CN1171551C - Production process of cohesive cloth - Google Patents
Production process of cohesive cloth Download PDFInfo
- Publication number
- CN1171551C CN1171551C CNB011082054A CN01108205A CN1171551C CN 1171551 C CN1171551 C CN 1171551C CN B011082054 A CNB011082054 A CN B011082054A CN 01108205 A CN01108205 A CN 01108205A CN 1171551 C CN1171551 C CN 1171551C
- Authority
- CN
- China
- Prior art keywords
- cohesive cloth
- cloth
- cohesive
- adhesive
- production process
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The present invention relates to a production process of cohesive cloth, particularly to the production process of cohesive cloth which needs to have strong engaging force and is used for laying and displaying products. The production process of the present invention comprises a material selecting step, a warping step, a weaving step, a dyeing step, a softening treatment step, a shaping step, a looping step and a glue coating step. In the glue coating process, the traveling speed of the cohesive cloth is 10 to 18 meters per minute; the temperature of 140 EEG C to 210 DEG C is adopted; adhesive for textile use is used as glue; the main ingredient of the adhesive uses acrylic acid and the esters of the acrylic acid as main raw material, and after the acrylic acid and the esters are polymerized by emulsion, the polymer is mixed with water according to certain proportion to regulate viscosity. The present invention has the advantage that the engaging strength which is produced when the cohesive cloth is engaged with a male sheet which is provided with engaging teeth can be obtained under the condition of using the prior art steps without changing existing equipment.
Description
The present invention is a kind of production technology of cohesive cloth, especially for a kind of requirement have strong engagement force such as the production technology of arranging the cohesive cloth that the exhibition product is used.
Cohesive cloth mainly is meant the mother viscose button cloth, its purposes has progressively expanded to commercial enterprise sales promotion field such as arranging exhibits from daily life fields such as in the past clothes, shoes, liners, and the sticking machine cloth in the purposes of sheerly living in the past only need be made slivering, band shape, so to joggled strength or claim the requirement that hasp intensity need not be too high.For example the Chinese patent patent No. is 93117876.2, discloses a kind of name and be called " warp-knit cloth that is used for surface fastener ", as if it is to have proposed the property improved scheme at gas permeability, and the improvement of suitable engagement force is not proposed substantial solution.Because as previously mentioned, for the employed thread gluing bar of the above-mentioned daily life field of enumerating, band, really need not the too harsh joggled strength that requires.Certainly also have to propose to improve the property imagination to being intended to improve engagement force, as the Chinese patent patent No. be 96110681.6, name is called " a kind of hasp self-adhesive part and manufacture method and manufacturing equipment." essence of manufacture method of this technical scheme is the back side coating multi-layer adhesive of the cohesive cloth after soft treatment, typing, looping are finished, and whenever is coated with one deck, dry one deck, so that coating lower floor, the coating number of plies is at least three layers.Though Jia Gong cohesive cloth can suitably improve bonding strength to a certain extent in this way, but it must be equipped with corresponding special equipment, thereby for the present domestic production firm that has a common off-the-shelf equipment, be difficult to take over, in addition, its adhesive cost is higher, and processing step is loaded down with trivial details.
The objective of the invention is to provide a kind of technology simple, have a production technology of the cohesive cloth of stronger joggled strength.
The objective of the invention is to reach like this, a kind of production technology of cohesive cloth, it may further comprise the steps: select materials---warping---weave---dyeing---soft treatment, typing, looping---gluing, in described gluing process, the gait of march of cohesive cloth is 10~18 meters/minute; The temperature that is adopted is 140 ℃~210 ℃; Described glue adopts weaving to use adhesive, and the main composition of this adhesive is a main material with acrylic acid and ester class thereof, after emulsion polymerisation, is regulated viscosity by a certain percentage with water.
The present invention has the following advantages, and is not changing existing equipment and is utilizing under the ready-made processing step situation, can obtain the joggled strength that cohesive cloth is meshed with the public sheet of band engaging tooth.
Below the production technology of cohesive cloth of the present invention is further described below.
Fig. 1 is the local enlarged diagram of cohesive cloth of the present invention.
Fig. 2 is the A portion enlarged drawing of Fig. 1.
The proportioning of adhesive of the present invention and water is 1: 3~5; Described material is half of 80D20F~135D32F Delustring dacron thread or Polyamide Yarns; By warping machine dacron thread or Polyamide Yarns are carried out warping; With the 18E-32E tricot machine or Dacron thread after the warping or Polyamide Yarns are weaved with two comb joints with the little tricot machine of 303 types, made grey cloth, base The density of cloth is controlled at 160~280 gram/m2, fabric width is at 1~1.8 meter. In weaving process, sley bar L1 is protruding with 1012 Wheel, sley bar L2 1045 cams are equidirectional taking the needle and weave, and the mode of taking the needle is respectively 1-00-1-22,1-00-4-55; In this way with sley bar L1 1023 cams, sley bar L2 1056 cams so. The mode of taking the needle is respectively 1-00-2-33,1-00-5-66; For another example, sley bar L1 is with 1034 or 1045 cams, so corresponding 1067 or 1078 cams of using instead of sley bar L2. According to desired color, grey cloth is dyeed; To the grey cloth after the dyeing with softening agent carry out soft treatment, typing, Play pile loop, make the front of cohesive cloth form engagement pile loop 1; To the back side applying adhesive of cohesive cloth, form tack coat 3, Make base portion and base fabric striped 2 cementations of positive engagement pile loop 1, the gluing machine that is installed in the forming machine afterbody is adopted in gluing Finishing, specifically is by the gluing of gluing roller strap slurry, oven dry. In the gluing process, to the gait of march of cohesive cloth and Baking temperature is controlled respectively, reflects on the instrument board of its indicating value by forming machine. Wherein, used adhesive is Commercially available by Wuxi CityThe model that screen-like mountain peak textile auxiliary factory produces is the agent of WF-2 type spun bonded.
The above-mentioned cohesive cloth of making has the stronger joggled strength that is meshed with public sheet, cohesive cloth is stretched tight admittedly to exist in this way On the one exhibition grillage, the display material such as ceramic tile that show is fixed with public sheet earlier, then with public sheet and The engagement pile loop 1 of cohesive cloth of the present invention is nibbled solid mutually, and the display material of ceramic tile and so on can not come off from it.
Embodiment 1:
1. be to choose any one half delustring dacron thread 80D20F, 90D22F, 100D24F, 110D26F, 120D28F, the 135D32F or Polyamide Yarns is made raw material from specification;
2. selected dacron thread or Polyamide Yarns are carried out warping on warping machine;
3. be woven into grey cloth with the dacron thread or the Polyamide Yarns of common tricot machine after to warping, the density of grey cloth is 160 gram/m
2, fabric width is at 1 meter;
4. grey cloth is dyeed;
5. grey cloth is carried out soft treatment, typing, looping, make the front of cohesive cloth form engagement pile loop 1 earlier;
6. to the back side applying adhesive of cohesive cloth, form tack coat 3, make the base portion and base fabric striped 2 cementations of positive engagement pile loop 1, in coating process, the gait of march of cohesive cloth is controlled at 10 meters/minute; Temperature then is controlled at 140 ℃; The proportioning of adhesive and water is 1: 3.
Embodiment 2:
1. be that half delustring dacron thread or the Polyamide Yarns of choosing any one specification 80D20F, 90D22F, 100D24F, 110D26F, 120D28F, the 135D32F made raw material from specification;
2. selected dacron thread or Polyamide Yarns are carried out warping on warping machine;
3. be woven into grey cloth with the dacron thread or the Polyamide Yarns of common tricot machine after to warping, the density of grey cloth is 220 gram/m
2, fabric width is at 1.5 meters;
4. grey cloth is dyeed;
5. grey cloth is carried out soft treatment, typing, looping, make the front of cohesive cloth form engagement pile loop 1 earlier;
6. to the back side applying adhesive of cohesive cloth, form tack coat 3, make the base portion and base fabric striped 2 cementations of positive engagement pile loop 1, in coating process, the gait of march of cohesive cloth is controlled at 14 meters/minute; Temperature then is controlled at 175 ℃; The proportioning of adhesive and water is 1: 4.
Embodiment 3:
1. be that half delustring dacron thread or the Polyamide Yarns of choosing any one specification 80D20F, 90D22F, 100D24F, 110D26F, 120D28F, the 135D32F made raw material from specification;
2. selected dacron thread or Polyamide Yarns are carried out warping on warping machine;
3. be woven into grey cloth with the dacron thread or the Polyamide Yarns of common tricot machine after to warping, the density of grey cloth is 280 gram/m
2, fabric width is at 1.8 meters;
4. grey cloth is dyeed;
5. grey cloth is carried out soft treatment, typing, looping, make the front of cohesive cloth form engagement pile loop 1 earlier;
6. to the back side applying adhesive of cohesive cloth, form tack coat 3, make the base portion and sill strip line 2 cementations of positive engagement pile loop 1, in coating process, the gait of march of cohesive cloth is controlled at 18 meters/minute; Temperature then is controlled at 210 ℃; The proportioning of adhesive and water is 1: 5.
Claims (2)
1, a kind of production technology of cohesive cloth, it may further comprise the steps: select materials, and---warping---is weaved---dyeing---soft treatment, typing, looping---gluing, it is characterized in that in described gluing process, the gait of march of cohesive cloth is 10~18 meters/minute; The temperature that is adopted is 140 ℃~210 ℃; Described glue adopts weaving to use adhesive, and the main composition of this adhesive is a main material with acrylic acid and ester class thereof, after emulsion polymerisation, is regulated viscosity by a certain percentage with water.
2, the production technology of cohesive cloth according to claim 1, the proportioning that it is characterized in that adhesive and water is 1: 3~5.