CN201346615Y - 改善压铸料杯 - Google Patents
改善压铸料杯 Download PDFInfo
- Publication number
- CN201346615Y CN201346615Y CNU2008200728818U CN200820072881U CN201346615Y CN 201346615 Y CN201346615 Y CN 201346615Y CN U2008200728818 U CNU2008200728818 U CN U2008200728818U CN 200820072881 U CN200820072881 U CN 200820072881U CN 201346615 Y CN201346615 Y CN 201346615Y
- Authority
- CN
- China
- Prior art keywords
- material cup
- drift
- cup
- improved die
- casting material
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种改善压铸料杯,涉及一种铸铝设备的改进,其特征是:在料杯腔体的前端开有环形凹槽。其有益效果是:大大缓解了冲头和料杯研死或将料杯涨裂问题,延长了料杯和冲头的使用寿命,降低了加工成本,提高了劳动效率。
Description
技术领域
本实用新型属于机械热加工技术领域,涉及一种铸铝设备的改进。
背景技术
料杯和冲头是铝制压铸过程关键易损部件,且占生产成本较高。在压铸行业中,夹冲头及料杯和冲头的使用寿命低,一直困扰着压铸生产的正常进行。
目前国内外采用的冲头材料有H13耐热钢,球墨铸铁和铍青铜。在压铸机压射杆和料杯同心度正常,料杯孔径、圆度、粗糙度以及工艺参数等合理的情况下,H13耐热钢一般寿命在1000次以下,球墨铸铁寿命在500次以下,铍青铜寿命在7000-10000次左右。如果未满足上述理想的工作状态,那么冲头的磨损将急剧恶化,寿命大幅度降低。H13耐热钢和球墨铸铁对料杯的损害特别严重,有时冲头和料杯研死或将料杯涨裂,造成料杯报废。虽然铍青铜对料杯的伤害较轻,但铍青铜价格较贵,每公斤300元,一个直径为80的冲头需要1000多元。近些年来,有些机构在研究镶嵌铍青铜环技术以降低成本,但该技术结构复杂,要求操作过程非常严格,料杯恒温冷却,价格昂贵,一个冲头价格为2万多元,一般压铸厂使用也不理想。由于冲头和料杯的研伤,阻力加大,影响压射速度。可见冲头和料杯对压铸生产能否正常进行起到至关重要的作用。
发明内容
本实用新型的目的是:提供一种改善压铸料杯,它可有效地解决了冲头和料杯研死或将料杯涨裂,造成料杯报废的问题。
本实用新型的技术方案是:在料杯腔体的前端开有环形凹槽。
本实用新型的有益效果是:大大缓解了冲头和料杯研死或将料杯涨裂问题,延长了料杯和冲头的使用寿命,降低了加工成本,提高了劳动效率。以一般压铸企业为例,冲头料杯成本占生产成本的1%左右,使用本方法后,可降低到0.3%。生产规模年产在2000吨铝合金左右的压铸厂每年可降低成本40万元人民币。
附图说明
图1是本实用新型的结构剖视图。
具体实施方式
下面结合附图对本实用新型做进一步描述:
如图所示,1是料杯、2是入料口、3是模具接口、4是环形凹槽。
料杯和冲头损坏的主要原因是间隙问题。压铸生产用料杯和冲头是在高低温循环变化条件下做高速往复运动,料杯和冲头的热平衡没有办法控制,冲头和料杯常温下间隙为0.1毫米左右,多个循环后料杯温度逐渐升高,沿轴线方向内孔不均匀变大,形成锥度角(料杯前端变化程度大,后端变化程度小)。这种情况下,在压射近于终止时,冲头与料杯之间钻入铝液并迅速凝固包裹在冲头外面,变相导致冲头变大,冲头回程时,必然将料杯研伤或卡死在料杯里,导致压铸生产过程的中断。本方案靠料杯与冲头的自调整能有效解决其间隙问题:在料杯1前端一段范围加工环形凹槽4。
根据料杯1的大小确定环形凹槽4的宽窄和深度,这样在压射时在料杯1前端自然形成一种合金套,该套内径与冲头匹配,形成过渡配合,间隙大了自然补差,且该合金硬度低,有良好的导热性和耐磨性。通过该方法成功的解决了冲头与料杯1因间隙不当而导致的研、夹、卡等现象的发生,即保护了料杯1,又提高了冲头的使用寿命。
Claims (1)
1、一种改善压铸料杯,包括料杯,其特征是:在料杯腔体的前端开有环形凹槽。