CN113585795A - Waterproof coiled material damage repairing method - Google Patents
Waterproof coiled material damage repairing method Download PDFInfo
- Publication number
- CN113585795A CN113585795A CN202110685845.9A CN202110685845A CN113585795A CN 113585795 A CN113585795 A CN 113585795A CN 202110685845 A CN202110685845 A CN 202110685845A CN 113585795 A CN113585795 A CN 113585795A
- Authority
- CN
- China
- Prior art keywords
- repairing
- coiled material
- welding
- block
- spiral
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention discloses a waterproof coiled material damage repairing treatment method, which relates to the technical field of waterproof coiled material repairing and comprises the following steps: obtaining a repairing area and removing a reverse adhesive layer on the waterproof roll in the repairing area; welding the coiled material repairing block on the repairing area to form a spiral welding track; glue is injected between the coiled material repairing block and the waterproof coiled material; according to the method, the coiled material repairing block is welded on the repairing area to form a spiral welding track, glue is injected between the coiled material repairing block and the waterproof coiled material, the welding strength and the bonding strength between the coiled material repairing block and the waterproof coiled material are greatly increased, and the repairing quality of the waterproof coiled material after damage is improved.
Description
Technical Field
The invention belongs to the technical field of waterproof coiled material repair, and particularly relates to a waterproof coiled material damage repair processing method.
Background
At present, more and more engineering projects are aware of the advantages of the pre-paved anti-sticking waterproof system, and particularly, a waterproof coiled material with an anti-sticking function is paved on a building bottom plate, so that post-cast concrete is directly contacted with the bonding surface of the waterproof coiled material to form a bonding state, and the problem of water channeling is avoided to the greatest extent. Meanwhile, in order to ensure that post-cast concrete can be fully contacted with the waterproof coiled material, the waterproof system is not provided with a waterproof protective layer, so that the subsequent reinforcement binding operation is completely finished in a state that the waterproof layer is exposed. Therefore, the finished product protection work of the waterproof layer becomes a serious task, and a complete repair emergency plan is needed while the high polymer waterproof coiled material with excellent puncture resistance and damage resistance is selected for construction. However, from the current construction technology, no special technology for repairing the high polymer waterproof coiled material exists, and the reasons are as follows:
the difference of the performance of the high-molecular coiled material, the conventional pre-paved and anti-sticky high-molecular waterproof coiled material mainly uses high-density polyethylene (HDPE) or Thermoplastic Polyolefin (TPO), and the two materials are welded by mechanical equipment when being bonded, but the welding modes are different due to different material properties; if the High Density Polyethylene (HDPE) welding temperature window is narrow, the crystallinity is as high as 75 percent, the welding can be carried out only by an up-flow welding machine at present, and the waterproof coiled material forms a welding connection state after being heated by a hot wedge of the machine and being rolled by an external force exerted by an upper layer of idler wheel and a lower layer of idler wheel; like TPO waterproofing membrane welding temperature window very wide again, the degree of crystallinity is lower, can carry out welded connection through hot-blast welding machine or welder at present, through the hot-blast heating of machine and roll through upper portion gyro wheel and reach the back, make waterproofing membrane form the welded connection state. The above-mentioned welding operation is characterized by overlapping seams, i.e. welding from one side of the overlapping seam to the other side, i.e. welding from the free end of one side to the free end of the other side, and the whole waterproof roll is a sheet structure after welding, see fig. 1.
The invention patent with application number CN202011438545.2 relates to HDPE repair technology, and relates to step S4, a strong adhesive tape is adopted to temporarily seal a hole on a film surface; step S5, adopting HDPE repairing blocks to carry out extrusion welding repairing on the broken holes of the membrane surface to form permanent and firm HDPE repairing blocks; referring to fig. 2, after the temporary sealing by the strong adhesive tape 102, the welding seam is formed only at the edge of the HDPE repair block 102 by using the squeeze welding repair 103; the repairing mode is forced to solve the problem of welding equipment, and only closed welding can be carried out on the edge of the HDPE repairing block 102, otherwise, the welding width and the closed compactness are influenced due to the limited working face; therefore, under the condition of back water pressure, the edge welding seam of the repairing mode is easy to become leakage hidden trouble.
In addition, because of the temporary random and reliable waterproof coiled material repairing process, the HDPE coiled material is generally adhered by the double-sided adhesive tape on the construction site for simple repairing treatment, and the repairing effect is extremely poor.
Disclosure of Invention
The invention aims to provide a method for repairing and processing the damaged waterproof coiled material, aiming at the defects in the prior art, the method comprises the steps of welding a coiled material repairing block on a repairing area to form a spiral welding track, injecting glue between the coiled material repairing block and the waterproof coiled material, greatly increasing the welding and bonding strength between the coiled material repairing block and the waterproof coiled material, and improving the repairing quality of the damaged waterproof coiled material.
In order to achieve the above object, the present invention provides a method for repairing a damaged waterproof roll, comprising:
obtaining a repairing area and removing a reverse adhesive layer on the waterproof roll in the repairing area;
welding the coiled material repairing block on the repairing area to form a spiral welding track;
and injecting glue between the coiled material repairing block and the waterproof coiled material.
Optionally, the damaged position of the waterproof roll is located at a central position in the repair area.
Optionally, the repair area is circular.
Optionally, the welding the coil material repair block on the repair area to form a spiral welding track includes:
obtaining the coiled material repairing block which can completely cover the repairing area;
aligning the center of the coiled material repairing block to the center of the repairing area and covering the repairing area;
and welding the coiled material repairing block on the repairing area according to a spiral welding track by using an extrusion welding process.
Optionally, the damaged position of the waterproof roll is located in the center of the welding track in the shape of the spiral line, and the damaged position of the waterproof roll is surrounded by the innermost welding track of the welding track in the shape of the spiral line.
Optionally, the spiral welding track enables a spiral cavity to be formed between the coil repairing block and the waterproof coil, and the step of injecting glue between the coil repairing block and the waterproof coil includes: and injecting glue into the spiral cavity.
Optionally, sealant is injected into the spiral cavity by using a glue injection device, so that the spiral cavity is filled with the sealant.
Optionally, the material of the coiled material repairing block is an HDPE coiled material, and an anti-adhesion layer is arranged on the HDPE coiled material.
Optionally, to the coiled material repair piece with still include after the injecting glue between the waterproofing membrane:
and removing part of the edge of the coiled material repairing block, wherein the part of the edge is positioned at the outer side of the outermost circle of the welding track of the spiral line shape, and the part of the edge is not connected with the waterproof coiled material.
Optionally, a partial edge of the web patch is cut off with a wallpaper knife.
The invention provides a method for repairing and treating the damage of a waterproof coiled material, which has the beneficial effects that:
1. according to the method, the coiled material repairing block is welded on the repairing area to form a spiral welding track, glue is injected between the coiled material repairing block and the waterproof coiled material, the welding strength and the bonding strength between the coiled material repairing block and the waterproof coiled material are greatly increased, and the repairing quality of the waterproof coiled material after being damaged is improved;
2. the method adopts an extrusion welding process to effectively connect the coiled material repairing block with the waterproof coiled material and form a spiral cavity for injecting glue, so that the self limitation of welding equipment is solved to the maximum extent, and a continuous sealed repairing structure is formed after the spiral cavity is fully filled with the sealant, so that the repairing effect is ensured;
3. the method adopts the HDPE coiled material with the anti-adhesion layer as the coiled material repairing block, and removes the part of the edge of the coiled material repairing block which is not connected with the waterproof coiled material after the glue injection is finished, so that the anti-adhesion layer of the coiled material repairing block and the anti-adhesion layer of the waterproof coiled material form a continuous anti-adhesion structure, and the repairing requirement of the original pre-laid anti-adhesion waterproof system is fundamentally met.
Additional features and advantages of the invention will be set forth in the detailed description which follows.
Drawings
The above and other objects, features and advantages of the present invention will become more apparent by describing in more detail exemplary embodiments thereof with reference to the attached drawings, in which like reference numerals generally represent like parts throughout.
Fig. 1 shows a schematic view of a sheet structure formed after welding of a waterproof roll in the prior art.
Figure 2 shows a drawing of one prior art patent.
Fig. 3 is a diagram illustrating the construction steps of a method for repairing a damaged waterproofing membrane according to an embodiment of the present invention.
Fig. 4 is a view showing the construction steps of a waterproof roll damage repairing method according to an embodiment of the present invention.
Fig. 5 is a view showing the construction steps of a method for repairing a damaged waterproofing membrane according to an embodiment of the present invention.
Fig. 6 is a view showing the construction steps of a waterproof roll damage repairing method according to an embodiment of the present invention.
Fig. 7 shows a schematic cross-sectional structure of fig. 6.
Description of reference numerals:
in fig. 2:
101. a strong adhesive tape; 102. a HDPE repair block; 103. performing extrusion welding repair;
in fig. 3 to 7:
1. repairing the area; 2. waterproof coiled materials; 3. repairing the coiled material; 4. a helical welding trajectory; 5. a damaged position; 6. a helical cavity; 7. sealing glue; 8. an anti-adhesive layer; 9. a partial edge; 10. and (6) a glue injection port.
Detailed Description
Preferred embodiments of the present invention will be described in more detail below. While the following describes preferred embodiments of the present invention, it should be understood that the present invention may be embodied in various forms and should not be limited by the embodiments set forth herein. Rather, these embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the scope of the invention to those skilled in the art.
The invention provides a waterproof roll damage repairing method, which comprises the following steps:
obtaining a repairing area and removing a reverse adhesive layer on the waterproof roll in the repairing area;
welding the coiled material repairing block on the repairing area to form a spiral welding track;
and injecting glue between the coiled material repairing block and the waterproof coiled material.
Specifically, a repairing area can be marked on the waterproof coiled material, the damaged position of the waterproof coiled material is positioned in the repairing area, a sufficient connecting area is reserved between the edge of the repairing area and the damaged position, a scraper is adopted to scrape off a reverse adhesive layer on the waterproof coiled material in the repairing area, so that the waterproof coiled material in the repairing area is not bonded with a coiled material repairing block covered on the waterproof coiled material repairing block, an extrusion welding process can be adopted to weld the coiled material repairing block on the repairing area, the welding track is in a spiral shape, and is a welding line with a certain width formed by welding, thus a spiral cavity is formed between the waterproof coiled material and the coiled material repairing block in the repairing area by the spiral welding track, the spiral cavity is used for injecting glue, a glue injection gun can be used for injecting sealant into the spiral cavity, and the welding strength and the bonding strength between the coiled material repairing block and the waterproof coiled material are greatly increased, the repair quality of the waterproof roll after being damaged is improved.
Optionally, the waterproof roll is broken at a central position within the repair area.
Specifically, taking the damaged opening on the waterproof coiled material as an example, when the repairing area is defined, the damaged opening is positioned at the center of the repairing area, and a sufficient connecting area is reserved between the edge of the repairing area and the edge of the damaged opening, so that the bonding area can be ensured, and the repairing quality can be improved.
Optionally, the repair area is circular.
In one example, the coiled material repairing block is also cut into a circular shape and covers the repairing area, the circle center of the coiled material repairing block is concentric with the circle center of the repairing area as much as possible, the damaged position is ensured to be also positioned at the center of the coiled material repairing block, and then welding and glue injection are carried out on the periphery of the damaged position, so that the full-adhesion effect on the periphery of the damaged position is formed, and the repairing strength is ensured.
Optionally, welding the coiled material patch on the repair area to form a welding track in a spiral shape comprises:
acquiring a coiled material repairing block capable of completely covering a repairing area;
aligning the center of the coiled material repairing block to the center of the repairing area and covering the repairing area;
and welding the coiled material repairing block on the repairing area according to the spiral welding track by using an extrusion welding process.
Specifically, the center of the coil repairing block is aligned with the center of the repairing area, so that the initial position of welding can be conveniently determined in the subsequent welding process, and the position accuracy of a welding track is ensured.
Optionally, the damaged position of the waterproofing membrane is at the center of the welding track in the shape of a spiral, and the damaged position of the waterproofing membrane is surrounded by the innermost welding track of the welding track in the shape of a spiral.
Specifically, the number of turns of the spiral linear welding track can be confirmed according to position or hydraulic specific requirement, the spiral linear welding track forms the spiral cavity between coiled material repairing block and waterproofing membrane, the inner of spiral cavity is not sealed because the existence of damaged position, the outer end of spiral cavity forms the injecting glue mouth, damaged position is not sealed when injecting glue to the spiral cavity intracavity from the injecting glue mouth, be favorable to the air escape, prevent that the unable discharge of air of spiral cavity hinders sealed gluey colloid full, mechanical construction's drawback has been avoided to the welding mode of this kind of spiral linear welding track in addition, it leads to the ill with closely knit quality to be difficult in end to end department promptly.
Optionally, the welding track of helix shape makes to form the spiral cavity between coiled material repair piece and the waterproofing membrane, and the injecting glue includes between piece and the waterproofing membrane is repaired to the coiled material: and injecting glue into the spiral cavity.
Specifically, the welding track of helix shape has formed first connection structure between coiled material repair piece and waterproofing membrane, has formed the spiral cavity simultaneously, has formed the second connection structure again after sealed glue of injection in the spiral cavity, and first connection structure and second connection structure realize the coiled material jointly that repair piece and waterproofing membrane are connected, guarantee to repair intensity, improve and repair the quality.
Optionally, sealant is injected into the spiral cavity by using a glue injection device, so that the spiral cavity is filled with the sealant.
Specifically, glue injection construction is carried out from a glue injection opening by adopting a sealant matched with the materials of the waterproof coiled material and the coiled material repairing block and a matched glue injection gun, so that the sealant is fully and compactly filled in the spiral cavity.
Optionally, the material of the coil repair block is a HDPE coil, and an anti-adhesive layer is arranged on the HDPE coil.
Specifically, the HDPE coiled material with the anti-adhesion layer is used as the coiled material repairing block, and the part of the edge of the coiled material repairing block which is not connected with the waterproof coiled material is removed after glue injection is completed, so that the anti-adhesion layer of the coiled material repairing block and the anti-adhesion layer of the waterproof coiled material form a continuous anti-adhesion structure, and the repairing requirement of the original pre-laid anti-adhesion waterproof system is met fundamentally.
In one example, the HDPE web is a pre-laid reverse-adhesive type polymeric waterproofing web.
Optionally, still include after the injecting glue between piece and the waterproofing membrane is repaiied to the coiled material:
and removing part of the edge of the coiled material repairing block, wherein part of the edge is positioned at the outer side of the outermost circle of the welding track of the spiral line shape, and part of the edge is not connected with the waterproof coiled material.
Specifically, the peripheral edge of the outermost circle of the welding track along the spiral line shape cuts part of the edge of the coiled material repairing block, and when the edge is cut to the glue injection port, the edge is cut along the section direction of the glue injection port to form an annular cutting line, so that the sealant in the glue injection port is guaranteed to be filled fully and compactly.
Optionally, a wallpaper knife is used to cut off a portion of the edge of the web patch.
Examples
As shown in fig. 3 to 7, the present invention provides a method for repairing damaged waterproof roll, comprising:
obtaining a repairing area 1 and removing a reverse adhesive layer on the waterproof roll 2 in the repairing area 1;
welding the coiled material repairing block 3 on the repairing area 1 to form a spiral welding track 4;
and injecting glue between the coiled material repairing block 3 and the waterproof coiled material 2.
In the present embodiment, the damaged position of the waterproofing membrane 2 is at the center position within the repair area 1.
In the present embodiment, the repair area 1 is circular.
In the present embodiment, the welding track 4 for welding the coil material repair block 3 to the repair area 1 in a spiral shape includes:
obtaining a coiled material repairing block 3 which can completely cover the repairing area 1;
aligning the center of the coiled material repairing block 3 to the center of the repairing area 1 and covering the repairing area 1;
the coil repairing block 3 is welded on the repairing area 1 according to the spiral welding track 4 by using the extrusion welding process.
In the present embodiment, the damaged position 5 of the waterproofing membrane 2 is at the center of the welding locus 4 in the spiral shape, and the damaged position 5 of the waterproofing membrane 2 is surrounded by the innermost welding locus of the welding locus 4 in the spiral shape.
In this embodiment, the spiral welding track 4 forms the spiral cavity 6 between the coil material repairing block 3 and the waterproof coil material 2, and the glue injection between the coil material repairing block 3 and the waterproof coil material 2 includes: glue is injected into the spiral cavity 6.
In this embodiment, the glue injection device is used to inject the sealant 7 into the spiral cavity 6, so that the spiral cavity 6 is filled with the sealant 7.
In this embodiment, the material of the coil repair block 3 is an HDPE coil, and an anti-adhesion layer 8 is disposed on the HDPE coil.
In this embodiment, still include after the injecting glue to between coiled material repairing block 3 and waterproofing membrane 2:
part of the edge 9 of the coil repair block 3 is removed, the part of the edge 9 is positioned outside the outermost welding track of the spiral-shaped welding track 4, and the part of the edge 9 is not connected with the waterproof coil 2.
In this embodiment, a wallpaper knife is used to cut off a portion of the edge 9 of the web repair block 3.
In summary, when the method for repairing damaged waterproof roll provided by the present invention is implemented, taking the example that a damaged opening appears on a polymer waterproof roll: firstly, a repairing area 1 is obtained by referring to fig. 3, namely, a repairing range is determined, the repairing area is determined according to the shape and size of a damaged opening of a waterproof roll 2, the circular repairing area 1 can be drawn on the waterproof roll 2 by taking the center of the damaged opening as a circle center, the distance of at least 200mm is ensured between one end of the damaged opening, which is farthest away from the circle center, and the edge of the repairing area 1, and a scraper is adopted to scrape a viscose layer on the waterproof roll 2 in the repairing area 1 completely after the repairing area 1 is drawn; then, referring to fig. 4, taking a HDPE coiled material with an anti-adhesive layer, cutting a circular coiled material repairing block 3 capable of covering a repairing area, covering the coiled material repairing block 3 on the repairing area 1, ensuring that the circle center of the coiled material repairing block 3 is overlapped with the circle center of the repairing area 1 as much as possible, continuously and outwards performing welding operation between the coiled material repairing block 3 and the waterproof coiled material 2 by adopting an extrusion welding process by taking the center of a damaged port as a central point to form a spiral welding track 4 and ensure that the damaged port is surrounded by the innermost circle welding track of the spiral welding track 4, forming a spiral cavity 6 between the coiled material repairing block 3 and the waterproof coiled material 2 by the spiral welding track 4, wherein the inner end of the spiral cavity 6 is close to the damaged port, and the outer end of the spiral cavity 6 forms an adhesive injection port 10; referring to fig. 5, a glue injection gun is used for injecting the sealant 7 into the spiral cavity 6 from the glue injection port 10, so that the sealant 7 is fully and compactly injected into the spiral cavity 6; finally, referring to fig. 6 and 7, the area where the glue cannot be injected at the partial edge 9 of the coiled material repairing block 3 is completely cut by a wallpaper cutter, so that the periphery of the joint of the coiled material repairing block 9 and the waterproof coiled material 2 can be completely contacted with the concrete, and the pre-paving anti-sticking effect of the original design is formed.
Having described embodiments of the present invention, the foregoing description is intended to be exemplary, not exhaustive, and not limited to the embodiments disclosed. Many modifications and variations will be apparent to those of ordinary skill in the art without departing from the scope and spirit of the described embodiments.
Claims (10)
1. A waterproof roll damage repairing method is characterized by comprising the following steps:
obtaining a repairing area and removing a reverse adhesive layer on the waterproof roll in the repairing area;
welding the coiled material repairing block on the repairing area to form a spiral welding track;
and injecting glue between the coiled material repairing block and the waterproof coiled material.
2. The waterproofing membrane damage repair processing method according to claim 1, wherein the damage position of the waterproofing membrane is located at a central position within the repair area.
3. The method according to claim 2, wherein the repair area is a circular shape.
4. The method for repairing and processing the breakage of a waterproof roll according to claim 1, wherein the welding the repair block to the repair area to form a spiral welding track comprises:
obtaining the coiled material repairing block which can completely cover the repairing area;
aligning the center of the coiled material repairing block to the center of the repairing area and covering the repairing area;
and welding the coiled material repairing block on the repairing area according to a spiral welding track by using an extrusion welding process.
5. The waterproofing membrane damage repairing method according to claim 4, wherein the damage position of the waterproofing membrane is located at the center of the welding locus of the spiral shape, and the damage position of the waterproofing membrane is surrounded by the innermost welding locus of the spiral shape.
6. The method for repairing and processing the breakage of the waterproof roll according to claim 1, wherein the spiral welding track forms a spiral cavity between the roll repairing block and the waterproof roll, and the step of injecting glue between the roll repairing block and the waterproof roll comprises: and injecting glue into the spiral cavity.
7. The method for repairing damaged waterproof roll as claimed in claim 6, wherein a glue injection device is used to inject a sealant into the spiral cavity, so that the spiral cavity is filled with the sealant.
8. The method of claim 1, wherein the material of the coil repair block is a HDPE coil, and the HDPE coil is provided with an anti-adhesive layer.
9. The method for repairing and processing the breakage of a waterproof roll according to claim 1, further comprising, after injecting glue between the roll repairing block and the waterproof roll:
and removing part of the edge of the coiled material repairing block, wherein the part of the edge is positioned at the outer side of the outermost circle of the welding track of the spiral line shape, and the part of the edge is not connected with the waterproof coiled material.
10. The method of claim 9, wherein a partial edge of the web repair piece is cut off by a wallpaper knife.