CN1611908A - Heat tube sealing method - Google Patents

Heat tube sealing method Download PDF

Info

Publication number
CN1611908A
CN1611908A CN 200310104685 CN200310104685A CN1611908A CN 1611908 A CN1611908 A CN 1611908A CN 200310104685 CN200310104685 CN 200310104685 CN 200310104685 A CN200310104685 A CN 200310104685A CN 1611908 A CN1611908 A CN 1611908A
Authority
CN
China
Prior art keywords
substrate tube
opening port
sealing method
hollow substrate
mouth
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 200310104685
Other languages
Chinese (zh)
Inventor
骆俊光
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yanuo Superconducting Sci & Tech Co Ltd
Original Assignee
Yanuo Superconducting Sci & Tech Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yanuo Superconducting Sci & Tech Co Ltd filed Critical Yanuo Superconducting Sci & Tech Co Ltd
Priority to CN 200310104685 priority Critical patent/CN1611908A/en
Publication of CN1611908A publication Critical patent/CN1611908A/en
Pending legal-status Critical Current

Abstract

This invention provides a kind of heat-pipe sealing method, which is suitable to hollow base pipe with a open mouth. It is used for air removal after filling a working fluid. The sealing method is that make the open mouth of the hollow base pipe that has been filled and air removed be deformed in order to seal the open mouth. Then high energy of a bundle of laser is irradiated to the deformed part of the open mouth of the base pipe, at the same time the end segment of the deformed part is broken and weld in order to achieve the sealing and air-tight result.

Description

The mouth-sealing method of heat pipe
(1) technical field
The present invention relates to a kind of heat pipe, particularly relate to a kind of mouth-sealing method of heat pipe.
(2) background technology
A kind of manufacture method of existing heat pipe, be that first construction one has an opening port and the metal hollow substrate tube that defines an inner cavity chamber, again with an amount of working fluid after this opening port injects this hollow substrate tube, seal (opening port that promptly seals this hollow substrate tube) after this hollow substrate tube is vacuumized.
Wherein, the above-mentioned mouth-sealing method that should have heat pipe now is to comprise the following step:
(A) as shown in Figure 1, 2, after earlier the opening port 111 of this hollow tube 11 being processed by the facility clamping, make it form the basic kenel of a heat pipe 10.
(B) shown in Fig. 2,3, then utilize facility to cut off, and after cutting off, bestow spot welding (solder joint 12 as shown in Figure 4) and seal airtight effect to reach through the clamping processing flat section position, top 1121 of sealing end 112 (promptly sealing the mouth position) that operation produced.
The opening port 111 of above-mentioned hollow tube 11 in regular turn via clamping distortion, cut off this and seal three kinds of procedure of processings such as end 112 and this opening port 111 of spot welding driving fit after, seal airtight effect though can reach, but, the dealer is as satisfying, desire sealing in the manufacture field at heat pipe, the procedure of processing of seeking more to simplify is to reduce man-hour, manufacturing cost.
(3) summary of the invention
Purpose of the present invention is that a kind of mouth-sealing method of simplifying work flow with the heat pipe that reduces cost is being provided.
The mouth-sealing method of heat pipe of the present invention is applicable to that one has the hollow substrate tube of an opening port, be filled into a working fluid in this hollow substrate tube after, carry out the degasification operation, this mouth-sealing method comprises the following step:
(A) make opening port produce distortion, to seal this opening port through over packing and the post-job hollow substrate tube of degasification; And
(B) with the high energy radiation of the laser light deformation place at the opening port of this hollow substrate tube, and the end segment that can sweep the deformation place of disconnected, this hollow substrate tube of welding simultaneously reaches and seals airtight effect.
For further specifying above-mentioned purpose of the present invention, design feature and effect, the present invention is described in detail below with reference to accompanying drawing.
(4) description of drawings
Fig. 1 is an action diagram of the mouth-sealing method of an existing heat pipe, and an opening port of clamping facility desire clamping one hollow substrate tube is described.
Fig. 2 is an action diagram of the mouth-sealing method of this existing heat pipe, and the opening port of this clamping facility clamping in this hollow substrate tube is described.
Fig. 3 is an action diagram of the mouth-sealing method of this existing heat pipe, illustrates to utilize facility to cut off through the clamping processing flat end (promptly sealing the mouth position) of sealing that operation produced.
Fig. 4 is an action diagram of the mouth-sealing method of this existing heat pipe, illustrates that spot welding is bestowed in the flat end of sealing of this heat pipe after cutting off, and seals airtight effect to reach.
Fig. 5 is the flow chart of a preferred embodiment of the mouth-sealing method of heat pipe of the present invention.
Fig. 6 is not complete action diagram of this preferred embodiment, illustrates that an opening port of this heat pipe is the flat distortion of folder.
Fig. 7 is not complete action diagram of this preferred embodiment, illustrates that the opening port of this heat pipe is the bending distortion of the flat back of folder.
Fig. 8 is not complete action diagram of this preferred embodiment, illustrates that the opening port of this heat pipe is torsional deformation.
(5) specific embodiment
For convenience of description, at following embodiment, similar elements is to represent with same numeral.
Shown in Fig. 5,6, one preferred embodiment of the mouth-sealing method of heat pipe of the present invention, be applicable to that one has the hollow substrate tube 20 of an opening port 21, after in this hollow substrate tube 20, being filled into a working fluid (figure does not show), carry out the degasification operation, because of above-mentioned through the post-job hollow substrate tube of over packing and degasification 20 with existing identical, and be not to be key character of the present invention, so no longer describe in detail at this; And mouth-sealing method of the present invention comprises step 30,40.
In step 30, be just to be out of shape, to seal this opening port 21 through opening port 21 generations of over packing and the post-job hollow substrate tube 20 of degasification; In the present embodiment, this opening port 21 can be the flat back of the flat distortion of folder, folder as shown in Figure 7 bending distortion as shown in Figure 6, or three kinds of kenels such as torsional deformation as shown in Figure 8; As shown in Figure 6, when pressing from both sides flat distortion, be the pipe shaft of fixing this hollow substrate tube 20 earlier, utilize flat this opening port 21 of anchor clamps (figure does not show) folder again, reach the flat distortion of folder, in addition, as shown in Figure 7, if opening port 21 bendings that further will be through pressing from both sides flat distortion then can be finished the bending distortion of the flat back of folder; As shown in Figure 8, when carrying out torsional deformation, be the pipe shaft of fixing this hollow substrate tube 20 earlier, utilize rotation type anchor clamps (figure does not show) to reverse this opening port 21 again, reach torsional deformation.
Shown in Fig. 5,6, in step 40, a laser light that provides a laser aid (figure does not show) is radiated at the deformation place 22 of the opening port 21 of this hollow substrate tube 20, the high-energy of this laser light of mat and the end segment that can sweep the deformation place 22 of disconnected, this hollow substrate tube 20 of welding is simultaneously sealed airtight effect to reach.
By this, the mouth-sealing method of heat pipe of the present invention is to comprise: after making opening port 21 distortion, reach with laser light and to sweep two procedure of processings such as deformation place 22 disconnected, this hollow substrate tube 20 of welding, reach and seal airtight effect, its mouth-sealing method that is different from the existing heat pipe shown in Fig. 1 ~ 4 needs via the clamping distortion, cuts off and three kinds of procedure of processings such as spot welding driving fit, not only need use three kinds of machining machine and tools and when taking a lot of work because of processing is complicated, mouth-sealing method of the present invention relatively only need use two kinds of facility, and tool processing is simple and easy and save man-hour, can reduce eventually and seal cost.
Though the present invention describes with reference to current specific embodiment, but those of ordinary skill in the art will be appreciated that, above embodiment is used for illustrating the present invention, under the situation that does not break away from spirit of the present invention, also can make the variation and the modification of various equivalences, therefore, as long as variation, the modification to the foregoing description all will drop in the scope of claims of the present invention in connotation scope of the present invention.

Claims (4)

1. the mouth-sealing method of a heat pipe is applicable to that one has the hollow substrate tube of an opening port, be filled into a working fluid in this hollow substrate tube after, carry out the degasification operation, it is characterized in that this mouth-sealing method comprises the following step:
(A) make opening port produce distortion, to seal this opening port through over packing and the post-job hollow substrate tube of degasification; And
(B) with the high energy radiation of the laser light deformation place at the opening port of this hollow substrate tube, and the end segment that can sweep the deformation place of disconnected, this hollow substrate tube of welding simultaneously reaches and seals airtight effect.
2. as the mouth-sealing method of claim 1 a described heat pipe, it is characterized in that:
The opening port of the hollow substrate tube of step (A) is the flat distortion of folder.
3. as the mouth-sealing method of claim 1 a described heat pipe, it is characterized in that:
The opening port of the hollow substrate tube of step (A) is the bending distortion of the flat back of folder.
4. as the mouth-sealing method of claim 1 a described heat pipe, it is characterized in that:
The opening port of the hollow substrate tube of step (A) is a torsional deformation.
CN 200310104685 2003-10-30 2003-10-30 Heat tube sealing method Pending CN1611908A (en)