CN109701909A - A method of screening rectangular lithium ion battery leakage - Google Patents

A method of screening rectangular lithium ion battery leakage Download PDF

Info

Publication number
CN109701909A
CN109701909A CN201811545652.8A CN201811545652A CN109701909A CN 109701909 A CN109701909 A CN 109701909A CN 201811545652 A CN201811545652 A CN 201811545652A CN 109701909 A CN109701909 A CN 109701909A
Authority
CN
China
Prior art keywords
lithium ion
ion battery
leakage
battery
rectangular lithium
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201811545652.8A
Other languages
Chinese (zh)
Inventor
罗令
蔡锦章
林海军
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SINOWATT DONGGUAN Ltd
Original Assignee
SINOWATT DONGGUAN Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SINOWATT DONGGUAN Ltd filed Critical SINOWATT DONGGUAN Ltd
Priority to CN201811545652.8A priority Critical patent/CN109701909A/en
Publication of CN109701909A publication Critical patent/CN109701909A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of methods for screening rectangular lithium ion battery leakage, and rectangular lithium ion battery is placed in high humidity environment and is shelved a period of time, then by manually visualizing full inspection weld appearance, pick out the rectangular lithium ion battery of weld seam leakage.Screening technique provided by the invention is easy to operate, low in cost, and effect is obvious.

Description

A method of screening rectangular lithium ion battery leakage
Technical field
The present invention relates to battery manufacturing fields, and in particular to a method of screening rectangular lithium ion battery leakage.
Background technique
Rectangular lithium ion battery with aluminum shell production technology is generally to enter high temperature ageing process, the method for screening leakage after cleaning Also traditional artificial visual full inspection appearance is mostly used.Under normal circumstances, leakage is bad at steel ball sealing liquid injection hole, aluminum hull and Aluminum cover At the laser weld of interference fit, by manually visualizing full inspection, it is very easy to filter out leakage battery.But it is very subtle Weld seam trachoma is then difficult full inspection by visual observation and filters out, especially the material or surface because of aluminum hull and Aluminum cover interference fit There are impurity or dirty, or the interference fit factors such as defect or laser power deficiency, and seriously affect laser welding melting effect, But just not by the select lithium ion battery of leak detecting device, can not be filtered out at all by manually visualizing full inspection weld seam. There are the battery of weld seam trachoma leakage defect, outside moisture can be reacted with these electrolyte leaked out, and generation can accelerate trachoma The HF acid that leakage pitting corrosion becomes larger, while inside battery is entered by liquid-leaking nozzle, lithium ion battery super thick, low appearance are eventually led to, Even occur exploding.
Summary of the invention
The technical problem to be solved in the present invention is to overcome disadvantages described above, a kind of screening rectangular lithium ion battery leakage is provided Method, principle is: as long as being exposed in high humidity environment a period of time, rectangular lithium ion battery with aluminum shell can be because by high humidity environment Influence, and there is obviously weld seam trachoma.The battery of weld seam trachoma leakage defect is filtered out using high humidity environment.
Technical problem of the invention is achieved by the following technical programs.
The method of this rectangular lithium ion battery with aluminum shell leakage of screening: rectangular lithium ion battery with aluminum shell is placed on high humidity environment In shelve a period of time, then the battery of leakage is picked out by artificial visual full inspection.
The temperature of the high humidity environment is preferably 35~45 DEG C.
The relative humidity of the high humidity environment is preferably 85~95RH%.
Described shelves a period of time preferably 2~5 days.
The beneficial effects of the present invention are: first, solve those batteries for there was only very subtle weld seam trachoma leakage traces, In full inspection appearance, it is not easy to the problem of identifying, easily failing to judge;The second, solving those, there are potential weld seam trachoma leakage defects Battery, at all can not be by manually visualizing the problem of full inspection weld seam filters out.Compared with traditional screening leakage method, it can make The battery of those very subtle weld seam trachoma leakage traces, and there are the batteries of potential weld seam trachoma leakage defect, short Obviously weld seam trachoma leakage trace is exposed in time, when making to manually visualize full inspection weld appearance, is very easy to identification And it filters out.There is super thick, low appearance, even explosion equiprobability with great practice significance in end user location to battery is reduced.
Specific embodiment
Below in conjunction with specific embodiment, the invention will be further described.
The present invention relates to battery manufacturing fields, and in particular to a method of screen rectangular lithium ion battery with aluminum shell leakage. A certain number of rectangular lithium ion battery with aluminum shell are placed in a period of time, embodiment envionmental humidity in 35~45 DEG C of environment For 85~95RH%, reference examples envionmental humidity is 5~75RH%, and the leakage that Statistics Implementation example and reference examples are picked out respectively is not Good number of batteries.
Embodiment 1
Take model 993448AR with the ring that battery 1000pcs is placed in 35~45 DEG C, relative humidity is 85~95RH% after batch cleaning In border, successively in the 1st, 2,3,4,5,10,20,30 day full inspection battery appearance, picks out the bad battery number of weld seam leakage and be followed successively by 18pcs、1pcs、0、0、0、0、0、0。
Reference examples 1
Take model 993448AR with the ring that battery 1000pcs is placed in 35~45 DEG C, relative humidity is 5~75RH% after batch cleaning In border, successively in the 1st, 2,3,4,5,10,20,30 day full inspection battery appearance, picks out the bad battery number of weld seam leakage and be followed successively by 0、0、1pcs、0、0、7pcs、0、1pcs。
Embodiment 2
Take model 883038AR with the ring that battery 1000pcs is placed in 35~45 DEG C, relative humidity is 85~95RH% after batch cleaning In border, successively in the 1st, 2,3,4,5,10,20,30 day full inspection battery appearance, picks out the bad battery number of weld seam leakage and be followed successively by 23pcs、1pcs、1pcs、0、0、0、0、0。
Reference examples 2
Take model 883038AR with the ring that battery 1000pcs is placed in 35~45 DEG C, relative humidity is 5~75RH% after batch cleaning In border, successively in the 1st, 2,3,4,5,10,20,30 day full inspection battery appearance, picks out the bad battery number of weld seam leakage and be followed successively by 0、1pcs、0、0、0、10pcs、0、0。
Embodiment 3
Take model 603450AR with the ring that battery 1000pcs is placed in 35~45 DEG C, relative humidity is 85~95RH% after batch cleaning In border, successively in the 1st, 2,3,4,5,10,20,30 day full inspection battery appearance, picks out the bad battery number of weld seam leakage and be followed successively by 12pcs、0、0、0、0、0、0、0。
Reference examples 3
Take model 603450AR with the ring that battery 1000pcs is placed in 35~45 DEG C, relative humidity is 5~75RH% after batch cleaning In border, successively in the 1st, 2,3,4,5,10,20,30 day full inspection battery appearance, picks out the bad battery number of weld seam leakage and be followed successively by 0、0、0、0、0、4pcs、0、0。
Embodiment 4
Take model 563855AR with the ring that battery 1000pcs is placed in 35~45 DEG C, relative humidity is 85~95RH% after batch cleaning In border, successively in the 1st, 2,3,4,5,10,20,30 day full inspection battery appearance, picks out the bad battery number of weld seam leakage and be followed successively by 13pcs、2pcs、0、0、0、0、0、0。
Reference examples 4
Take model 563855AR with the ring that battery 1000pcs is placed in 35~45 DEG C, relative humidity is 5~75RH% after batch cleaning In border, successively in the 1st, 2,3,4,5,10,20,30 day full inspection battery appearance, picks out the bad battery number of weld seam leakage and be followed successively by 0、0、0、0、1pcs、3pcs、0、0。
Embodiment 5
Take model 423450AR with the ring that battery 1000pcs is placed in 35~45 DEG C, relative humidity is 85~95RH% after batch cleaning In border, successively in the 1st, 2,3,4,5,10,20,30 day full inspection battery appearance, picks out the bad battery number of weld seam leakage and be followed successively by 8pcs、0、0、0、0、0、0、0。
Reference examples 5
Take model 423450AR with the ring that battery 1000pcs is placed in 35~45 DEG C, relative humidity is 5~75RH% after batch cleaning In border, successively in the 1st, 2,3,4,5,10,20,30 day full inspection battery appearance, picks out the bad battery number of weld seam leakage and be followed successively by 0、0、0、0、0、2pcs、0、0。
It can be seen that the method phase with the screening battery weld seam leakage of traditional high temperature ageing process from the statistical data of table 1 Than after the method for the present invention, each bad number of batteries of model leakage that full inspection appearance process is sifted out is dramatically increased, and main Concentration occurs on day 1, and in subsequent 29 days, only has pole Individual cells at the 2nd~3 day and weld seam trachoma leakage occur. Illustrate those subtle weld seam leakages or there are the batteries of potential weld seam leakage defect, can be mentioned because of the influence that high humidity environment corrodes It is preceding to expose obviously weld seam leakage trace in full inspection appearance process and filtered out by identification easily.Also reflecting indirectly makes Leakage battery failing to judge there are certain ratio is screened with conventional high-temperature aging method.
Be content above it is that a further detailed description of the present invention in conjunction with specific preferred embodiments, cannot recognizes Fixed specific implementation of the invention is only limited to these explanations.Person of an ordinary skill in the technical field of the invention is come It says, without departing from the inventive concept of the premise, a number of simple deductions or replacements can also be made, all shall be regarded as belonging to this hair Bright protection scope.

Claims (4)

1. a kind of method for screening rectangular lithium ion battery leakage, which is characterized in that rectangular lithium ion battery is placed on high humidity ring A period of time is shelved in border, by manually visualizing full inspection weld appearance, filters out leakage rectangular lithium ion battery.
2. the method for screening rectangular lithium ion battery leakage according to claim 1, which is characterized in that high humidity environment temperature Preferably 35~45 DEG C.
3. the method for screening rectangular lithium ion battery leakage according to claim 1, which is characterized in that high humidity environment is opposite Humidity is preferably 85~95 RH%.
4. the method for screening rectangular lithium ion battery leakage according to claim 1, which is characterized in that described to shelve one section Time is preferably 2~5 days.
CN201811545652.8A 2018-12-18 2018-12-18 A method of screening rectangular lithium ion battery leakage Pending CN109701909A (en)