CN201778057U - Hydraulic slag skimming plate - Google Patents
Hydraulic slag skimming plate Download PDFInfo
- Publication number
- CN201778057U CN201778057U CN2010202513856U CN201020251385U CN201778057U CN 201778057 U CN201778057 U CN 201778057U CN 2010202513856 U CN2010202513856 U CN 2010202513856U CN 201020251385 U CN201020251385 U CN 201020251385U CN 201778057 U CN201778057 U CN 201778057U
- Authority
- CN
- China
- Prior art keywords
- skimming plate
- plate
- slag skimming
- hexsteel
- skimming
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
A hydraulic slag skimming plate comprises a slag skimming plate body (1) and a body (4), and is characterized in that a high-temperature resisting corrosion resisting coating is arranged on the surface of the slag skimming plate body (1), and the corrosion resisting coating adopts a pouring material layer (2); a hex mesh (3) is arranged between the pouring material layer (2) and the body (1); and the pouring material layer (2) is fixedly connected with the body (1) through the hex mesh (3). The slag skimming plate with the structure is high temperature resisting and corrosion resisting, and has a longer service life.
Description
Technical field
The utility model relates to a kind of hydraulic pressure and takes off slag plate.
Background technology
In steelmaking process, molten steel surface can be floating have impurity, is the quality that guarantees subsequent product, in the process of steel-making water, and need be with the Impurity removal of plate of skimming with molten steel surface.But because the temperature of molten steel is very high, taking off slag plate itself is that steel are made, and the life-span of therefore taking off slag plate is generally lower, has so just increased production cost.
Summary of the invention
The utility model provides a kind of hydraulic pressure to take off slag plate, and purpose is to solve the prior art problem, provides a kind of high temperature resistant, and the life-span prolongs takes off slag plate.
The technical scheme that the utility model is dealt with problems and adopted
Hydraulic pressure is taken off slag plate, is made of jointly skim plate body 1 and body 4, and plate body 1 surface of skimming is provided with the high-temperature resistant anti-corrosive layer, and described preservative coat is the cast bed of material 2.Also be provided with hexsteel 3 between the cast bed of material 2 and the body 1, and the cast bed of material 2 and body 1 be fixed together by hexsteel 3.
The beneficial effects of the utility model: be provided with the high-temperature resistant anti-corrosive layer at the plate body surface of skimming, this preservative coat adopts mould material, can effectively prolong the life-span of taking off slag plate.For making firm the lumping together of mould material energy, between mould material layer and body, be provided with hexsteel simultaneously with bulk junction.Hexsteel is high temperature resistant, corrosion-resistant, all porose mutual UNICOM of its hexagon, be welded on the plate body of skimming after, mould material is watered in the above, what mould material can be firm after the cooling is combined on the plate body of skimming, and can not come off, thereby prolong whole work-ing life of taking off slag plate.
Description of drawings
Fig. 1 is an one-piece construction synoptic diagram of the present utility model;
Fig. 2 is that the A of Fig. 1 is to sectional view.
Embodiment
The utility model is described in further detail below in conjunction with the drawings and specific embodiments.
Hydraulic pressure as shown in Fig. 1, Fig. 2 is taken off slag plate, is made of jointly skim plate body 1 and body 4, and plate body 1 surface of skimming is provided with the high-temperature resistant anti-corrosive layer, and described preservative coat is the cast bed of material 2.Be provided with hexsteel 3 between the cast bed of material 2 and the body 1, and the cast bed of material 2 and body 1 be fixed together by hexsteel 3.
Be provided with the high-temperature resistant anti-corrosive layer on plate body 1 surface of skimming, this preservative coat adopts mould material, can effectively prolong the life-span of taking off slag plate.Simultaneously because mould material is non-metallic material,, between mould material layer 2 and body 1, be provided with hexsteel 3 for making combining that it can be firm with body 1.Hexsteel 3 is high temperature resistant, corrosion-resistant, all porose mutual UNICOM of its hexagon, be welded on the plate body 1 of skimming after, mould material is watered in the above, and cooling back forms the cast bed of material 2, can be firm be combined on the plate body 1 of skimming, can not come off, thereby prolong whole work-ing life of taking off slag plate.
Claims (1)
1. hydraulic pressure is taken off slag plate, constitutes by skim plate body (1) and body (4) are common, and it is characterized in that: plate body (1) surface of skimming is provided with the high-temperature resistant anti-corrosive layer, and described preservative coat is the cast bed of material (2); Also be provided with hexsteel (3) between the cast bed of material (2) and the body (1), and the cast bed of material (2) and body (1) be fixed together by hexsteel (3).