CN201549275U - Single-surface paint coater for enamelled rectangular section conductor - Google Patents

Single-surface paint coater for enamelled rectangular section conductor Download PDF

Info

Publication number
CN201549275U
CN201549275U CN2009202544724U CN200920254472U CN201549275U CN 201549275 U CN201549275 U CN 201549275U CN 2009202544724 U CN2009202544724 U CN 2009202544724U CN 200920254472 U CN200920254472 U CN 200920254472U CN 201549275 U CN201549275 U CN 201549275U
Authority
CN
China
Prior art keywords
paint
wire
enameled
notes
baffler
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN2009202544724U
Other languages
Chinese (zh)
Inventor
李雄壮
王志勇
王晓光
赵葛
韩新生
赵秀生
景崇友
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Baoding Tianwei Group Co Ltd
Original Assignee
Baoding Tianwei Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Baoding Tianwei Group Co Ltd filed Critical Baoding Tianwei Group Co Ltd
Priority to CN2009202544724U priority Critical patent/CN201549275U/en
Application granted granted Critical
Publication of CN201549275U publication Critical patent/CN201549275U/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

A single-surface paint coater for enamelled rectangular section conductor is used for settling a problem of single-surface paint coating. The technical solution is characterized in that: the single-surface paint coater comprises a paint injection block which is equipped to a base through a dovetail groove linear guide rail. The front side surface of the paint injection block is fixedly provided with a flow guiding plate. The flow guiding plate is provided with a flow guiding elongated hole which is opposite with wide edge of the enamelled rectangular section conductor and is communicated with the paint injection opening on the paint injection block. The paint injection channel between the flow guiding elongated hole and the paint injection opening is also provided with a flow adjusting screw. Rectangular section conductor guide wheel are provided in front of the light guiding plate. A spring bracket which is fixedly connected with the base is provided behind the paint injection block. A compression spring is provided between a spring bracket and the paint injection block. The single-surface paint coater for enamelled rectangular section conductor has the advantages of simple structure and high paint coating efficiency. Not only is paint saved, but also the thickness of the paint film is uniform and consistent.

Description

A kind of device for painting only one surface of enameled flat wire
Technical field
The utility model relates to the device of a kind of Transformer Winding with the only one surface of enameled flat wire coating self-adhesion lacquer of transposed conductor, belongs to the transformer technology field.
Background technology
The Transformer Winding transposed conductor is formed by the folded system of many enameled sheet wires, and its outside is wrapped with insulating paper or net band.Enameled sheet wire as transposed conductor is generally self-adhesive enameled wire, and it is coated with the self-adhesion lacquer outward and forms based on the acetal enameled sheet wire.In the winding dry run, the self-adhesion lacquer between adjacent enameled sheet wire is bonding mutually, makes transposed conductor form an integral body, thereby improves whole transposed conductor and mechanical Strength for Winding greatly.
Existing transposed conductor all is to be made by the enameled sheet wire that outer surface all covers the self-adhesion paint film, but the leptoprosopy of enameled sheet wire does not generally contact with other enameled sheet wire in the transposed conductor, thereby the lacquer of the self-adhesion on the narrow limit does not have the effect of bonding, this self-adhesion enameled sheet wire is not only wasted the self-adhesion lacquer, and the self-adhesion lacquer that is coated on the leptoprosopy can flow in the transformer coil solidification process, the self-adhesion lacquer that flows may be brought together and form the lacquer knurl, also may form the bubble that can not be full of with oil at the splicing seams place of adjacent two enameled sheet wire leptoprosopy, thereby cause the partial discharge under the high voltage.
Experiment shows, adopt the enameled sheet wire manufacturing transposition that only on wide, scribbles the self-adhesion lacquer to lead and can solve the problems referred to above, but the widely used coating apparatus of enamelled wire industry can only make the self-adhesion lacquer cover whole lead at present, therefore, designing a kind of device for painting only one surface of enameled flat wire, is the current problems that face of relevant technologies personnel.
The utility model content
The purpose of this utility model is the device for painting only one surface of enameled flat wire that overcomes the deficiencies in the prior art, a kind of dependable performance is provided.
Problem described in the utility model realizes with following technical proposals:
A kind of device for painting only one surface of enameled flat wire, it comprises that is annotated a paint block, described notes paint block is installed on the pedestal by the dovetail groove line slideway; Be fixed with baffler on its leading flank, described baffler is provided with a water conservancy diversion slotted hole relative with the enameled sheet wire broadside and that communicate with notes lacquer mouth on annotating paint block; The front portion of described baffler is provided with the lenticular wire guide wheel; The rear of described notes paint block is provided with the spring support affixed with pedestal, is provided with stage clip between described spring support and the notes paint block.
Above-mentioned device for painting only one surface of enameled flat wire, the upper end of described baffler is provided with spacing rib, and described spacing rib is provided with the lenticular wire spacing edge-cut.
Above-mentioned device for painting only one surface of enameled flat wire also is provided with flow on the notes lacquer passage between described water conservancy diversion slotted hole and the notes lacquer mouth and adjusts bolt.
Above-mentioned device for painting only one surface of enameled flat wire is provided with regulator bolts between described stage clip and the spring support.
The utility model utilizes the water conservancy diversion slotted hole on the baffler to paint to enameled sheet wire, and self-adhesion is coated with lacquer on one wide that can only be coated in enameled sheet wire, and the effect of the lenticular wire spacing edge-cut on the spacing rib of baffler is to guarantee that lead is relative with the water conservancy diversion slotted hole all the time.The lenticular wire guide wheel can make flat being close on the baffler of enamel-cover also can move swimmingly, the effect of stage clip is to promote to annotate paint block to press to the lenticular wire guide wheel along the dovetail groove line slideway, make between enameled sheet wire and the baffler to keep certain pressure, improve coating quality, regulator bolts is used to regulate the pressure of stage clip.The utility model is simple in structure, dependable performance, japanning efficient height, can be only wide of enameled sheet wire be applied the self-adhesion lacquer, produce self-adhesive enameled wire with it and not only economize lacquer, and self-adhesive enameled wire self-adhesion lacquer in the transformer coil solidification process can not form lacquer knurl and bubble, film thickness uniformity.
Description of drawings
The utility model is described in further detail below in conjunction with accompanying drawing.
Fig. 1 is the cross-sectional structure schematic diagram of enameled sheet wire after single face is coated with the self-adhesion lacquer;
Fig. 2 is a structural representation of the present utility model;
Fig. 3 is the vertical view of Fig. 2;
Fig. 4 is that the position between enameled sheet wire and baffler and the lenticular wire guide wheel concerns schematic diagram;
Fig. 5 is the structural representation of baffler;
Fig. 6 is the left view of Fig. 5;
Fig. 7 is the vertical view of Fig. 5.
Each label is among the figure: 1, pedestal; 2, annotate paint block; 3, lenticular wire guide wheel; 4, baffler; 5, spring support; 6, stage clip; 7, regulator bolts; 8, bolt; 9, dovetail groove line slideway; 10, bolt; 11, flow is adjusted bolt; 12, enameled sheet wire; 13, annotate the lacquer mouth; 14, water conservancy diversion slotted hole; 15, acetal paint; 16, flat type copper wire; 17, self-adhesion lacquer, 18, spacing rib; 19, lenticular wire spacing edge-cut.
Embodiment
The utility model only applies the self-adhesion lacquer to one wide of enameled sheet wire, the scribbling wide of self-adhesion lacquer and do not scribble the wide face that self-adhesion coats with lacquer with adjacent self-adhesion enameled sheet wire and contact of each self-adhesion enameled sheet wire, and wide the adjacent self-adhesion enameled sheet wire with another that does not scribble self-adhesion lacquer scribbles the wide face of self-adhesion lacquer and contacts the bonding between the realization enameled sheet wire.
Referring to Fig. 2, Fig. 3, Fig. 4, pedestal 1 and notes paint block 2 cooperate, annotating paint block 2 can be free to slide on pedestal 1 along dovetail groove line slideway 9, baffler 4 is fixed on by bolt 10 and annotates on the paint block 2, and flow is adjusted bolt 11 and is installed in the top of annotating paint block 2, and lenticular wire guide wheel 3 is fixed on pedestal 1 both sides by the guide wheel fixed head, at the rear of annotating paint block 2, spring support 5 is fixed on the pedestal 1 by bolt 8, and stage clip 6 is installed in annotates between paint block 2 and the spring support 5 pressure of regulator bolts 7 scalable stage clips 6.
After this device assembling finishes, screw hole by slotted hole on the pedestal 1 and notes paint block 2 side-lowers is fixed on pedestal 1 on the coating apparatus, then enameled sheet wire 12 is passed between baffler 4 and lenticular wire guide wheel 3, rotate regulator bolts 7 then and adjust 6 pairs of pressure of annotating paint block 2 of stage clip, make notes paint block 2 promote bafflers 4 and hold out against enameled sheet wire 12 (flow velocity according to enamelled wire speed and self-adhesion lacquer is determined stretch pressure).Behind the opening device, adjust bolt 11 fine setting self-adhesion lacquer flows by flow again, self-adhesion lacquer flow velocity and enameled sheet wire 12 speed are complementary, guarantee that the self-adhesion lacquer coats the one-sided of enamelled wire 12 equably.
When enameled sheet wire 12 during by baffler 4, can promote baffler 4, annotate paint block 2 according to the difference of self thickness, so that control spring 6 strokes, make enameled sheet wire keep constant compression force with annotating between the paint block 2, thus control japanning thickness.
The utility model carries out the adjustable self-adhesion lacquer of single face, paint film width and thickness to enameled sheet wire and coats by the enameled sheet wire processing mode is improved, and makes the not overflow in the transformer oven dry of self-adhesion lacquer.The utility model can be realized the continuous production of painting only one surface of enameled flat wire.

Claims (4)

1. a device for painting only one surface of enameled flat wire is characterized in that, it comprises that is annotated a paint block (2), and described notes paint block (2) is installed on the pedestal (1) by dovetail groove line slideway (9); Be fixed with baffler (4) on its leading flank, described baffler (4) is provided with water conservancy diversion slotted hole (14) relative with enameled sheet wire (12) broadside and that communicate with notes lacquer mouthful (13) on annotating paint blocks (2); The front portion of described baffler (4) is provided with lenticular wire guide wheel (3); The rear of described notes paint block (2) is provided with and the affixed spring support (5) of pedestal (1), is provided with stage clip (6) between described spring support (5) and the notes paint blocks (2).
2. according to the described device for painting only one surface of enameled flat wire of claim 1, it is characterized in that the upper end of described baffler (4) is provided with spacing rib (18), is lenticular wire spacing edge-cut (19) between the described two spacing ribs (18).
3. according to claim 1 or 2 described device for painting only one surface of enameled flat wire, it is characterized in that, also be provided with flow on the notes lacquer passage between described water conservancy diversion slotted hole (14) and the notes lacquer mouthful (13) and adjust bolt (11).
4. according to the described device for painting only one surface of enameled flat wire of claim 3, it is characterized in that, be provided with regulator bolts (7) between described stage clip (6) and the spring support (5).
CN2009202544724U 2009-11-16 2009-11-16 Single-surface paint coater for enamelled rectangular section conductor Expired - Lifetime CN201549275U (en)