CN1613401A - Machining method for ox horn comb - Google Patents

Machining method for ox horn comb Download PDF

Info

Publication number
CN1613401A
CN1613401A CN 200410040918 CN200410040918A CN1613401A CN 1613401 A CN1613401 A CN 1613401A CN 200410040918 CN200410040918 CN 200410040918 CN 200410040918 A CN200410040918 A CN 200410040918A CN 1613401 A CN1613401 A CN 1613401A
Authority
CN
China
Prior art keywords
comb
horn
twice
angle
blank
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200410040918
Other languages
Chinese (zh)
Inventor
段首生
谭必达
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 200410040918 priority Critical patent/CN1613401A/en
Publication of CN1613401A publication Critical patent/CN1613401A/en
Pending legal-status Critical Current

Abstract

A technology for manufacturing the comb with cattle horn includes such steps as choosing raw cattle horn, splitting, trimming, heating in oil, mechanical flatening, drawing, sawing to obtain blank, machining teeth, abrasing, coarse polishing and fine polishing.

Description

The processing method of ox horn comb
Technical field
The present invention relates to a kind of processing method of small stores, particularly is the processing method of the ox horn comb of raw material with natural ox angle.
Technical background
It is 96101167.X that the Chinese patent net discloses a kind of application number, name is called the patent application of " a kind of preparation method of horn comb ", with the patent No. be 01 1 08785.4, name is called the patent of invention of " yak horn comb and processing method ", and preceding application is not enough, and point is: the one, and heating-up temperature is unexpectedly up to " 280-380 ℃ " in the mould of the 3rd procedure! Similar technical staff knows, gets final product deliquescing in the boiling water of ox horn about 100 ℃, if comb is deformable.The 280-380 ℃ of former organic matter that just can destroy ox horn completely makes its raw material lose toughness and becomes fragile, and the broach that causes processing fractures easily.Two is that the 4th procedure " stamps out broach ", has had a fantastic idea only not! Similar technical staff knows that ox horn matter is the fiber plastid, and its fiber is crisscross composition, and it is not a sheet metal, and the metallographic unanimity is sheared or punching press all can.And ox horn matter is similar to multilayer layer and hardens and be combined in one, shears or punching press is absolutely not.
The deficiency point of consequent patent is that the yak horn raw material more and more lacks, and its three big reason that consumes raw material is: the one, and the advantage of yak horn comb and fair margin of profit make manufacturer grab raw material, jack screwing; The 2nd, make various handicrafts with yak horn, consume part material again; The 3rd, it is refreshing ox that the compatriot of Tibetan looks yak, after death yak horn and yak skulls is plugged together, and makes a kind of totem or totem culture handicraft.Above-mentioned three reasons have been arranged, and original in addition yak is grown in the plateau cold zone exactly, and it is slower to grow up, and has only the western part of China highlands just to have.Along with original storage consumption of raw materials is most soon, new growth is slow again, can expect that the yak horn raw material will be more and more rare or more and more expensive.
Summary of the invention
The purpose of this invention is to provide a kind of raw material is easy to get, the comb that processes can keep natural lines of original ox horn and color, and light and comfortable feel are different from the yak horn comb processing method, have ox angle processing characteristic, the processing method of ox horn comb.
For reaching technical scheme that above-mentioned purpose adopts is that the manufacturing procedure of ox horn comb is
1, selects materials for twice: be for the first time to select to pick out the angle material that rots; For the second time be since ox angle material not as the yak horn material, though raw material is easy to get, angle material size is relatively shorter and wall is thin, processing comb will cut away two brilliance mouths thin part and the little part of the top of the horn.
2, twice blanking: for the first time be that the ox angle material that first procedure is selected is cut open is half-and-half or quarter-wave plate; For the second time be that the angle material that descends is for the first time repaired, or scrape or grind, make the thickness basically identical of its material.
3, heating binder: the method for heating be will trim the angle material put into 80-200 ℃ oil cauldron and boiled 3-18 minute; Put into purl machine after from oil cauldron, taking out the angle material, before cooling, flatten the angle material straight.
4, line sampling: on the straight angle material of pressing,, delineate out the shape line of comb according to raw material shape and requirement; Shape line according to comb on circular saw cuts away clout, extracts the blank of comb.To the blank finishing of polishing.
5, twice tooth punching: be that the comb blank is clamped on the material handling shaft for the first time, fitly card full encloses always; What install on the knife rest is circular saw or Milling cutter; Add man-hour, material axle and circular saw or Milling cutter be rotation simultaneously all, and depth of cut and tooth pitch, are controlled by the scale of coordinate in length and breadth on the gulleting machine according to the needs of comb dimensioned apart from size; For the second time be primary base just to be repaired out with burr between the broach and broach point with sheave, become the blank of comb with emery disc.
6, twice polishing: be rough polishing for the first time, on artificial full-disk buff, add 500 order quartz sands and polish; Be finishing polish for the second time, on pure white cloth, add antiscuffing paste and polish.
Be finished product through the comb after the finishing polish, passer, packing warehouse-in.
The invention has the advantages that:
1, raw material is easy to get, price steadiness.All parts of the country and a large amount of output oxes in Yadu, the southeast and ox angle needn't be worried on pushing up price.
2, the present invention's the 3rd procedure can guarantee the ox horn material in heating process, and grease is to the compensation of ox horn water evaporates or moisten, and makes ox horn in the technology that flattens, and can not produce breach because the ox horn material is dry, causes higher scrappage, has increased the comb cost.This be the ox horn material in process, the technical staff is had a headache and unsolved technical barrier.
3, the feature of the 5th procedure is mechanical tooth punching, and processing work and cutter rotate the still utilization first of method of the tooth punching first time of processing horn comb simultaneously.On cloth wheel, add corner angle that diamond dust grinds off corner angle and broach point between the broach as the tooth punching second time, make between broach and the broach point slick and sly, can not damage hair and scalp especially beyond example.
4, the 6th procedure adopts the twice polishing technology, this method comb of processing can keep natural lines of original ox horn and color, gloss and comfortable feel, original ox horn comb matter does not suffer any destruction, has kept all characteristics at natural ox angle.
5, because the former organic matter of horn comb does not suffer any destruction, common people among the people and traditional Chinese medical science Tibetan medicine are accustomed to being used for popular treatment for sunstroke by scraping the patient's neck, chest or back.Only original horn comb processing method is coarse, during popular treatment for sunstroke by scraping the patient's neck, chest or back easily with the patient skin scratch, scrape the pain.
Concrete real-time mode
1, selects materials for twice: be for the first time to select to pick out the angle material that rots; For the second time be since ox angle material not as the yak horn material, though raw material is easy to get, angle material size is relatively shorter and wall is thin, processing comb will cut away the thin part of mouth and the little part of the top of the horn of two brilliance.
2, twice blanking: for the first time be that the ox angle material that first procedure is selected is cut open is half-and-half or quarter-wave plate; For the second time be that the angle material that descends is for the first time repaired, or scrape or grind, make the thickness basically identical of its angle flitch.
3, heating binder: the method for heating be will trim the angle material put into 80-200 ℃ oil cauldron and boiled 3-18 minute; Put into purl machine after from oil cauldron, taking out the angle material, before cooling, flatten the angle material straight.
4, line sampling: on the straight angle material of pressing,, delineate out the shape line of comb according to raw material shape and requirement; Shape line according to comb on circular saw cuts away clout, extracts the blank of comb.To the blank finishing of polishing.
5, twice tooth punching: be that the comb blank is clamped on the material handling shaft for the first time, fitly card full encloses always; What install on the knife rest is circular saw or Milling cutter; Add man-hour, material axle and circular saw or Milling cutter be rotation simultaneously all, and depth of cut and tooth pitch, are controlled by the scale of coordinate in length and breadth on the gulleting machine according to the needs of comb dimensioned apart from size; For the second time be primary base just to be repaired out with burr between the broach and broach point with sheave, become the blank of comb with emery disc.
6, twice polishing: be rough polishing for the first time, on artificial full-disk buff, add 500 order quartz sands and polish; Be finishing polish for the second time, on pure white cloth, add antiscuffing paste and polish.

Claims (5)

1, a kind of processing method of ox horn comb is characterized in that operation is that to select materials for twice be to pick to have selected ox angle material; Twice blanking is to cut open and the angle of trim material; The heating binder is heating and machine pressing in the oil; The line sampling is to mark the comb sample to saw out the comb blank; Twice tooth punching is to be trimmed to the comb blank with gulleting machine processing and emery disc polishing; Twice thick, finishing polish goes out finished product.
2, according to the processing method of claim 1 ox horn comb, it is characterized in that described heating binder be will trim the angle material put into 80-200 ℃ oil cauldron and boiled 3-18 minute; Put into purl machine after from oil cauldron, taking out the angle material, before cooling, flatten the angle material straight.
3, according to the processing method of claim 1 ox horn comb, it is characterized in that described line sampling be on the material of angle according to raw material shape and requirement, delineate out the shape line of comb; Shape line according to comb on circular saw cuts away clout, extracts the blank of comb.
4, according to the processing method of claim 1 ox horn comb, it is characterized in that described twice tooth punching one is that the comb blank is clamped on the material handling shaft, circular saw or Milling cutter add man-hour, all rotation simultaneously, depth of cut and tooth pitch are controlled by the scale of coordinate in length and breadth on the gulleting machine apart from size; For the second time be primary base just to be repaired out with burr between the broach and broach point with sheave, become the blank of comb with emery disc.
5, according to the processing method of claim 1 ox horn comb, it is characterized in that described twice polishing: be rough polishing for the first time, on artificial full-disk buff, add 500 order quartz sands and polish; Be finishing polish for the second time, on pure white cloth, add antiscuffing paste and polish.
CN 200410040918 2004-10-26 2004-10-26 Machining method for ox horn comb Pending CN1613401A (en)