Prior art keywords
pot body
iron
irony
pot
layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN2010205437318U
Other languages
Chinese (zh)
Inventor
肖建伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Supor Co Ltd
Wuhan Supor Cookware Co Ltd
Original Assignee
Zhejiang Supor Co Ltd
Wuhan Supor Cookware Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhejiang Supor Co Ltd, Wuhan Supor Cookware Co Ltd filed Critical Zhejiang Supor Co Ltd
Priority to CN2010205437318U priority Critical patent/CN201861407U/en
Application granted granted Critical
Publication of CN201861407U publication Critical patent/CN201861407U/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

Images

Landscapes

  • Cookers (AREA)

Abstract

The utility model discloses an iron cooking pot. The iron cooking pot comprises an iron pot body (1), a layer of ferroaluminium structure (2) is arranged respectively on the inner layer and the outer layer of the iron pot body (1), the thickness of the iron pot body (1) is 0.6 to 2.5 microns, and the thickness of the ferroaluminium structures (2) is 5 to 200 microns. Through the process that aluminum plating is combined with aluminizing, no other coating needs to be added on the surface of the iron cooking pot. The processed layer on the inner side of the pot body solves the rustiness and the heat transfer problems of the inner surface of the pot body, and the color does not change under high temperatures. The processed layer on the outer side of the pot body solves the heat-resisting and the oxidation-resisting problems of the outer surface of the iron cooking pot body.

Description

The irony frying pan
Technical field
The utility model relates to a kind of kitchen cooker, and more particularly it is a kind of irony frying pan.
Background technology
Pot is indispensable kitchen articles in the life, is broadly divided into: iron pot (comprising cast iron pan and wrought iron pan), aluminum pot, aluminum alloy pan, stainless-steel pan etc.Cast iron pan is heavy, the easy oxidation of wrought iron pan high temperature, and the life-span is short, and cast iron pan can replenish the ferro element of needed by human body, helps health.Aluminum pot, aluminum alloy pan, stainless-steel pan performance are preferable, but be considered to long-term use health harmful.Along with science and technology development, the mankind are not only studying the various good pot bodies of good property that have.
Existing by retrieval patent is found: 1, name is called Chinese healthy infiltration layer iron pan, the patent No.: CN87100220.5, and it is the aluminized coating that has anti-oxidation thermal stability on heating surface one side of pot body; The iron pan of this structure has solved the anti-oxidant thermally-stabilised problem of heating surface, but does not solve the problem that inner surface of pot body easily gets rusty.2. cooking utensil, patent No. CN200620154112.3, it is by hot aluminising sheet material drawing and forming, described hot aluminising sheet material constitutes by three layers, the centre is an iron plate, the two sides of iron plate is coated with interior aluminium lamination, outer aluminium lamination with dissolving coating process, scribbles the non-viscous paint protective layer on the described interior aluminium lamination, scribbles high-temperaure coating on the described outer aluminium lamination; The iron pan structure of this structure is complicated, and it is to aluminize on the surface of iron plate, for overcome aluminium to the harm of human body again at aluminium plated surface coating and high-temperaure coating again; The price of product is also higher.3. heat-resisting oxidation-resistance iron pan, the patent No.: CN89200759.1, it is that outer surface at the matrix iron pan oozes system layer of aluminum ferroalloy with the technology of iron and steel aluminising; This structure also is the heat-resisting and oxidation resistant problem that has only solved the outer surface of iron pan matrix.4. ferroalloy rust-less kitchenware pot, the patent No.: CN03211968.2, its pot body thin plate are the compound formation of upper, middle and lower-ranking, and upper and lower two layers of material is the alfer layer, and intermediate materials is the sheet metal layer; Though the iron pan of this structure is a three-decker, it is to adopt compound mode to form the alfer layer at outer and internal layer, but this compound mode complex process, the working strength of workers degree is big.
Therefore research and develop a kind of heat-resisting and oxidation resistant problem that can solve the iron pan pot body outer surface, also can solve getting rusty and heat transfer problem of inner surface of pot body simultaneously, and simple in structure, and the simple irony frying pan of production technology becomes a urgent and important job.
Summary of the invention
The purpose of this utility model is to overcome above-mentioned existing disadvantages of background technology part, and a kind of irony frying pan is provided.
The purpose of this utility model reaches by following measure: the irony frying pan, and it comprises irony pot body, it is characterized in that all has one deck ferroaluminium structure at the internal layer and the skin of irony pot body.
In technique scheme, the thickness of described irony pot body is the 0.6-2.5 micron, and described ferroaluminium thickness of structure is the 5-200 micron.
The thickness of described irony pot body is 1.5 microns, described ferroaluminium thickness of structure 25-40 micron.
1., aluminizing by employing adds alumetizing process the utility model irony frying pan has following advantage:, the surface need not to add any other coating again; 2., the inboard processing layer of its pot body solved getting rusty of inner surface of pot body and heat transfer problem, nondiscolouring under the high temperature, the external side processing layer of its pot has solved the heat-resisting and oxidation resistant problem of iron pan pot body outer surface; 3., after testing: the pot surface operational characteristic after the processing is stable, uniform film thickness, and the hardness height can be used for the inboard of pot body, directly contacts with food, and is durable in use, easy to clean; 4., the case hardness height, avoided the harmful defective in the edible back of aluminum pot aluminium lamination; 5., the long-term use can not form the spot corrosion penetration phenomenon down yet; 6., the technology environmental protection, low cost product, price is low.
Description of drawings
Fig. 1 is the structural representation of the utility model irony frying pan pot body.
1. irony pot body, 2. ferroaluminium structures among the figure.
The specific embodiment
Describe performance of the present utility model in detail below in conjunction with accompanying drawing, but they do not constitute to qualification of the present utility model, only do for example.Simultaneously by illustrating that advantage of the present utility model will become clear more and understanding easily.
Consult Fig. 1 as can be known: the utility model irony frying pan, it comprises irony pot body 1, it is characterized in that all has one deck ferroaluminium structure 2 at the internal layer and the skin of irony pot body 1.The thickness of described irony pot body 1 is the 0.6-2.5 micron, and the thickness of described ferroaluminium structure 2 is the 5-200 micron.
Preferred version is: the thickness of irony pot body 1 is 1.5 microns, the thickness 25-40 micron of ferroaluminium structure 2.
The utility model also can be used for the irony rust-less kitchenware of being correlated with. as: slaughterhouse, milk pot, pressure cooker, steamer etc.

Claims (3)

1. irony frying pan, it comprises irony pot body (1), it is characterized in that all has one deck ferroaluminium structure (2) at the internal layer and the skin of irony pot body (1).
2. irony frying pan according to claim 1, the thickness that it is characterized in that described irony pot body (1) is the 0.6-2.5 micron, the thickness of described ferroaluminium structure (2) is the 5-200 micron.
3. irony frying pan according to claim 2, the thickness that it is characterized in that described irony pot body (1) is 1.5 microns, the thickness 25-40 micron of described ferroaluminium structure (2).
CN2010205437318U 2010-09-27 2010-09-27 Iron cooking pot Expired - Lifetime CN201861407U (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2010205437318U CN201861407U (en) 2010-09-27 2010-09-27 Iron cooking pot

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2010205437318U CN201861407U (en) 2010-09-27 2010-09-27 Iron cooking pot

Publications (1)

Publication Number Publication Date
CN201861407U true CN201861407U (en) 2011-06-15

Family

ID=44132575

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2010205437318U Expired - Lifetime CN201861407U (en) 2010-09-27 2010-09-27 Iron cooking pot

Country Status (1)

Country Link
CN (1) CN201861407U (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103122434A (en) * 2011-11-19 2013-05-29 大连得达科技发展有限公司 Alloy material for making frying pan

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103122434A (en) * 2011-11-19 2013-05-29 大连得达科技发展有限公司 Alloy material for making frying pan

Similar Documents

Publication Publication Date Title
TWI466650B (en) Cooking utensil and manufacturing method thereof
CN205162726U (en) Double -deck composite pot
CN201150477Y (en) Frying pan of electromagentic furnace
CN201223273Y (en) Electromagnetic heating non-iron metal cooker
CN100496359C (en) A cooking utensil having three-layered composite plate fitting for various stoves and its processing method
CN201070282Y (en) Combined healthy non-cooking fume frying-pan of iron and aluminum
CN208876041U (en) Cookware and cooking apparatus
CN201861407U (en) Iron cooking pot
CN207940630U (en) A kind of compound pot
CN201046070Y (en) Complex sole aluminum electromagnetic cooking vessel
CN202567741U (en) Aluminum alloy cooker hot spray coating electromagnetic sensing pot with protection layer
CN203122057U (en) Pan
CN103110337A (en) Pan
CN2899675Y (en) Fumeless iron pot using multilayer material composite bottom
CN201115596Y (en) Composite type board pan
CN201379409Y (en) Electromagnetic heating ceramic and glass cooker
CN203937248U (en) A kind of stainless compound steel plate
CN206137855U (en) Multi -layer compound -bottom aluminum pot
CN202355173U (en) Composite-bottom pan
CN206275577U (en) A kind of non-stick pan
CN202426269U (en) Composite pot
CN201070251Y (en) Combined boiler
CN205162723U (en) Smokeless frying pan of soaking
CN202457811U (en) Double-layer composite pot with combined bottom
CN206182985U (en) Electromagnetism stove is suitable for iron pan

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
CX01 Expiry of patent term

Granted publication date: 20110615

CX01 Expiry of patent term