CN108325736A
CN108325736A CN201810032055.9A CN201810032055A CN108325736A CN 108325736 A CN108325736 A CN 108325736A CN 201810032055 A CN201810032055 A CN 201810032055A CN 108325736 A CN108325736 A CN 108325736A
Authority
CN
China
Prior art keywords
low
concentrate
magnetic separation
obtains
tailing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810032055.9A
Other languages
Chinese (zh)
Inventor
张敏
张一敏
许承宝
刘涛
黄晶
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wuhan University of Science and Engineering WUSE
Wuhan University of Science and Technology WHUST
Original Assignee
Wuhan University of Science and Engineering WUSE
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wuhan University of Science and Engineering WUSE filed Critical Wuhan University of Science and Engineering WUSE
Priority to CN201810032055.9A priority Critical patent/CN108325736A/en
Publication of CN108325736A publication Critical patent/CN108325736A/en
Pending legal-status Critical Current

Links

Classifications

    • BPERFORMING OPERATIONS; TRANSPORTING
    • B03SEPARATION OF SOLID MATERIALS USING LIQUIDS OR USING PNEUMATIC TABLES OR JIGS; MAGNETIC OR ELECTROSTATIC SEPARATION OF SOLID MATERIALS FROM SOLID MATERIALS OR FLUIDS; SEPARATION BY HIGH-VOLTAGE ELECTRIC FIELDS
    • B03BSEPARATING SOLID MATERIALS USING LIQUIDS OR USING PNEUMATIC TABLES OR JIGS
    • B03B7/00Combinations of wet processes or apparatus with other processes or apparatus, e.g. for dressing ores or garbage
    • BPERFORMING OPERATIONS; TRANSPORTING
    • B03SEPARATION OF SOLID MATERIALS USING LIQUIDS OR USING PNEUMATIC TABLES OR JIGS; MAGNETIC OR ELECTROSTATIC SEPARATION OF SOLID MATERIALS FROM SOLID MATERIALS OR FLUIDS; SEPARATION BY HIGH-VOLTAGE ELECTRIC FIELDS
    • B03BSEPARATING SOLID MATERIALS USING LIQUIDS OR USING PNEUMATIC TABLES OR JIGS
    • B03B9/00General arrangement of separating plant, e.g. flow sheets

Abstract

The present invention relates to a kind of Preconcentrations of low-grade vanadium titano-magnetite.Its technical solution is:By low-grade vanadium titano-magnetite crushing raw ore to grain size≤3mm, one section of high intensity magnetic separation is carried out under conditions of magnetic field intensity is 0.6 ~ 1.2T, obtains one section of high intensity magnetic separation concentrate and tailings;One section of high intensity magnetic separation concentrate is milled to grain size again and accounts for 50 ~ 80wt% less than 0.074mm, obtains ore milling product;The ore milling product is subjected to one section of low intensity magnetic separation under conditions of magnetic field intensity is 0.08 ~ 0.20T, obtains weak magnetic concentrate selection and low intensity magnetic separation tailing;Then the low intensity magnetic separation tailing is subjected to sluicing, obtains gravity concentrate and tailing;The gravity concentrate is subjected to two sections of high intensity magnetic separations under conditions of magnetic field intensity is 0.4 ~ 0.8T, obtains two stages of magnetic separation concentrate and tailings.The present invention has the characteristics that reduction throughput is notable, concentration ratio is high and at low cost.

Description

A kind of Preconcentration of low-grade vanadium titano-magnetite
Technical field
The invention belongs to vanadium titano-magnetite ore dressing technical fields.More particularly to a kind of preenrichment of low-grade vanadium titano-magnetite Method.
Background technology
Vanadium titano-magnetite is a kind of more metal mineral intergrowths containing vanadium, titanium, iron, has higher comprehensive utilization value.China Vanadium titano-magnetite rich reserves, in addition to being mainly distributed on Pan Xi and Chengde area, China Chaoyang area keeps a large amount of low-grade Vanadium titano-magnetite, prospective reserves are currently in state to be developed at 20,000,000,000 tons or more.When vanadium in v-ti magnetite green ore, titanium, When the grade of iron is relatively low, ore-dressing technique will face the problem that throughput is big, ore grinding high energy consumption and production cost are high, therefore pass through Efficient preenrichment technology of helping is the key that ensure that low-grade vanadium titano-magnetite realizes vanadium, titanium, iron high-efficiency comprehensive utilization.
In vanadium titano-magnetite, mainly preservation is in titanomagnetite in the form of isomorphous for vanadium, and the main preservation of titanium is in titanium In iron ore.Currently, the technique of preparing of vanadium titano-magnetite is general first to recycle titanomagnetite, then the recovery Pd from weakly magnetic tailings with weak magnetic Iron ore.Ilmenite technique of preparing mainly has:Gravity treatment, magnetic separation, flotation and electric separation;Though the separating effect of flotation and electric separation is good, it Commonly used in selected, and when head grade is relatively low, since throughput is big, flotation and electric separation are respectively present reagent consumption Greatly, the problem of high energy consumption.Therefore, inexpensive and environment amenable gravity treatment and magnetic separation work are first used to low-grade vanadium titano-magnetite Skill carries out preenrichment, provides quality raw materials for flotation or electric separation and is of great significance.
" a kind of efficient ore dressing of synthetical recovery low-grade vanadium titano-magnetite "(CN 103736588 A)Patented technology, adopt 50% or more tailing is abandoned with primary grinding-low intensity magnetic separation pretreatment, to reduce two sections of workload.But this method allows originally The tailing that can directly abandon enters primary grinding operation so that the energy consumption of primary grinding operation increases.
Han Yuanyan(Han Yuanyan, wears the new Yunnan low-grade ilmenite ore-dressing technique research [J] the mining and metallurgys of favour, and 2010,19 (4))Using low-grade ilmenite as research object, tailing is abandoned using gravity treatment in advance to raw ore, to reduce into sorting operation Ore amount.Though this method can abandon a large amount of tailing, not high to the concentration ratio of ilmenite.
" side of the method and recycling ilmenite of ilmenite and its Treatment of Middling is recycled in iron tailings of low-grade vanadium titano gravity treatment Method "(CN 106216083 A)Patented technology, ilmenite is recycled from iron tailings of low-grade vanadium titano using single gravity concentration.It should Though method can obtain more high-grade ilmenite concentrate, the rate of recovery of titanium is relatively low.
" extreme poverty v-ti magnetite ore comprehensive reutilization method "(CN 103785518 A)Patented technology, with vanadium titanium magnetic Tailing after Iron Mine iron uses single high intensity magnetic separation preenrichment ilmenite before flotation operation, can get as titanium raw ore is selected TiO2The high intensity magnetic mineral of grade >=20%, though improve the grade into floating raw material.But poor value is handled with this method, can be deposited The problem of throughput is big, high energy consumption.
Invention content
The present invention is directed to overcome prior art defect, it is therefore an objective to provide that a kind of reduction throughput is notable, concentration ratio is high With the Preconcentration of low-grade vanadium titano-magnetite at low cost.
To achieve the above object, the step of the technical solution adopted by the present invention is:
(1)First by low-grade vanadium titano-magnetite crushing raw ore to grain size≤3mm, then in the condition that magnetic field intensity is 0.6 ~ 1.2T One section of high intensity magnetic separation of lower progress obtains one section of high intensity magnetic separation concentrate and tailings.
(2)One section of high intensity magnetic separation concentrate is milled to grain size and accounts for 50 ~ 80wt% less than 0.074mm, obtains ore milling product;Again The ore milling product is subjected to one section of low intensity magnetic separation under conditions of magnetic field intensity is 0.08 ~ 0.20T, obtains weak magnetic concentrate selection and weak Magnetic tailing.
(3)The low intensity magnetic separation tailing is subjected to sluicing, obtains gravity concentrate and tailing.
(4)The gravity concentrate is subjected to two sections of high intensity magnetic separations under conditions of magnetic field intensity is 0.4 ~ 0.8T, obtains two sections Magnetic concentrate and tailing.
The low-grade vanadium titano-magnetite raw ore:V2O5Grade is 0.03 ~ 0.20wt%;TiO2Grade be 1.50 ~ 4.50wt%;TFe grades are 8.00 ~ 18.00wt%.
Due to the adoption of the above technical scheme, the present invention has following good effect compared with prior art:
1, the present invention first passes through the tailing that strong magnetic abandons 60 ~ 90%, is greatly reduced into grinding operation before grinding operation Ore amount, to significantly reduce the energy consumption of grinding operation.
2, the present invention first uses the gravity separation technology that treating capacity is big, low energy consumption to weakly magnetic tailings, abandons 40 ~ 70% tailing in advance, The throughput for significantly reducing follow-up high intensity magnetic separation process, to reduce cost.
3, the present invention uses weight-magnetic process integration preenrichment weakly magnetic tailings, can get TiO2The titanium that grade is 21 ~ 25% is thick Concentrate, concentration ratio is high, can provide quality raw materials for follow-up flotation or electric separation operation.
Therefore, the present invention has the characteristics that reduction throughput is notable, concentration ratio is high and at low cost.
Specific implementation mode
For a better understanding of the present invention, present disclosure is described further with reference to embodiment, but this The content of invention is not limited solely to the following examples.Made by all substantive contents according to the present invention it is any it is simple modification and Equivalent structure transformation or modification, are covered by the protection scope of the present invention.
Embodiment 1
A kind of Preconcentration of low-grade vanadium titano-magnetite.
The present embodiment use low-grade vanadium titano-magnetite raw ore be:V2O5Grade is 0.03 ~ 0.11wt%;TiO2Grade is 1.50~2.70wt%;TFe grades are 8.00 ~ 12.00wt%.
It is the step of Preconcentration described in the present embodiment:
(1)First by low-grade vanadium titano-magnetite crushing raw ore to grain size≤3mm, then in the condition that magnetic field intensity is 0.8 ~ 1.2T One section of high intensity magnetic separation of lower progress obtains one section of high intensity magnetic separation concentrate and tailings.
(2)One section of high intensity magnetic separation concentrate is milled to grain size and accounts for 60 ~ 70wt% less than 0.074mm, obtains ore milling product;Again The ore milling product is subjected to one section of low intensity magnetic separation under conditions of magnetic field intensity is 0.10 ~ 0.17T, obtains weak magnetic concentrate selection and weak Magnetic tailing.
(3)The low intensity magnetic separation tailing is subjected to sluicing, obtains gravity concentrate and tailing.
(4)The gravity concentrate is subjected to two sections of high intensity magnetic separations under conditions of magnetic field intensity is 0.5 ~ 0.7T, obtains two sections Magnetic concentrate and tailing.
The present embodiment first passes through the tailing that strong magnetic abandons 60 ~ 80%, then use chute to weakly magnetic tailings before grinding operation 50 ~ 70% tailing is abandoned in sorting, and TiO is obtained finally by strong magnetic2The titanium rough concentrate that grade is 22 ~ 24%.
Embodiment 2
A kind of Preconcentration of low-grade vanadium titano-magnetite.
The present embodiment use low-grade vanadium titano-magnetite raw ore be:V2O5Grade is 0.08 ~ 0.16wt%;TiO2Grade is 2.40~3.60wt%;TFe grades are 11.00 ~ 15.00wt%.
It is the step of Preconcentration described in the present embodiment:
(1)First by low-grade vanadium titano-magnetite crushing raw ore to grain size≤3mm, then in the condition that magnetic field intensity is 0.7 ~ 1.0T One section of high intensity magnetic separation of lower progress obtains one section of high intensity magnetic separation concentrate and tailings.
(2)One section of high intensity magnetic separation concentrate is milled to grain size and accounts for 50 ~ 60wt% less than 0.074mm, obtains ore milling product;Again The ore milling product is subjected to one section of low intensity magnetic separation under conditions of magnetic field intensity is 0.14 ~ 0.20T, obtains weak magnetic concentrate selection and weak Magnetic tailing.
(3)The low intensity magnetic separation tailing is subjected to sluicing, obtains gravity concentrate and tailing.
(4)The gravity concentrate is subjected to two sections of high intensity magnetic separations under conditions of magnetic field intensity is 0.4 ~ 0.6T, obtains two sections Magnetic concentrate and tailing.
The present embodiment first passes through the tailing that strong magnetic abandons 70 ~ 90%, then use chute to weakly magnetic tailings before grinding operation 40 ~ 60% tailing is abandoned in sorting, and TiO is obtained finally by strong magnetic2The titanium rough concentrate that grade is 21 ~ 23%.
Embodiment 3
A kind of Preconcentration of low-grade vanadium titano-magnetite.
The present embodiment use low-grade vanadium titano-magnetite raw ore be:V2O5Grade is 0.12 ~ 0.20wt%;TiO2Grade is 3.30~4.50wt%;TFe grades are 14.00 ~ 18.00wt%.
It is the step of Preconcentration described in the present embodiment:
(1)First by low-grade vanadium titano-magnetite crushing raw ore to grain size≤3mm, then in the condition that magnetic field intensity is 0.6 ~ 0.9T One section of high intensity magnetic separation of lower progress obtains one section of high intensity magnetic separation concentrate and tailings.
(2)One section of high intensity magnetic separation concentrate is milled to grain size and accounts for 70 ~ 80wt% less than 0.074mm, obtains ore milling product;Again The ore milling product is subjected to one section of low intensity magnetic separation under conditions of magnetic field intensity is 0.08 ~ 0.14T, obtains weak magnetic concentrate selection and weak Magnetic tailing.
(3)The low intensity magnetic separation tailing is subjected to sluicing, obtains gravity concentrate and tailing.
(4)The gravity concentrate is subjected to two sections of high intensity magnetic separations under conditions of magnetic field intensity is 0.6 ~ 0.8T, obtains two sections Magnetic concentrate and tailing.
The present embodiment first passes through the tailing that strong magnetic abandons 80 ~ 90%, then use chute to weakly magnetic tailings before grinding operation 40 ~ 50% tailing is abandoned in sorting, and TiO is obtained finally by strong magnetic2The titanium rough concentrate that grade is 22 ~ 25%.
Present embodiment compared with prior art, has the positive effect that:
1, present embodiment first passes through the tailing that strong magnetic abandons 60 ~ 90% before grinding operation, is greatly reduced into mill The ore amount of mine operation, to significantly reduce the energy consumption of grinding operation.
2, present embodiment first uses the gravity separation technology that treating capacity is big, low energy consumption to weakly magnetic tailings, abandon 40 in advance ~ 70% tailing significantly reduces the throughput of follow-up high intensity magnetic separation process, to reduce cost.
3, present embodiment uses weight-magnetic process integration preenrichment weakly magnetic tailings, can get TiO2Grade be 21 ~ 25% titanium rough concentrate, concentration ratio is high, can provide quality raw materials for follow-up flotation or electric separation operation.
Therefore, present embodiment has the characteristics that reduction throughput is notable, concentration ratio is high and at low cost.

Claims (2)

1. a kind of Preconcentration of low-grade vanadium titano-magnetite, which is characterized in that it is as follows:
(1)First by low-grade vanadium titano-magnetite crushing raw ore to grain size≤3mm, then in the condition that magnetic field intensity is 0.6 ~ 1.2T One section of high intensity magnetic separation of lower progress obtains one section of high intensity magnetic separation concentrate and tailings;
(2)One section of high intensity magnetic separation concentrate is milled to grain size and accounts for 50 ~ 80wt% less than 0.074mm, obtains ore milling product;Again by institute It states ore milling product and carries out one section of low intensity magnetic separation under conditions of magnetic field intensity is 0.08 ~ 0.20T, obtain weak magnetic concentrate selection and low intensity magnetic separation Tailing;
(3)The low intensity magnetic separation tailing is subjected to sluicing, obtains gravity concentrate and tailing;
(4)The gravity concentrate is subjected to two sections of high intensity magnetic separations under conditions of magnetic field intensity is 0.4 ~ 0.8T, obtains two stages of magnetic separation Concentrate and tailings.
2. the Preconcentration of low-grade vanadium titano-magnetite according to claim 1, it is characterised in that the low grade vanadium Titanomagnetite raw ore:V2O5Grade is 0.03 ~ 0.20wt%;TiO2Grade is 1.50 ~ 4.50wt%;TFe grades be 8.00 ~ 18.00wt%。
CN201810032055.9A 2018-01-12 2018-01-12 A kind of Preconcentration of low-grade vanadium titano-magnetite Pending CN108325736A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201810032055.9A CN108325736A (en) 2018-01-12 2018-01-12 A kind of Preconcentration of low-grade vanadium titano-magnetite

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201810032055.9A CN108325736A (en) 2018-01-12 2018-01-12 A kind of Preconcentration of low-grade vanadium titano-magnetite

Publications (1)

Publication Number Publication Date
CN108325736A true CN108325736A (en) 2018-07-27

Family

ID=62924188

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201810032055.9A Pending CN108325736A (en) 2018-01-12 2018-01-12 A kind of Preconcentration of low-grade vanadium titano-magnetite

Country Status (1)

Country Link
CN (1) CN108325736A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN111841881A (en) * 2020-07-29 2020-10-30 攀钢集团矿业有限公司 Method for recovering titanomagnetite in beneficiation process

Citations (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101564707A (en) * 2009-05-15 2009-10-28 四川安宁铁钛股份有限公司 Vanadium titano-magnetite screen method
CN102814230A (en) * 2012-09-06 2012-12-12 昆明冶金研究院 Beneficiation method for separating and comprehensively recycling ferrotitanium in titaniferous iron ore concentrate
CN103551582A (en) * 2013-11-12 2014-02-05 攀枝花钢城集团有限公司 Method for producing fine iron powder with converter sludge in vanadium-titano magnetite smelting
CN103736588A (en) * 2014-01-16 2014-04-23 玉溪大红山矿业有限公司 Efficient beneficiation method of comprehensively recovering low-grade vanadium titano-magnetite
CN104394993A (en) * 2013-02-01 2015-03-04 河北联合大学 method for pre-treating ilmenite tailings after iron-beneficiation
CN204448257U (en) * 2015-03-04 2015-07-08 山东兴盛矿业有限责任公司 A kind ofly select iron device for super low-grade vanadium titano-magnetite

Patent Citations (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101564707A (en) * 2009-05-15 2009-10-28 四川安宁铁钛股份有限公司 Vanadium titano-magnetite screen method
CN102814230A (en) * 2012-09-06 2012-12-12 昆明冶金研究院 Beneficiation method for separating and comprehensively recycling ferrotitanium in titaniferous iron ore concentrate
CN104394993A (en) * 2013-02-01 2015-03-04 河北联合大学 method for pre-treating ilmenite tailings after iron-beneficiation
CN103551582A (en) * 2013-11-12 2014-02-05 攀枝花钢城集团有限公司 Method for producing fine iron powder with converter sludge in vanadium-titano magnetite smelting
CN103736588A (en) * 2014-01-16 2014-04-23 玉溪大红山矿业有限公司 Efficient beneficiation method of comprehensively recovering low-grade vanadium titano-magnetite
CN204448257U (en) * 2015-03-04 2015-07-08 山东兴盛矿业有限责任公司 A kind ofly select iron device for super low-grade vanadium titano-magnetite

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN111841881A (en) * 2020-07-29 2020-10-30 攀钢集团矿业有限公司 Method for recovering titanomagnetite in beneficiation process

Similar Documents

Publication Publication Date Title
WO2022032922A1 (en) Series elutriation and deep beneficiation process for magnetite extremely difficult to be beneficiated
CN101502819B (en) Pre-selection method of low-ore grade magnetic iron ore
CN103736588B (en) Efficient beneficiation method of comprehensively recovering low-grade vanadium titano-magnetite
CN102814230A (en) Beneficiation method for separating and comprehensively recycling ferrotitanium in titaniferous iron ore concentrate
CN107470013A (en) Feldspar concentrate separated from vanadium titano-magnetite tailings and separation method thereof
CN108393192B (en) Beneficiation method for ilmenite
CN102172560A (en) Method for recovering tin by centrifugal concentration
CN108993764A (en) Miscellaneous process drops in a kind of chromium depleted zone upgrading
CN111013811A (en) Thickness separation-gravity-magnetic combined mineral separation process for treating Anshan type iron ore
CN112024120B (en) Beneficiation method for micro-fine-particle-grade hematite and limonite
CN108855583A (en) A kind of method of vanadium titano-magnetite ore dressing preenrichment
CN111068897A (en) Fine particle magnetite beneficiation process
CN107649278B (en) A kind of method for separating of low-grade titanium-containing magnet mine
CN104888939A (en) Magnetic separation and gravity separation pre-concentration and rough concentrate regrinding and re-concentration hematite tailing recovery process
CN108993760B (en) Weathered low-grade refractory manganese ore sorting process
CN114178043B (en) Beneficiation process for copper-containing iron ore
CN107824331A (en) A kind of magnetic of low-grade ilmenite stone-floating beneficiation combined method method
CN113909154A (en) Beneficiation method for copper oxide ore containing malachite and peacock stone
CN108325736A (en) A kind of Preconcentration of low-grade vanadium titano-magnetite
CN105665133A (en) Comprehensive recycling method of stone tailing resources
CN109127122B (en) Beneficiation method for improving iron and reducing silicon of magnetite concentrate
CN113182076B (en) Comprehensive treatment method of titanium concentrate for titanium chloride slag raw material
CN102861668A (en) Coarse tail throwing device of dry-type magnetic rotary drum
CN107243406A (en) A kind of method of the feldspar of niobium containing tantalum tailing resource recycling
CN109847923A (en) Efficient recovery process of extremely-poor weathered primary ilmenite

Legal Events

Date Code Title Description
PB01 Publication
PB01 Publication
SE01 Entry into force of request for substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication

Application publication date: 20180727