CN109352789A - A kind of solid wood furniture production method - Google Patents

A kind of solid wood furniture production method Download PDF

Info

Publication number
CN109352789A
CN109352789A CN201811583324.7A CN201811583324A CN109352789A CN 109352789 A CN109352789 A CN 109352789A CN 201811583324 A CN201811583324 A CN 201811583324A CN 109352789 A CN109352789 A CN 109352789A
Authority
CN
China
Prior art keywords
furniture
wax
timber
carried out
production method
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201811583324.7A
Other languages
Chinese (zh)
Inventor
滑子轶
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hebei Huashi Redwood Furniture Co Ltd
Original Assignee
Hebei Huashi Redwood Furniture Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hebei Huashi Redwood Furniture Co Ltd filed Critical Hebei Huashi Redwood Furniture Co Ltd
Priority to CN201811583324.7A priority Critical patent/CN109352789A/en
Publication of CN109352789A publication Critical patent/CN109352789A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of solid wood furniture production methods, comprising the following steps: timber feeding;First scraper is carried out to timber to beat except wet hole;Timber is dried;Timber clamping is secured, and be put into steam and carry out thermophilic digestion realization wax water replacement Treatment in wax pond;Secondary scraper is carried out to dewatered wood surface;Each component is assembled into furniture finished product according to furniture style;Lasaxing Oilfield is scraped after carrying out brush wax to the furniture surface after being completed;Water mill processing is carried out to furniture surface;Lasaxing Oilfield is scraped after carrying out brush wax to the interface position of furniture;Whole polishing is carried out to furniture;Dyeing processing is carried out to furniture surface;It waxed the furniture surface after dyeing, polished.3.6%, significantly larger than Industry code requirements are not higher than using Hepplewhite moisture content of the present invention, and construction split is tight, is not easy into water, is when in use not in uncoiling warpage, mouldy problem of whitening.Furniture surface reaches mirror effect, can reveal wet texture.

Description

A kind of solid wood furniture production method
Technical field
The present invention relates to technical field of furniture manufacturing more particularly to a kind of solid wood furniture production methods.
Background technique
Furniture is closely bound up with daily life, and as the improvement of people's living standards, people to article of furniture The pursuit of matter is also higher and higher.With socio-economic development, the superfine product in furniture has more value preserving and value-added functionality, such as European Old teak in furniture and the old redwood in Chinese Furniture.And the moisture content of wood material for furniture extremely closes in the indices of raw material It is important, the problem of directly affecting furniture quality and vast Furniture manufacturing manufacturing firm most headache.
Causing crack on furniture deformation on the one hand is because moisture content is higher, and the moisture content of general wood material for furniture must not Higher than the average moisture content of consumer locality, the production moisture content of furniture moisture content after working process is excessively high, is entering In use, the test of local climate variation can be unable to undergo in family, cause product cracking and warpage, explosion is shunk, structure pine Dynamic, color is whitened, many problems such as absciss layer, mouldy are painted on surface;Another major reason is precisely due to manufacture craft is improper, family The connecting structure of tool limits and connecting portion is easily intake, and occurs connecting portion loosening or timber during prolonged use Section at there is secondary cracking, cause furniture craze and transfiguration occur, influence furniture quality and service life.
And the surface effect of furniture be consumer when choosing furniture to the most visual impression of furniture, so furniture surface Effect is to evaluate an important indicator of furniture quality.For most when if furniture surface effect can reach vivid as mirror surface It is good, but the furniture surface of existing furniture production method production is generally unable to reach bright mirror effect, moreover, by for a long time Use, furniture surface will appear aging, it is dimmed situations such as.
Summary of the invention
The object of the present invention is to provide a kind of solid wood furniture production methods, solve the craze and transfiguration that furniture easily occurs, The technical problem of surface mirror effect difference.
In order to solve the above technical problems, the present invention adopts the following technical scheme:
A kind of solid wood furniture production method of the present invention, comprising the following steps:
(1) timber feeding is greater than the specification of finished product, it is ensured that and it is every timber free from flaw, not damaged, and to wooden after feeding Then the cross section of material bath of glass margin to seam covers timber wet cloth or with the wet humidity to guarantee timber of bubble;
(2) first scraper is carried out to timber, wood surface is struck off, and beaten in wood surface except wet hole;
(3) timber after first scraper is dried, moisture content is made to make to reach 12%;
(4) will be secured at pile timber clamping after first scraper, and be put into steam and carry out thermophilic digestion realization wax water in wax pond Replacement Treatment, treatment temperature are 120 DEG C -150 DEG C, and the time is 20-30 days or so, make moisture content not higher than 3.6%;
(5) secondary scraper is carried out to dewatered wood surface, forms each component of finished product;
(6) split assembling is carried out by making joinery and its construction to each component, and each parts surface is carried out after tentatively waxing, Each component is assembled into furniture finished product according to furniture style;
(7) Lasaxing Oilfield is scraped after carrying out brush wax to the furniture surface after being completed, paraffin cutting after the brush wax of furniture surface is needed Processing 2 times -3 times;
(8) water mill processing successively is carried out to furniture surface using No. 600-No. 5000 silicon carbide papers;
(9) Lasaxing Oilfield is scraped after carrying out brush wax to the interface position of furniture, paraffin cutting after the brush wax at furniture interface position is needed to locate Reason 2 times -3 times;
(10) whole polishing is carried out to furniture;
(11) dyeing processing is carried out to furniture surface;
(12) it waxed the furniture surface after dyeing, polished.
Further, the timber size in step (1) when materials is greater than the specification 5-8mm of finished product.
Further, the aperture except wet hole is 2 millimeters, and hole depth is not less than 8 centimetres.
Further, the step (4) specifically:
(4-1) piles up timber in feeding rack according to thickness specification in layer, and after fixing timber with fixture, on Tight locking nut;
After (4-2) fills tap water into wax pond, feeding rack is put into wax pond with suspending way;
(4-3) beeswax, paraffin and additive are added into wax pond, open wax Chi Gai, start to melt wax, the time is 2-3 days;
It is every 24 hours, heating apparatus temperature up-regulation 2 is Celsius after beeswax and paraffin in (4-4) wax pond melt completely Degree, until heating apparatus temperature is increased to 150 degrees Celsius, wood digestion is completed;
(4-5) closes heating equipment power supply, after the wax liquor natural cooling in wax pond, feeding rack is proposed wax pond, wait set After wax liquor on material frame and timber drains, feeding rack fixture is opened, timber is individually separated.
Further, the specific addition manner of the additive is that every cube of wax adds 10 kilograms of tung oil, adds 5 jin of rosin, and 30 is public Jin setting agent.
Further, the step (4-1) further includes production testing material, and the testing material is fixedly placed in described set Expect the top of timber in frame.
Further, it is 4-6 centimetres that the specification of the testing material, which is length, the square stock that side length is 4-6 centimetres;It is with length 4-6 centimetres, with a thickness of the plate of 12mm;The number of the square stock and plate is respectively 1-2 root.
Further, the error in the step (5) when secondary scraper between the timber of every kind of specification is no more than 10.
Further, specifically used alcohol color carries out dyeing processing to furniture surface in the step (11).
Further, the wax-layer thickness required after waxing in the step (12) is 5mm.
Compared with prior art, advantageous effects of the invention:
After wood surface is opened up except wet hole, by wood fastening in feeding rack, beeswax, stone is added in the present invention in wax pond Wax and additive carry out boiling, moreover, using the cooking wax mode of interruption heating, not destroying timber certainly after wax melts completely Under the premise of body structure, what the wax of liquid condition can continue is oozed by removing wet hole into the lumen pore of wood structure, will be in timber Portion's moisture constantly squeezes out evaporation, realizes desiccated wood and stablizes wooden purpose, through the invention dewatered furniture wood Material moisture content is not higher than 3.6%, and significantly larger than Industry code requirements, the weather for making finished product furniture can adapt to different regions is wanted It asks, is when in use not in uncoiling warpage, mouldy problem of whitening.
The present invention carries out bath of glass margin to seam to the cross section of timber after timber feeding, realizes to the cross-sectional lumen seam of timber Sealing, avoids chamber from being sewn in timber subsequent process and becomes larger, and timber is caused secondary cracking occur;By joinery and its construction by each connection structure Node between part, which is connected with each other, to coincide, and constitutes firm furniture frame, it is ensured that expanding with heat and contract with cold for timber itself does not destroy its table The structure and Nei Li structure in face.Guarantee the cooperation of tenon mortise securely, it is vertebration, it is unlikely to deform;Component is tentatively being beaten Assembling combination is carried out again after mill and waxing, it is ensured that construction split is tight, is not easy into water.
The present invention carries out furniture surface to scrape Lasaxing Oilfield after multiple brush wax, guarantees furniture surface pore-free, by No. 600- No. 5000 silicon carbide papers from thick to thin finely polish to furniture surface, obtain smooth furniture surface and can also increase The adhesive force of strong furniture surface coating;With the stronger alcohol color of adhesive force, dyeing processing is carried out to furniture surface, makes furniture surface The fresh amount of color, does not fall off color;After furniture surface is waxed and polished, furniture surface is made to reach mirror effect, and furniture Surface shows wet texture.
Specific embodiment
A kind of solid wood furniture production method, comprising the following steps:
(1) timber is processed into the woollen of different size according to production requirement, and choose respective model into after factory by timber Timber, it is desirable that the size of feeding timber is greater than the specification 5-8mm of finished product to give over to machining allowance, needs in reclaiming process pair Timber carries out close inspection, it is ensured that and it is every timber free from flaw, not damaged, to the cross section bath of glass margin to seam of timber after feeding, It prevents timber from secondary cracking occur, then covers timber wet cloth or with the wet humidity to guarantee timber after feeding of bubble.
(2) first scraper being carried out to timber wood surface with thicknesser, this need to only strike off the surface of timber in the process, Purpose is to guarantee that timber stacking in subsequent clamping is smooth, convenient for mounting and clamping, plays dehumidifying on the surface of the timber after striking off later Hole, it is desirable that except the aperture of wet hole is 2 millimeters, hole depth is not less than 8 centimetres;
(3) timber after first scraper is dried, moisture content is made to make to reach 12%;
(4) will be secured at pile timber clamping after first scraper, and be put into steam and carry out thermophilic digestion realization wax water in wax pond Replacement Treatment, treatment temperature are 120 DEG C -150 DEG C, and the time is 20-30 days or so, make moisture content not higher than 3.6%, specifically Step are as follows:
(4-1) piles up timber in feeding rack according to thickness specification in layer, and after fixing timber with fixture, on Tight locking nut, needs production testing material during this, and the testing material is fixedly placed in the feeding rack timber most Top layer, the specification of the testing material are that length is 4-6 centimetres, the square stock that side length is 4-6 centimetres;It is 4-6 centimetres with length, it is thick Degree is the plate of 12mm;The number of the square stock and plate is respectively 1-2 root;
After (4-2) fills tap water into wax pond, feeding rack is put into wax pond with suspending way;
(4-3) beeswax, paraffin and additive are added into wax pond, open wax Chi Gai, start to melt wax, and the time is 2-3 days, The specific addition manner of the additive is that every cube of wax adds 10 kilograms of tung oil, adds 5 jin of rosin, 30 kilograms of setting agents;Here it needs It should be noted that the additive amount of beeswax, paraffin and additive is in wax pond after wax pond is small wax pond and timber fills small wax pond 0.95-1.05 tons.When wax pond is big wax pond and after timber fills big wax pond, beeswax, paraffin and the addition of addition big wax pond in The additive amount of agent is 1.9-2.1 tons.
It is every 24 hours, heating apparatus temperature up-regulation 2 is Celsius after beeswax and paraffin in (4-4) wax pond melt completely Degree, until heating apparatus temperature is increased to 150 degrees Celsius, wood digestion is completed;
(4-5) testing material, which is truncated, observes whether wax permeates completely in timber, and check test material moisture content, contains Water rate is qualified for verifying less than 3.6%.
(4-6) closes heating equipment power supply, after the wax liquor natural cooling in wax pond, feeding rack is proposed wax pond, wait set After wax liquor on material frame and timber drains, feeding rack fixture is opened, timber is individually separated.
(5) secondary scraper is carried out to dewatered wood surface, forms each component of finished product, it is desirable that secondary scraper The timber of every kind of specification afterwards is no more than 10 compared with the error of standard size dimensions, to guarantee to form each component of finished product Afterwards, the accurate size of each component and consistent.
(6) according to furniture style requirement and each component connection, tenon or mortise, Tenon knot are opened up in respective members Node between each connecting elements can be connected with each other by structure to coincide, and constitutes firm furniture frame, it is ensured that the heat of timber itself Swollen shrinkage does not destroy the structure and Nei Li structure on its surface, to guarantee that the cooperation of tenon mortise is securely tight;Use No. 600 sand paper pair The surface of each component is tentatively polished, after parts surface is polished smooth, the dust wiped clean that polishing is generated, and air exercise Component surface after mill is tentatively waxed, it is desirable that the wax-layer thickness tentatively waxed is 0.5-0.8mm, later to surface preparation Component afterwards carries out split assembling, is fabricated to furniture finished product.
(7) wax is brushed to the furniture surface after being completed, with carrying out scraping Lasaxing Oilfield to cere after brush wax, when first pass is scraped After the completion of wax, repeat to the operation process of twice of first brush wax paraffin cutting again, making the surface of furniture components, there is no pores.
(8) water mill processing successively is carried out to furniture surface using No. 600-No. 5000 silicon carbide papers, with silicon carbide paper pair When furniture surface is polished, from most thick mill, first use No. 600 silicon carbide papers, then No. 800, and so on, always Water mill will thoroughly be rinsed with water clear buffed surface to No. 5000, when changing sand paper every time again could replace the thinner sand of use Paper.The furniture surface of conscientious minute inspection is required, in per pass water mill treatment process to prevent going out during water mill is handled Existing subtle pore and dirt.
(9) wax is brushed to the interface position of furniture, is opened after brush wax with wax and cere is carried out to scrape Lasaxing Oilfield, when first pass paraffin cutting After the completion, the operation process of first brush wax paraffin cutting again is repeated, to guarantee to match with the component of original milled.
(10) whole polishing is carried out to furniture surface with sand paper, and made the dust wiped clean after polishing with rag Furniture surface is smooth clean and tidy.
(11) dyeing processing is carried out to furniture surface with alcohol color, makes the solid colour of furniture surface, and be in bright colors not Easily decoloration.
(12) whole waxing, wax-layer thickness 5mm are carried out after color contaminates well to furniture, and is polished with sand paper, furniture is made Surface is as smooth as jade, reaches mirror effect, and wax layer makes furniture surface show wet texture.
After wood surface is opened up except wet hole, by wood fastening in feeding rack, beeswax, stone is added in the present invention in wax pond Wax and additive carry out boiling, moreover, using the cooking wax mode of interruption heating, not destroying timber certainly after wax melts completely Under the premise of body structure, what the wax of liquid condition can continue is oozed by removing wet hole into the lumen pore of wood structure, will be in timber Portion's moisture constantly squeezes out evaporation, realizes desiccated wood and stablizes wooden purpose, through the invention dewatered furniture wood Material moisture content is not higher than 3.6%, and significantly larger than Industry code requirements, the weather for making finished product furniture can adapt to different regions is wanted It asks, is when in use not in uncoiling warpage, mouldy problem of whitening.
The present invention carries out bath of glass margin to seam to the cross section of timber after timber feeding, realizes to the cross-sectional lumen seam of timber Sealing, avoids chamber from being sewn in timber subsequent process and becomes larger, and timber is caused secondary cracking occur;By joinery and its construction by each connection structure Node between part, which is connected with each other, to coincide, and constitutes firm furniture frame, it is ensured that expanding with heat and contract with cold for timber itself does not destroy its table The structure and Nei Li structure in face.Guarantee the cooperation of tenon mortise securely, it is vertebration, it is unlikely to deform;Component is tentatively being beaten Assembling combination is carried out again after mill and waxing, it is ensured that construction split is tight, is not easy into water.
The present invention carries out furniture surface to scrape Lasaxing Oilfield after multiple brush wax, guarantees furniture surface pore-free, by No. 600- No. 5000 silicon carbide papers from thick to thin finely polish to furniture surface, obtain smooth furniture surface and can also increase The adhesive force of strong furniture surface coating;With the stronger alcohol color of adhesive force, dyeing processing is carried out to furniture surface, makes furniture surface The fresh amount of color, does not fall off color;After furniture surface is waxed and polished, furniture surface is made to reach mirror effect, and furniture Surface shows wet texture.
Embodiment described above is only that preferred embodiment of the invention is described, and is not carried out to the scope of the present invention It limits, without departing from the spirit of the design of the present invention, those of ordinary skill in the art make technical solution of the present invention Various changes and improvements, should all fall into claims of the present invention determine protection scope in.

Claims (10)

1. a kind of solid wood furniture production method, it is characterised in that: the following steps are included:
(1) timber feeding is greater than the specification of finished product, it is ensured that and it is every timber free from flaw, not damaged, and to timber after feeding Then cross section bath of glass margin to seam covers timber wet cloth or with the wet humidity to guarantee timber of bubble;
(2) first scraper is carried out to timber, wood surface is struck off, and beaten in wood surface except wet hole;
(3) timber after first scraper is dried, moisture content is made to make to reach 12%;
(4) will be secured at pile timber clamping after first scraper, and be put into steam and carry out thermophilic digestion realization wax water displacement in wax pond Processing, treatment temperature are 120 DEG C -150 DEG C, and the time is 20-30 days or so, make moisture content not higher than 3.6%;
(5) secondary scraper is carried out to dewatered wood surface, forms each component of finished product;
(6) split assembling is carried out by making joinery and its construction to each component, and each parts surface is carried out after tentatively waxing, it will be each Component is assembled into furniture finished product according to furniture style;
(7) Lasaxing Oilfield is scraped after carrying out brush wax to the furniture surface after being completed, 2 need to be handled to paraffin cutting after the brush wax of furniture surface All over -3 times;
(8) water mill processing successively is carried out to furniture surface using No. 600-No. 5000 silicon carbide papers;
(9) Lasaxing Oilfield is scraped after carrying out brush wax to the interface position of furniture, 2 need to be handled to paraffin cutting after the brush wax at furniture interface position All over -3 times;
(10) whole polishing is carried out to furniture;
(11) dyeing processing is carried out to furniture surface;
(12) it waxed the furniture surface after dyeing, polished.
2. solid wood furniture production method according to claim 1, it is characterised in that: the wood in step (1) when materials Material size is greater than the specification 5-8mm of finished product.
3. solid wood furniture production method according to claim 2, it is characterised in that: the aperture except wet hole is 2 Millimeter, hole depth are not less than 8 centimetres.
4. solid wood furniture production method according to claim 1, it is characterised in that: the step (4) specifically:
(4-1) piles up timber in feeding rack according to thickness specification in layer, and after fixing timber with fixture, tightens lock Tight nut;
After (4-2) fills tap water into wax pond, feeding rack is put into wax pond with suspending way;
(4-3) beeswax, paraffin and additive are added into wax pond, open wax Chi Gai, start to melt wax, the time is 2-3 days;
After beeswax and paraffin in (4-4) wax pond melt completely, every 24 hours, heating apparatus temperature is raised 2 degrees Celsius, directly 150 degrees Celsius are increased to heating apparatus temperature, wood digestion is completed;
(4-5) closes heating equipment power supply, after the wax liquor natural cooling in wax pond, feeding rack is proposed wax pond, to feeding rack And after the wax liquor on timber drains, feeding rack fixture is opened, timber is individually separated.
5. solid wood furniture production method according to claim 4, it is characterised in that: the specific side of addition of the additive Formula is that every cube of wax adds 10 kilograms of tung oil, adds 5 jin of rosin, 30 kilograms of setting agents.
6. wood material for furniture dehydrating processing method according to claim 4, it is characterised in that: the step (4-1) is also wrapped Production testing material is included, and the testing material is fixedly placed in the top of timber in the feeding rack.
7. solid wood furniture production method according to claim 4, it is characterised in that: the specification of the testing material is Length is 4-6 centimetres, the square stock that side length is 4-6 centimetres;It is 4-6 centimetres with length, with a thickness of the plate of 12mm;The square stock and The number of plate is respectively 1-2 root.
8. solid wood furniture production method according to claim 1, it is characterised in that: secondary in the step (5) to scrape Error when material between the timber of every kind of specification is no more than 10.
9. solid wood furniture production method according to claim 1, it is characterised in that: specifically make in the step (11) Dyeing processing is carried out to furniture surface with alcohol color.
10. solid wood furniture production method according to claim 1, it is characterised in that: waxing in the step (12) The wax-layer thickness required afterwards is 5mm.
CN201811583324.7A 2018-12-24 2018-12-24 A kind of solid wood furniture production method Pending CN109352789A (en)