by KUNSHAN JINLI SURFACE MATERIALS APPLICATION TECHNOLOGY Co Ltd filed Critical KUNSHAN JINLI SURFACE MATERIALS APPLICATION TECHNOLOGY Co Ltd
Priority to CN2011202371351U priority Critical patent/CN202123749U/en
Application granted granted Critical
Publication of CN202123749U publication Critical patent/CN202123749U/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

The utility model discloses a light metal or light metal alloy material. A micro-arc oxidation ceramic membrane is deposited on the surface of the light metal or light metal alloy material according to the design in an avoidance manner, and a plastic layer is arranged on the surface of the light metal or light metal alloy material except the micro-arc oxidization ceramic membrane. The ceramic membrane is arranged on a portion, needing the ceramic membrane, of the light metal or light metal alloy material, the plastic layer is further arranged on the other portion of the light metal or light metal alloy material, the ceramic membrane with the excellent performance is kept, furthermore, the material has various appearances and textures, simultaneously, the plastic layer further can increase the structural strength of the material, and the light metal or light metal alloy material is low in cost. A plastic metal adhesive layer further can be arranged between the plastic layer and the surface of the light metal or light metal alloy material so as to increase bonding strength of the plastic layer.

Description

Light metal or light metal alloy material
Technical field
The utility model relates to a kind of light metal or light metal alloy material, has particularly combined the light metal or the light metal alloy material of ceramic membrane and plastics, belongs to the material application.
Background technology
As everyone knows, before the material to light metal or light metal alloy carries out practical application, all can handle its surface.Common way is that the material of light metal or light metal alloy is formed a kind of ceramic membrane through the differential arc oxidization technique deposition, and this ceramic membrane has good hardness and wearability, can increase the service life of material; Simultaneously, ceramic membrane also has well and insulating properties.From these advantages, seldom there is substitute can substitute ceramic membrane.But the non-constant of the plasticity of ceramic membrane is difficult to form appearance tactile impression various, attractive in appearance in appearance.
The utility model content
The technical problem that the utility model will solve is: overcome the defective that exists in the prior art; Provide a kind of when keeping ceramic membrane; Various material appearance texture can be created, the structural strength of material can also be increased, and light metal with low cost or light metal alloy material.
In order to address the above problem, what the utility model adopted is contemplated that basically: utilize plastics and light metal or light metal alloy material fit.Because plastics can carry out complicated deformation processing, thereby can improve the aesthetic feeling of material; Simultaneously because cooperating of plastics and metal can improve the structural strength of material; And plastics itself also are good insulating materials.
Basically conceive based on this, the technical scheme that the utility model adopts is:
Light metal or light metal alloy material; Keep away the position at light metal or light metal alloy material surface according to design and deposit one deck ceramic coating formed by micro-arc oxidation, it is characterized in that: there is one deck plastic layer the position of avoiding ceramic coating formed by micro-arc oxidation at light metal or light metal alloy material surface.
As a kind of improvement, between plastic layer and light metal or light metal alloy material surface, also has one deck plastic-metal glue-line to this technical scheme.
Adopt technique scheme, the utility model has reached following beneficial effect with respect to prior art:
The position that applies ceramic membrane at light metal or light metal alloy material require applies ceramic membrane; These external other positions also are provided with plastic layer; Not only kept the ceramic membrane that excellent properties is arranged; Can also on material, create various appearance tactile impression, plastic layer can also increase the structural strength of material simultaneously, and with low cost; The plastic-metal glue-line that between plastic layer and light metal or light metal alloy material surface, is provided with can increase the bond strength of plastic layer.
Description of drawings
Fig. 1 is the structural representation of the utility model light metal or light metal alloy material first embodiment; Fig. 2 is the structural representation of the utility model light metal or light metal alloy material second embodiment.
The specific embodiment
Be example with light metal or light metal alloy board-like material below, the utility model done further explanation in conjunction with accompanying drawing.
What Fig. 1 showed is the structural representation of the utility model light metal or light metal alloy material first embodiment.As shown in the figure, light metal or light metal alloy material 1 are board-like material, have first surface 11 and with first surface 11 opposing second surface 12.Avoid the second surface 12 of light metal or light metal alloy material 1, on first surface 11, deposit layer of ceramic film 2; On light metal or light metal alloy material 1, avoid ceramic membrane 2, one deck plastic layer 3 is arranged on second surface 12.
The tabular light metal that forms thus or the first surface 11 of light metal alloy material have wearability good, and the ceramic membrane that insulating properties are high has the strong plastic layer of plastic performance at second surface 12.Like this tabular light metal or light metal alloy material had both kept ceramic membrane, can also create various material appearance texture on its surface, and plastic layer can also increase the structural strength of material simultaneously.
What Fig. 2 showed is the structural representation of the utility model light metal or light metal alloy material second embodiment, and this embodiment is a kind of improvement to first embodiment.As shown in the figure, between the second surface 12 and plastic layer 3 of light metal or light metal alloy material 1, also have one deck plastic-metal glue-line 4.
Wherein, said plastic-metal glue-line 4 can be PUR, metal adhesive or other plastic-metal glue etc.
The shape of light metal or light metal alloy material does not become the restriction that the utility model is implemented, and except that board-like material, on the light metal of other shapes or light metal alloy material, can combine ceramic membrane and plastic layer simultaneously yet.
Combine the accompanying drawing and the specific embodiment that the utility model has been done detailed explanation above, but the utility model is not limited to this.The technical staff in any present technique field under the prerequisite of the utility model aim, can make various distortion and modification to the utility model in the ken that is possessed.

Claims (4)

1. light metal or light metal alloy material; Keep away the position at light metal or light metal alloy material surface according to design and deposit one deck ceramic coating formed by micro-arc oxidation, it is characterized in that: there is one deck plastic layer the position of avoiding ceramic coating formed by micro-arc oxidation at light metal or light metal alloy material surface.
2. light metal according to claim 1 or light metal alloy material is characterized in that: between plastic layer and light metal or light metal alloy material surface, also have one deck plastic-metal glue-line.
3. light metal according to claim 1 or light metal alloy material; It is characterized in that: said material is tabular; Board-like material has first and relative with it second, on first, deposits one deck ceramic coating formed by micro-arc oxidation, and one deck plastic layer is arranged on second.
4. light metal according to claim 3 or light metal alloy material is characterized in that: between second the plastic layer and light metal or light metal alloy material surface of board-like material, also have one deck plastic-metal glue-line.
CN2011202371351U 2011-07-07 2011-07-07 Light metal or light metal alloy material Expired - Lifetime CN202123749U (en)