CN107939383B - A method of expanding narrow ' Safe Density Windows - Google Patents

A method of expanding narrow ' Safe Density Windows Download PDF

Info

Publication number
CN107939383B
CN107939383B CN201711124146.7A CN201711124146A CN107939383B CN 107939383 B CN107939383 B CN 107939383B CN 201711124146 A CN201711124146 A CN 201711124146A CN 107939383 B CN107939383 B CN 107939383B
Authority
CN
China
Prior art keywords
weight
dosage
parts
mixture
method described
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201711124146.7A
Other languages
Chinese (zh)
Other versions
CN107939383A (en
Inventor
罗平亚
梁大川
王平全
邓明毅
黄进军
白杨
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Southwest Petroleum University
Original Assignee
Southwest Petroleum University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Southwest Petroleum University filed Critical Southwest Petroleum University
Priority to CN201711124146.7A priority Critical patent/CN107939383B/en
Priority to PCT/CN2017/112625 priority patent/WO2019095420A1/en
Publication of CN107939383A publication Critical patent/CN107939383A/en
Application granted granted Critical
Publication of CN107939383B publication Critical patent/CN107939383B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention relates to oil/gas well reagent fields, disclose a kind of method expanding narrow ' Safe Density Windows, wherein this approach includes the following steps:(1) it is injected in shale formation after aggravating drilling fluid and surveys it and miss situation;(2) mixture of step (1) is mixed with bridging materials, stirred and surveyed it and miss situation;(3) mixture of step (2) is mixed with quartz sand, stirred and surveyed it and miss situation;(4) mixture of step (3) is mixed with swollen material, stirred and surveyed it and miss situation;(5) mixture of step (4) mixed with packing material, stirred.This method can simplify live complex operations, and effect is fast illustrated, while substep real-time testing misses situation, in light of the circumstances specific processing, realize pressure-bearing and block the controllableization operation for expanding narrow ' Safe Density Windows.

Description

A method of expanding narrow ' Safe Density Windows
Technical field
The present invention relates to oil/gas well reagent fields, and in particular to a method of expanding narrow ' Safe Density Windows.
Background technology
The drilling liquid technology of narrow mud ' Safe Density Windows (including window width is zero or is negative) safety drilling is to ensure High pressure, high yield, high sour gas well prevent blowout out of control, the necessary technology of safety drilling.It is also current drilling engineering circle both at home and abroad Common concern is badly in need of solving and fails the significant technology issues being fully solved.It is one System engineering, this special topic pertain only to ensure the drilling liquid technology of safety itself.It is narrow mud ' Safe Density Windows safety drilling skill The important foundation of art and necessary component part, especially project propose to expand the theory of ' Safe Density Windows and corresponding reality Existing technology is even more to provide important technical support to solving the significant technology issues that this seriously affects drilling safety.
According to it research and field engineering practice analysis, such issues that can be divided into three kinds of situations:
Δ P 1. (narrow) > 0, and numerical value is smaller (narrow):At this point, the approach solved is to try to reduce the annular space pressure of mud cycle Drop, is less than Δ P (narrow);This is to reduce the series matching technology that mud Cyclic Rings pneumatics is reduced to core, is in recent years The series technique tackled problems and be attended by the most momentous results always;That is Δ P (narrow) > 0 and Mud Technology can make Δ P (mud follows) < Δ P (narrow).
Δ P 2. (narrow) > 0, but it is too small, so that being always less than Δ P (mud follows) (i.e. since Δ P (mud follows) cannot be unlimited It makes small, then Δ P (mud follows) > Δs P (narrow) > 0 occurs).
This is the significant technology issues currently encountered, it is most common when boring chance high pressure, high yield, low pressure-bearing gas-bearing formation.At For the advanced subject of existing domestic and international emphasis tackling key problem.It has formed specific technology path:I.e. " to drop low delta p (mud to greatest extent Follow) based on controlled pressure drilling technology ".Currently, all also organizing great tackling key problem both at home and abroad.
The problem of Δ P 3. (narrow) < 0, i.e. negative ' Safe Density Windows:
This is the problem when brill chance " spray, leakage same layer ", " same deposit is leaked in spray " and leakage pressure are less than strata pressure.
This problem is met when boring, drilling engineering can not be successfully progress, often:It wants well not leak, blowout will necessarily be caused, And it can not kill-job control if blowout;Otherwise spray will necessarily then leak, and a leakage will necessarily induce blowout again, can not if blowout Kill-job controls, to cause great engineering accident, and when payzone is oily, gas will likely cause great public safety accident. Especially when payzone is three HI ALT High Altitude, by the great danger source as critical public safety.
The reliable approach for solving the problems, such as this is effectively blocking and the leakage pressure of its drop ply is made to be increased to greatly to drop ply In strata pressure, even if its ' Safe Density Windows is just, and it is more than the well mud annular circulation pressure drop.
The case where leakage, is sufficiently complex, and existing technical merit can block most of leakages, and most difficult is tight Weight situation may also pass through plugging operations repeatedly, finally always can effectively block it, but extremely for the severe mud losses of large fracture The present has no effective method.
Moreover, ' Safe Density Windows are expanded to positive value by leak stopping under negative ' Safe Density Windows and are more than Δ P (mud follows), Leak stopping with ordinary circumstance is very different and higher requirement.It is required in the process that well control pushes down gas-bearing formation or kill-job is speedily carried out rescue work In fast and effectively block drop ply, otherwise safety accident and engineering accident can not avoid.
It does not reach a standard completely the situation substantially unqualified with the leakage stopping technology of fractured reservoir severe mud losses in leakage stopping technology Under, it effectively solve the problems, such as that this is one of current maximum technological difficulties and the brill maximum risk of three HI ALT High Altitudes.
Invention content
The purpose of the invention is to overcome the above problem of the existing technology, a kind of narrow Safe Density window of expansion is provided The method of mouth, this method can simplify live complex operations, and effect is fast illustrated, while substep real-time testing misses situation, Specific processing in light of the circumstances realizes pressure-bearing and blocks the controllableization operation for expanding narrow ' Safe Density Windows.
To achieve the goals above, the present invention provides a kind of methods expanding narrow ' Safe Density Windows, wherein this method Include the following steps:
(1) it is injected in shale formation after aggravating drilling fluid and surveys it and miss situation;
(2) mixture that 20-100mL steps (1) are invaded in 28-32min, in the condition that depth of invasion is 0.5-1cm Under, the mixture of step (1) is mixed with bridging materials, stirred and surveyed it and misses situation;
(3) mixture that 20-100mL steps (2) are invaded in 28-32min, in the condition that depth of invasion is 0.5-1cm Under, the mixture of step (2) is mixed with quartz sand, stirred and surveyed it and misses situation;
(4) mixture that 20-100mL steps (3) are invaded in 28-32min, in the condition that depth of invasion is 0.5-1cm Under, the mixture of step (3) is mixed with swollen material, stirred and surveyed it and misses situation;
(5) mixture that 20-100mL steps (4) are invaded in 28-32min, in the condition that depth of invasion is 0.5-1cm Under, the mixture of step (4) is mixed with packing material, is stirred.
Preferably, on the basis of the drilling fluid of 100 parts by weight, the dosage of the bridging materials is 0.5-5 parts by weight, The dosage of the quartz sand is 4-19 parts by weight, and the dosage of the swellable material is 1-7 parts by weight, the use of the packing material Amount is 0.5-5 parts by weight.
Preferably, on the basis of the drilling fluid of 100 parts by weight, the dosage of the bridging materials is 1-4 parts by weight, institute The dosage for stating quartz sand is 8-16 parts by weight, and the dosage of the swellable material is 2-6 parts by weight, the dosage of the packing material For 1-4 parts by weight;
Preferably, on the basis of the drilling fluid of 100 parts by weight, the dosage of the bridging materials is 1.5-3 parts by weight, The dosage of the quartz sand is 10-12 parts by weight, and the dosage of the swellable material is 3-4 parts by weight, the packing material Dosage is 1.5-3 parts by weight.
Preferably, the bridging materials are one or more in Paris white A, Paris white B and rigid sealing agent;
Preferably, the bridging materials are the mixture of Paris white A, Paris white B and rigid sealing agent, and the carbon The weight ratio of the dosage of sour calcium powder A, Paris white B and rigid sealing agent is (0.5-0.7):(0.1-0.3):1;
It is highly preferred that the grain size of the Paris white A is 0.300-0.450mm;The grain size of the calcium carbonate B is 0.150- 0.200mm。
Preferably, the rigid sealing agent is the mixture of walnut shell and shell, and the dosage of the walnut shell and shell Weight ratio be 1:(0.4-0.6);
Preferably, the grain size of the rigid sealing agent is 0.5-1mm.
Preferably, the quartz sand is silica dioxide granule;
Preferably, the quartz sand particle size is 0.425-0.850mm.
Preferably, the swellable material is one or more in nanmu silver powder, cotton peach and resin, and the resin is Polyethylene and/or polyvinyl chloride;
Preferably, the grain size of the nanmu silver powder is 0.15-0.26mm, and the grain size of the cotton peach is 0.2-0.29mm, The grain diameter of the resin is 0.09-0.15mm.
Preferably, the packing material is composite material of plant fiber;
Preferably, the composite material of plant fiber is wood fiber and/or wheat straw fiber;
It is highly preferred that the grain size of the packing material is 0.02-0.3mm.
Preferably, this method further includes by the mixture of step (5) and macromolecular inhibitor mixed, stirring and surveying its leakage Situation;
Preferably, the macromolecular inhibitor is potassium ammonium hydrolyzed polyacrylonitrile and/or sulfonation nitro khm;
It is further preferred that the macromolecular inhibitor is potassium ammonium hydrolyzed polyacrylonitrile and sulfonation nitro khm Mixture, and the weight ratio of the dosage of the potassium ammonium hydrolyzed polyacrylonitrile and the sulfonation nitro khm is (0.38- 0.61):1;
It is highly preferred that on the basis of the drilling fluid of 100 parts by weight, the dosage of the macromolecular inhibitor is 2-6 weights Measure part;
It is further preferred that the dosage of the macromolecular inhibitor is 3-5 parts by weight.
Preferably, the stirring condition includes:Stir speed (S.S.) is 7000-10000 revs/min, preferably 8000-9000 Rev/min.
Through the above technical solutions, the beneficial effects of the present invention are:This method can simplify live complex operations, effect Fruit is fast illustrated, while substep real-time testing misses situation, in light of the circumstances specific processing, realizes pressure-bearing and blocks i.e. expansion Controllableization of narrow ' Safe Density Windows operates.
Description of the drawings
Fig. 1 is the flow diagram of the method for the narrow ' Safe Density Windows of expansion of the present invention;
Fig. 2 is the schematic diagram of the device of the leakage method of present invention test drilling fluid.
Specific implementation mode
The endpoint of disclosed range and any value are not limited to the accurate range or value herein, these ranges or Value should be understood as comprising the value close to these ranges or value.For numberical range, between the endpoint value of each range, respectively It can be combined with each other between the endpoint value of a range and individual point value, and individually between point value and obtain one or more New numberical range, these numberical ranges should be considered as specific open herein.
The present invention provides a kind of methods expanding narrow ' Safe Density Windows, wherein this approach includes the following steps:
(1) it is injected in shale formation after aggravating drilling fluid and surveys it and miss situation;
(2) mixture that 20-100mL steps (1) are invaded in 28-32min, in the condition that depth of invasion is 0.5-1cm Under, the mixture of step (1) is mixed with bridging materials, stirred and surveyed it and misses situation;
(3) mixture that 20-100mL steps (2) are invaded in 28-32min, in the condition that depth of invasion is 0.5-1cm Under, the mixture of step (2) is mixed with quartz sand, stirred and surveyed it and misses situation;
(4) mixture that 20-100mL steps (3) are invaded in 28-32min, in the condition that depth of invasion is 0.5-1cm Under, the mixture of step (3) is mixed with swollen material, stirred and surveyed it and misses situation;
(5) mixture that 20-100mL steps (4) are invaded in 28-32min, in the condition that depth of invasion is 0.5-1cm Under, the mixture of step (4) is mixed with packing material, is stirred.
According to the method for the present invention, on the basis of the drilling fluid of 100 parts by weight, the dosages of the bridging materials can be with Dosage for 0.5-5 parts by weight, the quartz sand can be 4-19 parts by weight, and the dosage of the swellable material can be 1-7 The dosage of parts by weight, the packing material can be 0.5-5 parts by weight.In the present invention, this method can be according to live complicated The case where, according to the leakage situation of test, as long as bridging materials, quartz sand, swellable material and packing material meet above-mentioned ratio Example relationship can achieve the object of the present invention to a certain extent.
The present inventor has found under study for action, although as long as bridging materials, quartz sand, swellable material and filling material Material, which meets aforementioned proportion relationship, to be achieved the object of the present invention to a certain extent, but under preferable case, with 100 parts by weight On the basis of the drilling fluid, the dosage of the bridging materials is 1-4 parts by weight, and the dosage of the quartz sand is 8-16 parts by weight, The dosage of the swellable material is 2-6 parts by weight, and when the dosage of the packing material is 1-4 parts by weight, effect is more preferable;With On the basis of the drilling fluid of 100 parts by weight, the dosage of the bridging materials is 1.5-3 parts by weight, the dosage of the quartz sand Dosage for 10-12 parts by weight, the swellable material is 3-4 parts by weight, and the dosage of the packing material is 1.5-3 parts by weight When, effect is more preferable.
According to the method for the present invention, in step (1), the drilling fluid is not particularly limited, for example, can be arbitrarily to take The drilling fluid for shale formation from scene, the ingredient of the drilling fluid may include bentonite, water, calcium carbonate, extracting and cutting agent, drop It is one or more in fluid loss agents, inhibitor, lubricant and heavy weight additive.
According to the method for the present invention, in step (1), the method that drilling fluid aggravates is not particularly limited, for example, can be with Quantitative drilling fluid is added to required proportion, referred to as quantitatively drilling fluid aggravates, wherein needed for the exacerbation of quantitative drilling fluid The quality W of weighting material can be obtained according to following formula:
W=V starches * ρ3*(ρ21)/(ρ32);
V slurries-magma volume,
ρ1Magma density;
ρ2(it is ρ that drilling fluid is weighed out to density to drilling fluid density to be matched2);
ρ3Weighting material density.
Wherein, weighting material is not particularly limited, as long as the density of the weighting material meets above-mentioned requirements.
In addition, in the present invention, it is ρ that drilling fluid, which is weighed out to density,2, that is to say, that drilling fluid density ρ to be matched2Can be 1.6-2.2g/cm3, preferably 1.8-2.0g/cm3
According to the method for the present invention, the bridging materials can be in Paris white A, Paris white B and rigid sealing agent It is one or more;
Preferably, the bridging materials are the mixture of Paris white A, Paris white B and rigid sealing agent, and the carbon The weight ratio of the dosage of sour calcium powder A, Paris white B and rigid sealing agent can be (0.5-0.7):(0.1-0.3):1;More preferably The weight ratio of the dosage of ground, the Paris white A, Paris white B and rigid sealing agent is (0.55-0.65):(0.15- 0.25):1.
In the method for the invention, the grain size of the Paris white A can be 0.300-0.450mm;The calcium carbonate B's Grain size can be 0.150-0.200mm;Preferably, the grain size of the Paris white A is 0.34-0.4mm;The calcium carbonate B's Grain size is 0.16-0.18mm.
In the method for the invention, the rigid sealing agent can be the mixture of walnut shell and shell, and the walnut The weight ratio of the dosage of shell and shell can be 1:(0.4-0.6);Preferably, the weight ratio of the dosage of the walnut shell and shell It is 1:(0.45-0.55).
In the method for the invention, the grain size of the rigid sealing agent can be 0.5-1mm, it is preferable that the rigidity envelope The grain size of blocking agent can be 0.6-0.8mm.
In the method for the invention, the component of the bridging structure, that is, Paris white A, Paris white B and rigid sealing agent, Dosage and grain size are limited to above range, can form the small hole of reticular structure, have efficient, quick blocking performance, and And pressure-bearing can be realized and block the controllableization operation for expanding narrow ' Safe Density Windows.
According to the method for the present invention, the quartz sand can be silica dioxide granule;Preferably, the quartz sand particle size can Think 0.425-0.850mm;It is highly preferred that the quartz sand particle size is 0.5-0.7mm.
In the method for the invention, quartz sand is the broken quartz particles being process of quartz warp, and quartz sand is a kind of Hard, wear-resisting, stable chemical performance silicate mineral, main mineral constituent are SiO2, the color of quartz sand is milky Or semi-transparent clear shape, hardness 7 utilize the very strong acid-resisting medium etch ability of quartz under construction, it is acidproof mixed for producing Solidifying soil and acid resisting mortar, have preferable plugging effect, are good plugging materials.
In the method for the invention, the grain size of the quartz sand is limited to above range, can fill in bridging structure Small hole forms one layer of fine and close leak stopping thin layer, has efficient, quick blocking performance, and can realize pressure-bearing closure Expand the controllableization operation of narrow ' Safe Density Windows.
According to the method for the present invention, the swellable material can be nanmu silver powder, cotton peach and one kind in resin or A variety of, the resin can be polyethylene and/or polyvinyl chloride;Preferably, the grain size of the nanmu silver powder can be 0.15- The grain size of 0.26mm, the cotton peach can be 0.2-0.29mm, and the grain diameter of the resin can be 0.09-0.15mm.
In the method for the invention, the component of the swollen material and grain size are limited to above range, can be preferably molten It is swollen, and then the small hole that bridging structure is formed with quartz sand can be filled, there is efficient, quick blocking performance, and can It realizes pressure-bearing and blocks the controllableization operation for expanding narrow ' Safe Density Windows.
According to the method for the present invention, the packing material can be composite material of plant fiber;Preferably, the plant is fine It can be wood fiber and/or wheat straw fiber to tie up composite material;It is highly preferred that the grain size of the packing material can be 0.02- 0.3mm。
In the method for the invention, the component of the packing material and grain size are limited to above range, can further capture Bridge formation particle, quartz sand and the swellable material obtained in suspension forms rock-steady structure, is then mutually wound in leakage channel Netted bridging structure is formed, and certain pressure can be born, there is efficient, quick blocking performance, and can realize and hold The stifled controllableization operation for expanding narrow ' Safe Density Windows of press seal.
According to the method for the present invention, this method further includes by the mixture of step (5) and macromolecular inhibitor mixed, stirring And it surveys it and misses situation;
Preferably, the macromolecular inhibitor is potassium ammonium hydrolyzed polyacrylonitrile and/or sulfonation nitro khm;
It is further preferred that the macromolecular inhibitor is potassium ammonium hydrolyzed polyacrylonitrile and sulfonation nitro khm Mixture, and the weight ratio of the dosage of the potassium ammonium hydrolyzed polyacrylonitrile and the sulfonation nitro khm can be (0.38-0.61):1;
It is highly preferred that on the basis of the drilling fluid of 100 parts by weight, the dosage of the macromolecular inhibitor can be 2- 6 parts by weight;
It is further preferred that the dosage of the macromolecular inhibitor is 3-5 parts by weight.
In the method for the invention, the macromolecular inhibitor can effectively prevent formation rock aquation from causing crack into one The characteristics of step development, there is more excellent plugging effect, and pressure-bearing closure can be realized and expand narrow ' Safe Density Windows Controllableization operation.
According to the method for the present invention, the stirring condition may include:Stir speed (S.S.) can be 7000-10000 revs/min Clock, preferably 8000-9000 revs/min;Wherein, the equipment of stirring is not particularly limited, and can be the conventional selection of this field.
According to the method for the present invention, the schematic diagram that the device of the leakage method of drilling fluid is tested with reference to such as Fig. 2 present invention, is surveyed The leakage method of test drilling well liquid is:Site operation situation is simulated, the shale for being derived from situ of drilling well stratum is polished into a diameter of 66 The cylinder that mm length is 10 millimeters, is then embedded under a diameter of 66 millimeters of conventional high temperature high pressure filtration device autoclave body 100ml drilling fluids from autoclave body top pour into after sealing lower cover in portion, and screwing upper cover makes entire autoclave body be in sealing state, from upper kettle It is passed through 3.5MPa pressure nitrogen gas at body air valve and continues 30 minutes, observes and records lower filtrate port leakage situation and intrusion shale drilling well The volume of liquid, then open upper cover after pressure release and sequentially add bridging materials, quartz, swollen material, packing material, often add a kind of component When be sufficiently stirred after repeat aforesaid operations step, observe and record the leakage situation of each step and invade the body of shale drilling fluid Product.
The beneficial effects of the present invention are:This method can simplify live complex operations, and effect is fast illustrated, the same to time-division It walks real-time testing and misses situation, in light of the circumstances specific processing, realize pressure-bearing closure and expand narrow ' Safe Density Windows Controllableization operates.
The present invention will be described in detail by way of examples below.
Drilling fluid is the drilling fluid for shale formation for being arbitrarily derived from scene.
Quartz sand is purchased from Jiangsu Zhong Sheng silicon materials Science and Technology Ltd., main component SiO2
Fibrous material is purchased from Shandong gold Nore building materials Science and Technology Ltd., model PPF.
Potassium ammonium hydrolyzed polyacrylonitrile and sulfonation nitro khm are purchased from Renqiu City Peng Yu Chemical Co., Ltd.s, model KNPAN and SNK-2.
Calcium carbonate A and calcium carbonate B is purchased from Guizhou millimicro powder industry Co., Ltd, main component CaCO3
Embodiment 1
The present embodiment indicates that method using the present invention expands narrow ' Safe Density Windows, and with reference to 1 present invention of figure The flow diagrams of method of the narrow ' Safe Density Windows of expansion carry out:
(1) drilling fluid is weighed out to ρ2For 1.9g/cm3, observe and record it and miss situation;
(2) mixture of 80mL (1) is invaded in 30min, depth of invasion 0.8cm is 8500 revs/min in stir speed (S.S.) Under conditions of clock, by calcium carbonate A that 0.7 parts by weight grain size is 0.4mm, 0.3 parts by weight grain size be 0.18mm calcium carbonate B, 1 weight The rigid sealing agent that amount part grain size is 0.7mm is added in the mixture of step (1), observes and records it and misses situation;
(3) mixture of 60mL (2) is invaded in 30min, depth of invasion 0.7cm is 8500 revs/min in stir speed (S.S.) Under conditions of clock, the quartz sand that 11 parts by weight grain sizes are 0.6mm is added in the mixture of step (2), it is observed and recorded Miss situation;
(4) mixture of 40mL (3) is invaded in 30min, depth of invasion 0.6cm is 8500 revs/min in stir speed (S.S.) Under conditions of clock, the cotton peach and 1.3 for being 0.25mm by nanmu silver powder that 1.2 parts by weight grain sizes are 0.2mm, 1 parts by weight grain size Parts by weight grain size is that the Corvic of 0.12mm is added in the mixture of step (3), observes and records it and misses situation;
(5) mixture of 30mL (4) is invaded in 30min, depth of invasion 0.6cm is 8500 revs/min in stir speed (S.S.) Under conditions of clock, the composite material of plant fiber that 3 parts by weight grain sizes are 0.13mm is added in the mixture of step (4).
As a result the leakage situation measured is as shown in table 1, is labeled as S1.
Embodiment 2
Expand narrow ' Safe Density Windows in the same manner as shown in Example 1, the difference is that being 8500 in stir speed (S.S.) Under conditions of rev/min, 2 parts by weight potassium ammonium hydrolyzed polyacrylonitriles and 4 parts by weight sulfonation nitro khms are added to step Suddenly in the mixture of (5).
As a result the leakage situation measured is as shown in table 1, is labeled as S2.
Embodiment 3
Expand narrow ' Safe Density Windows according to method same as Example 2, the difference is that Paris white A, calcium carbonate Powder B, rigid sealing agent, quartz sand, packing material, nanmu silver powder, cotton peach are different with the grain size of resin, specifically:
The grain size of Paris white A is 0.3mm, and the grain size of Paris white B is 0.15mm, and the grain size of rigid sealing agent is The grain size of 0.52mm, quartz sand are 0.43mm, and the grain size of packing material is 0.02mm, and the grain size of nanmu silver powder is 0.15mm, cotton The grain size of Hua Tao is 0.2mm and the grain size of the grain size of resin is 0.09mm.
As a result the leakage situation measured is as shown in table 1, is labeled as S3.
Embodiment 4
Expand narrow ' Safe Density Windows according to method same as Example 2, the difference is that Paris white A, calcium carbonate Powder B is different with the rigid weight ratio of dosage of sealing agent, specifically:
The weight ratio of the dosage of Paris white A, Paris white B and rigid sealing agent is 0.5:0.1:1.
As a result the leakage situation measured is as shown in table 1, is labeled as S4.
Embodiment 5
Expand narrow ' Safe Density Windows according to method same as Example 2, the difference is that potassium ammonium hydrolysis is poly- Acrylonitrile is different with the dosage of the sulfonation nitro khm, specifically:
The weight ratio of the dosage of the potassium ammonium hydrolyzed polyacrylonitrile and the sulfonation nitro khm is 0.4:1.
As a result the leakage situation measured is as shown in table 1, is labeled as S5.
Embodiment 6
The present embodiment indicates that method using the present invention expands narrow ' Safe Density Windows, and with reference to 1 present invention of figure The flow diagrams of method of the narrow ' Safe Density Windows of expansion carry out:
(1) drilling fluid is weighed out to ρ2For 1.9g/cm3, observe and record it and miss situation;
(2) mixture of 90mL (1) is invaded in 30min, depth of invasion 0.9cm is 8500 revs/min in stir speed (S.S.) Under conditions of clock, by calcium carbonate A that 0.7 parts by weight grain size is 0.4mm, 0.3 parts by weight grain size be 0.18mm calcium carbonate B, 1 weight The rigid sealing agent that amount part grain size is 0.7mm is added in the mixture of step (1), observes and records it and misses situation;
(3) mixture of 70mL (2) is invaded in 30min, depth of invasion 0.8cm is 8500 revs/min in stir speed (S.S.) Under conditions of clock, the quartz sand that 11 parts by weight grain sizes are 0.6mm is added in the mixture of step (2), it is observed and recorded Miss situation;
(4) mixture of 50mL steps (3) is invaded in 30min, depth of invasion 0.7cm is 8500 in stir speed (S.S.) Under conditions of rev/min, the cotton peach for being 0.25mm by nanmu silver powder that 1.2 parts by weight grain sizes are 0.2mm, 1 parts by weight grain size It is added in the mixture of step (3) for the Corvic of 0.12mm with 1.3 parts by weight grain sizes, observes and records its leakage Situation;
(5) mixture of 35mL steps (4) is invaded in 30min, depth of invasion 0.65cm is 8500 in stir speed (S.S.) Under conditions of rev/min, the composite material of plant fiber that 3 parts by weight grain sizes are 0.13mm is added to the mixture of step (4) In, it observes and records it and misses situation;
(6) mixture of 30mL steps (5) is invaded in 30min, depth of invasion 0.6cm is 8500 in stir speed (S.S.) Under conditions of rev/min, 2 parts by weight potassium ammonium hydrolyzed polyacrylonitriles and 4 parts by weight sulfonation nitro khms are added to step Suddenly in the mixture of (5).
As a result the leakage situation measured is as shown in table 1, is labeled as S6.
Comparative example 1
Expand narrow ' Safe Density Windows according to method same as Example 2, the difference is that packing material dosage subtracts It is few, that is, 0.5 parts by weight composite material of plant fiber.
As a result the leakage situation measured is as shown in table 1, is labeled as D1.
Comparative example 2
Expand narrow ' Safe Density Windows according to method same as Example 2, the difference is that bridging materials dosage subtracts It is few, that is, 0.3 weight parts of calcium carbonate B, 0.5 parts by weight rigidity sealing agent.
As a result the leakage situation measured is as shown in table 1, is labeled as D2.
Comparative example 3
Expand narrow ' Safe Density Windows according to method same as Example 2, the difference is that swollen material dosage subtracts It is few, that is, 1 parts by weight swellable material.
As a result the leakage situation measured is as shown in table 1, is labeled as D3.
Comparative example 4
Expand narrow ' Safe Density Windows according to method same as Example 2, the difference is that Paris white A, calcium carbonate Powder B, rigid sealing agent, quartz sand, packing material, nanmu silver powder, cotton peach and resin grain size do not limited of the invention Within the scope of, specifically:
The grain size of Paris white A is 0.65mm, and the grain size of Paris white B is 0.3mm, and the grain size of rigid sealing agent is The grain size of 1.2mm, quartz sand are 0.8mm, and the grain size of packing material is 0.5mm, and the grain size of nanmu silver powder is 0.3mm, cotton peach Grain size be 0.35mm and the grain size of resin is 0.25mm.
As a result the leakage situation measured is as shown in table 1, is labeled as D4.
Comparative example 5
Expand narrow ' Safe Density Windows according to method same as Example 2, the difference is that Paris white A, calcium carbonate The weight ratio of the dosage of powder B and rigid sealing agent is not within limited range of the present invention, specifically:
The weight ratio of the dosage of Paris white A, Paris white B and rigid sealing agent is 0.1:0.8:1.
As a result the leakage situation measured is as shown in table 1, is labeled as D5.
Comparative example 6
Expand narrow ' Safe Density Windows according to method same as Example 2, the difference is that potassium ammonium hydrolysis is poly- The dosage of acrylonitrile and the sulfonation nitro khm is not within limited range of the present invention, specifically:
The weight ratio of the dosage of the potassium ammonium hydrolyzed polyacrylonitrile and the sulfonation nitro khm is 0.1:1.
As a result the leakage situation measured is as shown in table 1, is labeled as D6.
Table 1
It can be seen that using the method for the present invention by above-described embodiment, comparative example and 1 data of table, directly by situ of drilling well Cylinder is made as experiment condition in the shale on stratum, more close to field condition, live complex operations is simplified, effect is quick It is illustrated, while substep real-time testing misses situation, in light of the circumstances specific processing, specifically, such as 1 data of table, side of the present invention Test is divided into drilling fluid, addition bridging materials, quartz, addition swollen material, addition packing material, addition macromolecular is added by method Six stage of inhibitor carries out;Data horizontal analysis can be achieved the purpose that into substep real-time testing, specifically fixed depending on leakage situation Component grain size and dosage needed for one step, specifically, embodiment 2 and embodiment 1 it is different be only macromolecular inhibitor addition, As can be seen from the data, the drilling fluid experiment slurry intrusion page after sequentially adding bridging materials, quartz, swollen material and packing material Rock depth is only 1.5 millimeters, and intrusion volume is only 7 milliliters, and performance is very excellent, its property after macromolecular inhibitor is added Can further be optimized, according to the method for the present invention, choose whether to be added macromolecular inhibitor can according to site operation cost and From the aspect of specific requirement performance indicator two, embodiment 1-6 be each component grain size or dosage limited range of the present invention it Interior variation, comparative example 1-6 changes each component grain size or dosage and not within limited range of the present invention, according to this hair Bright method tests the data obtained, and the property of drilling fluid of comparative example 1-6 cannot reach pressure-bearing and block requirement, be obtained most through successive optimization Excellent scheme is embodiment 2;Data horizontal analysis can be made to the specific place of next step according to the specific steps institute problem Reason scheme realizes pressure-bearing and blocks the controllableization operation for expanding narrow ' Safe Density Windows, data vertical analysis can be compared Optimized particle size, ratio and the dosage of component (bridging materials, quartz, swollen material, packing material, macromolecular inhibitor), make The shut-off capacity for obtaining drilling fluid is optimal, and thus illustrates the method for the present invention, can simplify live complex operations, effect is quick It is illustrated, while substep real-time testing misses situation, in light of the circumstances specific processing, realizes pressure-bearing closure and expand narrow safety Controllableization of Density Window operates.
The preferred embodiment of the present invention has been described above in detail, and still, the present invention is not limited thereto.In the skill of the present invention In art conception range, technical scheme of the present invention can be carried out a variety of simple variants, including each technical characteristic with it is any its Its suitable method is combined, and it should also be regarded as the disclosure of the present invention for these simple variants and combination, belongs to Protection scope of the present invention.

Claims (23)

1. a kind of method expanding narrow ' Safe Density Windows, which is characterized in that this approach includes the following steps:
(1) it is injected in shale formation after aggravating drilling fluid and surveys it and miss situation;
(2) mixture that 20-100mL steps (1) are invaded in 28-32min will under conditions of depth of invasion is 0.5-1cm The mixture of step (1), which is mixed with bridging materials, stirred and surveys it, misses situation;
(3) mixture that 20-100mL steps (2) are invaded in 28-32min will under conditions of depth of invasion is 0.5-1cm The mixture of step (2), which is mixed with quartz sand, stirred and surveys it, misses situation;
(4) mixture that 20-100mL steps (3) are invaded in 28-32min will under conditions of depth of invasion is 0.5-1cm The mixture of step (3), which is mixed with swollen material, stirred and surveys it, misses situation;
(5) mixture that 20-100mL steps (4) are invaded in 28-32min will under conditions of depth of invasion is 0.5-1cm The mixture of step (4) is mixed with packing material, is stirred.
2. according to the method described in claim 1, wherein, on the basis of the drilling fluid of 100 parts by weight, the bridging materials Dosage be 0.5-5 parts by weight, the dosage of the quartz sand is 4-19 parts by weight, and the dosage of the swellable material is that 1-7 is weighed Part is measured, the dosage of the packing material is 0.5-5 parts by weight.
3. according to the method described in claim 2, wherein, on the basis of the drilling fluid of 100 parts by weight, the bridging materials Dosage be 1-4 parts by weight, the dosage of the quartz sand is 8-16 parts by weight, and the dosage of the swellable material is 2-6 weight Part, the dosage of the packing material is 1-4 parts by weight.
4. according to the method described in claim 3, wherein, on the basis of the drilling fluid of 100 parts by weight, the bridging materials Dosage be 1.5-3 parts by weight, the dosage of the quartz sand is 10-12 parts by weight, and the dosage of the swellable material is that 3-4 is weighed Part is measured, the dosage of the packing material is 1.5-3 parts by weight.
5. according to the method described in any one of claim 1-4, wherein the bridging materials are Paris white A, calcium carbonate It is one or more in powder B and rigid sealing agent.
6. according to the method described in claim 5, wherein, the bridging materials are Paris white A, Paris white B and rigidity envelope The mixture of blocking agent, and the weight ratio of the dosage of the Paris white A, Paris white B and rigid sealing agent is (0.5-0.7): (0.1-0.3):1.
7. according to the method described in claim 6, wherein, the grain size of the Paris white A is 0.300-0.450mm;The carbon The grain size of sour calcium B is 0.150-0.200mm.
8. according to the method described in claim 6, wherein, the rigidity sealing agent is the mixture of walnut shell and shell, and institute The weight ratio for stating the dosage of walnut shell and shell is 1:(0.4-0.6).
9. according to the method described in claim 8, wherein, the grain size of the rigidity sealing agent is 0.5-1mm.
10. according to the method described in any one of claim 1-4, wherein the quartz sand is silica dioxide granule.
11. according to the method described in claim 10, wherein, the quartz sand particle size is 0.425-0.850mm.
12. according to the method described in any one of claim 1-4, wherein the swellable material is nanmu silver powder, cotton One or more in peach and resin, the resin is polyethylene and/or polyvinyl chloride.
13. according to the method for claim 12, wherein the grain size of the nanmu silver powder is 0.15-0.26mm, the cotton The grain size of peach is 0.20-0.29mm, and the grain diameter of the resin is 0.09-0.15mm.
14. according to the method described in any one of claim 1-4, wherein the packing material is plant fiber composite wood Material.
15. according to the method for claim 14, wherein the composite material of plant fiber is wood fiber and/or wheat straw Fiber.
16. according to the method for claim 15, wherein the grain size of the packing material is 0.02-0.3mm.
17. according to the method described in claim 1, wherein, this method further includes inhibiting the mixture of step (5) and macromolecular Agent mixing stirs and surveys it and misses situation.
18. according to the method for claim 17, wherein the macromolecular inhibitor be potassium ammonium hydrolyzed polyacrylonitrile and/ Or sulfonation nitro khm.
19. according to the method for claim 18, wherein the macromolecular inhibitor is potassium ammonium hydrolyzed polyacrylonitrile and sulphur The mixture of change nitro khm, and the dosage of the potassium ammonium hydrolyzed polyacrylonitrile and the sulfonation nitro khm Weight ratio is (0.38-0.61):1.
20. according to the method for claim 19, wherein on the basis of the drilling fluid of 100 parts by weight, the macromolecular The dosage of inhibitor is 2-6 parts by weight.
21. according to the method for claim 20, wherein the dosage of the macromolecular inhibitor is 3-5 parts by weight.
22. according to the method described in claims 1 or 21, wherein the stirring condition includes:Stir speed (S.S.) is 7000-10000 Rev/min.
23. according to the method for claim 22, wherein stir speed (S.S.) is 8000-9000 revs/min.
CN201711124146.7A 2017-11-14 2017-11-14 A method of expanding narrow ' Safe Density Windows Active CN107939383B (en)