CN114165068A CN202010958382.4A CN202010958382A CN114165068A CN 114165068 A CN114165068 A CN 114165068A CN 202010958382 A CN202010958382 A CN 202010958382A CN 114165068 A CN114165068 A CN 114165068A
Authority
CN
China
Prior art keywords
ground
skid
water
liquid
treatment
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN202010958382.4A
Other languages
Chinese (zh)
Inventor
戴建华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Always Reach Safety Ground Slip Engineering Technology Co ltd
Original Assignee
Shanghai Always Reach Safety Ground Slip Engineering Technology Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Always Reach Safety Ground Slip Engineering Technology Co ltd filed Critical Shanghai Always Reach Safety Ground Slip Engineering Technology Co ltd
Priority to CN202010958382.4A priority Critical patent/CN114165068A/en
Publication of CN114165068A publication Critical patent/CN114165068A/en
Pending legal-status Critical Current

Links

Classifications

    • EFIXED CONSTRUCTIONS
    • E04BUILDING
    • E04GSCAFFOLDING; FORMS; SHUTTERING; BUILDING IMPLEMENTS OR AIDS, OR THEIR USE; HANDLING BUILDING MATERIALS ON THE SITE; REPAIRING, BREAKING-UP OR OTHER WORK ON EXISTING BUILDINGS
    • E04G23/00Working measures on existing buildings

Landscapes

  • Engineering & Computer Science (AREA)
  • Architecture (AREA)
  • Chemical & Material Sciences (AREA)
  • Chemical Kinetics & Catalysis (AREA)
  • Electrochemistry (AREA)
  • Mechanical Engineering (AREA)
  • Civil Engineering (AREA)
  • Structural Engineering (AREA)
  • Cleaning Implements For Floors, Carpets, Furniture, Walls, And The Like (AREA)
  • Floor Finish (AREA)

Abstract

The invention discloses a construction process of a ground anti-slip agent, which has an obvious effect after ground anti-slip treatment and does not influence the original ground beauty and subsequent cleaning and maintenance. The construction is relatively simple and convenient, is not limited by any time, and can quickly form an anti-skid ground system under the condition of not influencing the normal work and operation of customers.

Description

Construction process of ground anti-slip agent
Technical Field
The invention relates to the field of construction and service of constructional engineering and the field of building ground antiskid, in particular to a construction process of a ground antiskid agent (or called antiskid agent ground antiskid treatment method)
Background
In view of the fact that most economically developed areas and densely populated areas in China are in subtropical climate areas, people frequently slip and fall injuries due to the fact that the ground is wet and humid throughout the year, and the existing ground anti-slip measures are simple and crude and the ground materials have the anti-slip function, for example, the existing ground anti-slip measures are easy to slip when meeting water or being greasy, such as smooth floor tiles, granite, marble and the like, and therefore complaints, disputes and economic compensation of the events are increased day by day. Along with the increase of the population proportion of the old in China, the safety protection consciousness of consumers and laborers is enhanced, related regulation and system are complete, the antiskid safety is certainly to become the most important importance in the life of social people, and therefore, the adoption of effective antiskid measures to the ground is increasingly urgent.
Disclosure of Invention
The invention aims to provide a construction process of a ground anti-skid agent, which can quickly form an anti-skid ground system under the condition that normal work and operation of a client are influenced during coating.
In order to achieve the purpose, the invention adopts the following technical scheme:
a construction process of a ground anti-skid agent comprises the following steps:
s1, antiskid earlier stage: removing the barrier, vacating a construction surface, and cleaning and sweeping the place; preparing the all-round detergent and water according to a certain proportion by using a floor scrubbing machine to clean the ground, and scraping the ground by using a wiper or sucking the ground by using a water sucking machine; washing with clear water, and wiping with a wiper or sucking with a water sucking machine; the ground must be thoroughly cleaned and kept dry;
s2, before coating the anti-skid liquid, preparing the anti-skid matching liquid and water according to a certain proportion, and using a flat mop to holdIs well configured Is/are as followsThe anti-skid matching liquid is uniformly coated on the ground for about 10-15 minutes, and the capillary pores on the surfaces of the floor tiles and the ground stone can be opened under the action of the anti-skid matching liquid, so that the anti-skid liquid can easily permeate into the ground to play a role, and then the ground tiles and the ground stone are scraped dry by a wiper or sucked dry by a water sucking machine to enter the next procedure;
s3, preparing the anti-skid stock solution (mother solution) according to the construction site ground material or different materials by a certain ratio of 1: 5-15, and pulling with a flat mopIs ready for arrangementThe anti-skid liquid is coated on the ground, the liquid level thickness and the moisture retention time are required to be controlled when the anti-skid liquid is required to be coated evenly, if dry surfaces are required to be supplemented with moisture in time, the anti-skid effect is tested at regular time, and obvious resistance is achieved; if the anti-skid effect is not enough, the moisture retention time can be properly prolonged or the concentration of the anti-skid liquid can be adjusted for coating again, but attention must be paid to that if the anti-skid effect is too heavy, the corresponding fading of the color of the ground or the spots on the ground or even the phenomenon of garbage sticking can occur. If different ground materials in the same place are met, the ground materials are considered to be respectively treated, and then the next procedure is carried out;
s4, anti-skid later stage (anti-skid neutralization treatment): in order to stop the continuous action of the anti-skid liquid and avoid causing sequelae, the anti-skid neutralization treatment agent and water are adopted according to the proportion of 1: 10-30 proportion, using a flat mopIs ready for arrangementUniformly coating the anti-skid neutralizing treatment agent on the ground, or uniformly spraying the anti-skid neutralizing treatment agent on the ground by using a spraying method, or putting the anti-skid neutralizing treatment agent on the ground by using a floor scrubbing machine for grinding and brushing once;
s5, after the mixture is fully fused for 5 to 10 minutes, the mixture is scraped dry by a wiper or sucked dry by a water suction machine; requires that the acid and alkali substances on the ground be balanced through anti-skid neutralization treatment so as to ensure the removal and dischargeTime of flightThe requirement of environmental protection is met;
s6, finally, thoroughly washing the fabric with clean water, and wiping the fabric with a wiper or sucking the fabric with a water sucking machine;
s7: and performing maintenance treatment, and then entering into use.
Preferably, dewaxing water or an anti-skid stabilizer is adopted to dewax the floor tiles and the floor stones or solve the problem of oil stain treatment on the water surface so as to ensure that the subsequent anti-skid treatment can achieve the overall effect.
Preferably, the step of S3 requires uniform coating and a thickness of the liquid surface of 1-2 mm.
Preferably, the step S3 requires uniform coating, and the moisture retention time is controlled to be 15 to 40 minutes.
Preferably, the curing treatment time in the step S7 is 2 to 3 hours.
Preferably, the maintenance treatment time is prolonged according to the specific conditions of the ground material and the construction site; the maintenance treatment method adopts standing for drying.
The effect is obvious after the ground is subjected to anti-skid treatment, and the original ground appearance and subsequent cleaning and maintenance are not influenced. The construction is relatively simple and convenient, is not limited by any time, and can quickly form an anti-skid ground system under the condition of not influencing the normal work and operation of customers.
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all embodiments.
The invention provides a construction process of a ground anti-slip agent, which comprises the following steps:
s1, antiskid earlier stage: removing the barrier, vacating a construction surface, and cleaning and sweeping the place; preparing the all-round detergent and water according to a certain proportion by using a floor scrubbing machine to clean the ground, and scraping the ground by using a wiper or sucking the ground by using a water sucking machine; washing with clear water, and wiping with a wiper or sucking with a water sucking machine; the ground must be thoroughly cleaned and kept dry;
s2, if the surface of the floor tile and the floor stone has wax or generates oil on the water surface, wax removing water or an anti-skid stabilizer is adopted to carry out wax removing or water surface oil removing treatment on the floor tile and the floor stone so as to ensure that the subsequent anti-skid treatment can achieve the integral effect, and then the next procedure is carried out;
s3, before coating the anti-skid liquid, preparing the anti-skid matching liquid and water according to a certain proportion, and using a flat mop to holdIs well configured Is/are as followsThe anti-skid matching liquid is uniformly coated on the ground for about 10-15 minutes, and the capillary pores on the surfaces of the floor tiles and the ground stone can be opened under the action of the anti-skid matching liquid, so that the anti-skid liquid can easily permeate into the ground to play a role, and then the ground tiles and the ground stone are scraped dry by a wiper or sucked dry by a water sucking machine to enter the next procedure;
s4, preparing the anti-skid stock solution (mother solution) according to the construction site ground material or different materials by a certain ratio of 1: 5-15, and pulling with a flat mopIs ready for arrangementThe antiskid liquid is coated on the ground, the liquid level thickness and the moisturizing time need to be controlled when the antiskid liquid is required to be coated uniformly, if dry surfaces need to be moisturized in time, the antiskid effect is tested at regular time during the period, and obvious resistance is achieved. If the anti-skid effect is not enough, the moisture retention time can be properly prolonged or the concentration of the anti-skid liquid can be adjusted for coating again, but attention must be paid to that if the anti-skid effect is too heavy, the corresponding fading of the color of the ground or the spots on the ground or even the phenomenon of garbage sticking can occur. If different ground materials in the same place are met, the ground materials are considered to be respectively treated, and then the next procedure is carried out;
s5, anti-skid later stage (anti-skid neutralization treatment): in order to stop the continuous action of the anti-skid liquid and avoid causing sequelae, the anti-skid neutralization treatment agent and water are adopted according to the proportion of 1: 10-30 proportion, using a flat mopIs ready for arrangementUniformly coating the anti-skid neutralizing treatment agent on the ground, or uniformly spraying the anti-skid neutralizing treatment agent on the ground by using a spraying method, or putting the anti-skid neutralizing treatment agent on the ground by using a floor scrubbing machine for grinding and brushing once;
s6, after the mixture is fully fused for 5 to 10 minutes, the mixture is scraped dry by a wiper or sucked dry by a water suction machine; the acid and alkali substances on the ground are required to be balanced through anti-skid neutralization treatment so as to ensure that the environment-friendly requirement is met during removal and discharge;
s7, finally, thoroughly washing the fabric with clean water, and wiping the fabric with a wiper or sucking the fabric with a water sucking machine;
s8: and performing maintenance treatment, and then entering into use.
Further, the step of S4 requires uniform coating and a liquid level thickness of 1-2 mm.
Further, the step S4 requires uniform coating, and the moisture retention time is controlled to be 15 to 40 minutes.
Further, the maintenance treatment time in the step S8 is 2 to 3 hours, and the maintenance treatment time is prolonged according to the specific conditions of the ground material and the construction site; the maintenance treatment method adopts standing for drying.
Technical indexes in the embodiment of the invention are as follows:
anti-skid performance: coefficient of static friction (COF) > 0.5.
The execution standard is as follows: national standard GB/T4100-2015.
Marking an enterprise: Q31/0117000957C 001-2018.
The method is suitable for detection methods of various floor tiles, ground stones, grindstone terraces and the like.
The pendulum method detects the antiskid value (BPN) > 45.
The invention has obvious effect after ground anti-skid treatment, and can not influence the original ground beauty and subsequent cleaning and maintenance. The construction is relatively simple and convenient, is not limited by any time, and can quickly form an anti-skid ground system under the condition of not influencing the normal work and operation of customers.
In the description of the present invention, it is to be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "upper", "lower", "front", "rear", "left", "right", "vertical", "horizontal", "top", "bottom", "inner", "outer", "clockwise", "counterclockwise" are used to describe the invention "
Furthermore, the terms "first", "second" and "first" are used for descriptive purposes only and are not to be construed as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of the present invention, "a plurality" means two or more unless specifically defined otherwise.
The above description is only for the preferred embodiment of the present invention, but the scope of the present invention is not limited thereto, and any person skilled in the art should be considered to be within the technical scope of the present invention, and the technical solutions and the inventive concepts thereof according to the present invention should be equivalent or changed within the scope of the present invention.

Claims (6)

1. A construction process of a ground anti-slip agent is characterized by comprising the following steps:
s1, antiskid earlier stage: removing the barrier, vacating a construction surface, and cleaning and sweeping the place; preparing the all-round detergent and water according to a certain proportion by using a floor scrubbing machine to clean the ground, and scraping the ground by using a wiper or sucking the ground by using a water sucking machine; washing with clear water, and wiping with a wiper or sucking with a water sucking machine; the ground must be thoroughly cleaned and kept dry;
s2, before coating the anti-skid liquid, preparing the anti-skid matching liquid and water according to a certain proportion, and using a flat mop to holdIs ready for arrangementThe anti-skid matching liquid is uniformly coated on the ground for about 10-15 minutes, and the capillary pores on the surfaces of the floor tiles and the ground stone can be opened under the action of the anti-skid matching liquid, so that the anti-skid liquid can easily permeate into the ground to play a role, and then the ground tiles and the ground stone are scraped dry by a wiper or sucked dry by a water sucking machine to enter the next procedure;
s3, preparing the anti-skid stock solution (mother solution) according to the construction site ground material or different materials by a certain ratio of 1: 5-15, and pulling with a flat mopIs ready for arrangementThe anti-skid liquid is coated on the ground, the liquid level thickness and the moisture retention time are required to be controlled when the anti-skid liquid is required to be coated evenly, if dry surfaces are required to be supplemented with moisture in time, the anti-skid effect is tested at regular time, and obvious resistance is achieved; if the anti-skid effect is not enough, the moisture retention time can be properly prolonged or the concentration of the anti-skid liquid can be adjusted for coating again, but attention must be paid to that if the anti-skid effect is too heavy, the corresponding fading of the color of the ground or the spots on the ground or even the phenomenon of garbage sticking can occur. If different ground materials in the same place are met, the ground materials are considered to be respectively treated, and then the next procedure is carried out;
s4, anti-skid later stage (anti-skid neutralization treatment): to stop the continuous action of the anti-skid liquid and avoid sequelae, it is necessary toAdopting an anti-skid neutralization treating agent and water according to the proportion of 1: 10-30 proportion, using a flat mopIs ready for arrangementUniformly coating the anti-skid neutralizing treatment agent on the ground, or uniformly spraying the anti-skid neutralizing treatment agent on the ground by using a spraying method, or putting the anti-skid neutralizing treatment agent on the ground by using a floor scrubbing machine for grinding and brushing once;
s5, after the mixture is fully fused for 5 to 10 minutes, the mixture is scraped dry by a wiper or sucked dry by a water suction machine; requires that the acid and alkali substances on the ground be balanced through anti-skid neutralization treatment so as to ensure the removal and dischargeTime of flightThe requirement of environmental protection is met;
s6, finally, thoroughly washing the fabric with clean water, and wiping the fabric with a wiper or sucking the fabric with a water sucking machine;
s7: and performing maintenance treatment, and then entering into use.
2. The construction process of a ground anti-skid agent as claimed in claim 1, wherein the de-waxing water or anti-skid stabilizer is used to de-wax floor tiles and ground stone or solve the problem of oil stain on the water surface, so as to ensure the overall effect of the subsequent anti-skid treatment.
3. The process of claim 1, wherein the step S3 requires uniform coating and a liquid level thickness of 1-2 mm.
4. The process of claim 1, wherein the step S3 requires uniform coating and the moisture retention time is controlled to be 15-40 minutes.
5. The process of claim 1, wherein the curing time in the step S7 is 2 to 3 hours.
6. The construction process of the ground anti-slip agent according to claim 1 or 5, wherein the maintenance treatment time is prolonged according to the specific conditions of the ground material and the construction site; the maintenance treatment method adopts standing for drying.
CN202010958382.4A 2020-09-11 2020-09-11 Construction process of ground anti-slip agent Pending CN114165068A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN202010958382.4A CN114165068A (en) 2020-09-11 2020-09-11 Construction process of ground anti-slip agent

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN202010958382.4A CN114165068A (en) 2020-09-11 2020-09-11 Construction process of ground anti-slip agent

Publications (1)

Publication Number Publication Date
CN114165068A true CN114165068A (en) 2022-03-11

Family

ID=80476248

Family Applications (1)

Application Number Title Priority Date Filing Date
CN202010958382.4A Pending CN114165068A (en) 2020-09-11 2020-09-11 Construction process of ground anti-slip agent

Country Status (1)

Country Link
CN (1) CN114165068A (en)

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
GB201013575D0 (en) * 2010-08-13 2010-09-29 Wood Brian Slip resistant surface treatment
CN108485601A (en) * 2018-03-07 2018-09-04 上海安众达地面防滑工程技术有限公司 A kind of ground antilubricant
CN110129004A (en) * 2019-05-17 2019-08-16 广东极米新材料科技有限公司 A kind of processing method that ground is anti-skidding

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
GB201013575D0 (en) * 2010-08-13 2010-09-29 Wood Brian Slip resistant surface treatment
CN108485601A (en) * 2018-03-07 2018-09-04 上海安众达地面防滑工程技术有限公司 A kind of ground antilubricant
CN110129004A (en) * 2019-05-17 2019-08-16 广东极米新材料科技有限公司 A kind of processing method that ground is anti-skidding

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
全国第九次防水材料技术交流大会论文集编辑委员会: "《全国第九次防水材料技术交流大会论文集》", 31 May 2007 *

Similar Documents

Publication Publication Date Title
CN102357454B (en) Spraying process for fluorocarbon surface layer paint
EP1475426B1 (en) Process for the production of removable soil- and water-resistant surface coatings
US5902411A (en) Method for maintaining floors
Young et al. Maintenance and repair issues for stone cleaned sandstone and granite building façades
CN109826396A (en) A kind of construction method of A grades of fire prevention artistic floors
CN109098370A (en) A kind of construction techniques
US20120199249A1 (en) Floor treatment
CN114165068A (en) Construction process of ground anti-slip agent
CN108485601A (en) A kind of ground antilubricant
EP1935957A1 (en) Polishing agent
CN103382724B (en) Corrosion-prevention construction method for water pool by adopting vinyl ester
JP6484903B2 (en) Floor material coating structure, method for producing floor material coating structure, and method for regenerating floor material coating
DE4311713C1 (en) Cleaning lime-scale from glass, plastics and tiled surfaces - using cleaning fluid comprising citric or tartaric acid in glycerine, ethylene glycol, propylene glycol and polyethylene:glycol]
US5650016A (en) Method of cleaning a surface
US6383557B1 (en) Plumbing fixture surface restoration process
KR20130130154A (en) Method for manufacturing brass cleaner
JP6069092B2 (en) Anti-slip agent for floor
US6767586B1 (en) Method of application of anti-slip material for surfaces
JPS63159278A (en) Slip-preventing treatment for tile
JP6749009B1 (en) Anti-slip agent for floor
CN211286060U (en) Toilet waterproof material construction tool
DE102005013220A1 (en) Method for cleaning and impregnating acid-stable natural- and artificial stones, useful as building material, comprises applying a chemical composition comprising a stable acid or acid stabilized protective agent, on the stone surface
KR100515512B1 (en) Aging block of Restoration method and the restoration equipment thereof
JP6975969B2 (en) Cleaning agent composition for crosslinked coating film and floor management method
JP2007152189A (en) House cleaning system, floor stone cleaning system, non-slip floor cleaning system, carpet cleaning system, and overall cleaning system

Legal Events

Date Code Title Description
PB01 Publication
PB01 Publication
SE01 Entry into force of request for substantive examination
SE01 Entry into force of request for substantive examination