CN108723535A - A kind of core-spun yarn connection of broken lines method - Google Patents

A kind of core-spun yarn connection of broken lines method Download PDF

Info

Publication number
CN108723535A
CN108723535A CN201810496154.2A CN201810496154A CN108723535A CN 108723535 A CN108723535 A CN 108723535A CN 201810496154 A CN201810496154 A CN 201810496154A CN 108723535 A CN108723535 A CN 108723535A
Authority
CN
China
Prior art keywords
core
spun yarn
casing
rear end
outer diameter
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810496154.2A
Other languages
Chinese (zh)
Inventor
高卯根
石增辉
金志斌
马达
古宏渊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanxi Taigang Stainless Steel Co Ltd
Original Assignee
Shanxi Taigang Stainless Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanxi Taigang Stainless Steel Co Ltd filed Critical Shanxi Taigang Stainless Steel Co Ltd
Priority to CN201810496154.2A priority Critical patent/CN108723535A/en
Publication of CN108723535A publication Critical patent/CN108723535A/en
Pending legal-status Critical Current

Abstract

The present invention relates to core-spun yarn connection of broken lines fields.A kind of core-spun yarn connection of broken lines method, the pulvis 2 of the front end 1 of the core-spun yarn of broken string and the rear end 5 of core-spun yarn within the 1cm of end face is dug out, the pulvis 2 dug out is fitted into casing 4, the outer diameter of casing 4 is equal to the internal diameter of core-spun yarn, the length of casing is 2.5-3cm, then 1 other end of front end that one end of casing 4 is inserted into core-spun yarn is inserted into the rear end 5 of core-spun yarn, casing 4 is set to be in impaction state by rotating and squeezing the front end 1 of core-spun yarn and the rear end 5 of core-spun yarn, using cored solder wire to the front end 1 of core-spun yarn, the rear end 5 of core-spun yarn, the circular groove that casing 4 surrounds is welded, the outer diameter of weld is set to be equal to the outer diameter of core-spun yarn.

Description

A kind of core-spun yarn connection of broken lines method
Technical field
The present invention relates to core-spun yarn connection of broken lines fields.
Background technology
Core-spun yarn breed, external refining, the aspect of special elements alloying three are widely used in smelting process, core-spun yarn It is formed by band shape foreskin winding alloy powder, winds outer appearnce liny circle.It can be divided into according to the difference of institute's winding alloy powder: Silicon-calcium wire, barium aluminum steel, calcium iron wire etc..Core-spun yarn often will appear broken string phenomenon in use, due to pulvis characteristic influence, There are problems that welding junction is difficult to solder to or connects loosely, and since the pulvis in core-spun yarn is to the quality of institute's alloy smelting It is affected, harmful effect is often generated to the final mass of alloy smelting using existing welding.
Invention content
The technical problem to be solved by the present invention is to:How to solve the problems, such as that special core-spun yarn broken string interface is reliably connected.
The technical solution adopted in the present invention is:A kind of core-spun yarn connection of broken lines method, by the front end 1 of the core-spun yarn of broken string Dug out with the pulvis 2 of the rear end 5 of core-spun yarn within the 1cm of end face, the pulvis 2 dug out be fitted into casing 4, casing 4 it is outer Diameter is equal to the internal diameter of core-spun yarn, and the length of casing is 2.5-3cm, and then front end 1 that one end of casing 4 is inserted into core-spun yarn is another The rear end 5 of core-spun yarn is inserted at end, so that casing 4 is in compression by rotating and squeezing the front end 1 of core-spun yarn and the rear end 5 of core-spun yarn State, the circular groove surrounded to the front end 1 of core-spun yarn, the rear end 5 of core-spun yarn, casing 4 using cored solder wire are welded, and weld is made Outer diameter be equal to core-spun yarn outer diameter.
As a kind of preferred embodiment:The material identical of the material core-spun yarn outer layer foreskin of casing 4.
The beneficial effects of the invention are as follows:Can the core-spun yarn of broken string be effectively securely attached at one by the method for the invention It rises, and does not influence the use of core-spun yarn.
Description of the drawings
Fig. 1 is the connection relationship diagram of the present invention;
Wherein, 1, the front end of core-spun yarn, 2, pulvis, 3, at soldering, 4, casing, 5, the rear end of core-spun yarn.
Specific implementation mode
As shown in Figure 1, when invention core-spun yarn breaks, the front end of core-spun yarn 1 and the rear end of core-spun yarn 5 are repaired first flat It is whole, and the pulvis 2 within the end face 1cm apart from the front end of core-spun yarn 1 and the rear end of core-spun yarn 5 is dug out, pulvis 2 is packed into one A length is in 3cm materials casing identical with insurance wire wrapper and to be compacted, before core-spun yarn is then inserted into one end of casing 4 It holds 1 other end to be inserted into the rear end 5 of core-spun yarn, makes casing 4 by rotating and squeezing the front end 1 of core-spun yarn and the rear end 5 of core-spun yarn In impaction state(It cannot deeply be squeezed again under manual squeezing), using cored solder wire to the front end 1 of core-spun yarn, core-spun yarn Rear end 5, the circular groove that surrounds of casing 4 welded, so that the outer diameter of weld is equal to the outer diameter of core-spun yarn.

Claims (2)

1. a kind of core-spun yarn connection of broken lines method, it is characterised in that:By the front end of the core-spun yarn of broken string(1)With the rear end of core-spun yarn (5)Pulvis within the 1cm of end face(2)It digs out, the pulvis that will be dug out(2)It is packed into casing(4)In, casing(4)Outer diameter etc. In the internal diameter of core-spun yarn, the length of casing is 2.5-3cm, then by casing(4)One end be inserted into core-spun yarn front end(1)It is another The rear end of core-spun yarn is inserted at end(5), by the front end for rotating and squeezing core-spun yarn(1)With the rear end of core-spun yarn(5)Make casing(4) In impaction state, using cored solder wire to the front end of core-spun yarn(1), core-spun yarn rear end(5), casing(4)The circular groove surrounded into Row welding makes the outer diameter of weld be equal to the outer diameter of core-spun yarn.
2. a kind of core-spun yarn connection of broken lines method according to claim 1, it is characterised in that:Casing(4)Material cored The material identical of line outer layer foreskin.
CN201810496154.2A 2018-05-22 2018-05-22 A kind of core-spun yarn connection of broken lines method Pending CN108723535A (en)