CN107828352A - A kind of paper lantern has adhered to the preparation method of glutinous rice glue with not creasing easily - Google Patents
A kind of paper lantern has adhered to the preparation method of glutinous rice glue with not creasing easily Download PDFInfo
- Publication number
- CN107828352A CN107828352A CN201710879821.0A CN201710879821A CN107828352A CN 107828352 A CN107828352 A CN 107828352A CN 201710879821 A CN201710879821 A CN 201710879821A CN 107828352 A CN107828352 A CN 107828352A
- Authority
- CN
- China
- Prior art keywords
- parts
- glutinous rice
- prefabricated material
- adhered
- paper
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses the preparation method that a kind of paper lantern has adhered to glutinous rice glue with not creasing easily, comprise the following steps:Glutinous rice flour, starch Sodium Octenyl Succinate, water are stirred, add polysorbate60, urea, heating stirring obtains the first prefabricated material;Lignin fibre, diatomite, acetone are well mixed, epoxidized soybean oil is added and stirs, adds cocoyl ethylene hydroxy sulfuric acid sodium, water, maltitol, heating stirring obtains the second prefabricated material;Add that the second prefabricated material, epoxide-resin glue, defoamer, ethylene glycol, bactericide are well mixed to be obtained paper lantern and adhered to glutinous rice glue with not creasing easily into the first prefabricated material.Gained glutinous rice glue cohesive force of the invention is high, and the paper adhered to after solidification is not susceptible to wrinkling, and good toughness, tensile strength is high, it can effectively avoid reducing the aesthetics of paper because of hardness height after solidification, while wetting effect is good, effectively prevents the generation of skinning.
Description
Technical field
The present invention relates to paper lantern technical field, more particularly to the system that a kind of paper lantern has adhered to glutinous rice glue with not creasing easily
Preparation Method.
Background technology
Paper lantern is a kind of common traditional folk artifacts, is typically all by paper at present with the lantern made of paper being made
Lantern is used for viewing and admiring or decorating, to increase festive air, good illumination effect of the decorative effect of paper lantern than it at present;From name
It can be seen that the primary raw material made is paper, glue bonding papery profile, current paper lantern are coordinated typically on lantern frames
Typically adhered to glue using starch slurry, not only adhesion strength is low, and the corrugation of papery profile is easily caused after glue curing, sternly
Ghost image rings the decorative effect of lantern.
The content of the invention
Based on technical problem existing for background technology, the present invention proposes a kind of paper lantern and has adhered to glutinous rice with not creasing easily
The preparation method of glue, gained glutinous rice glue cohesive force is high, and the paper adhered to after solidification is not susceptible to wrinkling, and good toughness,
Tensile strength is high, can effectively avoid reducing the aesthetics of paper because of hardness height after solidification, while wetting effect is good, effectively prevents
The generation of skinning.
The preparation method that a kind of paper lantern proposed by the present invention has adhered to glutinous rice glue with not creasing easily, comprises the following steps:
S1, glutinous rice flour, starch Sodium Octenyl Succinate, water stirred, add polysorbate60, urea, heating is stirred
To the first prefabricated material;
S2, lignin fibre, diatomite, acetone is well mixed, adds epoxidized soybean oil and stir, add cocoyl
Ethylene hydroxy sulfuric acid sodium, water, maltitol, heating stirring obtain the second prefabricated material;
S3, add the second prefabricated material, epoxide-resin glue, defoamer, ethylene glycol, bactericide mixing into the first prefabricated material
The even paper lantern that obtains has adhered to glutinous rice glue with not creasing easily.
Preferably, in S1, glutinous rice flour, starch Sodium Octenyl Succinate, water are stirred, mixing speed 10-18r/
Min, polysorbate60, urea are added, be warming up to 60-75 DEG C of stirring 15-28min, obtain the first prefabricated material.
Preferably, in S1, by weight by 30-50 parts glutinous rice flour, 5-10 parts starch Sodium Octenyl Succinate, 100-150
Part water stirs, and mixing speed 10-18r/min, adds 1-2 parts polysorbate60,2-4 part urea, is warming up to 60-75 DEG C of stirring
15-28min, obtain the first prefabricated material.
Preferably, in S2, lignin fibre, diatomite, acetone are well mixed, epoxidized soybean oil is added and stirs,
Cocoyl ethylene hydroxy sulfuric acid sodium, water, maltitol are added, 65-75 DEG C of stirring 2-4h is warming up to, obtains the second prefabricated material.
Preferably, in S2,15-35 parts lignin fibre, 4-8 parts diatomite, 80-110 parts acetone are mixed by weight
Uniformly, 3-4 part epoxidized soybean oils are added to stir, adds 1-2 part cocoyl ethylene hydroxy sulfuric acids sodium, 25-35 parts water, 15-25
Part maltitol, 65-75 DEG C of stirring 2-4h is warming up to, obtains the second prefabricated material.
Preferably, in S3, the second prefabricated material of 100-110 parts, 1- are added by weight into the first prefabricated material of 130-140 parts
4 parts of epoxide-resin glues, 1-2 parts defoamer, 1-4 parts ethylene glycol, 1-2 parts bactericide be well mixed to obtain paper lantern with not creasing easily
Glutinous rice glue is adhered to.
The present invention is compounded using glutinous rice flour, starch Sodium Octenyl Succinate, and both strands are similar, and can be cross-linked with each other raising
Cohesive force, under the cooperation of polysorbate60, make the first prefabricated material colloid of gained is fine and smooth, and the second prefabricated material coordinates to be added thereto, can have
Effect enhancing oxygen flow gas permeability, the paper adhered to after solidification are not susceptible to wrinkling, and good toughness, and tensile strength is high, can have
The aesthetics for avoiding that paper is reduced because of hardness height after solidification is imitated, paper transition is good;And in the second prefabricated material, lignin fibre with
Tripolite compound is matched somebody with somebody, oxygen flow good permeability, is coordinated epoxidized soybean oil, can be effectively dispersed in maltitol, and tensile strength is high, and
Size uniformity, there is certain pliability, good toughness after drying;Second prefabricated material compounds with urea, can effectively improve colloid and resist
Jelly property, and the addition of epoxide-resin glue, the initial viscosity of gained glutinous rice glue is substantially increased, is less prone to extension flow phenomenon, coordinated
Ethylene glycol acts on, and wetting effect is good, effectively prevents the generation of skinning, and plasticization effect is notable, and toughness further enhances.
Embodiment
Below, technical scheme is described in detail by specific embodiment.
Embodiment 1
A kind of paper lantern has adhered to the preparation method of glutinous rice glue with not creasing easily, and comprises the following steps:
S1, glutinous rice flour, starch Sodium Octenyl Succinate, water stirred, add polysorbate60, urea, heating is stirred
To the first prefabricated material;
S2, lignin fibre, diatomite, acetone is well mixed, adds epoxidized soybean oil and stir, add cocoyl
Ethylene hydroxy sulfuric acid sodium, water, maltitol, heating stirring obtain the second prefabricated material;
S3, add the second prefabricated material, epoxide-resin glue, defoamer, ethylene glycol, bactericide mixing into the first prefabricated material
The even paper lantern that obtains has adhered to glutinous rice glue with not creasing easily.
Embodiment 2
A kind of paper lantern has adhered to the preparation method of glutinous rice glue with not creasing easily, and comprises the following steps:
S1,30 parts of glutinous rice flours, 10 parts of starch Sodium Octenyl Succinates, 100 parts of water are stirred by weight, stirring speed
Spend for 18r/min, add 1 part of polysorbate60,4 parts of urea, be warming up to 60 DEG C of stirring 28min, obtain the first prefabricated material;
S2,15 parts of lignin fibres, 8 parts of diatomite, 80 parts of acetone are well mixed by weight, it is big to add 4 parts of epoxies
Soya-bean oil stirs, and adds 1 part of cocoyl ethylene hydroxy sulfuric acid sodium, 35 parts of water, 15 parts of maltitols, is warming up to 75 DEG C of stirring 2h,
Obtain the second prefabricated material;
S3, by weight into 140 part of first prefabricated material add 100 part of second prefabricated material, 4 parts of epoxide-resin glues, 1 part disappear
Infusion, 4 parts of ethylene glycol, 1 part of bactericide be well mixed to be obtained paper lantern and has adhered to glutinous rice glue with not creasing easily.
Embodiment 3
A kind of paper lantern has adhered to the preparation method of glutinous rice glue with not creasing easily, and comprises the following steps:
S1,50 parts of glutinous rice flours, 5 parts of starch Sodium Octenyl Succinates, 150 parts of water are stirred by weight, stirring speed
Spend for 10r/min, add 2 parts of polysorbate60s, 2 parts of urea, be warming up to 75 DEG C of stirring 15min, obtain the first prefabricated material;
S2,35 parts of lignin fibres, 4 parts of diatomite, 110 parts of acetone are well mixed by weight, it is big to add 3 parts of epoxies
Soya-bean oil stirs, and adds 2 parts of cocoyl ethylene hydroxy sulfuric acid sodium, 25 parts of water, 25 parts of maltitols, is warming up to 65 DEG C of stirring 4h,
Obtain the second prefabricated material;
S3, by weight into 130 part of first prefabricated material add 110 part of second prefabricated material, 1 part of epoxide-resin glue, 2 parts disappear
Infusion, 1 part of ethylene glycol, 2 parts of bactericide are well mixed to be obtained paper lantern and has adhered to glutinous rice glue with not creasing easily.
Embodiment 4
A kind of paper lantern has adhered to the preparation method of glutinous rice glue with not creasing easily, and comprises the following steps:
S1,35 parts of glutinous rice flours, 8 parts of starch Sodium Octenyl Succinates, 120 parts of water are stirred by weight, stirring speed
Spend for 16r/min, add 1.2 parts of polysorbate60s, 3.5 parts of urea, be warming up to 65 DEG C of stirring 24min, obtain the first prefabricated material;
S2,30 parts of lignin fibres, 5 parts of diatomite, 100 parts of acetone are well mixed by weight, add 3.2 parts of epoxies
Soybean oil stirs, and adds 1.7 parts of cocoyl ethylene hydroxy sulfuric acid sodium, 28 parts of water, 22 parts of maltitols, is warming up to 68 DEG C of stirrings
3.5h, obtain the second prefabricated material;
S3, by weight into 132 part of first prefabricated material add 108 part of second prefabricated material, 2 parts of epoxide-resin glues, 1.7 parts
Defoamer, 2 parts of ethylene glycol, 1.7 parts of bactericide are well mixed to be obtained paper lantern and has adhered to glutinous rice glue with not creasing easily.
Embodiment 5
A kind of paper lantern has adhered to the preparation method of glutinous rice glue with not creasing easily, and comprises the following steps:
S1,45 parts of glutinous rice flours, 6 parts of starch Sodium Octenyl Succinates, 140 parts of water are stirred by weight, stirring speed
Spend for 12r/min, add 1.8 parts of polysorbate60s, 2.5 parts of urea, be warming up to 70 DEG C of stirring 20min, obtain the first prefabricated material;
S2,20 parts of lignin fibres, 7 parts of diatomite, 90 parts of acetone are well mixed by weight, add 3.8 parts of epoxies
Soybean oil stirs, and adds 1.3 parts of cocoyl ethylene hydroxy sulfuric acid sodium, 32 parts of water, 18 parts of maltitols, is warming up to 72 DEG C of stirrings
2.5h, obtain the second prefabricated material;
S3, by weight into 138 part of first prefabricated material add 102 part of second prefabricated material, 3 parts of epoxide-resin glues, 1.3 parts
Defoamer, 3 parts of ethylene glycol, 1.2 parts of bactericide are well mixed to be obtained paper lantern and has adhered to glutinous rice glue with not creasing easily.
Embodiment 6
A kind of paper lantern has adhered to the preparation method of glutinous rice glue with not creasing easily, and comprises the following steps:
S1,40 parts of glutinous rice flours, 7 parts of starch Sodium Octenyl Succinates, 130 parts of water are stirred by weight, stirring speed
Spend for 14r/min, add 1.5 parts of polysorbate60s, 3 parts of urea, be warming up to 68 DEG C of stirring 22min, obtain the first prefabricated material;
S2,25 parts of lignin fibres, 6 parts of diatomite, 95 parts of acetone are well mixed by weight, add 3.5 parts of epoxies
Soybean oil stirs, and adds 1.5 parts of cocoyl ethylene hydroxy sulfuric acid sodium, 30 parts of water, 20 parts of maltitols, is warming up to 70 DEG C of stirrings
3h, obtain the second prefabricated material;
S3,105 part of second prefabricated material, 2.5 parts of epoxide-resin glues, 1.5 are added into 135 part of first prefabricated material by weight
Part defoamer, 2.5 parts of ethylene glycol, 1.5 parts of bactericide are well mixed to be obtained paper lantern and has adhered to glutinous rice glue with not creasing easily.
The foregoing is only a preferred embodiment of the present invention, but protection scope of the present invention be not limited thereto,
Any one skilled in the art the invention discloses technical scope in, technique according to the invention scheme and its
Inventive concept is subject to equivalent substitution or change, should all be included within the scope of the present invention.
Claims (6)
1. a kind of paper lantern has adhered to the preparation method of glutinous rice glue with not creasing easily, it is characterised in that comprises the following steps:
S1, glutinous rice flour, starch Sodium Octenyl Succinate, water stirred, add polysorbate60, urea, heating stirring obtains the
One prefabricated material;
S2, lignin fibre, diatomite, acetone is well mixed, adds epoxidized soybean oil and stir, add cocoyl hydroxyl second
Base sodium sulphate, water, maltitol, heating stirring obtain the second prefabricated material;
S3, into the first prefabricated material, the second prefabricated material of addition, epoxide-resin glue, defoamer, ethylene glycol, bactericide are well mixed
To paper lantern glutinous rice glue has been adhered to not creasing easily.
2. the preparation method that paper lantern has adhered to glutinous rice glue with not creasing easily according to claim 1, it is characterised in that S1
In, glutinous rice flour, starch Sodium Octenyl Succinate, water are stirred, mixing speed 10-18r/min, add polysorbate60, urine
Element, 60-75 DEG C of stirring 15-28min is warming up to, obtains the first prefabricated material.
3. paper lantern according to claim 1 or claim 2 has adhered to the preparation method of glutinous rice glue with not creasing easily, it is characterised in that
In S1,30-50 parts glutinous rice flour, 5-10 parts starch Sodium Octenyl Succinate, 100-150 part water are stirred by weight, stirred
It is 10-18r/min to mix speed, adds 1-2 parts polysorbate60s, 2-4 part urea, is warming up to 60-75 DEG C of stirring 15-28min, obtains the
One prefabricated material.
4. the preparation method that glutinous rice glue has been adhered to not creasing easily according to any one of the claim 1-3 paper lanterns, its feature
It is, in S2, lignin fibre, diatomite, acetone is well mixed, adds epoxidized soybean oil and stir, add cocoyl
Ethylene hydroxy sulfuric acid sodium, water, maltitol, 65-75 DEG C of stirring 2-4h is warming up to, obtains the second prefabricated material.
5. the preparation method that glutinous rice glue has been adhered to not creasing easily according to any one of the claim 1-4 paper lanterns, its feature
It is, in S2, is by weight well mixed 15-35 parts lignin fibre, 4-8 parts diatomite, 80-110 part acetone, adds 3-
4 parts of epoxidized soybean oils stir, and add 1-2 part cocoyl ethylene hydroxy sulfuric acids sodium, 25-35 parts water, 15-25 part maltitols,
65-75 DEG C of stirring 2-4h is warming up to, obtains the second prefabricated material.
6. the preparation method that glutinous rice glue has been adhered to not creasing easily according to any one of the claim 1-5 paper lanterns, its feature
It is, in S3, the second prefabricated material of 100-110 parts, 1-4 part asphalt mixtures modified by epoxy resin is added by weight into the first prefabricated material of 130-140 parts
Fat glue, 1-2 parts defoamer, 1-4 parts ethylene glycol, 1-2 parts bactericide be well mixed obtain paper lantern got well with the adhesion that do not crease easily it is glutinous
Rice glue.