CN201442979U - Iron core of magnesium bar of antiskid water heater - Google Patents

Iron core of magnesium bar of antiskid water heater Download PDF

Info

Publication number
CN201442979U
CN201442979U CN2009200289957U CN200920028995U CN201442979U CN 201442979 U CN201442979 U CN 201442979U CN 2009200289957 U CN2009200289957 U CN 2009200289957U CN 200920028995 U CN200920028995 U CN 200920028995U CN 201442979 U CN201442979 U CN 201442979U
Authority
CN
China
Prior art keywords
iron core
magnesium
water heater
magnesium bar
bar
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2009200289957U
Other languages
Chinese (zh)
Inventor
翟慎宝
孙启明
王增委
吴忠文
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZIBO HONGTAI ANTISEPTIC CO Ltd
Original Assignee
ZIBO HONGTAI ANTISEPTIC CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZIBO HONGTAI ANTISEPTIC CO Ltd filed Critical ZIBO HONGTAI ANTISEPTIC CO Ltd
Priority to CN2009200289957U priority Critical patent/CN201442979U/en
Application granted granted Critical
Publication of CN201442979U publication Critical patent/CN201442979U/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The utility model relates to an iron core of a magnesium bar of an antiskid water heater, which belongs to the technical field of a sacrificial anode of magnesium alloy. The iron core of the magnesium bar of the antiskid water heater comprises a magnesium bar, wherein the iron core is coated in the center of the magnesium bar. The iron core of the magnesium bar of the antiskid water heater is characterized in that a coating part of the iron core is provided with a groove. Compared with the prior art, the utility model and the magnesium alloy are firmly combined and are not easy to loosen. By a boosting experiment, the iron core is not loosened under 40N, and the qualified rate of the magnesium bar is greatly enhanced.

Description

A kind of anti-skidding water-heater magnesium rod iron core
Technical field
The utility model belongs to the sacrificial magnesium alloy anode technical field, is specifically related to a kind of anti-skidding water-heater magnesium rod iron core.
Background technology
The sacrificial magnesium alloy anode rod that protection against corrosion is used (be called for short magnesium rod) as galvanic protection to the protection bather safety play crucial effects.
In the prior art, the making processes of magnesium rod is: 1) iron core car silk; 2) magnesium melting cast molding; 3) revise polishing; 4) check; 5) packing is dispatched from the factory.Wherein, generally need to detect iron core and magnesium alloy interfused firmness in the check, iron core and magnesium when 20N, occur becoming flexible be judged to defective.
Summary of the invention
The purpose of this utility model provides a kind of anti-skidding iron core, overcomes problems of the prior art, improves the qualification rate of magnesium rod.、
The following technical scheme of the concrete employing of the utility model:
A kind of anti-skidding water-heater magnesium rod iron core comprises the magnesium rod, and iron core is coated on the center of magnesium rod, it is characterized in that, is provided with groove in the coating portion of iron core.
Optimized technical scheme is: in the iron core front axle to being arranged with 2 grooves.
According to the prompting of prior art, also has screw thread at the rear portion of described iron core.
Method for making of the present utility model and prior art are basic identical, just stamp out groove in the iron core front portion before the magnesium melt casting.
Compared with prior art, the utility model combines firmly with magnesium alloy, is not easy to become flexible.Through afterburning test, iron core is not loosening under 40N, has improved the qualification rate of magnesium rod greatly.
Description of drawings
Fig. 1 is a structural representation of the present utility model;
Embodiment
Embodiment
As shown in Figure 1, iron core 2 is coated in the middle of the magnesium rod 1, is provided with two symmetric vertically grooves 3 in the front portion of iron core 2.
Iron core 2 of the present utility model is more firm than prior art with combining of magnesium rod 1, has reduced loosening possibility, has improved product percent of pass.

Claims (2)

1. an anti-skidding water-heater magnesium rod iron core comprises the magnesium rod, and iron core is coated on the center of magnesium rod, it is characterized in that, is provided with groove in the coating portion of iron core.
2. anti-skidding water-heater magnesium rod iron core according to claim 1 plays a feature and is, in the iron core front axle to being arranged with 2 grooves.
CN2009200289957U 2009-07-13 2009-07-13 Iron core of magnesium bar of antiskid water heater Expired - Fee Related CN201442979U (en)