CN1432622A - Black oil-displacing agent and its production process - Google Patents
Black oil-displacing agent and its production process Download PDFInfo
- Publication number
- CN1432622A CN1432622A CN 02102733 CN02102733A CN1432622A CN 1432622 A CN1432622 A CN 1432622A CN 02102733 CN02102733 CN 02102733 CN 02102733 A CN02102733 A CN 02102733A CN 1432622 A CN1432622 A CN 1432622A
- Authority
- CN
- China
- Prior art keywords
- displacing agent
- oil
- black oil
- coal
- powder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The black oil-displacing agent has the percentage composition of: sodium hydroxide and/or sodium silicate 15-25 wt%; nonly phenol 0-20 wt%; polyacrylamide 0.005-0.5 wt%; and coal gangue powder or efflorescent coal powder the rest. The production process includes the following steps: throwing coal gauge powder or efflorescent coal powder into reactor; adding sodium hydroxide and/or sodium silicate under stirring for reaction at 30-70 deg.C for 3-5 hr; and adding nonyl phenol and polyacrylamide under stirring for mixing to obtain the black oil-displacing agent. The present invention has the features of low cost, simple production process, simple usage and high efficiency. Its use in oil field can raise the oil yield and oil recovering rate greatly and lower water content in oil well.
Description
One, technical field:
Oil-displacing agent that the present invention relates to use on the oil field and production method thereof are a kind of black oil-displacing agents.
Two, background technology:
The oil-displacing agent cost that uses on the oil field is higher at present, thereby is difficult to apply.
Three, summary of the invention:
The invention provides low black oil-displacing agent of a kind of cost and production method thereof.
This black oil-displacing agent consists of by weight percentage: A, 15 to 25% sodium hydroxide, perhaps 15 to 25% water glass, perhaps 10 to 22% sodium hydroxide and 5 to 10% water glass; B, 0 to 20% appoint basic phenolic ether; C, 0.005 to 0.5% polyacrylamide; The coal drystone powder of D, surplus or weathering coal dust.
Above-mentioned coal drystone powder or weathering coal dust are 40 to 80 purpose powder.
This black oil-displacing agent production method is to carry out according to the following steps: the coal drystone powder or the weathering coal dust of aequum are put in the reactor, under agitation add sodium hydroxide or/and water glass, control reaction temperature is at 30 to 70 degree, reaction times is 3 to 5 hours, under agitation add times a basic phenolic ether and a polyacrylamide of aequum then, mix and obtain black oil-displacing agent.
The present invention has that cost is low, and production method is simple, and using method is also simple, the characteristics that efficient is high.After adopting this black oil-displacing agent on the oil field, can improve petroleum production and recovery ratio greatly, reduce well water.
Four, embodiment:
Embodiment 1, and this black oil-displacing agent consists of by weight percentage: 15% sodium hydroxide, the coal drystone powder of 0.005% polyacrylamide and surplus or weathering coal dust.
Embodiment 2, and this black oil-displacing agent consists of by weight percentage: 25% sodium hydroxide, the coal drystone powder of 0.05% or 0.5% polyacrylamide and surplus or weathering coal dust.
Embodiment 3, and this black oil-displacing agent consists of by weight percentage: 15% water glass, the coal drystone powder of 0.005% polyacrylamide and surplus or weathering coal dust.
Embodiment 4, and this black oil-displacing agent consists of by weight percentage: 25% water glass, the coal drystone powder of 0.05% or 0.5% polyacrylamide and surplus or weathering coal dust.
Embodiment 5, and this black oil-displacing agent consists of by weight percentage: 10% sodium hydroxide, 5% water glass, the coal drystone powder of 0.005% polyacrylamide and surplus or weathering coal dust.
Embodiment 6, and this black oil-displacing agent consists of by weight percentage: 22% sodium hydroxide, 10% water glass, the coal drystone powder of 0.05% or 0.5% polyacrylamide and surplus or weathering coal dust.
Embodiment 7, and this black oil-displacing agent consists of by weight percentage: 10% sodium hydroxide, 5% water glass, a basic phenolic ether of 1%, the coal drystone powder of 0.005% polyacrylamide and surplus or weathering coal dust.
Embodiment 8, and this black oil-displacing agent consists of by weight percentage: 22% sodium hydroxide, 10% water glass, a basic phenolic ether of 20%, the coal drystone powder of 0.05% or 0.5% polyacrylamide and surplus or weathering coal dust.
Embodiment 9, and this black oil-displacing agent consists of by weight percentage: 15% sodium hydroxide, 8% water glass, a basic phenolic ether of 5%, the coal drystone powder of 0.005% polyacrylamide and surplus or weathering coal dust.
Embodiment 10, and this black oil-displacing agent consists of by weight percentage: 22% sodium hydroxide, 10% water glass, a basic phenolic ether of 10% or 15%, the coal drystone powder of 0.05% or 0.5% polyacrylamide and surplus or weathering coal dust.
In the above-described embodiments, coal drystone powder or weathering coal dust are 40 orders or 60 orders or 80 purposes.
The black oil-displacing agent of the foregoing description obtains by following production method: the coal drystone powder or the weathering coal dust of aequum are put in the reactor, under agitation add sodium hydroxide or/and water glass, control reaction temperature is at 30 degree or 50 degree or 70 degree, reaction times is 3 or 5 hours, under agitation add times a basic phenolic ether and a polyacrylamide of aequum then, mix and obtain black oil-displacing agent.
The black oil-displacing agent of the foregoing description gained is carried out indoor evaluation, adopt the Q/XJQ451-91 standard, oil well oil-containing core is removed the oven dry of deoiling, clean with dimethylbenzene, the acetone cleaning, drying, saturated under 90 degree with a certain amount of crude oil then, 30 degree are placed after 48 hours down and are carried out oil displacement test, when the amount that adds black oil-displacing agent is 0.5% with do not add oil-displacing agent and compare, improving recovery ratio is 40%, when the amount that adds black oil-displacing agent is 0.05% with do not add oil-displacing agent and compare, improving recovery ratio is 20%.
Claims (3)
1, a kind of black oil-displacing agent is characterized in that consisting of by weight percentage:
A, 15 to 25% sodium hydroxide, perhaps 15 to 25% water glass, perhaps 10 to 22% sodium hydroxide and 5 to 10% water glass;
B, 0 to 20% appoint basic phenolic ether;
C, 0.005 to 0.5% polyacrylamide;
The coal drystone powder of D, surplus or weathering coal dust.
2, black oil-displacing agent according to claim 1 is characterized in that coal drystone powder or weathering coal dust are 40 to 80 purpose powder.
3, a kind of black oil-displacing agent production method according to claim 1 and 2, it is characterized in that the coal drystone powder or the weathering coal dust of aequum are put in the reactor, under agitation add sodium hydroxide or/and water glass, control reaction temperature is at 30 to 70 degree, reaction times is 3 to 5 hours, under agitation add times a basic phenolic ether and a polyacrylamide of aequum then, mix and obtain black oil-displacing agent.