CN109594414A - A kind of sizing agent of wrapping paper and preparation method thereof - Google Patents
A kind of sizing agent of wrapping paper and preparation method thereof Download PDFInfo
- Publication number
- CN109594414A CN109594414A CN201811478945.9A CN201811478945A CN109594414A CN 109594414 A CN109594414 A CN 109594414A CN 201811478945 A CN201811478945 A CN 201811478945A CN 109594414 A CN109594414 A CN 109594414A
- Authority
- CN
- China
- Prior art keywords
- parts
- water
- wrapping paper
- sizing agent
- initiator
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
A kind of sizing agent of wrapping paper, it calculates by weight, including 10-20 parts of starch sodium hydrogensulfite, 5-10 parts of potassium sulfate, 5-10 parts of magnesium sulfate, 10-16 parts of citric acid, 10-18 parts of deionized water, 20-30 parts of cationic rosin size, 1-10 parts of potassium dihydrogen phosphate, 10-20 parts of polyethylene glycol-1000,1-10 parts of sodium nitrate, 2-8 parts of vinyl imidazole, 1-10 parts of modified petroleum resin, 10-20 parts of surfactant, 1-5 parts of initiator, 100-150 parts of water.The present invention relates to sizing agents to have the characteristics that air permeability is good, water resistance is strong, adhesive strength is high, safety and environmental protection, stability are good.
Description
Technical field
The present invention relates to paper industries, and in particular to a kind of sizing agent of wrapping paper and preparation method thereof.
Background technique
With the economic development in China, material flow industry has also obtained quick development, since the article for needing to circulate is more next
It is more, it is also increasing for the demand for being packed for carton.Currently, being used for the generally existing sterilization process of wrapper surface sizing agent
Middle Cypres easily adhere to and destroy packing material health on packing material, and the heat seal strength of paper and film is inadequate, cause paper
Bag sealing is insecure, and paper is not completely separated with film when removing, and causes that paper bag is damaged or paper fibre is viscous out.
Summary of the invention
The purpose of the present invention is to provide sizing agent of a kind of wrapping paper and preparation method thereof, which has ventilative
It spends, the feature that water resistance is strong, adhesive strength is high, safety and environmental protection, stability are good.
Technical solution of the present invention: a kind of sizing agent of wrapping paper calculates by weight, including starch sodium hydrogensulfite
10-20 parts, 5-10 parts of potassium sulfate, 5-10 parts of magnesium sulfate, 10-16 parts of citric acid, 10-18 parts of deionized water, cationic rosin size
20-30 parts, 1-10 parts of potassium dihydrogen phosphate, 10-20 parts of polyethylene glycol-1000,1-10 parts of sodium nitrate, 2-8 parts of vinyl imidazole,
1-10 parts of modified petroleum resin, 10-20 parts of surfactant, 1-5 parts of initiator, 100-150 parts of water.
The sizing agent of aforementioned wrapping paper, calculates by weight, including 12-18 parts of starch sodium hydrogensulfite, potassium sulfate 6-9
Part, 6-9 parts of magnesium sulfate, 12-15 parts of citric acid, 12-16 parts of deionized water, 22-28 parts of cationic rosin size, potassium dihydrogen phosphate 2-
8 parts, 12-18 parts of polyethylene glycol-1000,2-8 parts of sodium nitrate, 3-7 parts of vinyl imidazole, 2-8 parts of modified petroleum resin, surface
12-18 parts of activating agent, 2-4 parts of initiator, 120-140 parts of water.
The sizing agent of aforementioned wrapping paper, calculates by weight, including 15 parts of starch sodium hydrogensulfite, 8 parts of potassium sulfate, sulphur
8 parts of sour magnesium, 13 parts of citric acid, 14 parts of deionized water, 25 parts of cationic rosin size, 6 parts of potassium dihydrogen phosphate, polyethylene glycol-
100015 parts, 5 parts of sodium nitrate, 5 parts of vinyl imidazole, 6 parts of modified petroleum resin, 15 parts of surfactant, 3 parts of initiator, water
130 parts.
The preparation method of the sizing agent of aforementioned wrapping paper, which comprises the following steps:
(1) starch sodium hydrogensulfite, potassium sulfate, magnesium sulfate, citric acid, deionized water are added in the water of part and are dissolved, is heated to
90-120 DEG C, 10-20min is stirred, adds cationic rosin size, potassium dihydrogen phosphate, polyethylene glycol-1000 stirring 60-90min;
(2) sodium nitrate, vinyl imidazole are added in remaining water, are heated to 90-120 DEG C, modified petroleum resin is added, surface is lived
Property agent, initiator, stir 30-45min;
(3) by step (1), (2) material and other residual components mix, be heated to 80-100 DEG C, be stirred to react 2-4h to get.
Compared with prior art, the invention has the following beneficial effects:
The present invention relates to sizing agents to have the characteristics that air permeability is good, water resistance is strong, adhesive strength is high, safety and environmental protection, stability are good.
Specific embodiment
Embodiment 1
A kind of sizing agent of wrapping paper, calculates by weight, including 10 parts of starch sodium hydrogensulfite, 5 parts of potassium sulfate, magnesium sulfate
5 parts, 10 parts of citric acid, 10 parts of deionized water, 20 parts of cationic rosin size, 1 part of potassium dihydrogen phosphate, polyethylene glycol-1000 10
Part, 1 part of sodium nitrate, 2 parts of vinyl imidazole, 1 part of modified petroleum resin, 10 parts of surfactant, 1 part of initiator, 100 parts of water.
The preparation method of the sizing agent of the wrapping paper, comprising the following steps:
(1) starch sodium hydrogensulfite, potassium sulfate, magnesium sulfate, citric acid, deionized water are added in the water of part and are dissolved, is heated to
90 DEG C, 10min is stirred, adds cationic rosin size, potassium dihydrogen phosphate, polyethylene glycol-1000 stirring 60min;
(2) sodium nitrate, vinyl imidazole are added in remaining water, are heated to 90 DEG C, modified petroleum resin, surface-active is added
30min is stirred in agent, initiator;
(3) by step (1), (2) material and other residual components mix, be heated to 80 DEG C, be stirred to react 2h to get.
Embodiment 2
A kind of sizing agent of wrapping paper, calculates by weight, including 15 parts of starch sodium hydrogensulfite, 8 parts of potassium sulfate, magnesium sulfate
8 parts, 13 parts of citric acid, 14 parts of deionized water, 25 parts of cationic rosin size, 6 parts of potassium dihydrogen phosphate, 15 parts of polyethylene glycol-1000,
5 parts of sodium nitrate, 5 parts of vinyl imidazole, 6 parts of modified petroleum resin, 15 parts of surfactant, 3 parts of initiator, 130 parts of water.
The preparation method of the sizing agent of the wrapping paper, comprising the following steps:
(1) starch sodium hydrogensulfite, potassium sulfate, magnesium sulfate, citric acid, deionized water are added in the water of part and are dissolved, is heated to
100 DEG C, 15min is stirred, adds cationic rosin size, potassium dihydrogen phosphate, polyethylene glycol-1000 stirring 75min;
(2) sodium nitrate, vinyl imidazole are added in remaining water, are heated to 100 DEG C, modified petroleum resin, surface-active is added
40min is stirred in agent, initiator;
(3) by step (1), (2) material and other residual components mix, be heated to 90 DEG C, be stirred to react 3h to get.
Embodiment 3
A kind of sizing agent of wrapping paper, calculates by weight, including 20 parts of starch sodium hydrogensulfite, 10 parts of potassium sulfate, sulfuric acid
10 parts of magnesium, 16 parts of citric acid, 18 parts of deionized water, 30 parts of cationic rosin size, 10 parts of potassium dihydrogen phosphate, polyethylene glycol-1000
20 parts, 10 parts of sodium nitrate, 8 parts of vinyl imidazole, 10 parts of modified petroleum resin, 20 parts of surfactant, 5 parts of initiator, water 150
Part.
The preparation method of the sizing agent of the wrapping paper, comprising the following steps:
(1) starch sodium hydrogensulfite, potassium sulfate, magnesium sulfate, citric acid, deionized water are added in the water of part and are dissolved, is heated to
120 DEG C, 20min is stirred, adds cationic rosin size, potassium dihydrogen phosphate, polyethylene glycol-1000 stirring 90min;
(2) sodium nitrate, vinyl imidazole are added in remaining water, are heated to 120 DEG C, modified petroleum resin, surface-active is added
45min is stirred in agent, initiator;
(3) by step (1), (2) material and other residual components mix, be heated to 100 DEG C, be stirred to react 4h to get.
Claims (4)
1. a kind of sizing agent of wrapping paper, calculates by weight, it is characterised in that: including 10-20 parts of starch sodium hydrogensulfite,
5-10 parts of potassium sulfate, 5-10 parts of magnesium sulfate, 10-16 parts of citric acid, 10-18 parts of deionized water, 20-30 parts of cationic rosin size,
1-10 parts of potassium dihydrogen phosphate, 10-20 parts of polyethylene glycol-1000,1-10 parts of sodium nitrate, 2-8 parts of vinyl imidazole, modified petroleum
1-10 parts of resin, 10-20 parts of surfactant, 1-5 parts of initiator, 100-150 parts of water.
2. the sizing agent of wrapping paper according to claim 1, calculates by weight, it is characterised in that: including starch sulfurous
12-18 parts of sour hydrogen sodium, 6-9 parts of potassium sulfate, 6-9 parts of magnesium sulfate, 12-15 parts of citric acid, 12-16 parts of deionized water, cation pine
22-28 parts of balosam, 2-8 parts of potassium dihydrogen phosphate, 12-18 parts of polyethylene glycol-1000,2-8 parts of sodium nitrate, vinyl imidazole 3-7
Part, 2-8 parts of modified petroleum resin, 12-18 parts of surfactant, 2-4 parts of initiator, 120-140 parts of water.
3. the sizing agent of wrapping paper according to claim 1, calculates by weight, it is characterised in that: including starch sulfurous
15 parts of sour hydrogen sodium, 8 parts of potassium sulfate, 8 parts of magnesium sulfate, 13 parts of citric acid, 14 parts of deionized water, 25 parts of cationic rosin size, phosphoric acid
6 parts of potassium dihydrogen, 15 parts of polyethylene glycol-1000,5 parts of sodium nitrate, 5 parts of vinyl imidazole, 6 parts of modified petroleum resin, surface-active
15 parts of agent, 3 parts of initiator, 130 parts of water.
4. the preparation method of the sizing agent of -3 any one wrapping paper according to claim 1, which is characterized in that including with
Lower step:
(1) starch sodium hydrogensulfite, potassium sulfate, magnesium sulfate, citric acid, deionized water are added in the water of part and are dissolved, is heated to
90-120 DEG C, 10-20min is stirred, adds cationic rosin size, potassium dihydrogen phosphate, polyethylene glycol-1000 stirring 60-90min;
(2) sodium nitrate, vinyl imidazole are added in remaining water, are heated to 90-120 DEG C, modified petroleum resin is added, surface is lived
Property agent, initiator, stir 30-45min;
(3) by step (1), (2) material and other residual components mix, be heated to 80-100 DEG C, be stirred to react 2-4h to get.