CN201584224U - Copper-clad aluminum wire production equipment - Google Patents

Copper-clad aluminum wire production equipment Download PDF

Info

Publication number
CN201584224U
CN201584224U CN2009202770053U CN200920277005U CN201584224U CN 201584224 U CN201584224 U CN 201584224U CN 2009202770053 U CN2009202770053 U CN 2009202770053U CN 200920277005 U CN200920277005 U CN 200920277005U CN 201584224 U CN201584224 U CN 201584224U
Authority
CN
China
Prior art keywords
copper
workbench
clad aluminum
production equipment
aluminum conductor
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2009202770053U
Other languages
Chinese (zh)
Inventor
傅利
高扬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
FUSHI INTERNATIONAL (DALIAN) BIMETALLIC CABLE Co Ltd
Original Assignee
FUSHI INTERNATIONAL (DALIAN) BIMETALLIC CABLE Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by FUSHI INTERNATIONAL (DALIAN) BIMETALLIC CABLE Co Ltd filed Critical FUSHI INTERNATIONAL (DALIAN) BIMETALLIC CABLE Co Ltd
Priority to CN2009202770053U priority Critical patent/CN201584224U/en
Application granted granted Critical
Publication of CN201584224U publication Critical patent/CN201584224U/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The utility model discloses copper-clad aluminum wire production equipment which includes an aluminum-bar feeder (1); the aluminum-bar feeder (1) is connected with one end of the sealing transmission channel (4) of the aluminum-bar through a surface cleaner (3); protective gas is arranged in the sealing transmission channel (4) of the aluminum-bar; the other end of the sealing transmission channel (4) of the aluminum-bar is arranged on a workbench (16); a copper belt cleaner (13), a copper belt storage unit (10) and a copper belt pay-off-rack (8) are arranged in front of the workbench (16) in sequence; a welding device (6) is arranged above the back side of the workbench (16); a reducing die (7) is arranged between the workbench (16) and a take-up reel (18); and a take-up roller (20) is arranged behind the take-up reel (18). The copper-clad aluminum wire production equipment can reduce the area reducing rate required by combining double metals below 35 percent and enhances the combination performance of copper and aluminum.

Description

The copper-clad aluminum conductor production equipment
Technical field
The utility model relates to a kind of copper-clad aluminum conductor production equipment.
Background technology
More noticeable in the patent of invention relevant for cladding wires at present is to be covered with one deck thin copper belt in the outsourcing of aluminium bar, and this product has the economic benefit that light quality is become reconciled, and also possesses the good electric conductivity of copper simultaneously.In general, and the equipment of producing copper-clad aluminum conductor at present is by electroplating or hot-dip coats another kind of metal in that core is outer, in uneven thickness with the copper-clad aluminum conductor coating layer of this device fabrication, and can't realize high-speed and continuous production.
The utility model content
The technical problems to be solved in the utility model provides a kind of copper-clad aluminum conductor production equipment, and is even with the copper-clad aluminum conductor coating thickness of this device fabrication, and the excellent bonding performance of copper-clad aluminum conductor can high-speed and continuous production.
In order to solve the problem that prior art exists, the technical scheme that this practicality is adopted is:
The copper-clad aluminum conductor production equipment; comprise aluminium bar feeder; described aluminium bar feeder links to each other by the end of removing surface device with aluminium rod seal transmission channel; go into to have protective gas in the aluminium rod seal transmission channel; the other end of aluminium rod seal transmission channel is arranged on the workbench; the place ahead of workbench sets gradually copper strips cleaning device, copper strips memory and copper strips pay off rack; the back side top of workbench is provided with welding equipment; be provided with the undergauge mould between workbench and the take-up reel, be provided with the take-up roller after the take-up reel.
Described workbench is provided with vertical format roll, horizontal format roll and format roll.
The oblique upper of described copper strips cleaning device one side is equipped with the copper tape guide device.
On described removing surface device and the welding equipment over cap is installed all.
Described removing surface device is scraping apparatus, turning equipment, dig and scrape a kind of in the equipment.
Described welding equipment is argon arc welding or multi-electrode welding electrode.
Described protective gas is a kind of in argon gas, helium, high pure nitrogen and the carbon dioxide or their gaseous mixture.
Advantage and effect that the utility model had are:
The utility model copper-clad aluminum conductor production equipment is provided with the removing surface device, by the method that scraping, turning or plane are scraped the surface of aluminium bar is handled, guarantee that aluminium rod surface cleans non-oxidation fully, make after the welding bimetallic copper cover aluminum blank through the draft drawing below 50% just can in conjunction with, improved the binding ability of copper-clad aluminum conductor; The utility model clad welded process is short, and after the clad welded operation, directly carry out drawing, and with continuous production line of they compositions, copper aluminium surface after can effectively preventing to clear up is continued oxidation follow-up melts combine is had a negative impact, and can make bimetallic junction close necessary draft and reduce to below 35%; Bimetallic conductor after the drawing is carried out diffusion heat treatments make copper aluminium produce flawless completely combination, obtain thickness and be no more than 10um or littler diffusion layer.
Description of drawings
Fig. 1 is the overall structure schematic diagram of the utility model copper-clad aluminum conductor production equipment;
Fig. 2 is the cross sectional representation of the product of the utility model copper-clad aluminum conductor production equipment coating.
Among the figure: aluminium bar feeder 1; Aluminium bar 2; Removing surface device 3; Aluminium rod seal transmission channel 4; Copper tape guide device 5; Welding equipment 6; Undergauge mould 7; Copper strips pay off rack 8; Copper strips 9; Copper strips memory 10; Directive wheel 11; Directive wheel 12; Copper strips cleaning device 13; Vertical format roll 14; Horizontal format roll 15; Workbench 16; Format roll 17; Take-up reel 18; Copper-clad aluminum conductor 19; Take-up roller 20.
Embodiment
As shown in Figure 1; the aluminium bar feeder 1 of the utility model copper-clad aluminum conductor production equipment links to each other by the end of removing surface device 3 with aluminium rod seal transmission channel 4; feed in the aluminium rod seal transmission channel 4 that protective gas, described protective gas are arranged is a kind of in argon gas, helium, high pure nitrogen and the carbon dioxide or their gaseous mixture.The other end of aluminium rod seal transmission channel 4 is arranged on the workbench 16, and the place ahead of workbench 16 sets gradually copper strips cleaning device 13, copper strips memory 10 and copper strips pay off rack 8, and the oblique upper of described copper strips cleaning device 13 1 sides is equipped with copper tape guide device 5.On described removing surface device 3 and the welding equipment 6 over cap is installed all.The back side top of workbench 16 is provided with welding equipment 6, and described welding equipment 6 is argon arc welding or multi-electrode welding electrode.Be provided with undergauge mould 7 between workbench 16 and the take-up reel 18, be provided with take-up roller 20 after the take-up reel 18.Described workbench 16 is provided with vertical format roll 14, laterally format roll 15 and format roll 17, and format roll 17 is a series of hard-wired format rolls, makes the copper strips after the brushing form tubulose.The device at cutting copper strips edge also is installed on the described workbench.Described removing surface device 3 for scraping apparatus, turning equipment, dig and scrape a kind of in the equipment.
Using method of the present utility model is as follows:
Aluminium bar feeder 1 provides aluminium bar 2, and aluminium bar 2 can certainly adopt turning or plane to scrape equipment and replace scraping apparatus by scraping apparatus 3.Scraping apparatus 3 and welding equipment 6 are provided with over cap.The aluminium bar will prevent that the surface is contaminated, the surface should be cleaned, smooth rounding, and size is even, defectives such as no edging, wrong circle, crackle field trash, kink.The aluminium bar enters the aluminium rod seal transmission channel 4 of a kind of in the gases such as being connected with argon gas, helium, high pure nitrogen and carbon dioxide or their mixture by the roll-type straightener.Copper strips 9 transmits by copper strips pay off rack 8, and enters into copper strips cleaning device 13 by memory 10, and storeroom mainly is to be used for replenishing enough copper strips to guarantee continuous coating when copper strips butt joint welding.Between directive wheel 11 and directive wheel 12, can store 100 meters long copper strips, store length and mainly be fixed against on-line velocity and weld time.Copper strips is by the shaped device 17 of setting on the workbench 16 then, and copper strips is by argon arc or 6 welding of multi-electrode welding electrode.Copper cover aluminum 19 lines behind the welding fabrication carry out undergauge by take-up 18 preceding undergauge moulds 7, then by take-up 18 traction take-ups.Reel by take-up roller 20 again.The cross section of copper-clad aluminum conductor 19 as shown in Figure 2.

Claims (8)

1. copper-clad aluminum conductor production equipment; comprise aluminium bar feeder (1); it is characterized in that described aluminium bar feeder (1) links to each other by the end of removing surface device (3) with aluminium rod seal transmission channel (4); feed in the aluminium rod seal transmission channel (4) protective gas is arranged; the other end of aluminium rod seal transmission channel (4) is arranged on the workbench (16); the place ahead of workbench (16) sets gradually copper strips cleaning device (13); copper strips memory (10) and copper strips pay off rack (8); the back side top of workbench (16) is provided with welding equipment (6); be provided with undergauge mould (7) between workbench (16) and the take-up reel (18), take-up reel (18) is provided with take-up roller (20) afterwards.
2. copper-clad aluminum conductor production equipment according to claim 1 is characterized in that described workbench (16) is provided with vertical format roll (14), horizontal format roll (15) and format roll (17).
3. copper-clad aluminum conductor production equipment according to claim 1 is characterized in that the oblique upper of described copper strips cleaning device (13) one sides is equipped with copper tape guide device (5).
4. copper-clad aluminum conductor production equipment according to claim 1 is characterized in that on described removing surface device (3) and the welding equipment (6) over cap being installed all.
5. according to claim 1 or 4 described copper-clad aluminum conductor production equipments, it is characterized in that described removing surface device (3) for scraping apparatus, turning equipment, dig and scrape a kind of in the equipment.
6. copper-clad aluminum conductor production equipment according to claim 1 is characterized in that described welding equipment (6) is argon arc welding or multi-electrode welding electrode.
7. copper-clad aluminum conductor production equipment according to claim 1 is characterized in that described protective gas is a kind of in argon gas, helium, high pure nitrogen and the carbon dioxide or their gaseous mixture.
8. copper-clad aluminum conductor production equipment according to claim 1 is characterized in that also being equipped with on the described workbench (16) device at cutting copper strips edge.
CN2009202770053U 2009-12-04 2009-12-04 Copper-clad aluminum wire production equipment Expired - Fee Related CN201584224U (en)