CN201397827Y - 一种锂电池密封绝缘子 - Google Patents
一种锂电池密封绝缘子 Download PDFInfo
- Publication number
- CN201397827Y CN201397827Y CN2009200324700U CN200920032470U CN201397827Y CN 201397827 Y CN201397827 Y CN 201397827Y CN 2009200324700 U CN2009200324700 U CN 2009200324700U CN 200920032470 U CN200920032470 U CN 200920032470U CN 201397827 Y CN201397827 Y CN 201397827Y
- Authority
- CN
- China
- Prior art keywords
- stem
- hole
- lithium battery
- vitreum
- utility
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本实用新型公开了一种锂电池密封绝缘子,包括开有通孔的上盖和通过所述通孔穿插在上盖上的芯柱,通孔内设置有玻璃体,并通过玻璃体对上盖和芯柱进行封接,通孔内且位于玻璃体的下方设置有碳氟化合物。本实用新型结构简单,成本低,密封效果好,能有效保护玻璃体不被腐蚀,从而避免出现锂电池的漏液和短路现象,提高了锂电池的使用寿命。
Description
技术领域
本实用新型涉及一种密封绝缘子,尤其是涉及一种锂电池用密封绝缘子。
背景技术
现有的锂电池密封绝缘子的上盖和芯柱通过玻璃体封接而成,在电池锂被长期储存后,与锂电池电解液直接接触的玻璃体下层会被腐蚀。如法国SAFT公司通过加速老化试验方法对玻璃封接绝缘子进行抗腐蚀测试,将密封绝缘子组装成锂电池后,在150℃下放置7天,结果发现玻璃体表面被腐蚀,绝缘子的气密性降低,小于1.0×10-7m3·Pa/s。产生这种现象的主要原因是:金属锂会还原玻璃中的二氧化硅,且会不断地渗入到玻璃体中,不仅降低玻璃的绝缘性能,更会造成锂电池的漏液。目前,国外解决此类问题主要通过开发不含二氧化硅的抗腐蚀性绝缘玻璃,而这种玻璃的封接温度较高,对设备及工艺条件的要求都非常苛刻;而国内对于适用于锂电池的耐腐蚀性玻璃粉还处于研发阶段,性能还有待于提高。
实用新型内容
本实用新型所要解决的技术问题在于针对上述现有技术中的不足,提供一种锂电池密封绝缘子,其结构简单,成本低,密封效果好,能有效保护玻璃体不被腐蚀,从而避免出现锂电池的漏液和短路现象,提高了锂电池的使用寿命。
为解决上述技术问题,本实用新型采用的技术方案是:一种锂电池密封绝缘子,包括开有通孔的上盖和通过所述通孔穿插在上盖上的芯柱,所述通孔内设置有玻璃体,并通过所述玻璃体对上盖和芯柱进行封接,其特征在于:所述通孔内且位于玻璃体的下方设置有碳氟化合物。
所述碳氟化合物为三氟氯乙烯与乙烯共聚物、四氟乙烯与乙烯共聚物、聚四氟乙烯、聚全氟代乙丙烯、聚三氟氯乙烯、聚偏氟乙烯或聚氟乙烯。
所述玻璃体的主要成分为二氧化硅、氧化铝和氧化硼粉末混合物的烧结体。
所述上盖和芯柱均为金属材质。
所述芯柱的上端设置有T形焊接头,且所述焊接头和芯柱为整体式结构。
本实用新型与现有技术相比具有以下优点:本实用新型上盖与芯柱之间通过玻璃体和碳氟化合物进行双重密封,所以密封性好;另外,由于碳氟化合物具有很强的抗腐蚀性,不会与电解液和金属锂发生反应,并能有效阻止金属锂与玻璃体的接触,因此,本实用新型能有效避免玻璃体被腐蚀,避免出现锂电池的漏液和短路现象,从而有效提高锂电池的使用寿命。
下面通过附图和实施例,对本实用新型的技术方案做进一步的详细描述。
附图说明
图1为本实用新型第一种具体实施方式的结构示意图。
图2为本实用新型第二种具体实施方式的结构示意图。
附图标记说明:
1-上盖; 2-芯柱; 3-玻璃体;
4-碳氟化合物。
具体实施方式
如图1和图2所示,本实用新型包括开有通孔的上盖1和通过通孔穿插在上盖1上的芯柱2,在通孔内上下设置有玻璃体3,在通孔内且位于玻璃体3的下方设置有碳氟化合物4,并通过玻璃体3和碳氟化合物4对上盖与芯柱进行双重密封。其中,碳氟化合物4为三氟氯乙烯与乙烯共聚物、四氟乙烯与乙烯共聚物、聚四氟乙烯、聚全氟代乙丙烯、聚三氟氯乙烯、聚偏氟乙烯或聚氟乙烯,玻璃体3的主要成分为二氧化硅、氧化铝和氧化硼粉末混合物的烧结体。
上盖1和芯柱2均为金属材质。如图2所示,为了适应不同锂电池密封绝缘子的需要,且便于焊接,在芯柱2的上端设置有T形焊接头,焊接头和芯柱2为整体式结构。
本实用新型的生产过程为:将上盖1、芯柱2以及成形的玻璃体3装配在石墨模具中,将该石墨模具放入高温炉中烧结,在高温环境下,玻璃体3与上盖1和芯柱2熔封在一起,待冷却后,去除上盖1的表面氧化皮和玻璃体3的表面粘黑,最后将碳氟化合物4热压在上盖1通孔内的玻璃体3下方。
以上所述,仅是本实用新型的较佳实施例,并非对本实用新型作任何限制,凡是根据本实用新型技术实质对以上实施例所作的任何简单修改、变更以及等效结构变换,均仍属于本实用新型技术方案的保护范围内。
Claims (3)
1.一种锂电池密封绝缘子,包括开有通孔的上盖(1)和通过所述通孔穿插在上盖(1)上的芯柱(2),所述通孔内设置有玻璃体(3),并通过所述玻璃体(3)对上盖(1)和芯柱(2)进行封接,其特征在于:所述通孔内且位于玻璃体(3)的下方设置有碳氟化合物(4)。
2.按照权利要求1所述的一种锂电池密封绝缘子,其特征在于:所述上盖(1)和芯柱(2)均为金属材质。
3.按照权利要求2所述的一种锂电池密封绝缘子,其特征在于:所述芯柱(2)的上端设置有T形焊接头,且所述焊接头和芯柱(2)为整体式结构。