CN107858112A - The compound kraft paper gummed tape being layered for fireworks - Google Patents
The compound kraft paper gummed tape being layered for fireworks Download PDFInfo
- Publication number
- CN107858112A CN107858112A CN201711374301.0A CN201711374301A CN107858112A CN 107858112 A CN107858112 A CN 107858112A CN 201711374301 A CN201711374301 A CN 201711374301A CN 107858112 A CN107858112 A CN 107858112A
- Authority
- CN
- China
- Prior art keywords
- layer
- fireworks
- kraft paper
- layered
- outer layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of compound kraft paper gummed tape being layered for fireworks, including the three-layer composite structure that the first outer layer, intermediate layer and the second outer layer are formed;First outer layer is that thickness is 10~26g/m2Layers of kraft paper, intermediate layer is that thickness is 15~25g/m2Hot melt adhesive layer, the second outer layer be adhere to release layer ply of paper or film layer;The release layer of second outer layer is between intermediate layer and the second outer layer.The situation that the adhesive tape has prevented can not to peel off or peel off difficulty occurs, guarantee peeling effect that can be very, substantially increases production efficiency;Significantly reduce production and application cost;Ensure that firework display order and rhythm are seted off by the design requirement of producer, at the same effectively avoid Mars sputter caused by " jump is drawn " unordered set off phenomenon.
Description
Technical field
The present invention relates to a kind of kraft paper gummed tape being layered.
Background technology
Layering kraft paper gummed tape of the prior art is widely used in the production technology of all kinds of refrigerators, refrigerator-freezer.Its structure
As shown in figure 1, including PE leaching membrane layers 2, layering brown paper, rubberised layer 5.The upper surface for being layered brown paper is thickness (with grammes per square metre table
Show, similarly hereinafter) it is 15~18g/m2PE leaching membrane layers 2, lower surface even spread rubberised layer 5, bondline thickness is 35~45g/m2.Institute
State the upper surface of PE leaching membrane layers 2 and be attached with release layer 1.The release layer 1 is usually to coat what the silicone oil through processing was formed, in adhesive tape
Prevent PE leaching membrane layers 2 from can not be separated with 5 excessive adhesion of rubberised layer after coiled.
The layering brown paper 3 is made up of the special brown paper that can be layered as upper paper 4 and lower floor's paper 5, the ox-hide
Paper uses the log of Russia to starch as raw material, and papermaking pressure and tension force are automatically adjusted with advanced infrared control system, so as to
Make existing 65~70g/m of grammes per square metre2Layering brown paper 3.If its delamination is two layers of upper paper 3 and lower floor's paper 4,
The grammes per square metre of every layer of paper is in 32~35g/m2Between.
Employ above-mentioned layering animal glue band in present fireworks industry to be used to paste the lead that fixed ignition passes fire, mainly
It is that stickup for ignition fuse on fireworks cylinder is fixed, dosage is very big, belongs to indispensable former auxiliary material in fireworks industry
Material.After adhesive tape is separated from tape roll, to avoid adhering to insecure and causing smog to need to peel off PE leaching with lead burning
The side of film layer 2 can be used, but brown paper can only be layered by separating by peeling off PE leaching membrane layers 2, by upper paper 3 and attached to it
Adhering-resistant layer 1, PE leaching membrane layers 2, which are peeled off, to be abandoned, and lead is pasted with lower floor's paper 4 of coating rubberised layer 5.
But there are following drawbacks in existing layering kraft paper gummed tape for fireworks industry:
1. its peeling effect can only ensure by the material of control paper, grammes per square metre, pressure, the content of moisture:For material,
Existing product must use the former wood pulp papermaking of Russia, greatly add cost to ensure peeling effect;With regard to grammes per square metre
For, existing layering kraft paper gummed tape can not decline the grammes per square metre of paper, in order to ensure peeling effect and pulling force, tension force etc.,
Grammes per square metre can only be controlled in 65~70g/m2Between, grammes per square metre, which is declined, can not just ensure that its layered effect meets that basic use will
Ask;For pressure, moisture, relevant control factor also is difficult to further improve in process of production;Even so, existing layering
The peeling effect of kraft paper gummed tape is still difficult to the requirement for meeting fireworks industry, has seriously blocked the raising of production efficiency.
2. peeling off discarded object to waste greatly, the PE leaching membrane layers 2 of attachment adhering-resistant layer 1 are not because the also attachment of upper paper 3 can
Recovery uses;Grammes per square metre reaches 32~35g/m2Upper paper also go out of use.Production cost is improved, wastes resource, is unfavorable for
Environmental protection and saving.
The content of the invention
In order to solve above-mentioned drawback, dividing for fireworks is exclusively used in the technical problem to be solved by the invention is to provide a kind of
The kraft paper gummed tape of layer, is easily peeled off, use cost is greatly reduced.In order to solve the above-mentioned technical problem, the skill that the present invention uses
Art scheme is the compound kraft paper gummed tape being layered for fireworks, it is characterised in that including the first outer layer, intermediate layer and
The three-layer composite structure that two outer layers are formed;First outer layer is that thickness is 10~26g/m2Layers of kraft paper, intermediate layer is that thickness is
15~25g/m2Hot melt adhesive layer, the second outer layer be adhere to release layer ply of paper or film layer;The release layer of second outer layer is located at
Between intermediate layer and the second outer layer.
Preferably, first outer layer is that thickness is 12~18g/m2Layers of kraft paper.Further, first outer layer
It is that thickness is 13~15g/m2Layers of kraft paper.
The production method of the compound kraft paper gummed tape being layered for fireworks comprises the following steps:
A. the brown paper as first outer layer is prepared in paper production line, brown paper thickness control is in 10~26g/m2
Between;
B. as uniformly applied on the mould release membrance of second outer layer or the layer upper surface of release liners be covered with thickness for 15~
25g/m2Hot melt adhesive layer;
C. on the obtained kraft compounded hot melt adhesive layer to described in step B, being produced in step A.
In aforementioned production method, the A, step B have no point of priority.
The application method of the compound kraft paper gummed tape being layered for fireworks is to peel off the second outer layer, and use is compound
The brown paper (the first outer layer) of hot melt adhesive layer (intermediate layer) pastes ignition fuse fixation on fireworks body.Outside second peeled off
Layer, which can reclaim, to be reused.
The beneficial effects of the present invention are,
1. kraft paper gummed tape provided by the invention, the situation for having prevented to peel off or peel off difficulty occurs, being capable of percentage
Hundred guarantee peeling effect, substantially increases production efficiency.
2. significantly reduce production and application cost:First, the brown paper thickness used is reduced to 12~18g/m2Between, phase
Declined to a great extent for existing product thickness;Second, can be with recycling mould release membrance or release liners;Third, it can use general
Logical log slurry makes brown paper, is starched without using the Russian imported log of costliness;Fourth, because the brown paper for being used to paste surpasses
Thin and flexibility, can also meet to require so as to which bondline thickness reduces, and glue consumption 75% is reduced relative to existing product;Fourth,
Reduce the use damage rate of adhesive tape.
3. after peeling off the second outer layer, intermediate layer and the first outer layer glue, which cover to be placed on lead, can easily form a ring
Around the three-dimensional closed cavity of lead, the cavity inner wall is brought into close contact with lead outer wall.Ensure to be in by fixed lead when standby
The state of sealing;After exposed lead riser is ignited, with the burning of lead, brown paper is burned out so that lead contacts with oxygen
It can realize that lead burns, so as to prevent the burning of lead great-jump-forward, ensure that firework display order and rhythm press the design of producer
It is required that set off, at the same effectively avoid Mars sputter caused by " jump is drawn " unordered set off phenomenon.
Traditional fireworks make for paper material, and the PUR uses PUR purchased in market.But for present mould
For pressing fireworks, its material includes land plaster, tapioca starch, waste paper, potassium permanganate, acrylic acid colloid, anti-blushing agent etc., and surface
It is coated with releasing agent.Larger damaging influence can be all produced on these materials to glueability.So, it is preferable that it is described
For hot melt adhesive layer using molding fireworks glue special, the component and its weight proportion of the glue are rubber oils:Thermoplastic elastic rubber
Glue:Resin:Liquid rubber:Antioxidant:Lightweight carbon dust=16~20:33~37:42~48:1~3:0.5~1.5:4~6.
Stirred by conventional method Hybrid Heating.Preferably, the component of the glue and its weight proportion are rubber oils:Thermoplastic
Property elastic caoutchouc:Resin:Liquid rubber:Antioxidant:Lightweight carbon dust=18:35:45:2:1:5.The glue each component raw material
Compatibility and all fine with the compatibility of adherend material, can overcome above-mentioned influence, be advantageous to gummed paper with being molded the jail of fireworks
By bonding.
In order to facilitate the understanding of the purposes, features and advantages of the present invention, below in conjunction with the accompanying drawings to the present invention
Embodiment be described in detail.Many details are elaborated in the following description in order to fully understand this hair
It is bright.But the invention can be embodied in many other ways as described herein, those skilled in the art can be not
Similar improvement is done in the case of running counter to intension of the present invention, therefore the present invention is not limited by following public specific embodiment.
Brief description of the drawings
Fig. 1 is the theory structure schematic diagram of existing layering kraft paper gummed tape;
Fig. 2 is the theory structure schematic diagram of kraft paper gummed tape of the present invention;
Fig. 3 is the use state principle schematic diagram (cross section, amplification) of existing layering kraft paper gummed tape;
Fig. 4 is the use state principle schematic diagram (cross section, amplification) of kraft paper gummed tape of the present invention.
Embodiment
Embodiment 1:Referring to accompanying drawing 2,4, reflect a kind of concrete structure of the present invention, it is described to be layered for the compound of fireworks
Kraft paper gummed tape 400 include the first outer layer 104, the outer layer 101 of intermediate layer 103 and second form three-layer composite structure;First
Outer layer 104 is that thickness is 10~26g/m2Layers of kraft paper, intermediate layer 103 is that thickness is 15~25g/m2Hot melt adhesive layer, second
Outer layer 101 is the ply of paper or film layer for adhering to release layer 102;The release layer 102 of second outer layer 101 is located at intermediate layer 103 and
Between two outer layers 101.
The production method of the compound kraft paper gummed tape being layered for fireworks comprises the following steps:
A. the brown paper as first outer layer 104, ox-hide thickness of paper are prepared in paper production line using log slurry paper pulp
(grammes per square metre) control is spent in 10~26g/m2Between, especially 12~18g/m2Between, preferably 13~15g/m2, to realize performance
Optimization;
B. uniformly applied on the release layer 102 in the film layer as second outer layer 101 or ply of paper and be covered with thickness as 15
~25g/m2Hot melt adhesive layer;
C. obtained brown paper in step A is fitted on the hot melt adhesive layer described in step B, produced.
In aforementioned production method, the A, step B have no point of priority.
The application method of the compound kraft paper gummed tape being layered for fireworks is that it is (release to peel off the second outer layer 101
Layer 102 is peeled off therewith), ignition fuse 300 is existed with the brown paper (the first outer layer 104) in composite hot melt glue-line (intermediate layer 103)
Stickup on fireworks body 200 is fixed.The second outer layer 101 peeled off, which can reclaim, to be reused.
Referring to Fig. 3, after lead 300 is adhered on fireworks body 200 by layering kraft paper gummed tape 100 of the prior art,
Even if (for example the lead 300 of parcel adhesive tape is clipped with two finger fingertips, and along the length side of lead 300 from A, B direction force
To smoothing out with the fingers), the completely docile and obedient parcel lead 300 of adhesive tape 100 can not be caused.It is closed the cavity that lead is formed and remains able to circulate
Air.This is also habitual state in industry.
Compares figure 4, equally exerted a force using adhesive tape 400 provided by the invention from A, B direction, due to the brown paper for pasting
Thin and flexible property is good, flexible good, and gluing be covered in can easily, permanently form one around lead on lead 300
Three-dimensional closed cavity, the cavity inner wall are brought into close contact with the outer wall of lead 300.Ensure to be in close by fixed lead 300 when standby
The state of envelope;After exposed lead riser is ignited, with the burning of lead 300, brown paper is burned out so that lead 300 and oxygen
Contact can realize that lead 300 burns, and so as to prevent the burning of the great-jump-forward of lead 300, ensure that firework display order and rhythm are pressed
The design requirement of producer is seted off, at the same effectively avoid Mars sputter caused by " jump is drawn " unordered set off phenomenon.To improve fireworks life
Yield and quality provides a unexpected new way.
Embodiment 2:In the adhesive tape of production molding fireworks, production method and structure are same as described above, with embodiment 1
Difference is to configure the component used during PUR and its weight proportion as rubber oil:Thermoplastic elastic rubber:Resin:
Liquid rubber:Antioxidant:Lightweight carbon dust=18:35:45:2:1:5.It is heated to after mixing between 130~160 DEG C, stirring 2~
3 hours well mixed.
In embodiment 3~8, it is with the difference of embodiment 2, the weight proportion such as following table institute of the component of the glue
Show:
Above-mentioned implementation is merely to clearly illustrate technical scheme, and it is not intended that to the present invention
Make any restrictions.The present invention has known a variety of replacements or deformation in the art, is not departing from essence of the invention
On the premise of meaning, protection scope of the present invention is each fallen within.
Claims (8)
1. the compound kraft paper gummed tape being layered for fireworks, it is characterised in that outside including the first outer layer, intermediate layer and second
The three-layer composite structure that layer is formed;First outer layer is that thickness is 10~26g/m2Layers of kraft paper, intermediate layer is thickness for 15~
25g/m2Hot melt adhesive layer, the second outer layer be adhere to release layer ply of paper or film layer;The release layer of second outer layer is positioned at centre
Between layer and the second outer layer.
2. it is used for the compound kraft paper gummed tape being layered of fireworks as claimed in claim 1, it is characterised in that outside described first
Layer is that thickness is 12~18g/m2Layers of kraft paper.
3. it is used for the compound kraft paper gummed tape being layered of fireworks as claimed in claim 2, it is characterised in that outside described first
Layer is that thickness is 13~15g/m2Layers of kraft paper.
4. the compound kraft paper gummed tape being layered for fireworks as described in claim any one of 1-3, it is characterised in that institute
The production method for stating the compound kraft paper gummed tape being layered for fireworks comprises the following steps:
A. the brown paper as first outer layer is prepared in paper production line, controls brown paper thickness on request;
B. it is being 15~25g/m as uniformly painting is covered with thickness on the mould release membrance of second outer layer or the layer upper surface of release liners2's
Hot melt adhesive layer;
C. on the obtained kraft compounded hot melt adhesive layer to described in step B, being produced in step A.
5. the compound kraft paper gummed tape being layered for fireworks as described in claim any one of 1-3, it is characterised in that institute
Stating the application method of the compound kraft paper gummed tape being layered for fireworks is, the second outer layer is peeled off, with composite hot melt glue-line
Brown paper pastes ignition fuse fixation on fireworks body.
6. the compound kraft paper gummed tape being layered for fireworks as described in claim any one of 1-3, it is characterised in that institute
Hot melt adhesive layer is stated using molding fireworks glue special, the component and its weight proportion of the glue are rubber oils:Thermoplastic elastic
Rubber:Resin:Liquid rubber:Antioxidant:Lightweight carbon dust=16~20:33~37:42~48:1~3:0.5~1.5:4~
6。
7. the compound kraft paper gummed tape being layered for fireworks as described in claim any one of 1-3, it is characterised in that institute
It is rubber oil to state the component of glue and its weight proportion:Thermoplastic elastic rubber:Resin:Liquid rubber:Antioxidant:Lightweight carbon
Powder=18:35:45:2:1:5.
8. the compound kraft paper gummed tape being layered for fireworks as described in claim any one of 1-3, it is characterised in that stripping
After the second outer layer, intermediate layer and the first outer layer glue cover to be placed on lead and form a three-dimensional closed cavity around lead,
The cavity inner wall is brought into close contact with lead outer wall.