CN110079854A - A kind of environment-friendly type nitric acid fog inhibitor - Google Patents

A kind of environment-friendly type nitric acid fog inhibitor Download PDF

Info

Publication number
CN110079854A
CN110079854A CN201910296789.2A CN201910296789A CN110079854A CN 110079854 A CN110079854 A CN 110079854A CN 201910296789 A CN201910296789 A CN 201910296789A CN 110079854 A CN110079854 A CN 110079854A
Authority
CN
China
Prior art keywords
acid
nitric acid
environment
friendly type
salt
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201910296789.2A
Other languages
Chinese (zh)
Inventor
李华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangzhou Heng Rong Electronic Technology Co Ltd
Original Assignee
Guangzhou Heng Rong Electronic Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangzhou Heng Rong Electronic Technology Co Ltd filed Critical Guangzhou Heng Rong Electronic Technology Co Ltd
Priority to CN201910296789.2A priority Critical patent/CN110079854A/en
Publication of CN110079854A publication Critical patent/CN110079854A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of environment-friendly type nitric acid fog inhibitors, including following raw material: taking water as a solvent, volume ratio number meter by weight, urea 6-10g/L, citric acid 6-10g/L, sulfamic acid 6-10g/L, salt 8-12g/L, preparation method are as follows: mix urea, citric acid, sulfamic acid, salt, then slowly add water and stir to all dissolution to get.The present invention is used as additive, and the nitric acid slot after plating copper and tin is able to suppress NO2The acid mists such as gas, it is environmental-friendly, the irritating NO of yellow is not generated2Gas.Nitric acid fog inhibitor prepared by the present invention is rapid-action, after this agent is added, after a few minutes can automatical and efficient suppression mist, preparation method is simple, at low cost, safety and stability.

Description

A kind of environment-friendly type nitric acid fog inhibitor
Technical field
The present invention relates to electroless plating strip field, in particular to a kind of environment-friendly type nitric acid fog inhibitor.
Background technique
In electroplating process, typically use nitric acid as stripper.But nitric acid is a kind of deep-etching, it is toxic, The liquid medicine of high pollution, it is high containing ammonia nitrogen, to equipment, to personnel, environment is influenced very big.Nitric acid when stripping the metals such as copper and tin, Can emerge sharp aroma and NO2Toxic tobacco, these acid mists not only result in environmental pollution, and the workshop that can also corrode surrounding is set Standby, facility, or even human health is had an impact.Therefore research and development use cost is cheap, suppression fog effect is good, corrosion mitigating effect Good, environment amenable fog inhibitor, undoubtedly has important practical value.
Summary of the invention
The technical problem to be solved in the present invention is to provide a kind of environment-friendly type nitric acid fog inhibitors.
In order to solve the above-mentioned technical problem, the technical solution of the present invention is as follows:
A kind of environment-friendly type nitric acid fog inhibitor, including following raw material: taking water as a solvent, by weight volume ratio number meter, urea 6- 10g/L, citric acid 6-10g/L, sulfamic acid 6-10g/L, salt 8-12g/L.
Preferably, including following raw material: take water as a solvent, by weight volume ratio number meter, urea 8g/L, citric acid 8g/L, Sulfamic acid 8g/L, salt 10g/L.
Preferably, including following raw material: take water as a solvent, by weight volume ratio number meter, urea 6g/L, citric acid 6g/L, Sulfamic acid 6g/L, salt 8g/L.
Preferably, including following raw material: taking water as a solvent, by weight volume ratio number meter, urea 10g/L, citric acid 10g/ L, sulfamic acid 10g/L, salt 12g/L.
The present invention also provides the preparation methods of the environment-friendly type nitric acid fog inhibitor: by urea, citric acid, sulfamic acid, salt Mixing, then slowly add water and stir to all dissolution to get.
Compared with prior art, the invention has the following beneficial effects: the present invention uses as additive, is used in electro-coppering Nitric acid slot after tin, is able to suppress NO2The acid mists such as gas, it is environmental-friendly, the irritating NO of yellow is not generated2Gas.System of the present invention Standby nitric acid fog inhibitor is rapid-action, after this agent is added, after a few minutes can automatical and efficient suppression mist, preparation method is simple, at low cost, Safety and stability.
Specific embodiment
It to facilitate the understanding of the present invention, below will be to invention is more fully described.But the present invention can be to be permitted Mostly different form is realized, however it is not limited to embodiment described herein.On the contrary, purpose of providing these embodiments is makes It is more thorough and comprehensive to the understanding of the disclosure.
Unless otherwise defined, all technical and scientific terms used herein and belong to technical field of the invention The normally understood meaning of technical staff is identical.Term as used herein in the specification of the present invention is intended merely to description tool The purpose of the embodiment of body, it is not intended that in the limitation present invention.
Embodiment 1
1L environment-friendly type nitric acid fog inhibitor is prepared, urea 8g, citric acid 8g, sulfamic acid 8g, salt 10g are mixed, then delayed It is slow be added water stir to all dissolutions to get.
Embodiment 2
1L environment-friendly type nitric acid fog inhibitor is prepared, urea 6g, citric acid 6g, sulfamic acid 6g, salt 8g are mixed, then slowly Be added water stir to all dissolution to get.
Embodiment 3
1L environment-friendly type nitric acid fog inhibitor is prepared, urea 10g, citric acid 10g, sulfamic acid 10g, salt 12g are mixed, then Be slowly added to water stir to all dissolution to get.
The nitric acid fog inhibitor prepared in above-described embodiment 1 to 3 is detected respectively, by the 1-2%% of strip sump volume Addition, the results are shown in Table 1:
1 testing result of table
By upper table 1 it is found that the nitric acid fog inhibitor prepared in above-described embodiment 1 to 3, suppression fog effect more than 96% with On, wherein being most preferred embodiment with the nitric acid fog inhibitor cost performance highest prepared in embodiment 1.
The foregoing is only a preferred embodiment of the present invention, is not intended to restrict the invention, for the general of this field For logical technical staff, the invention may be variously modified and varied, all within the spirits and principles of the present invention, made What modification, equivalent replacement, improvement etc., should all be included in the protection scope of the present invention.

Claims (5)

1. a kind of environment-friendly type nitric acid fog inhibitor, it is characterised in that: including following raw material: taking water as a solvent, by weight volume ratio number Meter, urea 6-10g/L, citric acid 6-10g/L, sulfamic acid 6-10g/L, salt 8-12g/L.
2. environment-friendly type nitric acid fog inhibitor according to claim 1, it is characterised in that: including following raw material: it takes water as a solvent, Volume ratio number meter by weight, urea 8g/L, citric acid 8g/L, sulfamic acid 8g/L, salt 10g/L.
3. environment-friendly type nitric acid fog inhibitor according to claim 1, it is characterised in that: including following raw material: it takes water as a solvent, Volume ratio number meter by weight, urea 6g/L, citric acid 6g/L, sulfamic acid 6g/L, salt 8g/L.
4. environment-friendly type nitric acid fog inhibitor according to claim 1, it is characterised in that: including following raw material: it takes water as a solvent, Volume ratio number meter by weight, urea 10g/L, citric acid 10g/L, sulfamic acid 10g/L, salt 12g/L.
5. environment-friendly type nitric acid fog inhibitor according to claim 1-4, it is characterised in that: by urea, citric acid, ammonia Base sulfonic acid, salt mixing, then slowly add water and stir to all dissolution to get.
CN201910296789.2A 2019-04-14 2019-04-14 A kind of environment-friendly type nitric acid fog inhibitor Pending CN110079854A (en)