CN201260962Y - Streamlined ceramic valley peak regular corrugated filler - Google Patents

Streamlined ceramic valley peak regular corrugated filler Download PDF

Info

Publication number
CN201260962Y
CN201260962Y CNU2008201375442U CN200820137544U CN201260962Y CN 201260962 Y CN201260962 Y CN 201260962Y CN U2008201375442 U CNU2008201375442 U CN U2008201375442U CN 200820137544 U CN200820137544 U CN 200820137544U CN 201260962 Y CN201260962 Y CN 201260962Y
Authority
CN
China
Prior art keywords
streamlined
liquid
raised line
filler
raised lines
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNU2008201375442U
Other languages
Chinese (zh)
Inventor
刘裕秋
刘辉
刘钢
刘玲
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CNU2008201375442U priority Critical patent/CN201260962Y/en
Application granted granted Critical
Publication of CN201260962Y publication Critical patent/CN201260962Y/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The utility model discloses streamlined ceramic dip peak structural wave packing. A streamlined ceramic dip peak structural wave packing body (1) is formed by mutually crossing and overlapping ceramic plates (3) formed by inclined raised lines (6) which are arranged at intervals, channels (2) are formed among the raised lines, the channels which are formed among the raised lines and are positioned at the upper end and the lower end of the packing body are arranged vertically, and the vertically arranged channels are connected with channel joints arranged aslant in a smooth transition way. Grooves (4) are arranged on the raised lines (6) and among the raised lines, through holes (5) are arranged on the grooves, and the grooves are arranged crossly. Liquid can vertically flow from top to bottom when flowing the packing body, the flowing direction can not be changed, the flowing resistance is greatly reduced, the liquid flows more smoothly and uniformly, and the packing pore ratio is increased; when the liquid is rectified and separated, the liquid flowing resistance is lowered, the flowing direction is dispersed in an eddy flow state, the time of liquid water droplet analysis is improved, and the rectifying and the separating effects of the liquid are improved.

Description

Streamlined pottery paddy peak regular corrugation filler
Technical field
The utility model relates in the industrial tower equipment uses filler, especially relates to the streamlined pottery paddy peak regular corrugation filler that industrial rectifying knockout towers such as being used for chemical industry, petrochemical industry uses.
Background technology
Current, the filler that is used for drying tower, scrubbing tower and the rectifying knockout tower equipment of industry such as chemical industry, petrochemical industry has varied, and be used for the filler of rectifying knockout tower, because the requirement of rectifying separation process technique is mostly used the structured packing that is formed by the some interlaced stacks of corrugated ceramic wafer to carry out rectifying at present and is separated.But when liquid separates in rectifying, because corrugated regular filler is when piling up mutually up and down, flow channel on its filler contact-making surface is shape and vertical interlaced linearly, thereby the flow direction of liquid between the filler body layer will produce change, flow resistance increases, liquid flowing velocity between the filler body layer is descended, cause the flow distribution of liquid on the total that the filler body layer forms inhomogeneous, thereby reduced the liquid distillation separating effect.Be that liquid is identical with corrugated plate ramp way direction at the flow direction of existing corrugated regular filler inside again, it is little to produce the tendency that flows at the inner above-below direction liquid of filler, when liquid flows in the ripple packing body interior, can not circulate mutually on the inner above-below direction of its filler body, flow to more single, liquid flowing resistance is increased, liquid is few at the inner water spot analysis number of times that forms of ripple packing, liquid can not be in the inner turbulent condition that interweaves in length and breadth uniformly that forms of ripple packing, it is few that liquid distillation separates number of times, reduced the clear cut of liquid equally from effect.
The utility model content
The purpose of this utility model is to provide a kind of not only rectifying good separating effect, and the high streamlined pottery paddy peak regular corrugation filler of rectifying separative efficiency.
The technical scheme that the technical problems to be solved in the utility model is taked is: described streamlined pottery paddy peak regular corrugation filler body is formed by the interlaced stack of the formed ceramic wafer monomer of the skewed raised line that is set in distance, be formed with passage between the described raised line, the channel vertical setting that is positioned at the filler body top and bottom that forms between the described raised line, the vertically disposed passage in described filler body top and bottom links to each other with the passage junction rounding off that the filler body intermediate, inclined is provided with.
For further improving the rectifying separating effect of liquid, increase the water spot analysis number of times of liquid in filler inside, between raised line top and raised line, be provided with groove, groove is provided with through hole, and the groove space is crisscross arranged; Also can be provided with convex or/and through hole by raised line two canting walls.
The utility model is because with the formed channel vertical setting that is positioned at the filler body top and bottom between the inclination raised line, and with raised line between formed skewed passage rounding off be connected, when liquid is flowed through between the filler body, liquid can vertically flow from top to bottom, flow direction can not change, and flow resistance reduces greatly, and liquid flow is more unimpeded, liquid distribution is more even, thereby can improve the liquid distillation separating effect; Be owing to being provided with groove between raised line top that tilts at the ceramic wafer monomer and the raised line again, groove is provided with through hole, or the raised line two side is provided with convex or/and through hole, thereby go alone the structured packing inside that body stack forms by the corrugated ceramic wafer of polylith and on all directions, can both communicate mutually, its inside can form the netted pore space structure of peak nest, its filler porosity increases, when liquid distillation separates, reduced liquid flowing resistance, flow to and disperse to be turbulent condition, improve the number of times of liquid water spot analysis, further improved the rectifying separating effect of liquid.
Description of drawings
Fig. 1 is the front view of first kind of structure of the utility model,
Fig. 2 is the vertical view of first kind of structure of the utility model,
Fig. 3 is the front view of second kind of structure of the utility model,
Fig. 4 is the A-A profile of Fig. 3,
Fig. 5 is the profile of the third structure of the utility model.
Filler body 2, passage 3, ceramic wafer monomer 4, groove 5, through hole 6, raised line 7, convex in the drawings, 1,
The specific embodiment
Embodiment 1, be specifically described in conjunction with Fig. 1 and Fig. 2, described streamlined pottery paddy peak regular corrugation filler body 1 is by bonding the forming of eight ceramic wafer monomers, 3 stacks, filler body 1 is cuboid, the also bonding formation of other interlaced stack of polylith ceramic wafer monomer, be arranged at intervals with skewed raised line 6 on the described ceramic wafer monomer 3, described raised line 6 cross sections are triangular in shape, described ceramic wafer monomer cross section is corrugated, be formed with passage 2 between the described raised line 6, the passage that is positioned at the filler body top and bottom 2 that forms between the described skewed raised line vertically is provided with, and the vertically disposed passage in described filler body top and bottom links to each other with the circular arc rounding off with the passage junction that the filler body intermediate, inclined is provided with.
Embodiment 2, be specifically described in conjunction with Fig. 3 and Fig. 4, present embodiment 2 described streamlined pottery paddy peak regular corrugation filler bodies are by bonding the forming of ten ceramic wafer monomers, 3 stacks, filler body 1 is square, the also bonding formation of other interlaced stack of polylith ceramic wafer monomer, be arranged at intervals with skewed raised line 6 on the described ceramic wafer monomer, described raised line 6 cross sections are triangular in shape, described ceramic wafer monomer cross section is corrugated, be formed with passage 2 between the described raised line 6, the passage that is positioned at the filler body top and bottom 2 that forms between the described skewed raised line vertically is provided with, the vertically disposed passage in described filler body top and bottom is connected with the circular arc rounding off with the passage junction that the filler body intermediate, inclined is provided with, be provided with groove 4 at skewed raised line top, also be provided with groove 4 between skewed raised line, described groove is a rectangle, in groove, offer two through holes 5, the groove space is provided with, and described through hole is a circular hole, also can be tri-angle-holed or polygonal hole.
Embodiment 3, describe in conjunction with Fig. 5, present embodiment 3 described streamlined pottery paddy peak regular corrugation filler primary structures are identical with embodiment 1, difference is: be arranged at intervals with convex 7 on the two side of raised line 6, also space set has through hole 5, or on the raised line two side, being arranged at intervals with convex and through hole simultaneously, described convex 7 is circular, also can be triangle or polygon.

Claims (5)

1, streamlined pottery paddy peak regular corrugation filler, it is characterized in that: described streamlined pottery paddy peak regular corrugation filler body (1) is formed by the interlaced stack of the formed ceramic wafer monomer of skewed raised line (6) (3) that is set in distance, be formed with passage (2) between the described raised line, the channel vertical setting that is positioned at the filler body top and bottom that forms between the described raised line, the vertically disposed passage in described filler body top and bottom links to each other with the passage junction rounding off that the filler body intermediate, inclined is provided with.
2, streamlined according to claim 1 pottery paddy peak regular corrugation filler is characterized in that: be provided with groove (4) between raised line (6) top and raised line, be provided with through hole (5) in groove, the setting that is interspersed of groove space.
3, the ceramic paddy of streamlined according to claim 1 peak regular corrugation filler is characterized in that: be arranged at intervals with convex (7) or/and through hole (5) on the two side of raised line (6).
4, according to claim 2 or 3 described streamlined pottery paddy peak regular corrugation fillers, it is characterized in that: described through hole (5) is circular hole, tri-angle-holed or polygonal hole.
5, the ceramic paddy of streamlined according to claim 3 peak regular corrugation filler, it is characterized in that: described convex (7) is circle, triangle or polygon.
CNU2008201375442U 2008-09-06 2008-09-06 Streamlined ceramic valley peak regular corrugated filler Expired - Fee Related CN201260962Y (en)