CN201525894U - 一种组合式多阴极多阳极石墨电解槽 - Google Patents
一种组合式多阴极多阳极石墨电解槽 Download PDFInfo
- Publication number
- CN201525894U CN201525894U CN2009202577817U CN200920257781U CN201525894U CN 201525894 U CN201525894 U CN 201525894U CN 2009202577817 U CN2009202577817 U CN 2009202577817U CN 200920257781 U CN200920257781 U CN 200920257781U CN 201525894 U CN201525894 U CN 201525894U
- Authority
- CN
- China
- Prior art keywords
- tank
- graphite
- tank body
- electrolytic tank
- electrolytic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种组合式多阴极多阳极石墨电解槽,包括石墨槽,石墨槽外设有保温层,所述石墨槽为矩形,其由上槽体和下槽体构成,上槽体和下槽体通过台阶配合连接;石墨槽内壁环绕设有阳极板,沿石墨槽纵向轴线间隔排列6-15根阴极。上槽体和下槽体组合而成电解槽,延长了电解槽的使用寿命,与传统电解槽相比,烧损后更换时间大大缩短,降低生产成本,提高生产效率;电解槽由石墨块砌筑而成,在电解槽内壁设有矩形框状阳极板,矩形框内排列多根阴极,槽体增大、电流提高、能耗降低、单产提高,电解槽综合利用率得到提高。
Description
技术领域
本实用新型属于石墨生产设备技术领域,特别涉及一种组合式多阴极多阳极石墨电解槽。
背景技术
传统的电解槽槽体为圆桶形石墨坩埚,阳极为石墨圆筒,阴极为一根钨棒或者钼棒。这种电解槽槽体小、电流小、能耗高和单产低的缺陷导致生产效率低。另外,传统电解槽为圆形整体,电解槽在冶炼时上部内侧直接与空气接触,在高温条件下易氧化烧损,上部烧损严重,其它地方受损程度小,若要更换则需要整体更换,更换过程耗时长,不仅降低电解槽使用周期,还增加生产成本、降低生产效率。
实用新型内容
本实用新型的目的是提供一种使用寿命长、生产效率高的组合式多阴极多阳极石墨电解槽。
为实现上述目的,本实用新型的技术方案是:一种组合式多阴极多阳极石墨电解槽,包括石墨槽,石墨槽外设有保温层,所述石墨槽为矩形,其由上槽体和下槽体构成,上槽体和下槽体通过台阶配合连接;石墨槽内壁环绕设有阳极板,沿石墨槽纵向轴线间隔排列6-15根阴极。
所述阳极板由多块构成,且沿石墨槽内壁围成矩形框。
本实用新型由上槽体和下槽体组合而成电解槽,延长了电解槽的使用寿命,与传统电解槽相比,烧损后更换时间大大缩短,降低生产成本,提高生产效率;电解槽由石墨块砌筑而成,在电解槽内壁设有矩形框状阳极板,矩形框内排列多根阴极,槽体增大、电流提高、能耗降低、单产提高,电解槽综合利用率得到提高。
附图说明
图1为本实用新型的结构示意图;
图2为图1的A-A剖视图。
具体实施方式
如图1、图2所示的组合式多阴极多阳极石墨电解槽,包括矩形石墨槽1,所述的石墨槽1由上槽体11和下槽体12构成,上槽体11和下槽体12之间通过台阶配合连接。这样的结构,在电解过程中电解槽上部烧损后,只需将烧损的上槽体11更换即可。在石墨槽1的内壁环绕设有阳极板2,多块阳极板2沿石墨槽1内壁围成矩形框;在阳极板2矩形框内侧,沿石墨槽1纵向轴线间隔排列多根阴极3,一般选择6-15根。在石墨槽1外部设有保温层4,以起到保温保压的作用。
在本实施方式中,阳极板2为8块,阴极3为6根,构成多阴极多阳极石墨电解槽。
石墨槽1可由石墨块按照槽体形状砌筑而成,大小根据需要设定,并按需要设定阴极3和阳极板2的数目,以适应不同的生产规模。
Claims (2)
1.一种组合式多阴极多阳极石墨电解槽,包括石墨槽,石墨槽外设有保温层,其特征在于:所述石墨槽为矩形,其由上槽体和下槽体构成,上槽体和下槽体通过台阶配合连接;石墨槽内壁环绕设有阳极板,沿石墨槽纵向轴线间隔排列6-15根阴极。
2.如权利要求1所述的组合式多阴极多阳极石墨电解槽,其特征在于:所述阳极板由多块构成,且沿石墨槽内壁围成矩形框。