CN109206933A - 一种微胶囊自修复技术 - Google Patents
一种微胶囊自修复技术 Download PDFInfo
- Publication number
- CN109206933A CN109206933A CN201710520262.4A CN201710520262A CN109206933A CN 109206933 A CN109206933 A CN 109206933A CN 201710520262 A CN201710520262 A CN 201710520262A CN 109206933 A CN109206933 A CN 109206933A
- Authority
- CN
- China
- Prior art keywords
- capsule
- micro
- repair
- healant
- self
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
本发明公开了一种微胶囊自修复技术,包括微胶囊、聚合物复合材料,所述具有催化活性的化学物质发生反应,如果聚合物材料受到伤害,可以通过胶囊的自感知、裂纹尖端的应力进行集中性的激励,使得为胶囊出现破裂的现象,将修补剂利用毛细管进入到受损的位置上,如果修补剂与之前埋置在基体中的催化剂发生反应,将裂纹表面进行粘接,使受损的区域得以修复。通过上述技术方案使复合材料的使用寿命得以延长,也能够减少维护的成本。
Description
技术领域
本发明涉及新材料技术领域,具体为一种微胶囊自修复技术。
背景技术
动力以及运动传递的主要形式是齿轮传动,金属齿轮传动一般是应用在传统的食品机械中的,这种传动方式比较重,噪声也比较大。当前复合材料不断发展,食品、纺织机械中也开始使用新型的复合材料齿轮,提高复合材料齿轮的性能是近些年来关注和研究的重点问题。
发明内容
本发明的目的在于提供一种微胶囊自修复技术,以解决上述背景技术中提出的现有的技术的问题。
为实现上述目的,本发明提供如下技术方案,一种微胶囊自修复技术,包括微胶囊、聚合物复合材料,所述具有催化活性的化学物质发生反应,如果聚合物材料受到伤害,可以通过胶囊的自感知、裂纹尖端的应力进行集中性的激励,使得为胶囊出现破裂的现象,将修补剂利用毛细管进入到受损的位置上。
所述的在复合材料齿轮中建设新的自修复的系统,结合微胶囊的自修复原理,在聚合物基复合材料齿轮中加入自修复微胶囊,防止复合材料出现烧伤、裂纹等问题,使食品机械设备能够长时间使用,并且降噪减震。
与现有技术相比,本发明的有益效果是:本技术方自修复微胶囊能够使复合材料的齿轮噪声降低,为了使实验得以完善,还需要进一步分析与研究,使微胶囊自修复技术在食品机械齿轮中得到更好地应用。
具体实施方式
下面将结合本发明实施例中的工艺步骤,对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅仅是本发明一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其他实施例,都属于本发明保护的范围。
本发明提供一种技术方案:一种微胶囊自修复技术,包括微胶囊、聚合物复合材料,所述具有催化活性的化学物质发生反应,如果聚合物材料受到伤害,可以通过胶囊的自感知、裂纹尖端的应力进行集中性的激励,使得为胶囊出现破裂的现象,将修补剂利用毛细管进入到受损的位置上。
所述的在复合材料齿轮中建设新的自修复的系统,结合微胶囊的自修复原理,在聚合物基复合材料齿轮中加入自修复微胶囊,防止复合材料出现烧伤、裂纹等问题,使食品机械设备能够长时间使用,并且降噪减震。
尽管参照前述实施例对本发明进行了详细的说明,对于本领域的技术人员来说,其依然可以对前述各实施例所记载的技术方案进行修改,或者对其中部分技术特征进行等同替换,凡在本发明的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本发明的保护范围之内。
Claims (2)
1.一种微胶囊自修复技术,包括微胶囊、聚合物复合材料,所述具有催化活性的化学物质发生反应,如果聚合物材料受到伤害,可以通过胶囊的自感知、裂纹尖端的应力进行集中性的激励,使得为胶囊出现破裂的现象,将修补剂利用毛细管进入到受损的位置上。
2.根据权利要求1所述的一种微胶囊自修复技术,其特征在于:所述的修补剂与之前埋置在基体中的催化剂发生反应,将裂纹表面进行粘接,使受损的区域得以修复。