CN109228710A - The technology of information source tracing is realized by product spray printing two dimensional code - Google Patents

The technology of information source tracing is realized by product spray printing two dimensional code Download PDF

Info

Publication number
CN109228710A
CN109228710A CN201810732526.7A CN201810732526A CN109228710A CN 109228710 A CN109228710 A CN 109228710A CN 201810732526 A CN201810732526 A CN 201810732526A CN 109228710 A CN109228710 A CN 109228710A
Authority
CN
China
Prior art keywords
dimensional code
product
spray printing
parts
technology
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810732526.7A
Other languages
Chinese (zh)
Inventor
张庆瑞
张建伟
金正鹏
熊棚生
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Shengli Precision Manufacturing Technology Co Ltd
Original Assignee
Anhui Shengli Precision Manufacturing Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Shengli Precision Manufacturing Technology Co Ltd filed Critical Anhui Shengli Precision Manufacturing Technology Co Ltd
Priority to CN201810732526.7A priority Critical patent/CN109228710A/en
Publication of CN109228710A publication Critical patent/CN109228710A/en
Pending legal-status Critical Current

Abstract

The technology of information source tracing is realized by product spray printing two dimensional code, and product starts the two dimensional code marking confirmed when production to spray printing unique identification on the product, and these information collections is stored by SCADA system;In subsequent all production processes, equipment, which can read, identifies this unique two dimensional code marking, then is acquired by SCADA system and read these information and store.The defective products can be fast and accurately navigated to when a certain part or a collection of product occur bad and the defective products is which the part equipment by which kind of process, and targetedly equipment and production technology are adjusted, and optimized, realized that the production of higher efficiency is made.

Description

The technology of information source tracing is realized by product spray printing two dimensional code
Technical field
The present invention relates to information source tracing technical fields, and in particular to the skill of information source tracing is realized by product spray printing two dimensional code Art.
Background technique
In the daily production process of factory, there are problems that fast and effectively identifying a certain single products, When a certain product or a collection of product occur abnormal, the process point and equipment of product problem appearance cannot be quickly navigated to, thus Make targetedly measure;
When passing through equipment component and process, the two dimensional code on glass cannot be cleaned out;Prior art two dimensional code holds very much It is easily removed, is wiped, the loss damage for the information that causes to trace to the source.
Summary of the invention
Technical problem to be solved by the present invention lies in provide the technology that information source tracing is realized by product spray printing two dimensional code.
The technical problems to be solved by the invention are realized using following technical scheme:
The technology of information source tracing is realized by product spray printing two dimensional code, it is characterised in that: to the production when product starts to produce The two dimensional code marking that spray printing unique identification confirms on product, and stored these information collections by SCADA system;
In subsequent all production processes, equipment, which can read, identifies this unique two dimensional code marking, then by SCADA system Acquisition is read these information and is stored;
The defective products can be fast and accurately navigated to when a certain part or a collection of product occur bad and the defective products is By which kind of process, any part equipment, and targetedly equipment and production technology are adjusted, optimizes, realize higher efficiency Production is made.
Further technology, when passing through equipment component and process, the two dimensional code on glass cannot be cleaned out, therefore, this Technology is preparing to coat one layer of glue at spray printing, after gelling is solid, is drying rifle and heat glue surface, spray metal with spray gun before spray printing Grain, then the two dimensional code marking of spray printing unique identification confirmation.
Further technology: the glue is prepared from the following parts by weight of the components: 100-150 parts of E-44 epoxy resin, 16-19 parts of liquid low-molecular polyamide, 20-30 parts of organosilicon acrylic resin lotion, 2-5 parts of thickener, 10-15 parts of mica powder, carbonization 10-15 parts of silicon powder, 10-15 parts of mild-clay powder
Further technology, the glue the preparation method comprises the following steps:
Step 1: all components being mixed, is put into dispersion machine and disperses 2-5 minutes at revolving speed 600-800rpm;
Step 2: being fitted into mixer and carry out melt blending, blending temperature is 220-240 DEG C, and rheometer revolving speed is 60- 80rpm, it is 10-20 minutes that the time, which is blended,;
Step 3: being handled in flakes by two-roll mill, temperature is 180-220 DEG C;
Step 4: being vulcanized with compression molding instrument, temperature is 200-210 DEG C, pressure 8-12MPa, and the time is 5-10 points Clock;
Step 5: cold pressing is carried out under 18-25 DEG C of temperature, pressure 5-7MPa 3-5 minutes to obtain the final product.
The invention has the benefit that
Compared with production procedure now, the present invention, which mainly protrudes, assigns the identity of single products, according to this identity Uniqueness can carry out the data analysis in later period and optimizing and revising for production technology and equipment, realize production IT application in product.
When product is glass, ink-jet is easily removed, and the present invention smears one layer of high viscosity glue, complexed metal on glass Grain, increase is wear-resisting, avoids direct friction glue, meanwhile, the two dimensional code for also avoiding ink-jet is not rubbed off, after metal spraying metal particles, A possibility that two dimensional code is endowed stereochemical structure, can not replace halfway, two dimensional code is avoided maliciously to be exchanged.
Specific embodiment
Below in conjunction with the embodiment of the present invention, technical solution of the present invention is clearly and completely described, it is clear that retouched The embodiment stated is only a part of the embodiment of the present invention, instead of all the embodiments.Based on the embodiments of the present invention, originally Field those of ordinary skill every other embodiment obtained without making creative work, belongs to the present invention The range of protection.
Embodiment: glass after sawing sheet, in glass front spray 25 digit word bits, the two dimensional code having a size of 12mm*12mm, And these identity information acquisitions are stored by SCADA system.When by each workshop appliance glass processing, code reader can automatic identification The information of two dimensional code and these information collections are stored by SCADA system is synchronous on glass.If the quality inspection after a certain procedure Place's discovery product is bad, then by the identification number of identification defective products, traces the process and equipment that the defective products passes through, thus Equipment and technique are safeguarded and optimized, realizes the optimization of production capacity yield.Furthermore it is identified by the information of single products, it can be with What kind of manufacturing procedure the product for accurately viewing some number is carrying out, and realizes and manages to the real-time tracing of product and planning Reason.
When passing through equipment component and process, the two dimensional code on glass cannot be cleaned out, and therefore, this technology is in spray printing Before, preparing to coat one layer of glue at spray printing, after gelling is solid, is drying rifle and heat glue surface, spray metallic particles with spray gun, then spray printing is only The two dimensional code marking of one recognition and verification.
The embodiment 1 of glue: glue is prepared from the following parts by weight of the components: 100 parts of E-44 epoxy resin, liquid low molecule Measure 16 parts of polyamide, 20 parts of organosilicon acrylic resin lotion, 2 parts of thickener, 10 parts of mica powder, 10 parts of carborundum powder, mild-clay powder 10 Part.
The embodiment 2 of glue: glue is prepared from the following parts by weight of the components: 150 parts of E-44 epoxy resin, liquid low molecule Measure 19 parts of polyamide, 30 parts of organosilicon acrylic resin lotion, 5 parts of thickener, 15 parts of mica powder, 15 parts of carborundum powder, mild-clay powder 15 Part.
The glue of two kinds of embodiments through carrying out test comparison throughout the year:
Embodiment 1, adhesive strength reach 7.61n/cm2, and the physical properties such as side pressure strength are more than common adhesive 20- 30% or so, summer and autumn can store 7 days and never degenerate, and winter in spring can store 14 days and never degenerate;
It in the case that air humidity is greater than 90%, guarantees the quality 60 days, glass ducks in drink, not degumming in 48 hours, and carton is dry Afterwards, good bonding, mass conservation.
Embodiment 2, adhesive strength reach 7.20n/cm2, and the physical properties such as side pressure strength are more than common adhesive 20- 30% or so, summer and autumn can store 7 days and never degenerate, and winter in spring can store 14 days and never degenerate;
It in the case that air humidity is greater than 90%, guarantees the quality 60 days, glass ducks in drink, not degumming in 48 hours, and carton is dry Afterwards, good bonding, mass conservation.
Glue the preparation method comprises the following steps:
Step 1: all components being mixed, is put into dispersion machine and disperses 2-5 minutes at revolving speed 600-800rpm;
Step 2: being fitted into mixer and carry out melt blending, blending temperature is 220-240 DEG C, and rheometer revolving speed is 60- 80rpm, it is 10-20 minutes that the time, which is blended,;
Step 3: being handled in flakes by two-roll mill, temperature is 180-220 DEG C;
Step 4: being vulcanized with compression molding instrument, temperature is 200-210 DEG C, pressure 8-12MPa, and the time is 5-10 points Clock;
Step 5: cold pressing is carried out under 18-25 DEG C of temperature, pressure 5-7MPa 3-5 minutes to obtain the final product.
It although an embodiment of the present invention has been shown and described, for the ordinary skill in the art, can be with A variety of variations, modification, replacement can be carried out to these embodiments without departing from the principles and spirit of the present invention by understanding And modification, the scope of the present invention is defined by the appended.

Claims (4)

1. realizing the technology of information source tracing by product spray printing two dimensional code, it is characterised in that: to the product when product starts to produce The two dimensional code marking of upper spray printing unique identification confirmation, and stored these information collections by SCADA system;
In subsequent all production processes, equipment, which can read, identifies this unique two dimensional code marking, then is acquired by SCADA system It reads these information and stores;
The defective products can be fast and accurately navigated to when a certain part or a collection of product occur bad and the defective products is to pass through Which kind of process, any part equipment, and targetedly equipment and production technology are adjusted, optimize, realizes the production of higher efficiency It is made.
2. the technology according to claim 1 for realizing information source tracing by product spray printing two dimensional code, it is characterised in that: logical When crossing equipment component and process, the two dimensional code on glass cannot be cleaned out, and therefore, this technology is preparing spray printing before spray printing Place coats one layer of glue, after gelling is solid, dries rifle and heats glue surface, sprays metallic particles with spray gun, then the confirmation of spray printing unique identification The two dimensional code marking.
3. the technology according to claim 2 for realizing information source tracing by product spray printing two dimensional code, it is characterised in that: described Glue be prepared from the following parts by weight of the components: 100-150 parts of E-44 epoxy resin, liquid low-molecular polyamide 16-19 Part, 20-30 parts of organosilicon acrylic resin lotion, 2-5 parts of thickener, 10-15 parts of mica powder, 10-15 parts of carborundum powder, mild-clay powder 10-15 parts.
4. the technology according to claim 2 for realizing information source tracing by product spray printing two dimensional code, it is characterised in that: described Glue the preparation method comprises the following steps:
Step 1: all components being mixed, is put into dispersion machine and disperses 2-5 minutes at revolving speed 600-800rpm;
Step 2: it is fitted into mixer and carries out melt blending, blending temperature is 220-240 DEG C, and rheometer revolving speed is 60-80rpm, It is 10-20 minutes that the time, which is blended,;
Step 3: being handled in flakes by two-roll mill, temperature is 180-220 DEG C;
Step 4: being vulcanized with compression molding instrument, temperature is 200-210 DEG C, pressure 8-12MPa, and the time is 5-10 minutes;
Step 5: cold pressing is carried out under 18-25 DEG C of temperature, pressure 5-7MPa 3-5 minutes to obtain the final product.
CN201810732526.7A 2018-07-05 2018-07-05 The technology of information source tracing is realized by product spray printing two dimensional code Pending CN109228710A (en)