CN1195688A - Strong building adhesive - Google Patents
Strong building adhesive Download PDFInfo
- Publication number
- CN1195688A CN1195688A CN97103940A CN97103940A CN1195688A CN 1195688 A CN1195688 A CN 1195688A CN 97103940 A CN97103940 A CN 97103940A CN 97103940 A CN97103940 A CN 97103940A CN 1195688 A CN1195688 A CN 1195688A
- Authority
- CN
- China
- Prior art keywords
- portions
- glue
- rosin
- bonding agent
- toluene
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention relates to a strong building bonding agent. It is characterized by that said bonding agent is made up by using 20-30 portions of waste polystyrene foam board, 30-40 portions of toluene, 1-3 portions of rosin, 0-10 portions of foam paint, 0-30 portions of talcum powder and 0-30 portions of coarse whiting through the processes of mixing and stirring treatment. Said invented bonding agent possesses the advantages of strong cohesive force, water-proofing, sun-proofing, anti-freezing, low cost and simple preparation method, so it is applicable to binding construction of indoor and outdoor decorative materials.
Description
The present invention relates to a kind of strong building adhesive, be used for the bonding construction of indoor and outdoor finishing material.
The adhesive for building that multiple model is arranged in the market, as 501 glue, 502 glue, 903 glue etc., these binding agents mainly are that acrylate is the multi-purpose adhesive of main component, and its shortcoming is the raw materials cost height, the component complexity, preparation method's complexity, and not sun-proof, non-watertight, not antifreeze, purposes is narrower, and very short time has just lost cohesive force, and preservation period is short.
Purpose of the present invention is the shortcoming and deficiency in order to overcome above-mentioned prior art just, and the waste polystyrene foam plate that provides a kind of raw material to be easy to get, solvent and compound are through the strong building adhesive of simple method preparation.
The objective of the invention is to realize by following technical proposal:
A kind of strong building adhesive is characterized in that it is made up of following component, and its consumption (by weight) is:
Waste polystyrene foam plate 20-30 part
Toluene 30-40 part
Rosin 1-3 part
Foam paint 0-10 part
Talcum powder 0-30 part
Water-ground limestone 0-30 part
Each component preferable amount is:
Waste polystyrene foam plate 25-30 part
Toluene 35-40 part
Rosin 1-2 part
Foam paint 0-10 part
Talcum powder 0-25 part
Water-ground limestone 0-25 part
The waste polystyrene foam board raw material that binding agent of the present invention adopts, it is a waste, because it is in light weight, volume is big, reclaims difficulty, very easily causes environmental pollution, therefore recycle that not only cost is low, and turn waste into wealth, when the waste polystyrene foam plate is handled through toluene solvant, just become the heavy-gravity colloid, have stronger viscosifying power, the settable cementitious effect of rosin by adding has improved viscosity again, brightness, water resistance.Add foam paint and improve dissolving power, talcum powder and water-ground limestone are compounds.
Binding agent of the present invention is divided into the product of glue and two kinds of forms of glue cream, wherein add the glue that toluene and rosin form through soaking and stirring by polystyrene foam plate, can be coated in container inner wall, form the waterproof application of anti-leakage layers, and as long as very thin coating one deck just can reach excellent waterproof, leak preventing effect, nontoxic pollution-free, in above-mentioned glue, add foam paint, talcum powder and water-ground limestone are through stirring the glue cream that forms body of paste, it is widely used in the bonding construction of indoor and outdoor decoration finishing material, as timber floor, ceramic tile, mosaic, marble, the plastic floor piece, the wood wall, glass, eyeglass, synthetic glass, plasterboard, pottery, the PVC rigid plastics, the bright and beautiful foam in sea, polyurethane hard foam, leatheroid, timber, furniture, workmanship, unearthed relics etc. are used for the kitchen, the lavatory, bathing pool, building, the waterproof, seepage control of vault, moistureproof mending-leakage and cement products, bridge, tunnel repairing etc.
Binding agent of the present invention is sun-proof through waterproof, and is antifreeze grade for performance measurement improve more than 2 times than 903 glue, and 903 glue can not be constructed below zero point, and binding agent of the present invention can be constructed in-20 ℃ of-+50 ℃ of scopes, still has powerful cohesive force.
Compared with the prior art the technology of the present invention has following advantage and effect:
A) have sun-proof, waterproof, ageing-resistant, long service life, the premium properties that cohesive force is strong;
Batching is few when B) using, consumption is also few, as when being used to decorate the indoor floor brick, needing in the past that binding agent was added sand adds cement mixing construction and will spread thick tack coat, and with binding agent of the present invention as long as with sand mix, be coated with the very thin glue-line of one deck and just can well bond, alleviated the load-bearing of building greatly;
C) make full use of tired polystyrene foam waste material, and turn waste into wealth, improve environmental pollution;
D) preparation method is simple, and raw material is easy to get, and cost is low, does not have and dyes.
Embodiment 1:
Get the waste polystyrene foam plate 20kg adding toluene 30kg that purchases and soaked 1 day, treat that all the dissolving back adds rosin 1kg, stir and promptly made glue type binding agent in 10 minutes.The waterproof leakproof coating that is used for container inner wall.
Embodiment 2:
Embodiment 1 glue is added foam paint 8kg talcum powder 25kg again, and water-ground limestone 25kg continues to stir for promptly becoming glue paste binding agent.
Embodiment 3:
Get the waste polystyrene foam plate 30kg that purchases and add toluene 40kg.Soaked 2 days, and treated that all the dissolving back added rosin 2kg stirring 15 minutes, promptly make glue type binding agent.
Embodiment 4:
The glue of embodiment 3 is added foam paint 10kg again, talcum powder 30kg, water-ground limestone 30kg continues to stir, and promptly makes glue cream type binding agent.
Claims (2)
1, a kind of strong building adhesive is characterized in that it is made up of following component, and its consumption (by weight) is:
Waste polystyrene foam plate 20-30 part
Toluene 30-40 part
Rosin 1-3 part
Foam paint 0-10 part
Talcum powder 0-30 part
Water-ground limestone 0-30 part
2, binding agent according to claim 1 is characterized in that each component preferable amount is:
Waste polystyrene foam plate 25-30 part
Toluene 35-40 part
Rosin 1-2 part
Foam paint 0-10 part
Talcum powder 0-25 part
Water-ground limestone 0-25 part