CN108000670A - For manufacturing the glue system and glue applying method of wood-based plate - Google Patents

For manufacturing the glue system and glue applying method of wood-based plate Download PDF

Info

Publication number
CN108000670A
CN108000670A CN201711415264.3A CN201711415264A CN108000670A CN 108000670 A CN108000670 A CN 108000670A CN 201711415264 A CN201711415264 A CN 201711415264A CN 108000670 A CN108000670 A CN 108000670A
Authority
CN
China
Prior art keywords
glue
moisture content
mixture
applying method
auxiliary agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201711415264.3A
Other languages
Chinese (zh)
Inventor
赵治美
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wanhua Hexiang Board Industry Co ltd
Original Assignee
Wanhua Ecoboard Xinyang Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wanhua Ecoboard Xinyang Co Ltd filed Critical Wanhua Ecoboard Xinyang Co Ltd
Priority to CN201711415264.3A priority Critical patent/CN108000670A/en
Publication of CN108000670A publication Critical patent/CN108000670A/en
Pending legal-status Critical Current

Abstract

The present invention discloses a kind of glue system for being used to manufacture wood-based plate, the glue system includes feedstock supply unit and sizing mixing arrangement, the feedstock supply unit includes being used to provide the material supplying device of material, the glue feeding mechanism for providing glue, the sizing mixing arrangement is used to mix in the material, the glue, forms mixture;The glue system further includes humidification unit, and the humidification unit includes the detecting device for moisture content for being used to detect the moisture content of the material and/or the mixture, and the humidifying device of the moisture content for improving the material and/or the mixture.The invention further relates to a kind of glue applying method for being used to manufacture wood-based plate.Preferably water content can be carried out to material and/or mixture to detect and control, avoid moisture content too low using the present invention.

Description

For manufacturing the glue system and glue applying method of wood-based plate
Technical field
The present invention relates to artificial board technology field, and in particular, to a kind of to be used to manufacture the glue system of wood-based plate and apply Gluing method.
Background technology
Stalk board is mainly using agricultural crop straw and the plate of the not release formaldehyde produced without aldehyde glue as raw material.With people Health environment-friendly consciousness steps up, and release formaldehyde wood-based plate is not the development trend and certainty of following wood-based plate.
In existing Wood-based Panel Production, without detection material water ratio before material sizing, and material humidification dress is not provided with Put, cause when material water ratio it is relatively low, humidification processing can not be carried out to material.And only ensure to produce back plate by applying glue The intensity and each side physicochemical property of material, do not carry out the addition of auxiliary agent (waterproofing agent, tackifier etc.) in production, cause easily to occur Material water ratio is relatively low, mat formation after after slab turned-down edge, veneer the defects of the sheet material edge moisture absorption.So how to ensure that material is aqueous It is one of main bugbear in Wood-based Panel Production that rate, which reaches technological requirement,.Therefore, to the glue system and method for manufacture wood-based plate Optimize necessary.
The content of the invention
The present invention solves at least one aspect of the above problem, there is provided a kind of glue system for wood-based plate, should System has humidification unit, it can be ensured that material water ratio reaches technological requirement, increases auxiliary agent in Process of Applying Glue, promotes product The raising of quality.
According to an aspect of the present invention, there is provided a kind of glue system for being used to manufacture wood-based plate, the glue system bag Include feedstock supply unit and sizing mixing arrangement, the feedstock supply unit include be used for provide material material supplying device, For providing the glue feeding mechanism of glue, the sizing mixing arrangement is used to mix in the material, the glue, forms mixture; The glue system further includes humidification unit, and the humidification unit includes being used for detecting the material and/or the mixture The detecting device for moisture content of moisture content, and the humidifying device of the moisture content for improving the material and/or the mixture.
In certain embodiments, the feedstock supply unit further includes the auxiliary agent feeding mechanism for providing auxiliary agent, described Mixture further includes auxiliary agent.
In certain embodiments, the auxiliary agent includes at least one of tackifier, waterproofing agent and mould inhibitor.
In certain embodiments, the sizing mixing arrangement includes continuous glue mixer and ring type glue mixer.
In certain embodiments, the auxiliary agent feeding mechanism is arranged at the continuous glue mixer and/or the ring type is mixed Jiao Jichu.
In certain embodiments, the humidification unit is arranged at the material supplying device and/or the ring type glue mixing At machine.
In certain embodiments, the glue system further includes the glue metering system for glue metering, for material metering Material measuring system, for auxiliary agent metering additive metering system and PLC control system.
In certain embodiments, when the detecting device for moisture content detects the aqueous of the material and/or the mixture When rate is less than technological requirement, the PLC control system controls the humidifying device to improve the material and/or the mixture Moisture content.
In certain embodiments, the system also includes glue heating unit.
In certain embodiments, it is 12~14% that the technological requirement, which includes top layer moisture content, sandwich layer moisture content for 7~ 8%.
According to another aspect of the present invention, there is provided a kind of glue applying method for being used to manufacture wood-based plate, including step:There is provided Material, glue;The material, the glue are mixed, forms mixture;Detect material and/or the mixing water content of matter;And work as institute When stating the moisture content of material and/or the mixture and being less than technological requirement, the aqueous of the material and/or the mixture is improved Rate.
In certain embodiments, the method further includes step:The material, the weight of the glue are calculated respectively.
In certain embodiments, the method further includes the step of heating glue.
According to a further aspect of the invention, there is provided a kind of glue applying method for being used to manufacture wood-based plate, including step:There is provided Material, glue, auxiliary agent;The material, the glue, the auxiliary agent are mixed, forms mixture;Detect material and/or the mixture Moisture content, when the moisture content of the material and/or the mixture is less than technological requirement, improves the material and/or described The moisture content of mixture.
In certain embodiments, the method further includes step:The material, the glue, the auxiliary agent are calculated respectively Weight.
In certain embodiments, the method further includes the step of heating glue.
Compared with existing glue system and glue applying method, the present invention has the following advantages:Sizing system according to the present invention System can detect and improve moisture content, avoid moisture content too low, additionally by application auxiliary agent (waterproofing agent, tackifier, mould inhibitor) Product quality can be improved.
Brief description of the drawings
By the description made for the present invention of below with reference to attached drawing, other objects and advantages of the present invention will be aobvious and easy See, and can help that complete understanding of the invention will be obtained.
Fig. 1 is a kind of embodiment schematic diagram for being used to manufacture the glue system of wood-based plate of the present invention.
Fig. 2 is the other embodiment schematic diagram for being used to manufacture the glue system of wood-based plate of the present invention.
Fig. 3 is the other embodiment schematic diagram for being used to manufacture the glue system of wood-based plate of the present invention.
Fig. 4 is the flow diagram for being used to manufacture the glue applying method of wood-based plate of the present invention.
Fig. 5 is the flow diagram for being used to manufacture the other embodiment of the glue applying method of wood-based plate of the present invention.
Fig. 6 is the flow diagram for being used to manufacture the other embodiment of the glue applying method of wood-based plate of the present invention.
Fig. 7 is the flow diagram for being used to manufacture the other embodiment of the glue applying method of wood-based plate of the present invention.
It should be noted that attached drawing is not necessarily to scale to draw, but only not influence the schematic of reader's understanding Mode is shown.
Embodiment
Below in conjunction with the attached drawing in the embodiment of the present invention, the technical solution in the embodiment of the present invention is carried out clear, complete Site preparation describes, it is clear that described embodiment is only part of the embodiment of the present invention, instead of all the embodiments.It is based on Embodiment in the present invention, those of ordinary skill in the art are obtained every other without creative efforts Embodiment, belongs to the scope of protection of the invention.
Specifically, referring to Fig. 1, show a kind of glue system for being used to manufacture wood-based plate according to embodiments of the present invention 1 schematic diagram.In the illustrated embodiment, the glue system 1 can include feedstock supply unit 11 and sizing mixing arrangement 12, the feedstock supply unit 11 can include material supplying device 111 and glue feeding mechanism 112.One according to the present invention Embodiment, the glue system 1 can also include humidification unit 13, glue metering system 15, material measuring system 16 and PLC controls System 18 processed.
Wherein, the material supplying device 111 is used to provide material, the material can be crush dried fiber, Stalk or wood shavings or other be used for manufacture material of wood-based plate etc..
The glue feeding mechanism 112 is used to provide glue, and the glue can be that isocyanate glue (MDI glue), moisture dissipate MDI Glue, bean gum or other be used for manufacture glue of wood-based plate etc..
The sizing mixing arrangement 12 is used to mix material and glue, forms mixture.In one example, the sizing Mixing arrangement 12 can include continuous glue mixer 121 and ring type glue mixer 122.
In one exemplary embodiment, the glue applying method being glued afterwards using first drying, the material crushed are advanced Enter drying system drying, dried material is sent into continuous 121 glue mixing of glue mixer, is then sent through in ring type glue mixer 122 and carries out two Secondary glue mixing, to reach the uniform purpose of glue mixing.First drying the characteristics of being glued afterwards is:Glue mixing is not easy uniformly, easy to knot groups, process equipment It is more complicated, take up a large area, but glue consumption is relatively low.For example, continuous glue mixer 121 can be the continuous glue mixer of atomizing, It includes the components such as roller and atomizer.
In one exemplary embodiment, the humidification unit 13 includes detecting device for moisture content 131 and humidifying device 132.Before the humidification unit can be arranged on sizing, i.e., at material supplying device 111.Detecting device for moisture content 131 can at this time Be moisture content detector or other be used for detect material moisture content devices.When detecting device for moisture content detects material When moisture content is less than technological requirement, such as the technological requirement can be that top layer material water ratio is 12~14%, sandwich layer material Moisture content be 7~8%, by the PLC control system 18 control humidifying device 132 open, to improve material water ratio, make The indexs such as the intensity for the wood-based plate that must be produced meet national standard.
In a preferred embodiment, the glue metering system 15 is used for the weight for calculating glue, and realizes accurate application glue Amount.The material measuring system 16 is used for the weight for calculating material, and realizes the accurate amount for applying material.
In further preferred embodiment, the glue system 1 further includes auxiliary agent feeding mechanism 14 and auxiliary agent metering system System 17.The auxiliary agent feeding mechanism 14 is used to provide auxiliary agent, and the auxiliary agent is included in tackifier, waterproofing agent, mould inhibitor at least It is a kind of.Additive metering system 17 is used for the weight for calculating auxiliary agent, and realizes accurate application auxiliary agent.Application tackifier, which can improve, mats formation Slab turned-down edge phenomenon afterwards, improves effect of mating formation;Finished product plate thickness swelling rate can be reduced by applying waterproofing agent;Apply mould inhibitor The mildew phenomena that finished product plate can be avoided to occur, so as to improve product quality.
In one exemplary embodiment, the auxiliary agent feeding mechanism 14 can be arranged at continuous glue mixer 121 so that Material, glue, auxiliary agent three mixing, form mixture.In other embodiments, the auxiliary agent feeding mechanism 14 can also be arranged on At ring type glue mixer 122 or continuous glue mixer 121 and ring type glue mixer 122.
In further preferred embodiment, the glue system 1 can also include glue heating unit 19 so that glue is even Preferably mixed in continuous glue mixer with material, auxiliary agent.
Refering to Fig. 2, in other embodiments, the humidification unit 13 can be arranged in Process of Applying Glue, that is, is arranged on ring At formula glue mixer 122, detecting device for moisture content 131 is used for detecting the moisture content of mixture at this time, when detecting device for moisture content is examined Measuring the moisture content of mixture, (such as top layer material water ratio is 12~14%, the moisture content of sandwich layer material less than technological requirement For 7~8%) when, control humidifying device 132 to open by the PLC control system 18, to improve mixing water content of matter.
Refering to Fig. 3, in another embodiment, the humidification unit 13 can be arranged at the same time before sizing and Process of Applying Glue In, that is, it is arranged at material supplying device 111 and at ring type glue mixer 122, detecting device for moisture content 131 is used for detectable substance at this time The moisture content of material and mixture, when the material and the moisture content of mixture that detecting device for moisture content 131 detects will less than technique When asking (such as top layer material water ratio is 12~14%, and the moisture content of sandwich layer material is 7~8%), system is controlled by the PLC The control humidifying device 132 of system 18 is opened, to improve the moisture content of material and mixture.Before sizing, work as detecting device for moisture content 131 detect that the moisture content of material is less than technological requirement, control humidifying device 132 to open by the PLC control system 18, come Improve the moisture content of material.In Process of Applying Glue, moisture content detection further can be carried out to mixture, if moisture content detection dress When putting 131 and detecting that the moisture content of mixture is less than technological requirement, then pass through the PLC control system 18 and control humidifying device 132 open, and further improve the moisture content of mixture.Humidification unit 13 can be arranged on before sizing and in Process of Applying Glue at the same time, The further moisture content that ensure that material and mixture can meet technological requirement (such as top layer material water ratio for 12~ 14%, the moisture content of sandwich layer material is 7~8%), so as to optimize glue system.
Refering to Fig. 4, the flow chart for being used to manufacture the glue applying method of wood-based plate according to embodiments of the present invention is shown.Need Illustrate, the glue applying method provided in an embodiment of the present invention for being used to manufacture wood-based plate is not limited in flow chart shown in Fig. 4 Step and order.According to different embodiments, the step in flow chart shown in Fig. 4 can increase, remove or change order. In one exemplary embodiment, the method can be since step S401.
Step S401, material is provided by the material supplying device 111, and glue feeding mechanism 112 provides glue.
Step S402, detects material water ratio, if the moisture content of the material detected is low by detecting device for moisture content 131 In technological requirement, then humidifying device 132 is controlled to improve material water ratio by PLC control system 18.
Step S403, the material for meeting technological requirement is mixed by being glued mixing arrangement 12 with glue, and mixture is made, with Carry out the flow of follow-up manufacture wood-based plate.
In the present embodiment, the step of can also including calculating the weight of material and glue (not shown), with realize material and The accurate application of glue, meets national standard with wood-based plate made from guarantee.In the present embodiment, the step of heating glue can also be included Suddenly so that glue preferably mixes in continuous glue mixer 121 with material.
In another embodiment, refering to Fig. 5, the mixing of material and glue can be first carried out, then pass through detecting device for moisture content The moisture content of 131 detection mixtures, if detecting, the moisture content of mixture is less than technological requirement, passes through PLC control system 18 Humidifying device 132 is controlled to improve the moisture content of mixture.
Refering to Fig. 6, the flow chart according to another embodiment of the present invention for manufacturing the glue applying method of wood-based plate is shown. It should be noted that the glue applying method provided in an embodiment of the present invention for being used to manufacture wood-based plate is not limited to flow chart shown in Fig. 6 In step and order.According to different embodiments, the step in flow chart shown in Fig. 6 can increase, remove or change suitable Sequence.In one exemplary embodiment, the method can be since step S601.
Step S601, provides material, glue feeding mechanism 112 provides glue and auxiliary agent by the material supplying device 111 Feeding mechanism 14 provides auxiliary agent.
Step S602, detects material water ratio, if the moisture content of the material detected is low by detecting device for moisture content 131 In technological requirement, then 132 devices of humidification are controlled to improve material water ratio by PLC control system 18.
Step S603, the material for meeting technological requirement is mixed by being glued mixing arrangement 12 with auxiliary agent, glue, and mixing is made Thing, to carry out the flow of follow-up manufacture wood-based plate.
In the present embodiment, the step (not shown) for calculating the weight of material and glue can also be included, and to realize material Accurate with glue applies, and meets national standard with wood-based plate made from guarantee.In the present embodiment, heating glue can also be included Step so that glue preferably mixes in continuous glue mixer 121 with material.
In another embodiment, refering to Fig. 7, the mixing of material and glue, auxiliary agent can be first carried out, then detect by moisture content Device 131 detects the moisture content of mixture, if detect that the moisture content of mixture is less than technological requirement, is controlled by PLC System 18 controls the moisture content of the raising mixture of humidifying device 132.
In several embodiments provided by the present invention, it should be understood that disclosed relevant apparatus and method, Ke Yitong Other modes are crossed to realize.For example, device embodiment described above is only schematical, for example, described device is drawn Point, it is only a kind of division of logic function, there can be other dividing mode when actually realizing, such as multiple devices can combine Or another system is desirably integrated into, or some features can be ignored, or do not perform.
Finally it should be noted that the above embodiments are merely illustrative of the technical solutions of the present invention and it is unrestricted, although reference The present invention is described in detail in preferred embodiment, it will be understood by those of ordinary skill in the art that, can be to the present invention's Technical solution is modified or equivalent substitution, without departing from the spirit and scope of technical solution of the present invention.

Claims (18)

1. a kind of glue system for being used to manufacture wood-based plate, the glue system includes feedstock supply unit and sizing mixing dress Put, the feedstock supply unit includes being used for the material supplying device for providing material and the glue feeding mechanism for providing glue, institute Sizing mixing arrangement is stated to be used to mix the material and the glue to form mixture, it is characterised in that:The glue system is also Including humidification unit, the humidification unit includes:
Detecting device for moisture content for the moisture content for detecting the material and/or the mixture, and
Humidifying device for the moisture content for improving the material and/or the mixture.
2. glue system as claimed in claim 1, it is characterised in that the feedstock supply unit is further included for providing auxiliary agent Auxiliary agent feeding mechanism, the mixture further includes auxiliary agent.
3. glue system as claimed in claim 2, it is characterised in that the auxiliary agent includes tackifier, waterproofing agent and mould proof At least one of agent.
4. glue system as claimed in claim 1, it is characterised in that the sizing mixing arrangement includes continuous glue mixer and ring Formula glue mixer.
5. glue system as claimed in claim 4, it is characterised in that the auxiliary agent feeding mechanism is arranged on the continuous glue mixing At machine and/or at the ring type glue mixer.
6. glue system as described in claim 4 or 5, it is characterised in that the humidification unit is arranged on the material supply At device and/or at the ring type glue mixer.
7. glue system as claimed in claim 1, it is characterised in that the glue system is further included based on the glue of glue metering Amount system, material measuring system and PLC control system for material metering.
8. glue system as claimed in claim 7, it is characterised in that when the detecting device for moisture content detects the material And/or the moisture content of the mixture is when being less than technological requirement, the PLC control system is controlled described in the humidifying device improves The moisture content of material and/or the mixture.
9. glue system as claimed in claim 1, it is characterised in that the glue system further includes glue heating unit.
10. glue system as claimed in claim 8, it is characterised in that the technological requirement include top layer moisture content for 12~ 14%, sandwich layer moisture content is 7~8%.
11. a kind of glue applying method for being used to manufacture wood-based plate, comprises the following steps:
Material and glue are provided;
The material and the glue are mixed, forms mixture;
Detect material and/or the mixing water content of matter;And
When the moisture content of the material and/or the mixture is less than technological requirement, the material and/or the mixing are improved The moisture content of thing.
12. glue applying method as claimed in claim 11, it is characterised in that the glue applying method further includes step:Calculate respectively The weight of the material, the glue.
13. glue applying method as claimed in claim 11, it is characterised in that the glue applying method further includes step:Heat glue.
14. glue applying method as claimed in claim 11, it is characterised in that the technological requirement include top layer moisture content for 12~ 14%, sandwich layer moisture content is 7~8%.
15. a kind of glue applying method for being used to manufacture wood-based plate, including step:
Material, glue and auxiliary agent are provided;
The material, the glue and the auxiliary agent are mixed, forms mixture;
Detect material and/or the mixing water content of matter;And
When the moisture content of the material and/or the mixture is less than technological requirement, the material and/or the mixing are improved The moisture content of thing.
16. glue applying method as claimed in claim 15, it is characterised in that the glue applying method further includes step:Calculate respectively The material, the glue, the weight of the auxiliary agent.
17. glue applying method as claimed in claim 15, it is characterised in that the glue applying method further includes step:Heat glue.
18. glue applying method as claimed in claim 15, it is characterised in that the technological requirement include top layer moisture content for 12~ 14%, sandwich layer moisture content is 7~8%.
CN201711415264.3A 2017-12-22 2017-12-22 For manufacturing the glue system and glue applying method of wood-based plate Pending CN108000670A (en)