CN201728479U - 板材焊接接口 - Google Patents
板材焊接接口 Download PDFInfo
- Publication number
- CN201728479U CN201728479U CN2010202236904U CN201020223690U CN201728479U CN 201728479 U CN201728479 U CN 201728479U CN 2010202236904 U CN2010202236904 U CN 2010202236904U CN 201020223690 U CN201020223690 U CN 201020223690U CN 201728479 U CN201728479 U CN 201728479U
- Authority
- CN
- China
- Prior art keywords
- welding
- welded
- plates
- sheet material
- connector
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型涉及一种板材焊接接口,包括两块待焊接板材,所述的待焊接板材的端部设置有焊接端,两块待焊接板材的焊接端之间形成焊接接口,所述的每块待焊接板材的焊接端均设置为一个单面坡口,所述的焊接接口的截面形成一个梯形结构。本实用新型焊接后的焊缝质量均能达到II级以上要求。本实用新型不需增加任何的装置,只需打单面坡口,减省了打另一面坡口及清理的时间,并且在对接处留有1-4mm间隙,即可实现单面坡口、单面焊接、双面成形。本实用新型焊接接口不需气刨,相对减少了焊接量,节省了能源,减少了气体排放量,节省了时间,提高了生产效率,降低了生产成本。
Description
技术领域
本实用新型涉及一种板材焊接接口。
背景技术
根据目前的工程及技术要求,很多的板材因设计标准提高,尺寸较大,又受原材料规格尺寸的限制,所以在各铁塔钢结构工程中,经常需要根据设计要求对板材进行拼接,焊接工艺技术及焊接质量要求较高。因而板材的焊接接口对于焊接质量起着重要的作用。现有的板材焊接接口的形状大多如图1所示,板材的对接端部为双面坡口,将打坡口中间的锐角边紧贴在一起。焊接的时候,先焊A面,将A面焊满,如图2所示。然后将板料翻转180°,因A面焊后根部焊接处未能熔合透,再有锐角边虽紧贴在一起,但会有空气进入A面的施焊腔内生成夹渣等缺陷,需要用气刨作清根处理。清根不但清去了焊上去的焊材,为了清除干净还清去了一部分母材,为后续焊接增加了焊接量,如图3所示。将气刨面彻底清理干净,用磨光机打磨出金属光泽后再焊接B面,此时B面形成了一个密闭的腔,不存在熔合不透及夹渣等现象,将B面填满,如图4所示。这种结构的焊接接口,在A面焊接完成后,必须在A面根部处用气刨做清根处理,将焊缝内部未熔透部分、夹渣刨掉。为更彻底清根,同时也会刨掉一部分母材,对后续焊接增大了焊接量;根据焊接工艺技术要求,气刨面必须用磨光机打磨干净,打磨清理又比较费事,所以气刨清根和打磨时间约占整个焊接量的三分之一还要多,不仅生产效率低下,浪费了能源,而且增加了生产成本。
实用新型内容
本实用新型的目的在于针对现有技术的不足,提供一种能够将板材快速焊接并且焊接质量高的板材焊接接口。
本实用新型的技术方案为:一种板材焊接接口,包括两块待焊接板材,所述的待焊接板材的端部设置有焊接端,两块待焊接板材的焊接端之间形成焊接接口,所述的每块待焊接板材的焊接端均设置为一个单面坡口,所述的焊接接口的截面形成一个梯形结构。
优选的是:所述的两块待焊接板材的焊接端之间的距离设置为1-4mm。
优选的是:所述的两块待焊接板材的焊接端之间的距离设置为4mm。
本实用新型的有益效果为:本实用新型焊接后的焊缝质量均能达到II级以上要求。本实用新型不需增加任何的装置,只需打单面坡口,减省了打另一面坡口及清理的时间,并且在对接处留有1-4mm间隙,即可实现单面坡口、单面焊接、双面成形。本实用新型焊接接口不需气刨,相对减少了焊接量,节省了能源,减少了气体排放量,节省了时间,提高了生产效率,降低了生产成本。
附图说明
图1-图4为现有技术的示意图
图5为本实用新型的结构示意图
图6为焊接状态示意图
图7为焊接完成示意图
具体实施方式
下面结合附图说明本实用新型的具体实施方式:
一种板材焊接接口,包括两块待焊接板材1,所述的待焊接板材1的端部设置有焊接端2,两块待焊接板材1的焊接端2之间形成焊接接口3,所述的每块待焊接板材1的焊接端2均设置为一个单面坡口,所述的焊接接口3的截面形成一个梯形结构。所述的两块待焊接板材1的焊接端2之间的距离设置为1-4mm。
工作时,如图5所示,将对接板材单面坡口面及周围彻底打磨干净,使其对接间隙以4mm为宜,用定位焊点住。如图6所示,开始在A面根据板厚、相应焊接工艺参数施焊,焊第一层是关键,焊接时既必须保证坡口处熔透,又不允许产生焊瘤,焊接速度可以根据间隙的大小来做适当调整,直至将坡口焊满。如图7所示,把板材翻转180°,B面向上,将B面根部,也就是焊A面根部熔透的焊材表面及氧化物用钢丝刷清理的干干净净,后施盖面焊,使B面焊道饱满美观,完成焊接。
Claims (3)
1.一种板材焊接接口,包括两块待焊接板材,所述的待焊接板材的端部设置有焊接端,两块待焊接板材的焊接端之间形成焊接接口,其特征在于:所述的每块待焊接板材的焊接端均设置为一个单面坡口,所述的焊接接口的截面形成一个梯形结构。
2.如权利要求1所述的板材焊接接口,其特征在于:所述的两块待焊接板材的焊接端之间的距离设置为1-4mm。
3.如权利要求2所述的板材焊接接口,其特征在于:所述的两块待焊接板材的焊接端之间的距离设置为4mm。