CN201503422U - 一种用于大型钢制套圈成品超声波检测的校准试块 - Google Patents
一种用于大型钢制套圈成品超声波检测的校准试块 Download PDFInfo
- Publication number
- CN201503422U CN201503422U CN2009202279269U CN200920227926U CN201503422U CN 201503422 U CN201503422 U CN 201503422U CN 2009202279269 U CN2009202279269 U CN 2009202279269U CN 200920227926 U CN200920227926 U CN 200920227926U CN 201503422 U CN201503422 U CN 201503422U
- Authority
- CN
- China
- Prior art keywords
- test block
- block
- bottom hole
- calibration test
- plane
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
一种用于大型钢制套圈成品超声波检测的校准试块,具有试块本体,其特征在于:所述试块本体为一梯形块,梯形块上表面与两侧的斜面之间的夹角a与所用的斜探头K值相匹配,在梯形块两侧的斜面上开有数量相等的若干圆形平底孔;所述平底孔的中心轴线与所述的斜面垂直;本实用新型结构简单,使用方便;与探伤辅助传动装置相结合,适用于各种直径大型钢制套圈成品的探伤检测。可以检测产品内部裂纹、夹杂、白点、缩孔、空隙和表面缺陷。
Description
(一)技术领域:本实用新型涉及一种无损检测技术中的超声波检测用具,具体是一种用于大型钢制套圈成品超声波检测的校准试块。
(二)现有技术:目前,我国大型钢制套圈成品使用的是磁粉探伤方法,磁粉探伤只对铁磁性钢铁材料表面、近表面进行探伤。而对钢铁材料自身缺陷和制造过程中产生的内部缺陷,磁粉探伤技术是无法解决。例如钢材内部的夹杂、白点、缩孔和产品生产过程中产生的孔隙、内裂等缺陷磁粉探伤是不能检测出来的。而这些缺陷很大程度上对产品的安全运行有很大的威胁。
我国由于没有针对于钢制套圈成品的超声波探伤方法,所以只在套圈的半成品进行超声波纵波内部质量探伤。经过热处理等工艺后成品没有进行超声波探伤检测。但经对套圈进行探伤试验,已发现少数套圈内部存在危害性缺陷,这会对其使用寿命有很大影响。所以有必要使用科学实用的探伤方法及相应的用具对套圈成品进行超声波探伤,保证产品的零缺陷。
一般超声波横波探伤方法的核心问题,是需用一种校准试块对超声波斜探头的灵敏度进行校准,制作距离-波幅曲线;经检索,目前尚没有发现与本发明中相同结构的校准试块。
(三)发明内容:本实用新型的目的就是提供一种用于大型钢制套圈成品超声波检测的校准试块,该试块结构简单,使用方便;与探伤辅助传动装置相结合,可以检测产品内部裂纹、夹杂、白点、缩孔、空隙和表面缺陷。
本实用新型的一种用于大型钢制套圈成品超声波检测的校准试块,具有试块本体,其特征在于:所述试块本体为一梯形块,梯形块上表面与两侧的斜面之间的夹角a与所用的超声波斜探头K值相匹配,在梯形块两侧的斜面上开有数量相等的若干圆形平底孔;所述平底孔的中心轴线与所述的斜面垂直。
所述的平底孔深度h为5mm,当斜探头K值一定时,所述平底孔中心轴线之间的距离相等。
所述的梯形块两侧的斜面上平底孔数量为8或12个。
所述的斜探头K值与梯形块上夹角a的关系如下表所示:
K值 | 0.75 | 1 | 1.5 | 2.0 | 2.5 |
夹角角度 | 36.87° | 45.00° | 56.31° | 63.43° | 68.20° |
所述的平底孔深度为5mm,当斜探头K值一定时,所述平底孔中心轴线之间的距离相等。
如当斜探头K值为0.75时,每个平底孔中心轴线之间的距离为16.7mm;当斜探头K值为1.5时,每个平底孔中心轴线之间的距离为12.0mm;
所述的梯形块两侧的斜面上平底孔数量为8或12个。
进行探伤操作时,首先将选定的超声波斜探头放在相配套的试块上表面即声波入射面上,将探头超声波入射方向对准斜面上的平底孔,对斜面上的平底孔通过超声波仪器显示屏观察,由近及远依次进行灵敏度校准,并绘制超声波探伤检测常用的距离-波幅灵敏度曲线,这时候就完成了探伤灵敏度的校准过程。然后,再与超声波探伤仪器和有关配套的传动装置配合,按探伤的正常步骤对钢制套圈工件进行探伤,直至探伤完成。
套圈经检验没有超过距离-波幅曲线高度的波幅信号即评为合格品,如发现有超过距离-波幅曲线高度的波幅信号即评为不合格品,并对缺陷部位进行标记,按规定进行隔离,装入不合格品区。
本实用新型填补了我国利用梯形平底孔试块校准方式对大型钢制套圈成品进行探伤检测的空白,探伤级别可使用国家GB/T4162-2008《锻轧钢棒超声波检验方法》中质量等级级别。本实用新型推荐用AA级标准制作不同距离平底孔标准,制作距离-波幅曲线。使用的AA标准级别严于铁路货车、客车轴承用钢的探伤标准,对大型钢制套圈产品内部、外部100%探伤检测,保证了产品的实物质量。
(四)附图说明
图1是本实用新型的结构示意图;
图2是图1的仰视方向结构示意图。
图中,1-梯形块,2-上表面,3-斜面,4-超声波斜探头,5-圆形平底孔。
(五)具体实施方式:
参见图1,本实用新型具有试块本体,所述试块本体为一梯形块1,梯形块上表面2为声波入射面,其与两侧的斜面3之间的夹角a与所用的超声波斜探头4的K值相匹配,在梯形块两侧的斜面上开有数量相等的若干圆形平底孔5;所述平底孔的中心轴线与所述的斜面垂直。
所述的平底孔深度h为5mm,当斜探头K值一定时,所述平底孔中心轴线之间的距离相等。
所述的梯形块两侧的斜面上平底孔数量为8或12个。
Claims (3)
1.一种用于大型钢制套圈成品超声波检测的校准试块,具有试块本体,其特征在于:所述试块本体为一梯形块,梯形块上表面与两侧的斜面之间的夹角a与所用的超声波斜探头K值相匹配,在梯形块两侧的斜面上开有数量相等的若干圆形平底孔;所述平底孔的中心轴线与所述的斜面垂直。
2.根据权利要求1所述的一种用于大型钢制套圈成品超声波检测的校准试块,其特征在于:所述的平底孔深度h为5mm,当斜探头K值一定时,所述平底孔中心轴线之间的距离相等。
3.根据权利要求1或2所述的一种用于大型钢制套圈成品超声波检测的校准试块,其特征在于:所述的梯形块两侧的斜面上平底孔数量为8或12个。