CN108663737A - A kind of safeguard film for cellular phone that can defend shortwave blue light - Google Patents

A kind of safeguard film for cellular phone that can defend shortwave blue light Download PDF

Info

Publication number
CN108663737A
CN108663737A CN201810364094.9A CN201810364094A CN108663737A CN 108663737 A CN108663737 A CN 108663737A CN 201810364094 A CN201810364094 A CN 201810364094A CN 108663737 A CN108663737 A CN 108663737A
Authority
CN
China
Prior art keywords
parts
blue light
ultraviolet
ranvier
proof
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201810364094.9A
Other languages
Chinese (zh)
Inventor
李阳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hefei Rende Electronic Technology Co Ltd
Original Assignee
Hefei Rende Electronic Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hefei Rende Electronic Technology Co Ltd filed Critical Hefei Rende Electronic Technology Co Ltd
Priority to CN201810364094.9A priority Critical patent/CN108663737A/en
Publication of CN108663737A publication Critical patent/CN108663737A/en
Withdrawn legal-status Critical Current

Abstract

The present invention provides a kind of safeguard film for cellular phone that can defend shortwave blue light; including Ranvier's membrane; the Ranvier's membrane side being connect with mobile phone sets gradually ultraviolet-proof and anti-blue light coating, is protected by the double-layer structure of antiultraviolet and anti-blue light, largely intercepts and sorption enhanced blue light.In addition, several grooves are arranged to one face edge of Ranvier's membrane in the ultraviolet-proof, centre setting through-hole, so design are to be discharged into anti-shortwave blue light coating sorption enhanced by intermediate through-hole in order to which the shape of the concavees lens formed by groove gathers together the blue light that mobile phone discharges.Meanwhile several grooves are arranged to one face edge of ultraviolet-proof in the anti-blue light coating, for preventing the shortwave blue light loss not by sorption enhanced from removing.By the design of above structure, it can absorb 99% or more ultraviolet light, 96% or more shortwave blue light.

Description

A kind of safeguard film for cellular phone that can defend shortwave blue light
Technical field
The invention belongs to communicate field of material technology, and in particular, to a kind of mobile phone that can defend shortwave blue light is protected Film.
Background technology
Tempered glass belongs to safety glass, and glass has fairly good antiwear characteristic, and very rigid, tempered glass its It is in fact a kind of prestressed glass, to improve the intensity of glass, usually using method chemically or physically, is formed and pressed in glass surface Stress, glass bear to offset skin stress first when external force, and to improve bearing capacity, but tempered glass runs mobile phone When the blue light that discharges there are very high energies without the effect defending and absorb, shortwave blue light, crystalline lens can be penetrated and gone directly view Film.Blue light illumination retina will produce free radical, and these free radicals can cause retinal pigment epithelium to become feeble and die, and epithelium is thin The decline of born of the same parents can cause photaesthesia cell to lack nutrient so as to cause vision impairment, and people's eyes when using mobile phone are easy blue Light damage endangers the health of people.
Therefore, in order to solve the deficiency of above-mentioned technology, the present invention provides a kind of mobile phones that can defend shortwave blue light to protect Cuticula.
Invention content
For the defects in the prior art, the object of the present invention is to provide a kind of mobile phones that can defend shortwave blue light to protect Film, described can to defend the safeguard film for cellular phone of shortwave blue light include Ranvier's membrane, and the Ranvier's membrane side being connect with mobile phone is set gradually Ultraviolet-proof and anti-blue light coating;
Several grooves, centre setting through-hole is arranged to one face edge of Ranvier's membrane in the ultraviolet-proof;
Several grooves are arranged to one face edge of ultraviolet-proof in the anti-blue light coating;
The anti-blue light coating includes the raw material of following parts by weight:40-55 parts of acrylic acid glue, 5-13 parts of phenol derivatives, 7-17 parts of guar gum, 4-7 parts of palmitamide propyl betaine, 7-21 parts of pearl powder, 3-7 parts of chitosan, castor oil polyoxyethylene 1.7-2.3 parts of ether, 1.5-1.9 parts of coupling agent.
Preferably, described can to defend the safeguard film for cellular phone of shortwave blue light include Ranvier's membrane, the Ranvier's membrane being connect with mobile phone Side sets gradually ultraviolet-proof and anti-blue light coating;
Several grooves, centre setting through-hole is arranged to one face edge of Ranvier's membrane in the ultraviolet-proof;
Several grooves are arranged to one face edge of ultraviolet-proof in the anti-blue light coating;
The anti-blue light coating includes the raw material of following parts by weight:40-45 parts of acrylic acid glue, 6-13 parts of phenol derivatives, 8-17 parts of guar gum, 5-7 parts of palmitamide propyl betaine, 9-21 parts of pearl powder, 4-7 parts of chitosan, castor oil polyoxyethylene 1.7-2.2 parts of ether, 1.5-1.6 parts of coupling agent.
Preferably, described can to defend the safeguard film for cellular phone of shortwave blue light include Ranvier's membrane, the Ranvier's membrane being connect with mobile phone Side sets gradually ultraviolet-proof and anti-blue light coating;
Several grooves, centre setting through-hole is arranged to one face edge of Ranvier's membrane in the ultraviolet-proof;
Several grooves are arranged to one face edge of ultraviolet-proof in the anti-blue light coating;
The anti-blue light coating includes the raw material of following parts by weight:43 parts of acrylic acid glue, 11 parts of phenol derivatives, guar gum 9 parts, 6 parts of palmitamide propyl betaine, 13 parts of pearl powder, 5 parts of chitosan, 1.7 parts of castor oil polyoxyethylene ether, coupling agent 1.5 part.
Preferably, the anti-blue light coating also sets up waterproof layer away from mobile phone side.
Preferably, the ultraviolet light coating is coated on the surface of anti-blue light coating and Ranvier's membrane by anti-ultraviolet paint and is passed through It is formed by curing.
Preferably, the ultraviolet light coating includes the raw material of following parts by weight:30-45 parts of epoxy resin, ultraviolet light are inhaled Receive 1.7-2.8 parts of agent, 1.7-2.8 parts of dispersant, color masterbatch 4-7 parts silver grey, 8-13 parts of PE waxes, polypropylene terephthalate 2-11 parts, 2-5 parts of nano silicon dioxide, 1.6-3.4 parts of antiager.
Preferably, the anti-blue light coating is solidificated in antiultraviolet after first heat cure by the way of UV photocurings On coating.
Preferably, the thickness of the Ranvier's membrane is 160-270um, and the thickness of the ultraviolet-proof is 6-14um, institute The thickness for stating anti-blue light coating is 12-17um.
Compared with prior art, the present invention has following advantageous effect:
A kind of safeguard film for cellular phone that can defend shortwave blue light provided by the invention, safeguard film for cellular phone of the invention is in general hand It is improved on the basis of machine protection membrane structure, improved structure of safeguard film for cellular phone is:Including Ranvier's membrane, it is connect with mobile phone Ranvier's membrane side set gradually ultraviolet-proof and anti-blue light coating, pass through the double-layer structure of antiultraviolet and anti-blue light protect Shield largely intercepts and sorption enhanced blue light.In addition, the ultraviolet-proof is several to the setting of one face edge of Ranvier's membrane Groove, centre setting through-hole, so design is to gather the blue light that mobile phone discharges for the shape of the concavees lens formed by groove Collection gets up is discharged into anti-shortwave blue light coating sorption enhanced by intermediate through-hole.Meanwhile the anti-blue light coating is to UV resistance Line applies laminated edge and several grooves is arranged, for preventing the shortwave blue light loss not by sorption enhanced from removing.Pass through above-mentioned knot The design of structure can absorb 99% or more ultraviolet light, 96% or more shortwave blue light.
Description of the drawings
Upon reading the detailed description of non-limiting embodiments with reference to the following drawings, other feature of the invention, Objects and advantages will become more apparent upon:
Fig. 1 is a kind of structure of safeguard film for cellular phone schematic diagram that can defend shortwave blue light provided by the invention;
Fig. 2 is a kind of ultraviolet-proof structural schematic diagram provided by the invention.
Specific implementation mode
Present invention will be further explained below with reference to specific examples.It should be understood that these embodiments are merely to illustrate the present invention Rather than it limits the scope of the invention.
Embodiment 1
In conjunction with Fig. 1, Fig. 2, on the one hand a kind of safeguard film for cellular phone that can defend shortwave blue light that the present embodiment provides, it is described can be with It includes Ranvier's membrane 1 to defend the safeguard film for cellular phone of shortwave blue light, and 1 side of Ranvier's membrane being connect with mobile phone sets gradually antiultraviolet painting Layer 2 and anti-blue light coating 3;
Several grooves 4, centre setting through-hole 5 is arranged to 1 one face edge of Ranvier's membrane in the ultraviolet-proof 2;
Several grooves 4 are arranged to 2 one face edge of ultraviolet-proof in the anti-blue light coating 3;
The anti-blue light coating 3 includes the raw material of following parts by weight:55 parts of acrylic acid glue, 5 parts of phenol derivatives, guar gum 17 parts, 4 parts of palmitamide propyl betaine, 21 parts of pearl powder, 3 parts of chitosan, 2.3 parts of castor oil polyoxyethylene ether, coupling agent 1.5 part.
Preferably, the anti-blue light coating 3 also sets up waterproof layer away from mobile phone side.
Preferably, the ultraviolet light coating is coated on anti-blue light coating 3 and Ranvier's membrane 1 by anti-ultraviolet paint Cured formation on surface.
Preferably, the ultraviolet light coating includes the raw material of following parts by weight:45 parts of epoxy resin, ultraviolet light 1.7 parts of absorbent, 2.8 parts of dispersant, 4 parts of silver grey color masterbatch, 13 parts of PE waxes, 2 part, nanometer two of polypropylene terephthalate 5 parts of silica, 1.6 parts of antiager.
Preferably, the anti-blue light coating 3 is solidificated in after first heat cure by the way of UV photocurings In ultraviolet-proof 2.
Preferably, the thickness of the Ranvier's membrane 1 is 270um, and the thickness of the ultraviolet-proof is 6um, institute The thickness for stating anti-blue light coating 3 is 17um.
Embodiment 2
In conjunction with Fig. 1, Fig. 2, on the one hand a kind of safeguard film for cellular phone that can defend shortwave blue light that the present embodiment provides, it is described can be with It includes Ranvier's membrane 1 to defend the safeguard film for cellular phone of shortwave blue light, and 1 side of Ranvier's membrane being connect with mobile phone sets gradually antiultraviolet painting Layer 2 and anti-blue light coating 3;
Several grooves 4, centre setting through-hole 5 is arranged to 1 one face edge of Ranvier's membrane in the ultraviolet-proof 2;
Several grooves 4 are arranged to 2 one face edge of ultraviolet-proof in the anti-blue light coating 3;
The anti-blue light coating 3 includes the raw material of following parts by weight:40 parts of acrylic acid glue, 6 parts of phenol derivatives, guar gum 17 parts, 5 parts of palmitamide propyl betaine, 21 parts of pearl powder, 4 parts of chitosan, 2.2 parts of castor oil polyoxyethylene ether, coupling agent 1.5 part.
Preferably, the anti-blue light coating 3 also sets up waterproof layer away from mobile phone side.
Preferably, the ultraviolet light coating is coated on anti-blue light coating 3 and Ranvier's membrane 1 by anti-ultraviolet paint Cured formation on surface.
Preferably, the ultraviolet light coating includes the raw material of following parts by weight:45 parts of epoxy resin, ultraviolet light 1.7 parts of absorbent, 2.8 parts of dispersant, 4 parts of silver grey color masterbatch, 13 parts of PE waxes, 2 part, nanometer two of polypropylene terephthalate 5 parts of silica, 1.6 parts of antiager.
Preferably, the anti-blue light coating 3 is solidificated in after first heat cure by the way of UV photocurings In ultraviolet-proof 2.
Preferably, the thickness of the Ranvier's membrane 1 is 270um, and the thickness of the ultraviolet-proof is 6um, institute The thickness for stating anti-blue light coating 3 is 17um.
Embodiment 3
In conjunction with Fig. 1, Fig. 2, on the one hand a kind of safeguard film for cellular phone that can defend shortwave blue light that the present embodiment provides, it is described can be with It includes Ranvier's membrane 1 to defend the safeguard film for cellular phone of shortwave blue light, and 1 side of Ranvier's membrane being connect with mobile phone sets gradually antiultraviolet painting Layer 2 and anti-blue light coating 3;
Several grooves 4, centre setting through-hole 5 is arranged to 1 one face edge of Ranvier's membrane in the ultraviolet-proof 2;
Several grooves 4 are arranged to 2 one face edge of ultraviolet-proof in the anti-blue light coating 3;
The anti-blue light coating 3 includes the raw material of following parts by weight:43 parts of acrylic acid glue, 11 parts of phenol derivatives, Gu Er 9 parts of glue, 6 parts of palmitamide propyl betaine, 13 parts of pearl powder, 5 parts of chitosan, 1.7 parts of castor oil polyoxyethylene ether, coupling agent 1.5 part.
Preferably, the anti-blue light coating 3 also sets up waterproof layer away from mobile phone side.
Preferably, the ultraviolet light coating is coated on anti-blue light coating 3 and Ranvier's membrane 1 by anti-ultraviolet paint Cured formation on surface.
Preferably, the ultraviolet light coating includes the raw material of following parts by weight:45 parts of epoxy resin, ultraviolet light 2.8 parts of absorbent, 2.8 parts of dispersant, 7 parts of silver grey color masterbatch, 13 parts of PE waxes, polypropylene terephthalate 11 part, nanometer 5 parts of silica, 3.4 parts of antiager.
Preferably, the anti-blue light coating 3 is solidificated in after first heat cure by the way of UV photocurings In ultraviolet-proof 2.
Preferably, the thickness of the Ranvier's membrane 1 is 160um, and the thickness of the ultraviolet-proof is 6um, institute The thickness for stating anti-blue light coating 3 is 12um.
Embodiment 4
In conjunction with Fig. 1, Fig. 2, on the one hand a kind of safeguard film for cellular phone that can defend shortwave blue light that the present embodiment provides, it is described can be with It includes Ranvier's membrane 1 to defend the safeguard film for cellular phone of shortwave blue light, and 1 side of Ranvier's membrane being connect with mobile phone sets gradually antiultraviolet painting Layer 2 and anti-blue light coating 3;
Several grooves 4, centre setting through-hole 5 is arranged to 1 one face edge of Ranvier's membrane in the ultraviolet-proof 2;
Several grooves 4 are arranged to 2 one face edge of ultraviolet-proof in the anti-blue light coating 3;
The anti-blue light coating 3 includes the raw material of following parts by weight:40 parts of acrylic acid glue, 6 parts of phenol derivatives, guar gum 17 parts, 5 parts of palmitamide propyl betaine, 21 parts of pearl powder, 4 parts of chitosan, 2.2 parts of castor oil polyoxyethylene ether, coupling agent 1.5 part.
Preferably, the anti-blue light coating 3 also sets up waterproof layer away from mobile phone side.
Preferably, the ultraviolet light coating is coated on anti-blue light coating 3 and Ranvier's membrane 1 by anti-ultraviolet paint Cured formation on surface.
Preferably, the ultraviolet light coating includes the raw material of following parts by weight:30 parts of epoxy resin, ultraviolet light 2.8 parts of absorbent, 1.7 parts of dispersant, 7 parts of silver grey color masterbatch, 8 parts of PE waxes, 11 part, nanometer two of polypropylene terephthalate 2 parts of silica, 3.4 parts of antiager.
Preferably, the anti-blue light coating 3 is solidificated in after first heat cure by the way of UV photocurings In ultraviolet-proof 2.
Preferably, the thickness of the Ranvier's membrane 1 is 160um, and the thickness of the ultraviolet-proof is 14um, institute The thickness for stating anti-blue light coating 3 is 12um.
Specific embodiments of the present invention are described above.It is to be appreciated that the invention is not limited in above-mentioned Particular implementation, those skilled in the art can make various deformations or amendments within the scope of the claims, this not shadow Ring the substantive content of the present invention.

Claims (8)

1. a kind of safeguard film for cellular phone that can defend shortwave blue light, it is characterised in that:The mobile phone that can defend shortwave blue light Protective film includes Ranvier's membrane, and the Ranvier's membrane side being connect with mobile phone sets gradually ultraviolet-proof and anti-blue light coating;
Several grooves, centre setting through-hole is arranged to one face edge of Ranvier's membrane in the ultraviolet-proof;
Several grooves are arranged to one face edge of ultraviolet-proof in the anti-blue light coating;
The anti-blue light coating includes the raw material of following parts by weight:40-55 parts of acrylic acid glue, 5-13 parts of phenol derivatives, 7-17 parts of guar gum, 4-7 parts of palmitamide propyl betaine, 7-21 parts of pearl powder, 3-7 parts of chitosan, castor oil polyoxyethylene 1.7-2.3 parts of ether, 1.5-1.9 parts of coupling agent.
2. the safeguard film for cellular phone according to claim 1 that shortwave blue light can be defendd, it is characterised in that:It is described to defend The safeguard film for cellular phone of shortwave blue light includes Ranvier's membrane, and the Ranvier's membrane side being connect with mobile phone sets gradually ultraviolet-proof and prevents Blue light coating;
Several grooves, centre setting through-hole is arranged to one face edge of Ranvier's membrane in the ultraviolet-proof;
Several grooves are arranged to one face edge of ultraviolet-proof in the anti-blue light coating;
The anti-blue light coating includes the raw material of following parts by weight:40-45 parts of acrylic acid glue, 6-13 parts of phenol derivatives, 8-17 parts of guar gum, 5-7 parts of palmitamide propyl betaine, 9-21 parts of pearl powder, 4-7 parts of chitosan, castor oil polyoxyethylene 1.7-2.2 parts of ether, 1.5-1.6 parts of coupling agent.
3. the safeguard film for cellular phone according to claim 1 that shortwave blue light can be defendd, it is characterised in that:It is described to defend The safeguard film for cellular phone of shortwave blue light includes Ranvier's membrane, and the Ranvier's membrane side being connect with mobile phone sets gradually ultraviolet-proof and prevents Blue light coating;
Several grooves, centre setting through-hole is arranged to one face edge of Ranvier's membrane in the ultraviolet-proof;
Several grooves are arranged to one face edge of ultraviolet-proof in the anti-blue light coating;
The anti-blue light coating includes the raw material of following parts by weight:43 parts of acrylic acid glue, 11 parts of phenol derivatives, guar gum 9 parts, 6 parts of palmitamide propyl betaine, 13 parts of pearl powder, 5 parts of chitosan, 1.7 parts of castor oil polyoxyethylene ether, coupling agent 1.5 part.
4. the safeguard film for cellular phone according to claim 1 that shortwave blue light can be defendd, it is characterised in that:The anti-blue light applies Layer also sets up waterproof layer away from mobile phone side.
5. the safeguard film for cellular phone according to claim 1 that shortwave blue light can be defendd, it is characterised in that:The ultraviolet light applies Layer is coated on cured formation on the surface of anti-blue light coating and Ranvier's membrane by anti-ultraviolet paint.
6. the safeguard film for cellular phone according to claim 5 that shortwave blue light can be defendd, it is characterised in that:The ultraviolet light applies Layer includes the raw material of following parts by weight:30-45 parts of epoxy resin, 1.7-2.8 parts of ultra-violet absorber, dispersant 1.7-2.8 It is part, color masterbatch 4-7 parts silver grey, 8-13 parts of PE waxes, 2-11 parts of polypropylene terephthalate, 2-5 parts of nano silicon dioxide, resistance to 1.6-3.4 parts of aging agent.
7. the safeguard film for cellular phone according to claim 1 that shortwave blue light can be defendd, it is characterised in that:The anti-blue light Coating is solidificated in by the way of UV photocurings in ultraviolet-proof after first heat cure.
8. the safeguard film for cellular phone according to claim 7 that shortwave blue light can be defendd, it is characterised in that:The Ranvier's membrane Thickness is 160-270um, and the thickness of the ultraviolet-proof is 6-14um, and the thickness of the anti-blue light coating is 12-17um.
CN201810364094.9A 2018-04-23 2018-04-23 A kind of safeguard film for cellular phone that can defend shortwave blue light Withdrawn CN108663737A (en)