CN110523844A - A kind of progressive die process for stamping of tubulose thin-walled parts - Google Patents

A kind of progressive die process for stamping of tubulose thin-walled parts Download PDF

Info

Publication number
CN110523844A
CN110523844A CN201910835891.5A CN201910835891A CN110523844A CN 110523844 A CN110523844 A CN 110523844A CN 201910835891 A CN201910835891 A CN 201910835891A CN 110523844 A CN110523844 A CN 110523844A
Authority
CN
China
Prior art keywords
tubing
top bar
predicament
strip
groove
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201910835891.5A
Other languages
Chinese (zh)
Other versions
CN110523844B (en
Inventor
庄严
王希亮
江程志
李志华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chengdu Homin Technology Co Ltd
Original Assignee
Chengdu Homin Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chengdu Homin Technology Co Ltd filed Critical Chengdu Homin Technology Co Ltd
Priority to CN201910835891.5A priority Critical patent/CN110523844B/en
Publication of CN110523844A publication Critical patent/CN110523844A/en
Application granted granted Critical
Publication of CN110523844B publication Critical patent/CN110523844B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a kind of progressive die process for stamping of tubulose thin-walled parts, S1, height is selected to be 3 ~ 4mm, wall thickness is 2 ~ 3mm, and tubing (1) is linearly arranged on frame to form strip by the smooth tubing in upper and lower end face (1);S2, by the tubing tooling of head end in strip on the top surface of the groove (3) of cavity plate (2), and ensure that the through-hole (4) of tubing (1) is connected to groove (3);S3, using the formed punch A(5 for being greater than through-hole (4) diameter) top that presses to tubing (1), after being pressed onto certain depth, form the first top bar (6) in tubing (1), while forming first on the outer wall of tubing (1) and getting out of a predicament or an embarrassing situation (7).The beneficial effects of the present invention are: improving processing efficiency, can be realized mass production, improve machining accuracy, simple process.

Description

A kind of progressive die process for stamping of tubulose thin-walled parts
Technical field
The present invention relates to the technical field of tubulose thin-walled parts processing, especially a kind of grading stampings of tubulose thin-walled parts Pressure method.
Background technique
The continuous upgrading of electronic product, the size of electronic component become small at present, and tubulose thin-walled parts are largely put into It uses, tubulose thin-walled parts are mesoporous tubulose, and the wall thickness of tubulose thin-walled parts is 0.35mm, and the planarity requirements of end face are less than In 0.05mm.It processes this tubulose thin-walled parts at present mainly to be processed by the way of cutting, i.e. selection wall thickness is The tubing of 0.35mm directlys adopt mach mode and is cut, although product can be processed, cutting part is generated A large amount of burr is unable to satisfy the requirement that end face plane degree is 0.05mm, to reduce the processing quality of product in order to reach It is required that also needing subsequent grinding process, this, which is undoubtedly, increases production process, reduces production efficiency.Therefore one kind is needed to mention High processing efficiency, improve machining accuracy, can be realized mass production, simple process stamping products method.
Summary of the invention
The purpose of the present invention is to overcome the shortcomings of the existing technology, provide a kind of raising processing efficiency, improve machining accuracy, Can be realized mass production, simple process tubulose thin-walled parts progressive die process for stamping.
The purpose of the present invention is achieved through the following technical solutions: a kind of progressive die process for stamping of tubulose thin-walled parts, It the following steps are included:
S1, height is selected to be 3 ~ 4mm, wall thickness is 2 ~ 3mm, the smooth tubing in upper and lower end face;By the tubing linearly row of interval It is listed on frame to form strip;
S2, the groove that tubing is placed in cavity plate top surface on, and ensure that the through-hole of tubing is connected to groove;
S3, the top that tubing is pressed to using the formed punch A for being greater than through-hole diameter, after being pressed onto certain depth, form first in tubing Top bar, while forming first on the outer wall of tubing and getting out of a predicament or an embarrassing situation;
S4, mobile strip, the first of semi-finished product tubing, which is got out of a predicament or an embarrassing situation, to be supported on the top surface of groove, is then used on less than first The formed punch B of stepped diameters is pressed on the top surface of the first top bar, and after being pressed onto certain depth, is formed on semi-finished product tubing Two top bars, while forming second on the outer wall of semi-finished product tubing and getting out of a predicament or an embarrassing situation;
S5, it is continued to move to strip, gets out of a predicament or an embarrassing situation when final stage and be equal to required tubulose thin-walled with the horizontal space of final stage top bar When the wall thickness 0.35mm of part, stop pressurization;
S6, using the formed punch C equal with final stage top bar diameter, final stage top bar is inserted into from top to bottom, to will obtain Tubulose thin-walled parts fall off, and finally obtain product.
The invention has the following advantages that the present invention improves processing efficiency, improves machining accuracy, simple process.
Detailed description of the invention
Fig. 1 is the operation schematic diagram of first time punching press tubing;
Fig. 2 is the structural schematic diagram of the tubing after first time punching press;
Fig. 3 is the operation schematic diagram of second of punching press tubing;
Fig. 4 is the structural schematic diagram of the tubing after second of punching press;
Fig. 5 is the structural schematic diagram of product after punching press;
In figure, 1- tubing, 2- cavity plate, 3- groove, 4- through-hole, the first top bar of 5- formed punch A, 6-, 7- first gets out of a predicament or an embarrassing situation, 8- second Top bar, 9- second get out of a predicament or an embarrassing situation, 10- formed punch B.
Specific embodiment
The present invention will be further described with reference to the accompanying drawing, and protection scope of the present invention is not limited to as described below:
As shown in Fig. 1 ~ 5, a kind of progressive die process for stamping of tubulose thin-walled parts, it the following steps are included:
S1, height is selected to be 3 ~ 4mm, wall thickness is 2 ~ 3mm, the smooth tubing 1 in upper and lower end face;
S2, the groove 3 that tubing is placed in cavity plate 2 top surface on, and ensure that the through-hole 4 of tubing 1 is connected to groove 3;
S3, the top that tubing 1 is pressed to using the formed punch A5 for being greater than 4 diameter of through-hole, after being pressed onto certain depth, are formed in tubing 1 First top bar 6, while forming first on the outer wall of tubing 1 and getting out of a predicament or an embarrassing situation 7;
S4, mobile strip, the first of semi-finished product tubing, which is got out of a predicament or an embarrassing situation, 7 to be supported on the top surface of groove 3, then using less than first The formed punch B10 of 6 diameter of top bar is pressed on the top surface of the first top bar 6, after being pressed onto certain depth, on semi-finished product tubing The second top bar 8 is formed, while forming second on the outer wall of semi-finished product tubing 1 and getting out of a predicament or an embarrassing situation 9;
S5, it is continued to move to strip, gets out of a predicament or an embarrassing situation when final stage and be equal to required tubulose thin-walled with the horizontal space of final stage top bar When the wall thickness 0.35mm of part, stop pressurization;
S6, using the formed punch C equal with final stage top bar diameter, final stage top bar is inserted into from top to bottom, to will obtain Tubulose thin-walled parts fall off, and finally obtain product.Therefore this method obtains thin-walled tubular part in the form of punching press, obtains Part upper and lower end face it is smooth, it is ensured that the machining accuracy of end face, furthermore instead of original cutting mode, without subsequent Upper and lower end face is ground again, the labor intensity of worker is greatly alleviated, further improves production efficiency.In addition, It is arranged with multiple products in strip, can be embarked on journey multiple products by time processing, realize the mass production of product.
The above is only a preferred embodiment of the present invention, it should be understood that the present invention is not limited to described herein Form should not be regarded as an exclusion of other examples, and can be used for other combinations, modifications, and environments, and can be at this In the text contemplated scope, modifications can be made through the above teachings or related fields of technology or knowledge.And those skilled in the art institute into Capable modifications and changes do not depart from the spirit and scope of the present invention, then all should be in the protection scope of appended claims of the present invention It is interior.

Claims (1)

1. a kind of progressive die process for stamping of tubulose thin-walled parts, it is characterised in that: it the following steps are included:
S1, height is selected to be 3 ~ 4mm, wall thickness is 2 ~ 3mm, the smooth tubing in upper and lower end face (1);Linearly by tubing (1) It is arranged on frame to form strip;
S2, by the tubing tooling of head end in strip on the top surface of the groove (3) of cavity plate (2), and ensure the through-hole of tubing (1) (4) it is connected to groove (3);
S3, using the formed punch A(5 for being greater than through-hole (4) diameter) top that presses to tubing (1), after being pressed onto certain depth, in tubing (1) the first top bar (6) are formed in, while forming first on the outer wall of tubing (1) and getting out of a predicament or an embarrassing situation (7);
S4, mobile strip, the first of semi-finished product tubing get out of a predicament or an embarrassing situation (7) be supported on the top surface of groove (3), then using being less than The formed punch B(10 of the first top bar (6) diameter) it is pressed on the top surface of the first top bar (6), after being pressed onto certain depth, half The second top bar (8) are formed on finished product tubing, while being formed second on the outer wall of semi-finished product tubing (1) and being got out of a predicament or an embarrassing situation (9);
S5, it is continued to move to strip, gets out of a predicament or an embarrassing situation when final stage and be equal to required tubulose thin-walled with the horizontal space of final stage top bar When the wall thickness 0.35mm of part, stop pressurization;
S6, using the formed punch C equal with final stage top bar diameter, final stage top bar is inserted into from top to bottom, to will obtain Tubulose thin-walled parts fall off, and finally obtain product.
CN201910835891.5A 2019-09-05 2019-09-05 Progressive die stamping method for tubular thin-wall part Active CN110523844B (en)