CN202016236U - 等离子粉末堆焊大型金属陶瓷耐磨板 - Google Patents

等离子粉末堆焊大型金属陶瓷耐磨板 Download PDF

Info

Publication number
CN202016236U
CN202016236U CN2011200823138U CN201120082313U CN202016236U CN 202016236 U CN202016236 U CN 202016236U CN 2011200823138 U CN2011200823138 U CN 2011200823138U CN 201120082313 U CN201120082313 U CN 201120082313U CN 202016236 U CN202016236 U CN 202016236U
Authority
CN
China
Prior art keywords
metal ceramic
ceramic wear
resistant plate
size metal
steel plate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN2011200823138U
Other languages
English (en)
Inventor
钱兵
花荣春
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NANTONG GAOXIN WEARABLE TECHNOLOGY CO., LTD.
Original Assignee
NANTONG GAOXIN CERAMENT COMPOSITES CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NANTONG GAOXIN CERAMENT COMPOSITES CO Ltd filed Critical NANTONG GAOXIN CERAMENT COMPOSITES CO Ltd
Priority to CN2011200823138U priority Critical patent/CN202016236U/zh
Application granted granted Critical
Publication of CN202016236U publication Critical patent/CN202016236U/zh
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

本实用新型公开了一种等离子粉末堆焊大型金属陶瓷耐磨板,包括普通钢板本体,在普通钢板本体表面设有厚度均匀的等离子粉末堆焊金属陶瓷层。本实用新型结构合理,金属陶瓷耐磨板成形平整、光滑,堆焊面积大,能使耐磨板达到耐温、抗冲击性能好的工况要求。可以提高或延长运行寿命数倍以上。

Description

等离子粉末堆焊大型金属陶瓷耐磨板
技术领域
本实用新型涉及一种耐磨板。
背景技术
复合耐磨钢板是在普通结构钢的钢板表面融敷一层耐磨合金,使其表面具备极优异的耐温、抗磨损性能。用复合耐磨钢板制成结构件或机械零件,由于表面具备极优异的耐温、抗磨损性能,大大延长了使用寿命,获得显著地直接经济效益和社会效益,广泛应用于电力、水泥、煤炭、矿山等工业领域的抗磨设备。
目前复合耐磨钢板大多采用自保护明弧焊或埋弧焊的方法堆焊制得,但堆焊层表面布满裂纹、表面粗糙、飞溅多、焊道与焊道之间存在明显高低不平等缺陷,堆焊的材料多为高铬铸铁型合金。粉末等离子堆焊方法(PTA或称等离子喷焊法),虽然在堆焊效率上尚不及埋弧焊和明弧焊,但由于其热量集中、保护气氛和可控性良好的等离子弧,填充材料是粉末状合金,因而堆焊过程稳定;堆焊层母材冲淡率低;成形平整、光滑;特别适用于堆焊钴基、镍基等高合金材料,但存在生产效率低缺陷。
发明内容
本实用新型的目的在于提供一种结构合理,生产效率高、耐温、抗冲击性能好的等离子粉末堆焊大型金属陶瓷耐磨板。
本实用新型的技术解决方案是:
一种等离子粉末堆焊大型金属陶瓷耐磨板,其特征是:包括普通钢板本体,在普通钢板本体表面设有厚度均匀的等离子粉末堆焊金属陶瓷耐磨层。
金属陶瓷复合板的长度为3000mm,宽度为2200mm。
本实用新型结构合理,金属陶瓷耐磨板成形平整、光滑,堆焊面积大,能使耐磨板达到耐温、抗冲击性能好的工况要求。可以提高或延长运行寿命数倍以上。
附图说明
下面结合附图和实施例对本实用新型作进一步说明。
图1是四机头大功率粉末等离子耐磨板数控自动堆焊机结构尺寸示意图。
图2是本实用新型一个实施例的结构示意图。
图3是图2的剖视图。
具体实施方式
一种等离子粉末堆焊大型金属陶瓷耐磨板,包括普通钢板本体1,在普通钢板本体表面采用等离子堆焊方法堆焊厚度均匀的等离子粉末堆焊金属陶瓷层2。金属陶瓷复合板的长度为3000mm,宽度为2200mm或其他合适形式。
堆焊设备采用四机头大功率粉末等离子耐磨板数控自动堆焊机。图中包括堆焊机头3、钢板运行系统4。
堆焊粉末为Fe基+WC、Ni基+WC或Co基+WC材料。

Claims (2)

1. 一种等离子粉末堆焊大型金属陶瓷耐磨板,其特征是:包括普通钢板本体,在普通钢板本体表面设有厚度均匀的等离子粉末堆焊金属陶瓷耐磨层。
2. 根据权利要求1或2所述的等离子粉末堆焊大型金属陶瓷耐磨板,其特征是:普通钢板本体的长度为3000mm,宽度为2200mm。
CN2011200823138U 2011-03-25 2011-03-25 等离子粉末堆焊大型金属陶瓷耐磨板 Expired - Lifetime CN202016236U (zh)