CN107841121A - PC, PET blending formula - Google Patents
PC, PET blending formula Download PDFInfo
- Publication number
- CN107841121A CN107841121A CN201711175327.2A CN201711175327A CN107841121A CN 107841121 A CN107841121 A CN 107841121A CN 201711175327 A CN201711175327 A CN 201711175327A CN 107841121 A CN107841121 A CN 107841121A
- Authority
- CN
- China
- Prior art keywords
- parts
- pet
- mah
- resins
- blending formula
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of PC, PET blending to be formulated, and is equipped with every 100 parts of PC resins:32~35 parts of PET, 5.1~5.4 parts of PE g MAH.The present invention significantly improves tensile property.
Description
Technical field
The present invention relates to a kind of polymer composite formula, particularly a kind of PC blendings formula.
Background technology
PC intermingling materials can be used for making building materials, but tensile property needs to improve.
The content of the invention
The present invention in view of the shortcomings of the prior art, proposes a kind of PC, PET blending formula that can significantly improve tensile property.
The present invention is achieved through the following technical solutions technical goal.
PC, PET blending formula, it is theed improvement is that:It is equipped with every 100 parts of PC resins:32~35 parts of PET, 5.1~
5.4 parts of PE-g-MAH.
Further improvement is that:It is equipped with every 100 parts of PC resins:33~34 parts of PET, 5.2~5.3 parts of PE-g-MAH.
The present invention compared with prior art, has the positive effect that:
1st, PC, PET are blended, and significantly improve tensile property.
2nd, it is equipped with every 100 parts of PC resins:33~34 parts of PET, 5.2~5.3 parts of PE-g-MAH, can further improve stretching
Performance.
Embodiment
With reference to embodiment, the invention will be further described.
Embodiment 1:
PC, PET blending are formulated, and are equipped with every 100 parts of PC resins:32 parts of PET, 5.1 parts of PE-g-MAH.
Embodiment 2:
PC, PET blending are formulated, and are equipped with every 100 parts of PC resins:35 parts of PET, 5.4 parts of PE-g-MAH.
Embodiment 3:
PC, PET blending are formulated, and are equipped with every 100 parts of PC resins:33 parts of PET, 5.2 parts of PE-g-MAH.
Embodiment 4:
PC, PET blending are formulated, and are equipped with every 100 parts of PC resins:34 parts of PET, 5.3 parts of PE-g-MAH.
Claims (2)
- A kind of 1. PC, PET blending formula, it is characterised in that:It is equipped with every 100 parts of PC resins:32~35 parts of PET, 5.1~5.4 Part PE-g-MAH.
- 2. PC, PET blending formula according to claim 1, it is characterised in that:It is equipped with every 100 parts of PC resins:33~34 Part PET, 5.2~5.3 parts of PE-g-MAH.