CN201399654Y - Electroslag welding arc-quenching device and arc-quenching blocks thereof - Google Patents
Electroslag welding arc-quenching device and arc-quenching blocks thereof Download PDFInfo
- Publication number
- CN201399654Y CN201399654Y CN2009200899642U CN200920089964U CN201399654Y CN 201399654 Y CN201399654 Y CN 201399654Y CN 2009200899642 U CN2009200899642 U CN 2009200899642U CN 200920089964 U CN200920089964 U CN 200920089964U CN 201399654 Y CN201399654 Y CN 201399654Y
- Authority
- CN
- China
- Prior art keywords
- blow
- out piece
- arc
- quenching
- piece
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The utility model discloses an electroslag welding arc-quenching device and arc-quenching blocks thereof. The arc-quenching device is a hollow sleeve body, the inner sleeve surface of the hollow sleeve body forms an arc-quenching pool (11), the sleeve body is formed through detachable abutting joint and enclosing of more than two arc-quenching blocks (12), each arc-quenching block is a tile-shapedbody or a block-shaped body with a concave inner sleeve surface, and the inner sleeve surfaces of the arc-quenching blocks have abutting joint mutually after arc-quenching block enclosing to form thearc-quenching pool (11). Because the sleeve body is formed through detachable abutting joint and enclosing of more than two arc-quenching blocks, the arc-quenching device can be conveniently separated from cooled slag, melted base material and filler metal through disassembling the arc-quenching blocks, even the deformation of the arc-quenching blocks arising from high temperature has no influence on the disassembly and the repeated use effect of the arc-quenching device, the service life is prolonged, the use time is increased, and the use cost is reduced.
Description
Technical field
The utility model relates to the electroslag welding field of steel-structure box ellbeam post, relates to a kind of spark blowout and blow-out piece thereof of electroslag welding in particular.
Background technology
Electroslag welding is when utilizing electric current to pass through slag, and the resistance heat of generation melts mother metal and fills a kind of process that metal welds as thermal source.The resistance heat that produces during electroslag welding is as thermal source as shown in Figure 1, fusing mother metal and fill metal 4 and weld.It also belongs to the scope of automatic weldering.Electroslag welding is generally welded in vertical vertical position of welding, and run-on tab 6, web 7, two baffle plates 2 and a dividing plate 5 constitute welding beads, and spark blowout 8 is arranged on the welding bead top.When electroslag welding begins, produce electric arc earlier between welding wire 1 and run-on tab 6, the solder melts around the heat energy that electric arc produces makes becomes molten slag 3.After treating to form the molten bath of certain depth in the space of molten slag 3 between welded piece and cooling slide block, arc extinction at this moment, transfers the electroslag welding process to by the arc welding process.Because molten slag has certain electric conductivity, when welding current reaches workpiece through the molten bath, produces a large amount of resistance heats, and bath temperature can be remained on more than 1700 ℃, simultaneously, welding wire 1 and welded piece are heated by the molten bath and melt, and form metal bath.During welding, welding wire 1 is constantly sent to and is melted, and molten bath and slag bath rise simultaneously with cooling, below metal cooled and solidified gradually in the molten bath, form weld seam, in the floating superincumbent slag bath of slag and impurity.During the blow-out ending, will guarantee that finally weld seam exceeds spark blowout 8, just welding is finished, be for slag in the slag bath and impurity all being stayed in the spark blowout 8, not influenced composition of weld line to improve welding quality like this.Cut off run-on tab and unnecessary weld seam after the cooling, and reconditioning is smooth consistent with mother metal, and spark blowout 8 is taken down, remove slag to reuse.
Electroslag welding is generally used in steel-structure box ellbeam column production process, and the existing spark blowout 8 that adopts is the overall structure form of round casing.The high-temperature slag, fusing mother metal and the filling metal that rise from welding bead owing to the welding back cause the spark blowout distortion, make spark blowout 8 after welding finishes, be difficult for breaking away from slag, fusing mother metal and the filling metal of cooling, influence recycling effect, reduction of service life, reduce access times, increase use cost.
The utility model content
The purpose of this utility model provides a kind of spark blowout and blow-out piece thereof of electroslag welding, even the distortion of blow-out piece does not influence the recycling effect yet, increases access times, increases the service life, and reduces use cost.
For finishing above-mentioned purpose, the technical scheme of the spark blowout of electroslag welding of the present utility model is: a kind of spark blowout of electroslag welding, this device is hollow sleeve, the interior cover face of hollow sleeve forms the blow-out pond, described body is surrounded by the removable butt joint of plural blow-out piece to be formed, described each blow-out piece is for all having watt body or the piece body of the interior cover face of indent, and the interior cover face of all blow-out pieces surrounds butt joint formation blow-out pond mutually, back at the blow-out piece.
The interior cover face of each blow-out piece is the conical surface, and described blow-out pond is a taper type, and the outer surface of described each blow-out piece is provided with is convenient to the boss that the blow-out piece splits mutually.
Have joint between described adjacent two blow-out pieces, described boss is positioned on the outer surface of the close junction of a blow-out piece wherein.
Described blow-out piece is two, and two blow-out pieces are corresponding half nested structure.
The outer surface of described blow-out piece is provided with distortion-free reinforcement, and reinforcement is provided with along blow-out piece generatrix direction.
The outer surface of described blow-out piece is provided with and steps up device.
Corresponding with the spark blowout of above-mentioned electroslag welding, the blow-out piece of a kind of spark blowout that the utility model adopts, the interior cover face of described each blow-out piece is the conical surface, described blow-out pond is a taper type.
Described blow-out piece is for all having watt body or the piece body of the interior cover face of indent.
One end of the outer surface of described blow-out piece is provided with boss.
The outer surface of described blow-out piece is provided with distortion-free reinforcement, and reinforcement is provided with along blow-out piece generatrix direction.
The spark blowout of the utility model electroslag welding and blow-out piece thereof, because body is surrounded by the removable butt joint of plural blow-out piece and forms, make things convenient for to such an extent that slag, fusing mother metal and the filling metal of spark blowout and cooling separated by splitting the blow-out piece, even blow-out piece Yin Gaowen causes distortion also not influence the dismounting and the recycling effect of spark blowout, prolonged service life, increase access times, reduced use cost.The pyramidal structure of the interior cover face of the piece of blow-out simultaneously can make things convenient for the slag that cools off, fusing mother metal and fill the metal disengaging.
Description of drawings
Fig. 1 is the part sectioned view of the spark blowout of existing electroslag welding;
Fig. 2 is the profile of two and half nested structure blow-out pieces of the slag bath device of the utility model electroslag welding;
Fig. 3 is the vertical view of two and half nested structure blow-out pieces of the spark blowout of the utility model electroslag welding;
Fig. 4 is the profile of half nested structure blow-out piece of the utility model blow-out piece;
Fig. 5 is the vertical view of half nested structure blow-out piece of the utility model blow-out piece.
1 welding wire among the figure, 2 baffle plates, 3 slags, 4 mother metals and filling metal, 5 dividing plates, 6 run-on tabs, 7 webs, 8 spark blowouts, 11 blow-out ponds, 12 blow-out pieces, 13 reinforcements, 14 boss, 15 step up device
The specific embodiment
The present invention will be further described in detail below in conjunction with accompanying drawing.
From the profile of slag bath the device two and half nested structure blow-out pieces of Fig. 2 or the electroslag welding of Fig. 3 the utility model and vertical view as can be known, the spark blowout of the utility model electroslag welding, this device is hollow sleeve, the interior cover face of hollow sleeve forms blow-out pond 11, described body is surrounded by the 12 removable butt joints of two blow-out pieces to be formed, described each blow-out piece 12 is for all having watt body of the interior cover face of indent, and the interior cover face of all blow-out pieces surrounds butt joint formation blow-out pond 11 mutually, back at the blow-out piece.The interior cover face of each blow-out piece 12 is the conical surface, and described blow-out pond 11 is a taper type, and the outer surface of described each blow-out piece 12 is provided with is convenient to the boss 14 that the blow-out piece splits mutually.Have joint between described adjacent two blow-out pieces 12, described boss 14 is positioned on the outer surface of the close junction of a blow-out piece wherein.Described blow-out piece 12 is two, and two blow-out pieces are corresponding half nested structure.The outer surface of described blow-out piece 12 is provided with distortion-free reinforcement 13, and reinforcement 13 is provided with along blow-out piece generatrix direction.The outer surface of described blow-out piece 12 is provided with and steps up device 15.
From the profile of half nested structure blow-out piece of Fig. 4 or Fig. 5 the utility model spark blowout and vertical view as can be known, the blow-out piece of the utility model spark blowout, the interior cover face of described blow-out piece 12 is the conical surface, described blow-out pond 11 is a taper type.Described blow-out piece 12 is for all having watt body of the interior cover face of indent.One end of the outer surface of described blow-out piece 12 is provided with boss 14.The outer surface of described blow-out piece 12 is provided with distortion-free reinforcement 13, and reinforcement 13 is along the 12 generatrix direction settings of blow-out piece.
Blow-out piece in the foregoing description is the half cover watt body of the outside for the cambered surface tiling, can certainly be that the blow-out piece more than three surrounds the formation spark blowout.In addition, the periphery or the lateral surface of blow-out piece can not be cambered surfaces also certainly, but the outer surface of plane or other shape makes the blow-out piece whole for having the blocks of inner concave.
Claims (10)
1, a kind of spark blowout of electroslag welding, this device is hollow sleeve, the interior cover face of hollow sleeve forms blow-out pond (11), it is characterized in that, described body is surrounded by the removable butt joint of plural blow-out piece (12) to be formed, described each blow-out piece (12) is for all having watt body or the piece body of the interior cover face of indent, and the interior cover face of all blow-out pieces surrounds butt joint formation blow-out pond (11) mutually, back at the blow-out piece.
2, according to the spark blowout of the described electroslag welding of claim 1, it is characterized in that, the interior cover face of each blow-out piece (12) is the conical surface, and described blow-out pond (11) is a taper type, and the outer surface of described each blow-out piece (12) is provided with the boss (14) of being convenient to the blow-out piece and splitting mutually.
3, according to the spark blowout of the described electroslag welding of claim 2, it is characterized in that, have joint between described adjacent two blow-out pieces (12), described boss (14) is positioned on the outer surface of the close junction of a blow-out piece wherein.
According to the spark blowout of the described electroslag welding of claim 1, it is characterized in that 4, described blow-out piece (12) is two, two blow-out pieces are corresponding half nested structure.
According to the spark blowout of the described electroslag welding of claim 1, it is characterized in that 5, the outer surface of described blow-out piece (12) is provided with distortion-free reinforcement (13), reinforcement (13) is provided with along blow-out piece generatrix direction.
6, according to the blow-out piece of the spark blowout of the described electroslag welding of claim 1, it is characterized in that the outer surface of described blow-out piece (12) is provided with and steps up device (15).
According to the spark blowout of any described electroslag welding in the claim 1~5, it is characterized in that 7, the interior cover face of described each blow-out piece (12) is the conical surface, described blow-out pond (11) is a taper type.
8, a kind of blow-out piece that is used to constitute the described spark blowout of claim 7 is characterized in that, described blow-out piece (12) is for all having watt body or the piece body of the interior cover face of indent.
According to the blow-out piece of the described spark blowout of claim 8, it is characterized in that 9, an end of the outer surface of described blow-out piece (12) is provided with boss (14).
According to the blow-out piece of the described spark blowout of claim 9, it is characterized in that 10, the outer surface of described blow-out piece (12) is provided with distortion-free reinforcement (13), reinforcement (13) is along blow-out piece (12) generatrix direction setting.