CN107620436A - The method that block of glass wool surface is evened up - Google Patents

The method that block of glass wool surface is evened up Download PDF

Info

Publication number
CN107620436A
CN107620436A CN201610549800.8A CN201610549800A CN107620436A CN 107620436 A CN107620436 A CN 107620436A CN 201610549800 A CN201610549800 A CN 201610549800A CN 107620436 A CN107620436 A CN 107620436A
Authority
CN
China
Prior art keywords
carrier bar
curing oven
glass
mineral wool
glass wool
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610549800.8A
Other languages
Chinese (zh)
Inventor
王攀
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201610549800.8A priority Critical patent/CN107620436A/en
Publication of CN107620436A publication Critical patent/CN107620436A/en
Pending legal-status Critical Current

Abstract

The continuously shaped method of block of glass wool that present invention design is a kind of a flat surface, is to solve the problems, such as that conventional glass wool ceiling and sound absorption decorative plate production efficiency are low.This method is that carrier bar above and below the curing oven on mineral wool production line is regulated and controled out into speed difference, is made in mineral wool pressurized cooking process, has a surface to be skidded with carrier bar, and cotton plate surface is flattened, so as to the mineral wool sheet material of continuous production surfacing.

Description

The method that block of glass wool surface is evened up
Technical field
The present invention relates to a kind of production method for the mineral wool sheet material for having a flat surface, the cotton plate of this method production can Making for ceiling and sound absorption decorative plate.
Background technology
At present, the method making that the substrate of glass wool ceiling and sound absorption decorative plate is all piece molded or hair plates polishes , efficiency is low, limits the development of industry.
Curing oven carrier bar all seam and passage on mineral wool production line.In pressurized, heated mineral wool, in cotton plate Two surfaces produce obvious carrier bar impression, it is impossible to are directly used as the base material of the products such as ceiling.
The content of the invention
In block of glass wool production process, the glass raw cotton of binding agent is jetted through, curing oven is fed by conveyer belt, raw cotton exists Carrier bar extrudes the lower thickness for keeping fixation to curing oven up and down, is heated when travelling forward, two carrier bars are regulated and controled out a speed difference, i.e., Upper link plate descends carrier bar slow or vice versa soon, and cotton plate can only be synchronous with holdings of one of carrier bar, and with the skidding of another carrier bar, cotton plate is beaten Sliding surface can not form the impression of gap and passage between carrier bar, so as to produce the block of glass wool of a flat surface. Further, one or two surface of raw cotton is plated in Chopped Strand Mat or glass-fiber-fabric before curing oven, and on Chopped Strand Mat or glass-fiber-fabric Applying glue, feeds curing oven pressurized, heated together with raw cotton, due to being compounded in the felt of cotton plate surface, cloth material and the difference of glue, on Lower surface forms different frictional force to carrier bar, so as to ensure that the big one side of cotton plate and frictional force is synchronous, small with frictional force one Face is skidded, and makes production stable operation, while produce the composite board of flat surface.
Brief description of the drawings
The present invention is further described below in conjunction with the accompanying drawings
1 centrifuge, 2 glue spraying ring, 3 expansion chamber, 4 conveyer belt, 5 glue spraying raw cotton, 6 curing oven, 7 upper link plate, 8 times carrier bars in figure 9 blocks of glass wool
The course of work is as follows
Glass fibre falls through glue spraying ring spray glue and is sent into solid in the bottom of expansion chamber 3, communicated band 4 as caused by centrifuge 1 Change in stove 6, under the extruding of upper link plate 7 and lower carrier bar 8, heated in advance, upper link plate speed is S1, and the speed of lower carrier bar is S2, if then mineral wool will be synchronous with the one side that frictional force is big by S1 > S2, skidded with the small one side of frictional force, the glass after curing molding The skidding surface of glass cotton plate 9 prints without carrier bar.

Claims (2)

1. a kind of production method of block of glass wool, it is characterised in that on tinuous production, the glass raw cotton for being jetted through binding agent exists The linear velocity of two carrier bars, is regulated and controled out speed difference by pressurized, heated between carrier bar above and below curing oven, and mineral wool can only be synchronous with a carrier bar, And skidded with another carrier bar, the surface of skidding can not form the impression of carrier bar, i.e. the surface of cotton plate is flattened.
2. the method as described in claim 1, it is characterised in that when glass raw cotton enters curing oven, one or two surface is plated in Chopped Strand Mat or glass-fiber-fabric, the difference of Facing material and gluing due to being compounded with felt or cloth, different frictional force is produced to carrier bar, Stable skidding face can be formed by carrier bar differential in curing oven pressurized cooking process, one side is smooth to answer so as to continuously produce Plywood material.
CN201610549800.8A 2016-07-13 2016-07-13 The method that block of glass wool surface is evened up Pending CN107620436A (en)