CN114561188A - Preparation method of ground anti-slip agent - Google Patents

Preparation method of ground anti-slip agent Download PDF

Info

Publication number
CN114561188A
CN114561188A CN202210218596.7A CN202210218596A CN114561188A CN 114561188 A CN114561188 A CN 114561188A CN 202210218596 A CN202210218596 A CN 202210218596A CN 114561188 A CN114561188 A CN 114561188A
Authority
CN
China
Prior art keywords
mixed solution
ground
ground anti
slip agent
stirrer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN202210218596.7A
Other languages
Chinese (zh)
Inventor
姜明
董霁莹
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yushuang Technology Shanghai Co ltd
Original Assignee
Yushuang Technology Shanghai Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yushuang Technology Shanghai Co ltd filed Critical Yushuang Technology Shanghai Co ltd
Priority to CN202210218596.7A priority Critical patent/CN114561188A/en
Publication of CN114561188A publication Critical patent/CN114561188A/en
Pending legal-status Critical Current

Abstract

The invention discloses a preparation method of a ground anti-skid agent, which relates to the technical field of ground anti-skid agents and comprises the following steps: s1: taking the following raw materials, by weight, 1.2% -1.5% of a surfactant, 8.5% -10% of fruit acid, 2.5% -7% of acetic acid, 7.5% -9.5% of sodium chloride, 1.5% -5% of potassium carbonate, 1.5% -2.5% of a corrosion inhibitor, 0.3% -0.5% of an aromatic, 2.2% -3.5% of crystal particles, 30% -35% of deionized water and 20% -25% of phenolic resin glue for later use. This preparation method of ground anti-skid agent for this ground anti-skid agent can effectively permeate the subaerial formation slight hole concave, when the sole exists water stain and oil stain, can the vacuole formation with the ground contact, the cavity plays an adsorption, utilize the adsorption of cavity to prevent skidding, increase the joint strength between this ground anti-skid agent and the ground through phenolic resin glue in addition, improve the life of this ground anti-skid agent, quartzy granule is inside attached to phenolic resin glue in addition, increase the roughness on ground, the result of use of this ground anti-skid agent has been improved.

Description

Preparation method of ground anti-slip agent
Technical Field
The invention relates to the technical field of ground anti-slip agents, in particular to a preparation method of a ground anti-slip agent.
Background
The ground anti-skid agent is also called as ground anti-skid penetrant, after being used, the ground anti-skid agent can effectively increase the friction coefficient when the surface of a floor is wetted, and prevent slipping, thereby avoiding accidents and body injuries caused by wet slipping.
Disclosure of Invention
Aiming at the defects of the prior art, the invention provides a preparation method of a ground anti-slip agent, which solves the problems in the background technology.
In order to achieve the purpose, the invention is realized by the following technical scheme: a preparation method of a ground anti-slip agent comprises the following steps:
s1: taking the following raw materials, by weight, 1.2% -1.5% of a surfactant, 8.5% -10% of fruit acid, 2.5% -7% of acetic acid, 7.5% -9.5% of sodium chloride, 1.5% -5% of potassium carbonate, 1.5% -2.5% of a corrosion inhibitor, 0.3% -0.5% of an aromatic, 2.2% -3.5% of crystal particles, 30% -35% of deionized water and 20% -25% of phenolic resin glue for later use;
s2: putting 1.2-1.5% of surfactant, 8.5-10% of fruit acid, 2.5-7% of acetic acid and 7.5-9.5% of sodium chloride into 15-20% of deionized water, heating the mixed solution to 50-60 ℃, and stirring the mixed solution by using a stirrer to obtain a first mixed solution;
s3: putting 1.5-5% of potassium carbonate and 1.5-2.5% of corrosion inhibitor into 15-20% of deionized water, heating the mixed solution to 50-60 ℃, and stirring the mixed solution by using a stirrer to obtain a second mixed solution;
s4: taking 2.2% -3.5% of crystal particles, placing the crystal particles in 20% -25% of phenolic resin glue, and heating and stirring the mixed solution to obtain a third mixed solution;
s5: pouring the second part of mixed solution and the third part of mixed solution into the first part of mixed solution, heating the mixed solution to 80-90 ℃, and stirring the mixed solution by using a stirrer to obtain a fourth part of mixed solution;
s6: pouring the mixed solution of 0.3% -0.5% of the aromatic into the fourth mixed solution, and uniformly stirring by using a stirrer to obtain a finished product of the ground anti-slip agent;
s7: and placing the prepared finished ground anti-slip agent in a sealed tank for storage.
Optionally, the rotation speed of the stirrer in S2 and S3 is 800 revolutions per minute, and the stirring time in S2 and S3 is 10 to 15 minutes.
Optionally, the rotation speed of the stirrer in the step S4 is 1500 revolutions per minute, and the stirring time period in the step S4 is 25 to 30 minutes.
Optionally, the rotation speed of the stirrer in the step S5 is 2000 rpm, and the stirring time in the step S5 is 30-35 minutes.
Optionally, the rotation speed of the stirrer in the step S6 is 1500 revolutions per minute, and the stirring time period in the step S6 is 8-10 minutes.
Optionally, the aromatic in S1 is a natural plant perfume.
Optionally, the surfactant in S1 is stearic acid.
The invention provides a preparation method of a ground anti-slip agent, which has the following beneficial effects:
the preparation method of the ground anti-slip agent utilizes the surfactant, tartaric acid, acetic acid, sodium chloride, potassium carbonate, a corrosion inhibitor and deionized water to be matched for use, so that the ground anti-slip agent can effectively permeate into the ground upper layer to form a fine pit, when water stain and oil stain exist on the sole, a cavity can be formed by contacting with the ground, the cavity plays a role in adsorption, the adsorption of the cavity is utilized for anti-slip, in addition, the connection strength between the ground anti-slip agent and the ground is increased through phenolic resin glue, the service life of the ground anti-slip agent is prolonged, crystal particles are attached to the inside of the phenolic resin glue, the roughness of the ground is increased, and the use effect of the ground anti-slip agent is improved.
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the embodiments of the present invention, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments.
The invention provides a technical scheme that: a preparation method of a ground anti-slip agent comprises the following steps:
s1: taking the following raw materials, by weight, 1.2% -1.5% of a surfactant, 8.5% -10% of tartaric acid, 2.5% -7% of acetic acid, 7.5% -9.5% of sodium chloride, 1.5% -5% of potassium carbonate, 1.5% -2.5% of a corrosion inhibitor, 0.3% -0.5% of an aromatic, 2.2% -3.5% of crystal particles, 30% -35% of deionized water and 20% -25% of phenolic resin glue for later use;
s2: putting 1.2-1.5% of surfactant, 8.5-10% of fruit acid, 2.5-7% of acetic acid and 7.5-9.5% of sodium chloride into 15-20% of deionized water, heating the mixed solution to 50-60 ℃, and stirring the mixed solution by using a stirrer to obtain a first mixed solution;
s3: putting 1.5-5% of potassium carbonate and 1.5-2.5% of corrosion inhibitor into 15-20% of deionized water, heating the mixed solution to 50-60 ℃, and stirring the mixed solution by using a stirrer to obtain a second mixed solution;
s4: taking 2.2% -3.5% of crystal particles, placing the crystal particles in 20% -25% of phenolic resin glue, and heating and stirring the mixed solution to obtain a third mixed solution;
s5: pouring the second part of mixed solution and the third part of mixed solution into the first part of mixed solution, heating the mixed solution to 80-90 ℃, and stirring the mixed solution by using a stirrer to obtain a fourth part of mixed solution;
s6: pouring the mixed solution of 0.3% -0.5% of the aromatic into the fourth mixed solution, and uniformly stirring by using a stirrer to obtain a finished product of the ground anti-slip agent;
s7: and placing the prepared finished ground anti-slip agent in a sealed tank for storage.
It can be understood by those skilled in the art that the above embodiment provides a method for preparing a ground anti-slip agent, the ground anti-slip agent is prepared by mixing a surfactant, tartaric acid, acetic acid, sodium chloride, potassium carbonate, a corrosion inhibitor, an aromatic, crystal particles, deionized water and phenolic resin glue, the surfactant, the tartaric acid, the acetic acid, the sodium chloride, the potassium carbonate, the corrosion inhibitor and the deionized water make the anti-slip agent effectively permeate into the upper layer of the ground to form fine pits, when water and oil stains exist on the sole of a foot, a cavity can be formed by contacting with the ground, the cavity has an adsorption effect, the adsorption effect of the cavity is used for anti-slip, the phenolic resin glue is used for increasing the connection strength between the ground anti-slip agent and the ground, the service life of the ground anti-slip agent is prolonged, and the crystal particles are attached to the inside of the phenolic resin glue to increase the roughness of the ground, the size of the crystal grains has various specifications, so that the roughness of the ground is changed.
Further, the rotation speed of the stirrer in the S2 and the S3 is 800 revolutions per minute, and the stirring time in the S2 and the S3 is 10 to 15 minutes.
As will be understood by those skilled in the art, the mixed solution of the surfactant, the fruit acid, the acetic acid, the sodium chloride and the deionized water is stirred and mixed for 10 to 15 minutes by a stirrer rotating at 800 revolutions per minute, and the mixed solution of the potassium carbonate, the corrosion inhibitor and the deionized water is stirred and mixed for 10 to 15 minutes by a stirrer rotating at 800 revolutions per minute.
Further, the rotation speed of the stirrer in the step S4 is 1500 revolutions per minute, and the stirring time period in the step S4 is 25-30 minutes.
As can be understood by those skilled in the art, the mixed solution of the crystal particles and the phenolic resin glue is stirred for 25-30 minutes by a stirrer rotating at 1500 rpm, and the phenolic resin glue has high viscosity, so that the crystal particles are stirred at a high speed, and are stirred for a long time, so that the uniformity of the distribution of the crystal particles in the phenolic resin glue is ensured.
Further, the rotation speed of the stirrer in the S5 is 2000 revolutions per minute, and the stirring time period in the S5 is 30-35 minutes.
As can be understood by those skilled in the art, the solution formed by mixing the second part of mixed solution, the third part of mixed solution and the first part of mixed solution is stirred at 2000 rpm, and because the solution amount is large and the phenolic resin glue is contained in the solution, the stirring speed is higher, and the stirring is carried out for a longer time, so that the uniformity after stirring is ensured.
Further, the rotation speed of the stirrer in the S6 is 1500 revolutions per minute, and the stirring time period in the S6 is 8-10 minutes.
As will be appreciated by those skilled in the art, this allows for the rapid addition of fragrance to the floor polish.
Further, the aromatic in S1 is a natural plant perfume.
It will be appreciated by those skilled in the art that the fragrance composition is guaranteed to emit a scent that does not harm the body of the consumer, and that the fragrance composition may have a variety of fragrances that are selected by the consumer.
Further, the surfactant in S1 is stearic acid.
The above description is only for the preferred embodiment of the present invention, but the scope of the present invention is not limited thereto, and any person skilled in the art should be considered to be within the technical scope of the present invention, and the technical solutions and the inventive concepts thereof according to the present invention should be equivalent or changed within the scope of the present invention.

Claims (7)

1. A preparation method of a ground anti-slip agent is characterized by comprising the following steps:
s1: taking the following raw materials, by weight, 1.2% -1.5% of a surfactant, 8.5% -10% of fruit acid, 2.5% -7% of acetic acid, 7.5% -9.5% of sodium chloride, 1.5% -5% of potassium carbonate, 1.5% -2.5% of a corrosion inhibitor, 0.3% -0.5% of an aromatic, 2.2% -3.5% of crystal particles, 30% -35% of deionized water and 20% -25% of phenolic resin glue for later use;
s2: putting 1.2-1.5% of surfactant, 8.5-10% of fruit acid, 2.5-7% of acetic acid and 7.5-9.5% of sodium chloride into 15-20% of deionized water, heating the mixed solution to 50-60 ℃, and stirring the mixed solution by using a stirrer to obtain a first mixed solution;
s3: putting 1.5-5% of potassium carbonate and 1.5-2.5% of corrosion inhibitor into 15-20% of deionized water, heating the mixed solution to 50-60 ℃, and stirring the mixed solution by using a stirrer to obtain a second mixed solution;
s4: taking 2.2% -3.5% of crystal particles, placing the crystal particles in 20% -25% of phenolic resin glue, and heating and stirring the mixed solution to obtain a third mixed solution;
s5: pouring the second part of mixed solution and the third part of mixed solution into the first part of mixed solution, heating the mixed solution to 80-90 ℃, and stirring the mixed solution by using a stirrer to obtain a fourth part of mixed solution;
s6: pouring the mixed solution of 0.3% -0.5% of the aromatic into the fourth mixed solution, and uniformly stirring by using a stirrer to obtain a finished product of the ground anti-slip agent;
s7: and placing the prepared finished ground anti-slip agent in a sealed tank for storage.
2. The method for preparing a ground anti-slip agent according to claim 1, wherein the method comprises the following steps: the rotating speed of the stirrer in the S2 and the S3 is 800 revolutions per minute, and the stirring time in the S2 and the S3 is 10-15 minutes.
3. The method for preparing a ground anti-slip agent according to claim 1, wherein the method comprises the following steps: the rotation speed of the stirrer in the S4 is 1500 revolutions per minute, and the stirring time in the S4 is 25-30 minutes.
4. The method for preparing a ground anti-slip agent according to claim 1, wherein the method comprises the following steps: the rotating speed of the stirrer in the S5 is 2000 revolutions per minute, and the stirring time in the S5 is 30-35 minutes.
5. The method for preparing a ground anti-slip agent according to claim 1, wherein the method comprises the following steps: the rotation speed of the stirrer in the step S6 is 1500 revolutions per minute, and the stirring time in the step S6 is 8-10 minutes.
6. The method for preparing a ground anti-slip agent according to claim 1, wherein the method comprises the following steps: the aromatic in S1 is natural plant perfume.
7. The method for preparing a ground anti-slip agent according to claim 1, wherein the method comprises the following steps: the surfactant in S1 is stearic acid.
CN202210218596.7A 2022-03-04 2022-03-04 Preparation method of ground anti-slip agent Pending CN114561188A (en)