CN111451194A - Pretreatment device and pretreatment method for copper foil processing - Google Patents

Pretreatment device and pretreatment method for copper foil processing Download PDF

Info

Publication number
CN111451194A
CN111451194A CN202010236878.0A CN202010236878A CN111451194A CN 111451194 A CN111451194 A CN 111451194A CN 202010236878 A CN202010236878 A CN 202010236878A CN 111451194 A CN111451194 A CN 111451194A
Authority
CN
China
Prior art keywords
copper foil
pretreatment
pickling
pipe
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN202010236878.0A
Other languages
Chinese (zh)
Inventor
李衔洋
杨忠岩
王永勤
高斌
贾万泽
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangxi Tongbo Technology Co ltd
Original Assignee
Jiangxi Tongbo Technology Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangxi Tongbo Technology Co ltd filed Critical Jiangxi Tongbo Technology Co ltd
Priority to CN202010236878.0A priority Critical patent/CN111451194A/en
Publication of CN111451194A publication Critical patent/CN111451194A/en
Pending legal-status Critical Current

Abstract

The invention discloses a pretreatment device and a pretreatment method for copper foil processing, and the pretreatment device comprises a pretreatment box, wherein the bottom end surface of the pretreatment box is connected with a plurality of support stand columns, a transverse partition plate is arranged in the middle of the pretreatment box, the front end surface of the transverse partition plate is fixedly connected with a longitudinal partition plate, a first pretreatment chamber is arranged on the left side of the longitudinal partition plate, a second pretreatment chamber is arranged on the right side of the longitudinal partition plate, a third pretreatment chamber is arranged on the rear side of the transverse partition plate, and an end cover is arranged on the upper end surface of the pretreatment box.

Description

Pretreatment device and pretreatment method for copper foil processing
Technical Field
The invention relates to the technical field of copper foil processing equipment, in particular to a pretreatment device and a pretreatment method for copper foil processing.
Background
The electrolytic copper foil is an important material for manufacturing copper clad laminates, printed circuit boards and lithium ion batteries; in the high-speed development of the current electronic information industry, the electrolytic copper foil is called a 'neural network' for signal and power transmission and communication of electronic products; in 2002, the production value of the printed circuit board in China has gone beyond the third world, and the copper clad laminate serving as a substrate material of the PCB also becomes the third world production country, so that the electrolytic copper foil industry in China has been developed rapidly in recent years; the copper foil is easily polluted by grease, sweat stain and the like in the transportation and storage processes, and the surface active polishing is easy to produce an oxide layer on the surface, so the copper foil is pretreated before surface treatment to improve the product quality, and therefore, a pretreatment device and a pretreatment method for processing the copper foil are needed.
Disclosure of Invention
The present invention is directed to a pretreatment apparatus and a pretreatment method for copper foil processing to solve the problems of the background art.
In order to achieve the purpose, the invention provides the following technical scheme:
the utility model provides a preprocessing device is used in copper foil processing, includes the preliminary treatment case, preliminary treatment case bottom end face is connected with a plurality of support posts, be provided with transverse baffle in the middle of the preliminary treatment incasement, terminal surface fixedly connected with longitudinal baffle before the transverse baffle, the longitudinal baffle left side is provided with first preliminary treatment room, the longitudinal baffle right side is provided with second preliminary treatment room, the transverse baffle rear side is provided with third preliminary treatment room, preliminary treatment case up end is provided with the end cover.
As a further scheme of the invention: the utility model discloses a pretreatment tank, including pretreatment tank, left and right sides wall fixedly connected with left mounting panel and right mounting panel respectively, both sides are provided with feeding deflector roll and ejection of compact deflector roll respectively around on the left side mounting panel, rotate on the right side mounting panel and install the transmission roller, both sides are provided with feed inlet and discharge gate respectively around the pretreatment tank left end face, both sides are provided with first transmission mouth and second transmission mouth respectively around the pretreatment tank right-hand member face, be provided with the third transmission mouth in the middle of the longitudinal baffle.
As a further scheme of the invention: the utility model discloses a pretreatment room, including first pretreatment room, first pretreatment room is provided with the water spray standpipe, the water spray standpipe sets up in the side around the copper foil, and the relative one end of front and back side water spray standpipe is connected with a plurality of sprinkler bead, the end cover up end left side is connected with the water spray connector, the water spray connector is connected with front and back side water spray standpipe, the water spray connector external connection has the inlet tube.
As a further scheme of the invention: the utility model discloses a pickling pipe, including first preliminary treatment room, second preliminary treatment room, pickling pipe, copper foil, pickling connector, pickling union coupling, pickling liquid inlet pipe, pickling pipe is provided with in the second preliminary treatment room, the pickling pipe sets up in the copper foil front and back side, and the relative one end of front and back side pickling pipe is connected with a plurality of pickling shower nozzles, the pickling connector is installed on end cover up end right side, the pickling union coupling of pickling connector and front and back side, the pickling.
As a further scheme of the invention: the hot-blast violently pipe that is provided with in the third preliminary treatment room, hot-blast violently pipe side setting around the copper foil, the hot-blast relative one end of violently managing of front and back side is connected with a plurality of hot air spray nozzle, the air heater is installed to end cover up end rear side, the air heater input is connected with the air and advances the pipe, be connected with hot-blast exit tube between the hot-blast violently pipe of air heater output and front and back side.
As a further scheme of the invention: and a plurality of liquid discharge holes are formed in the side walls of the bottoms of the first pretreatment chamber and the second pretreatment chamber.
A copper foil processing pretreatment method is characterized by comprising the following steps:
s1: the copper foil is conveyed through the feeding guide roller and enters the first pretreatment chamber from the feeding hole, the water is pumped into the water inlet pipe by the water pump, and is sprayed out through the water spraying vertical pipe and the water spraying head to spray and wash the front surface and the rear surface of the copper foil;
s2: the copper foil enters the second pretreatment chamber through the third transmission port, and the pickling solution is pumped into the pickling pipe from the pickling solution inlet pipe by the external pickling solution pump and is sprayed out through the pickling spray head to spray acid solution on the front surface and the rear surface of the copper foil;
s3: the copper foil is conveyed from the second pretreatment chamber through a conveying roller and enters the third pretreatment chamber from a second conveying port, and the air is heated by the hot air blower and is sprayed out through a hot air transverse pipe and a hot air spray head to carry out hot air drying treatment on the front surface and the rear surface of the copper foil;
s4: the copper foil is discharged from the discharge port after being dried by hot air and is transmitted by a discharge guide roller.
As a further scheme of the invention: the drying temperature in the step S4 is controlled at 60-80 ℃.
Compared with the prior art, the invention has the beneficial effects that: the invention has simple structure and clear and understandable structure, the copper foil is transmitted by a feeding guide roller and enters a first pretreatment chamber from a feeding hole, a water pump pumps water into a water inlet pipe, the water is sprayed out by a vertical water spraying pipe and a water spraying head to spray the front and back surfaces of the copper foil, then the copper foil enters a second pretreatment chamber through a third transmission hole, an external pickling liquid pump pumps pickling liquid into the pickling pipe from the pickling liquid inlet pipe and sprays the pickling liquid through the pickling head to spray the front and back surfaces of the copper foil, then the copper foil is transmitted by a transmission roller after coming out of the second pretreatment chamber and enters the third pretreatment chamber from the second transmission hole, a hot air blower heats air and sprays hot air through a hot air transverse pipe and a hot air spray head to perform hot air drying treatment on the front and back surfaces of the copper foil, finally the copper foil is discharged from a discharging hole after being subjected to the hot air drying treatment and, the pretreatment effect is good, and the product quality is improved.
Drawings
FIG. 1 is a schematic front view showing a pretreatment apparatus for copper foil processing;
FIG. 2 is a schematic cross-sectional view of a copper foil processing pretreatment apparatus.
In the figure: 1-second transfer port, 2-third pretreatment chamber, 3-hot air blow head, 4-horizontal hot air blow head, 5-transverse partition, 6-discharge port, 7-discharge guide roller, 8-feed guide roller, 9-feed port, 10-drain hole, 11-water blow head, 12-vertical water blow pipe, 13-first pretreatment chamber, 14-longitudinal partition, 15-pretreatment tank, 16-third transfer port, 17-acid washing blow head, 18-acid washing pipe, 19-second pretreatment chamber, 20-first transfer port, 21-right mounting plate, 22-transfer roller, 23-support column, 24-end cap, 25-water inlet pipe, 26-water spray connector, 27-hot air blower, 28-hot air outlet pipe, 29-air inlet pipe, 30-pickling solution inlet pipe, 31-pickling connector and 32-left mounting plate.
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present invention.
Referring to fig. 1-2, the present invention provides a technical solution: the utility model provides a preprocessing device is used in copper foil processing, includes pretreatment tank 15, pretreatment tank 15 bottom end face is connected with a plurality of support posts 23, the centre is provided with transverse partition plate 5 in pretreatment tank 15, transverse partition plate 5 preceding terminal surface fixedly connected with longitudinal baffle 14, longitudinal baffle 14 left side is provided with first pretreatment chamber 13, longitudinal baffle 14 right side is provided with second pretreatment chamber 19, transverse partition plate 5 rear side is provided with third pretreatment chamber 2, pretreatment tank 15 up end is provided with end cover 24.
Wherein, both sides wall is fixedly connected with left mounting panel 32 and right mounting panel 21 respectively about pretreatment tank 15, both sides are provided with feeding deflector roll 8 and ejection of compact deflector roll 7 respectively around on the left mounting panel 32, rotate on the right mounting panel 21 and install transmission roller 22, both sides are provided with feed inlet 9 and discharge gate 6 respectively around the pretreatment tank 15 left end face, both sides are provided with first transmission mouth 20 and second transmission mouth 1 respectively around the pretreatment tank 15 right end face, be provided with third transmission mouth 16 in the middle of longitudinal baffle 14, be provided with water spray standpipe 12 in the first pretreatment room 13, water spray standpipe 12 is set up around the copper foil, and the relative one end of front and back side water spray standpipe 12 is connected with a plurality of sprinkler heads 11, end cover 24 upper end face left side is connected with water spray connector 26, water spray connector 26 is connected with front and back side water spray standpipe 12, a water inlet pipe 25 is connected outside the water spraying connector 26, an acid washing pipe 18 is arranged in the second pretreatment chamber 19, the pickling pipes 18 are arranged at the front side and the rear side of the copper foil, one ends of the front pickling pipe 18 and the rear pickling pipe 18 opposite to each other are connected with a plurality of pickling nozzles 17, the right side of the upper end surface of the end cover 24 is provided with an acid cleaning connector 31, the acid cleaning connector 31 is connected with the acid cleaning pipes 18 at the front side and the rear side, the pickling joint 31 is externally connected with a pickling solution inlet pipe 30, a hot air transverse pipe 4 is arranged in the third pretreatment chamber 2, the hot air transverse pipes 4 are arranged at the front side and the rear side of the copper foil, one ends of the hot air transverse pipes 4 at the front side and the rear side are connected with a plurality of hot air spray heads 3, the rear side of the upper end surface of the end cover 24 is provided with a hot air blower 27, the input end of the hot air blower 27 is connected with an air inlet pipe 29, a hot air outlet pipe 28 is connected between the output end of the hot air blower 27 and the hot air transverse pipes 4 at the front and rear sides, the side walls of the bottoms in the first pretreatment chamber 13 and the second pretreatment chamber 19 are provided with a plurality of liquid discharge holes 10.
A copper foil processing pretreatment method is characterized by comprising the following steps:
s1: the copper foil is conveyed through a feeding guide roller 8 and enters a first pretreatment chamber 13 from a feeding hole 9, the water is pumped into a water inlet pipe 25 by a water pump and is sprayed out through a water spraying vertical pipe 12 and a water spraying head 11, and the front surface and the rear surface of the copper foil are sprayed and washed;
s2: the copper foil enters the second pretreatment chamber 19 through the third transmission port 16, and the pickling solution is pumped into the pickling pipe 18 from the pickling solution inlet pipe 30 by an external pickling solution pump and is sprayed out through the pickling spray head 17 to spray the acid solution on the front surface and the rear surface of the copper foil;
s3: the copper foil is conveyed from the second pretreatment chamber 19 through the conveying roller 22 and enters the third pretreatment chamber 2 from the second conveying port 1, the air is heated by the hot air blower 27 and is sprayed out through the hot air transverse pipe 4 and the hot air spray head 3, and hot air drying treatment is carried out on the front surface and the rear surface of the copper foil;
s4: the copper foil is dried by hot air and then discharged from a discharge port 6 and is conveyed by a discharge guide roller 7.
Wherein, the drying temperature in the step S4 is controlled at 60-80 ℃.
The copper foil is conveyed by the feeding guide roller 8 and enters the first pretreatment chamber 13 from the feeding hole 9, the water is pumped into the water inlet pipe 25 by the water pump and is sprayed out by the water spraying vertical pipe 12 and the water spraying head 11, the front and back surfaces of the copper foil are sprayed, then the copper foil enters a second pretreatment chamber 19 through a third transmission port 16, an external pickling liquid pump pumps pickling liquid into a pickling pipe 18 from a pickling liquid inlet pipe 30 and sprays the pickling liquid through a pickling spray head 17, acid solution is sprayed to the front and rear surfaces of the copper foil, and then, the copper foil is transferred through the transfer roller 22 after coming out of the second pre-treatment chamber 19, and enters the third pretreatment chamber 2 from the second transmission port 1, the air is heated by the hot air blower 27 and is sprayed out by the hot air transverse pipe 4 and the hot air spray head 3, and carrying out hot air drying treatment on the front and rear surfaces of the copper foil, and finally, discharging the copper foil from a discharge port 6 after the hot air drying treatment and conveying the copper foil through a discharge guide roller 7.
It will be evident to those skilled in the art that the invention is not limited to the details of the foregoing illustrative embodiments, and that the present invention may be embodied in other specific forms without departing from the spirit or essential attributes thereof. The present embodiments are therefore to be considered in all respects as illustrative and not restrictive, the scope of the invention being indicated by the appended claims rather than by the foregoing description, and all changes which come within the meaning and range of equivalency of the claims are therefore intended to be embraced therein. Any reference sign in a claim should not be construed as limiting the claim concerned.
Furthermore, it should be understood that although the present description refers to embodiments, not every embodiment may contain only a single embodiment, and such description is for clarity only, and those skilled in the art should integrate the description, and the embodiments may be combined as appropriate to form other embodiments understood by those skilled in the art.

Claims (8)

1. The utility model provides a preprocessing device is used in copper foil processing, includes pretreatment tank (15), its characterized in that: the pretreatment tank (15) bottom end face is connected with a plurality of support columns (23), be provided with horizontal separators (5) in the middle of in pretreatment tank (15), terminal surface fixedly connected with longitudinal baffle (14) before horizontal separators (5), longitudinal baffle (14) left side is provided with first pretreatment chamber (13), longitudinal baffle (14) right side is provided with second pretreatment chamber (19), horizontal separators (5) rear side is provided with third pretreatment chamber (2), pretreatment tank (15) up end is provided with end cover (24).
2. The pretreatment device for copper foil processing according to claim 1, wherein: it is respectively fixedly connected with left side mounting panel (32) and right side mounting panel (21) to pre-processing case (15) left and right sides wall, both sides are provided with feeding deflector roll (8) and ejection of compact deflector roll (7) respectively around left side mounting panel (32) is gone up, it installs transmission roller (22) to rotate on right side mounting panel (21), both sides are provided with feed inlet (9) and discharge gate (6) respectively around pre-processing case (15) left end face, both sides are provided with first transmission mouth (20) and second transmission mouth (1) respectively around pre-processing case (15) right-hand member face, be provided with third transmission mouth (16) in the middle of longitudinal baffle (14).
3. The pretreatment device for copper foil processing according to claim 2, wherein: be provided with water spray standpipe (12) in first preliminary treatment room (13), water spray standpipe (12) side sets up around the copper foil, and the relative one end of front and back side water spray standpipe (12) is connected with a plurality of sprinkler bead (11), end cover (24) up end left side is connected with water spray connector (26), water spray connector (26) are connected with front and back side water spray standpipe (12), water spray connector (26) outer joint has inlet tube (25).
4. The pretreatment device for copper foil processing according to claim 3, wherein: be provided with pickling pipe (18) in second preliminary treatment room (19), pickling pipe (18) side setting around the copper foil, the relative one end of front and back side pickling pipe (18) is connected with a plurality of pickling shower nozzles (17), pickling connector (31) are installed on end cover (24) up end right side, pickling connector (31) are connected with pickling pipe (18) of front and back side, pickling connector (31) outer joint has the pickler to advance pipe (30).
5. The pretreatment device for copper foil processing according to claim 4, wherein: be provided with hot-blast violently pipe (4) in third preliminary treatment room (2), hot-blast violently pipe (4) side setting around the copper foil, the hot-blast horizontal pipe (4) relative one end of front and back side is connected with a plurality of hot-blast shower nozzles (3), air heater (27) are installed to end cover (24) up end rear side, air heater (27) input is connected with air inlet pipe (29), be connected with hot-blast exit tube (28) between hot-blast violently pipe (4) of side around air heater (27) output and front and back.
6. The pretreatment device for copper foil processing according to claim 5, wherein: and a plurality of liquid discharge holes (10) are formed in the side walls of the bottoms in the first pretreatment chamber (13) and the second pretreatment chamber (19).
7. A copper foil processing pretreatment method is characterized by comprising the following steps:
s1: the copper foil is conveyed through a feeding guide roller (8) and enters a first pretreatment chamber (13) from a feeding hole (9), a water pump pumps water into a water inlet pipe (25), and the water is sprayed out through a water spraying vertical pipe (12) and a water spraying head (11) to spray and wash the front surface and the rear surface of the copper foil;
s2: the copper foil enters a second pretreatment chamber (19) through a third transmission port (16), an external pickling liquid pump pumps pickling liquid into a pickling pipe (18) from a pickling liquid inlet pipe (30), and the pickling liquid is sprayed out through a pickling spray head (17) to spray acid liquid on the front surface and the rear surface of the copper foil;
s3: the copper foil is conveyed from the second pretreatment chamber (19) through a conveying roller (22) and enters the third pretreatment chamber (2) from the second conveying port (1), and a hot air blower (27) heats air and sprays hot air through a hot air transverse pipe (4) and a hot air spray head (3) to perform hot air drying treatment on the front surface and the rear surface of the copper foil;
s4: the copper foil is dried by hot air and then discharged from a discharge hole (6) and is transmitted by a discharge guide roller (7).
8. The copper foil processing pretreatment method according to claim 7, characterized in that: the drying temperature in the step S4 is controlled at 60-80 ℃.
CN202010236878.0A 2020-03-30 2020-03-30 Pretreatment device and pretreatment method for copper foil processing Pending CN111451194A (en)