CN201796687U - 一种adsl变压器用锰锌铁氧体磁芯 - Google Patents

一种adsl变压器用锰锌铁氧体磁芯 Download PDF

Info

Publication number
CN201796687U
CN201796687U CN2010205070760U CN201020507076U CN201796687U CN 201796687 U CN201796687 U CN 201796687U CN 2010205070760 U CN2010205070760 U CN 2010205070760U CN 201020507076 U CN201020507076 U CN 201020507076U CN 201796687 U CN201796687 U CN 201796687U
Authority
CN
China
Prior art keywords
magnetic core
transformer
manganese
zinc ferrite
adsl
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2010205070760U
Other languages
English (en)
Inventor
刘先松
徐杰
胡锋
朱德如
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TIANCHANG CITY ZHAOTIAN MAGNETOELECTRICITY TECHNOLOGY Co Ltd
Original Assignee
TIANCHANG CITY ZHAOTIAN MAGNETOELECTRICITY TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TIANCHANG CITY ZHAOTIAN MAGNETOELECTRICITY TECHNOLOGY Co Ltd filed Critical TIANCHANG CITY ZHAOTIAN MAGNETOELECTRICITY TECHNOLOGY Co Ltd
Priority to CN2010205070760U priority Critical patent/CN201796687U/zh
Application granted granted Critical
Publication of CN201796687U publication Critical patent/CN201796687U/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

一种ADSL变压器用锰锌铁氧体磁芯,该磁芯包括矩形底板部、一个中心柱以及外围柱体,所述中心柱为中部为矩形,两端为半圆形,外围柱体将中心柱围成一半圆形的槽。该磁芯相比于圆柱状的中心柱结构磁芯,磁芯损耗、磁芯失真因子和形状失真因子小。本实用新型的有益效果为:降低了磁芯损耗、漏感、磁芯形状失真因子,选择该磁芯制作的变压器比用常规的EP型磁芯制作的变压器总谐波失真要低几个dB,延长了信号传输距离,提高了传输速率,提高了变压器的工作稳定性。

Description

一种ADSL变压器用锰锌铁氧体磁芯
技术领域
本实用新型涉及一种磁芯,尤其涉及一种ADSL变压器用锰锌铁氧体磁芯。
背景技术
常用的磁芯结构都是采用中心柱为圆柱状结构,为适应电子通信技术、网络技术及其设备的高电感量和轻小薄型化的发展,新一代ADSL技术对网络通信设备传输性能的要求更加严格,为保证设备系统稳定、可靠、高效运行,要求材料具有更低的比损耗系数和总谐波失真。而在ADSL网络变压器正常工作时,高性能的铁氧体磁芯起着关键的作用,具有低损耗、低总谐波失真(THD)的磁芯是变压器进行高速率、高保真信号传输的前提,因此需要设计优化磁芯,即选择磁芯损耗、磁芯失真因子和形状失真因子小的磁芯。
实用新型内容
针对以上缺陷,本实用新型提供一种ADSL变压器用锰锌铁氧体磁芯。
为实现上述目的,本实用新型通过以下技术方案实现:
一种ADSL变压器用锰锌铁氧体磁芯,该磁芯包括矩形底板部、一个中心柱以及外围柱体,所述中心柱为中部为矩形,两端为半圆形,外围柱体将中心柱围成一半圆形的槽。该磁芯相比于圆柱状的中心柱结构磁芯,磁芯损耗、磁芯失真因子和形状失真因子小。
本实用新型的有益效果为:降低了磁芯损耗、漏感、磁芯形状失真因子,选择该磁芯制作的变压器比用常规的EP型磁芯制作的变压器总谐波失真要低几个dB,延长了信号传输距离,提高了传输速率,提高了变压器的工作稳定性。
附图说明
图1是一种ADSL变压器用锰锌铁氧体磁芯的主视图;
图2是图1中A-A截面剖视图。
具体实施方式
下面根据实施例和附图对本实用新型作进一步详细说明。
如图1-2所示,一种ADSL变压器用锰锌铁氧体磁芯,该磁芯包括矩形底板部1、一个中心柱2以及外围柱体3,所述中心柱2为中部为矩形,两端为半圆形,外围柱体3将中心柱2围成一半圆形的槽。该磁芯相比于圆柱状的中心柱结构磁芯,磁芯损耗、磁芯失真因子和形状失真因子小。
本实用新型的有益效果为:降低了磁芯损耗、漏感、磁芯形状失真因子,选择该磁芯制作的变压器比用常规的EP型磁芯制作的变压器总谐波失真要低几个dB,延长了信号传输距离,提高了传输速率,提高了变压器的工作稳定性。

Claims (2)

1.一种ADSL变压器用锰锌铁氧体磁芯,该磁芯包括矩形底板部、一个中心柱以及外围柱体,其特征在于,所述中心柱为中部为矩形,两端为半圆形。
2.根据权利要求1所述的一种ADSL变压器用锰锌铁氧体磁芯,其特征在于,外围柱体将中心柱围成一半圆形的槽。
CN2010205070760U 2010-08-27 2010-08-27 一种adsl变压器用锰锌铁氧体磁芯 Expired - Fee Related CN201796687U (zh)