Prior art keywords
hard alloy
bearing
wear
gap
corrosion
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2010205599134U
Other languages
English (en)
Inventor
唐林
唐凯
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2010205599134U priority Critical patent/CN201818662U/zh
Application granted granted Critical
Publication of CN201818662U publication Critical patent/CN201818662U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Images

Landscapes

  • Rolling Contact Bearings (AREA)
  • Laminated Bodies (AREA)
  • Sliding-Contact Bearings (AREA)

Abstract

本实用新型提供一种耐磨耐蚀合金轴承,包括内套和间隙套装在内套上的外套,内套、外套均由耐腐蚀不锈钢材料制成,其特征在于:在内套、外套的间隙接合面上均设有一层硬质合金层。本实用新型由于在内套、外套的间隙接合面上均设有一层硬质合金层,使得轴承在原有抗强酸、强碱的耐蚀性的同时,又具有超长的耐磨性,耐磨度是原四氟乙烯套的数百倍,并且无污染,性能优良。

Description

耐磨耐蚀合金轴承
技术领域
本实用新型提供一种耐磨耐蚀合金轴承,属于医药、化工、生物等设备技术领域。
背景技术
磨擦轴承主要用于较大型搅拌设备中、搅拌轴的定位,在使用时将轴承外套固定在设备的底部或中部,将轴承内套装配于搅拌轴上,在设备工作时消除由于多种因素使中心搅拌轴摆动而不能正常使用的现象。它广泛应用于医药、化工、生物等行业。原来所用为四氟乙烯作内套,不锈钢材质作外套配合使用,效果欠佳,尤其在医药行业中的应用,使用原轴承的设备生产出的甘露醇,化验杂质超标且不耐用。
实用新型内容
本实用新型的目的是提供一种能克服上述缺陷、使用寿命长的耐磨耐蚀合金轴承。其技术内容为:
包括内套和间隙套装在内套上的外套,内套、外套均由耐腐蚀不锈钢材料制成,其特征在于:在内套、外套的间隙接合面上均设有一层硬质合金层。
所述的耐磨耐蚀合金轴承,硬质合金层包括间隙有序排列的若干硬质合金块,相邻硬质合金块之间填充有硬质合金粉,烧结而成。
所述的耐磨耐蚀合金轴承,相邻硬质合金块之间的间隙为
Figure BSA00000301518100011
本实用新型与现有技术相比,其优点是:由于在内套、外套的间隙接合面上均设有一层硬质合金层,使得轴承在原有抗强酸、强碱的耐蚀性的同时,又具有超长的耐磨性,耐磨度是原四氟乙烯套的数百倍,并且无污染,性能优良。
附图说明
图1是本实用新型实施例的结构示意图;
图2是本实用新型硬质合金层的展开图。
图中:1、内套2、外套3、硬质合金层4、硬质合金块5、硬质合金粉6、固定孔
具体实施方式
在图1-2所示的实施例中:内套1、外套2均由耐腐蚀不锈钢材料制成,且在内套1、外套2的间隙接合面上均设有一层硬质合金层3,硬质合金层3包括间隙有序排列的若干硬质合金块4,相邻硬质合金块4之间填充有硬质合金粉5,烧结而成。

Claims (3)

1.一种耐磨耐蚀合金轴承,包括内套(1)和间隙套装在内套(1)上的外套(2),内套(1)、外套(2)均由耐腐蚀不锈钢材料制成,其特征在于:在内套(1)、外套(2)的间隙接合面上均设有一层硬质合金层(3)。
2.如权利要求1所述的耐磨耐蚀合金轴承,其特征在于:硬质合金层(3)包括间隙有序排列的若干硬质合金块(4),相邻硬质合金块(4)之间填充有硬质合金粉(5),烧结而成。
3.如权利要求2所述的耐磨耐蚀合金轴承,其特征在于:相邻硬质合金块(4)之间的间隙为1.5mm~3mm。
CN2010205599134U 2010-10-14 2010-10-14 耐磨耐蚀合金轴承 Expired - Fee Related CN201818662U (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2010205599134U CN201818662U (zh) 2010-10-14 2010-10-14 耐磨耐蚀合金轴承

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2010205599134U CN201818662U (zh) 2010-10-14 2010-10-14 耐磨耐蚀合金轴承

Publications (1)

Publication Number Publication Date
CN201818662U true CN201818662U (zh) 2011-05-04

Family

ID=43916618

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2010205599134U Expired - Fee Related CN201818662U (zh) 2010-10-14 2010-10-14 耐磨耐蚀合金轴承

Country Status (1)

Country Link
CN (1) CN201818662U (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN107138922A (zh) * 2017-07-01 2017-09-08 济源华新石油机械有限公司 一种tc轴承的制作方法

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN107138922A (zh) * 2017-07-01 2017-09-08 济源华新石油机械有限公司 一种tc轴承的制作方法

Similar Documents

Publication Publication Date Title
Kumar et al. Solid lubrication at high-temperatures—A review
Greenberg et al. Bet Yerah: The Early Bronze Age Mound I: Excavation Reports, 1933-1986
US8646984B2 (en) Cellular encasement protection system for roller assembly
Zhu et al. PEEK composites as self-lubricating bush materials for articulating revolute pin joints
Li et al. Fabrication of Fe-based diamond composites by pressureless infiltration
Zhang et al. Preparation and tribological properties of WS2 hexagonal nanoplates and nanoflowers
Paleu et al. Microstructural analysis and tribological behavior of AMDRY 1371 (Mo–NiCrFeBSiC) atmospheric plasma spray deposited thin coatings
Huang et al. Tribological properties of porous PEEK composites containing ionic liquid under dry friction condition
CN201818662U (zh) 耐磨耐蚀合金轴承
Zhao et al. Study on friction and wear properties of new self-lubricating bearing materials
Zhao et al. The tribological performance of metal-/resin-impregnated graphite under harsh condition
Demirsöz Wear behavior of bronze vs. 100Cr6 friction pairs under different lubrication conditions for bearing applications
Zhao et al. Effect of CNTs in copper matrix on mechanical characteristics and tribological behavior under dry sliding and boundary lubrication conditions
Freschi et al. Employment of Micro-and Nano-WS2 structures to enhance the tribological properties of copper matrix composites
Yang et al. Effect of EDM and femtosecond-Laser groove-texture collision frequency on tribological properties of 0Cr17Ni7Al stainless steel
Burduhos-Nergis et al. Phosphate coatings: EIS and SEM applied to evaluate the corrosion behavior of steel in fire extinguishing solution
Liu et al. Enhancement of the water-lubricated tribological properties of hybrid PTFE/Nomex fabric laminate composite via epoxy resin and graphite filler
Karlina et al. Study of wear of an alloyed layer with chromium carbide particles after plasma melting
Pruncu et al. Surface Investigation of Physella Acuta Snail Shell Particle Reinforced Aluminium Matrix Composites
Fu et al. Tribological properties of solid lubricant WS2 in dimples on the cylinder of diesel engine at high temperature
Tan et al. Investigation of filling phase percentages on the performance of WC-Cu based hot-pressing diamond bit matrices
Zhu et al. Effect of Dissolved Oxygen Content on Tribo-Corrosion Behavior of Monel 400 Alloy in Seawater
Korzekwa et al. Investigation of selected polymer composite-aluminum oxide coating tribological systems
Liu et al. Friction and wear characteristics of microporous interface filled with mixed lubricants of M50 steel at different loads
CN203702852U (zh) 一种耐腐蚀抗干磨的径向滚柱轴承

Legal Events

Date Code Title Description
C14 Grant of patent or utility model
GR01 Patent grant
C17 Cessation of patent right
CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20110504

Termination date: 20121014