CN107620435A - A kind of assembled architecture indoor facing technique - Google Patents

A kind of assembled architecture indoor facing technique Download PDF

Info

Publication number
CN107620435A
CN107620435A CN201710848356.4A CN201710848356A CN107620435A CN 107620435 A CN107620435 A CN 107620435A CN 201710848356 A CN201710848356 A CN 201710848356A CN 107620435 A CN107620435 A CN 107620435A
Authority
CN
China
Prior art keywords
wall
assembled architecture
wall clothing
roller coat
architecture indoor
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710848356.4A
Other languages
Chinese (zh)
Inventor
黄建旺
黄自标
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Building Housing Technology Co Ltd
Original Assignee
Building Housing Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Building Housing Technology Co Ltd filed Critical Building Housing Technology Co Ltd
Priority to CN201710848356.4A priority Critical patent/CN107620435A/en
Publication of CN107620435A publication Critical patent/CN107620435A/en
Pending legal-status Critical Current

Abstract

The invention belongs to construction and decoration technical field, and in particular to a kind of assembled architecture indoor facing technique, comprise the following steps:(1) the piece processing between building element;(2) roller coat of waterproof priming paint;(3) interior decoration;(4) roller coat of wall clothing:At least in one layer of wall clothing of inner wall of building roller coat, and shell nosing treatment is carried out to finishing interface using wall clothing.The implementation of present invention process scheme, can effectively solve the technical problem that assembled architecture edge joint position is also easy to produce fine crack, by the roller coat for first completing to carry out after interior decoration wall clothing again, shell nosing treatment is carried out to finishing interface while wall clothing is arranged, closing in gluing processing is carried out without the later stage, facing toolability is good simultaneously, can prevent the shortcomings that traditional coating reparation construction is left a trace, slight out-of-flatness that can be effectively to PC inner wall surfaces is covered;Wall clothing uses roller coating technology and special construction tool, simple to operate, and 24 48 hours wall clothing curing moldings after wall clothing roller coat, can significantly shorten the duration, cost-effective.

Description

A kind of assembled architecture indoor facing technique
Technical field
The invention belongs to construction and decoration technical field, and in particular to a kind of assembled architecture indoor facing technique.
Background technology
Today's society, with the development of building industrialization, PC assembled architectures are greatly developed, new building construction mode Mainly by plant produced PC components, the advantages of scene is lifted, embodied is that main body assembled speed is fast, efficiency high.For In PC components room during fine fitment, the processing of interior wall is still mainly multiple using traditional Puttying or the technique coated, operation It is miscellaneous, and the duration is very long;Another aspect PC plate seam crossing metope is also easy to produce micro-crack, and the above method can not fundamentally solve this and ask Topic, later stage needs are caused largely to be repaired;Again, traditional metope processing method is generally required after specific fine fitment, is such as set Put and gluing shell nosing treatment is carried out to finishing interface after the completion of partition wall, furred ceiling, door and window cover, lines and ground construction, on the one hand one Determine to influence in degree attractive in appearance, reduce decoration quality, on the other hand increase finishing input, add decoration cost and extend work Phase, while carry out containing more harmful substance in the glue of gluing processing.
In summary, construction period can be shortened, improve finishing effect by needing offer one kind badly, can prevent going out for metope micro-crack Existing assembled architecture indoor facing technique.
The content of the invention
It can shorten construction period it is an object of the invention to provide one kind, improve finishing effect, metope micro-crack can be prevented The assembled architecture indoor facing technique of appearance.
Above-mentioned purpose is to be achieved through the following technical solutions:A kind of assembled architecture indoor facing technique, including following step Suddenly:
(1) the piece processing between building element;
(2) roller coat of waterproof priming paint:At least in one layer of waterproof priming paint of inner surface roller coat of inner wall of building;
(3) interior decoration:Including setting partition wall, furred ceiling, the installation of moulding and door and window cover, and ground construction;
(4) roller coat of wall clothing:At least in one layer of wall clothing of inner wall of building roller coat, and finishing interface is closed up using wall clothing Processing.
The implementation of present invention process scheme, waterproof priming paint can effectively reduce wall leakage phenomenon, and on the one hand utilize wall clothing The advantages of can effectively solve the technical problem that assembled architecture edge joint position tradition facing is also easy to produce fine crack, on the other hand pass through The roller coat of wall clothing is carried out after first completion interior decoration again, shell nosing treatment is carried out to finishing interface while wall clothing is arranged, without Later stage carries out closing in gluing processing, while facing toolability is good, can prevent the shortcomings that traditional coating reparation construction is left a trace, can Slight out-of-flatness effectively to PC inner wall surfaces is covered;Wall clothing uses roller coating technology and special construction tool, simple to operate, and 24-48 hour walls clothing curing molding, can significantly shorten the duration after wall clothing roller coat, cost-effective.
Further technical scheme of the invention is also to include the step of building element removing surface after the completion of the step (1) Suddenly.In this way, be advantageous to the roller coat of later stage waterproof priming paint and wall clothing.
Further technical scheme is that the waterproof priming paint used in the step (2) is white polyurethane waterproof priming paint. In this way, the polyurethane water-proof priming paint of white, is pre-processed to assembled architecture PC plate inner wall surface, it can reach waterproof and cover mixed Coagulate the purpose of native background color.
Further technical scheme is that the wall clothing is by purified cotton, wood fibre, cotton fiber, hydroxypropyl methyl fiber Element, water-soluble plant glue and functional filler are made.
Further technical scheme is that the preparation method of the wall clothing is as follows:By purified cotton, wood fibre and common cotton Fiber is woven into a diameter of 1~2 μm of one-ply yarn respectively, and is dyed on demand;By the fiber weaved cut into 5mm~ The segment of fiber of 25mm varying length;Basic viscose glue is made in hydroxypropyl methyl cellulose and water-soluble plant glue mixing;Will Segment of fiber, functional filler and basic viscose glue are put into mixing equipment, fully mix.
Further technical scheme is that the functional filler includes color filament, radium point and bright gold powder.
Further technical scheme is that the percentage by weight of the raw material of the wall clothing is as follows:Purified cotton 40-60%, wood Matter fiber 6-18%, cotton fiber 5-15%, color filament 7-12%, radium point and bright gold powder 5-10%, hydroxypropyl methyl fiber Plain 4-8% and water-soluble plant glue 10-15%.
Further technical scheme is that step (3) comprise the following steps that:First interior architecture space is surveyed Amount, obtain shape, the area size of each functional area;Then set according to the position of each functional area of acquisition, area size, really Determine ceiling structure and size, kitchen and bath's integrated morphology and size, the set location of indoor partition and its structure and size, moulding Set location and its structure and size;The installation of door and window cover and above-mentioned associated component is carried out again.
Further technical scheme is also to include indoor infrared after the step (4) and heat preset time and incite somebody to action Room air is evacuated to the step of outdoor.In this way, the harmful substance in decorating and renovating material comes out in a short time, avoid There is phenomenon repeatedly in indoor harmful gas concentration after conventional process, and shortens processing time.
Further technical scheme is that interior is provided with pollutant absorption plant, and the pollutant absorption plant is described Pollutant absorption plant bottom is provided with reative cell, and the reative cell internal memory contains sodium chlorite and citric acid, and the reative cell is pre- Hand-hole is left, solvent can be injected into reative cell by hand-hole;The top of reative cell is provided with adsorption chamber, in the adsorption chamber It is connected provided with adsorbent and with the reative cell, the adsorption chamber is provided with spout hole.
In this way, after using solvent is injected into reative cell in hand-hole, sodium chlorite and the generable chemistry of citric acid are anti- Chlorine dioxide and should be generated, chlorine dioxide escapes into the adsorbed agent of adsorption chamber and adsorbed, and adsorbent is slowly to interior Chlorine dioxide is discharged, continual elimination is carried out to indoor air pollutants, especially PARA FORMALDEHYDE PRILLS(91,95), toluene etc. can be effective Eliminate.Meanwhile can by control solvent injection rate and adsorbent and reactant between ratio control adsorbent release two Aoxidize the speed of chlorine body.
Brief description of the drawings
The accompanying drawing for forming the part of the present invention is used for providing a further understanding of the present invention, schematic reality of the invention Apply example and its illustrate to be used to explain the present invention, do not form inappropriate limitation of the present invention.
Fig. 1 is the inner wall of building " finishing process profile involved by one embodiment of the present invention;
Fig. 2 is the structural representation that door moulding closes up with wall clothing.
In figure:
The moulding of 1 wall clothing, 2 waterproof priming paint, 3 inner wall of building, 4 concrete ceiling 5
Embodiment
The present invention will be described in detail below in conjunction with the accompanying drawings, and the description of this part is only exemplary and explanatory, should not There is any restriction effect to protection scope of the present invention.In addition, description of the those skilled in the art according to this document, can be right Feature in this document in embodiment and in different embodiments carries out respective combination.
The embodiment of the present invention is as follows, referring to Figures 1 and 2, a kind of assembled architecture indoor facing technique, including following step Suddenly:
(1) the piece processing between building element;
(2) roller coat of waterproof priming paint 2:At least in one layer of waterproof priming paint 2 of inner surface roller coat of inner wall of building 3;
(3) interior decoration:Including setting partition wall, furred ceiling, the installation of moulding 5 and door and window cover, and ground construction;
(4) roller coat of wall clothing 1:At least in inner wall of building 3 roller coat, one layer of wall clothing 1, and finishing interface is carried out using wall clothing 1 Shell nosing treatment.
The implementation of present invention process scheme, waterproof priming paint 2 can effectively reduce wall leakage phenomenon, and on the one hand utilize wall clothing 1 the advantages of, can effectively solve the technical problem that assembled architecture edge joint position tradition facing is also easy to produce fine crack, on the other hand logical Carry out the roller coat of wall clothing 1 again after interior decoration is first completed, shell nosing treatment carried out to finishing interface while wall clothing 1 is arranged, Closing in gluing processing is carried out without the later stage, while facing toolability is good, can prevent that traditional coating reparation construction leaves a trace lacks Point, slight out-of-flatness that can be effectively to PC inner wall surfaces are covered;Wall clothing 1 uses roller coating technology and special construction tool, operation Simply, the curing molding of 24-48 hour walls clothing 1 and after the roller coat of wall clothing 1, can significantly shorten the duration, cost-effective.
It is preferred that such as Fig. 1, concrete ceiling 4 also is provided with wall clothing 1.
Further technical scheme of the invention is also to include the step of building element removing surface after the completion of the step (1) Suddenly.In this way, be advantageous to the roller coat of later stage waterproof priming paint 2 and wall clothing 1.
On the basis of above-described embodiment, in another embodiment of the present invention, the waterproof priming paint 2 of use in the step (2) For white polyurethane waterproof priming paint 2.In this way, the polyurethane water-proof priming paint 2 of white, is carried out pre- to assembled architecture PC plate inner wall surface Processing, it can reach waterproof and cover the purpose of concrete background color.
On the basis of above-described embodiment, in another embodiment of the present invention, the wall clothing 1 is by purified cotton, wood fibre, cotton Fiber, hydroxypropyl methyl cellulose, water-soluble plant glue and functional filler are made.
On the basis of above-described embodiment, in another embodiment of the present invention, the preparation method of the wall clothing 1 is as follows:By essence Cotton, wood fibre and common cotton fiber processed are woven into a diameter of 1~2 μm of one-ply yarn respectively, and are dyed on demand;It will spin The fiber woven cuts into the segment of fiber of 5mm~25mm varying length;By hydroxypropyl methyl cellulose and water-soluble plant glue Basic viscose glue is made in mixing;Segment of fiber, functional filler and basic viscose glue are put into mixing equipment, fully mixed.
On the basis of above-described embodiment, in another embodiment of the present invention, the functional filler include color filament, Radium point and bright gold powder.
On the basis of above-described embodiment, in another embodiment of the present invention, the weight percent of the raw material of the wall clothing 1 is such as Under:Purified cotton 40-60%, wood fibre 6-18%, cotton fiber 5-15%, color filament 7-12%, radium point and bright gold powder 5- 10%th, hydroxypropyl methyl cellulose 4-8% and water-soluble plant glue 10-15%.
On the basis of above-described embodiment, in another embodiment of the present invention, step (3) comprise the following steps that:First Interior architecture space is measured, obtains shape, the area size of each functional area;Then according to each functional area of acquisition Position, area size are set, determine ceiling structure and size, kitchen and bath's integrated morphology and size, the set location of indoor partition and Its structure and size, the set location of moulding 5 and its structure and size;The peace of door and window cover and above-mentioned associated component is carried out again Dress.
On the basis of above-described embodiment, in another embodiment of the present invention, also add after the step (4) including indoor infrared Heat treatment preset time and the step that room air is evacuated to outdoor.In this way, the harmful substance in decorating and renovating material is in short-term It is interior to come out, the phenomenon of indoor harmful gas concentration appearance repeatedly after conventional process is avoided, and shorten place Manage the time.
On the basis of above-described embodiment, in another embodiment of the present invention, interior is provided with pollutant absorption plant, described Pollutant absorption plant, the pollutant absorption plant bottom are provided with reative cell, the reative cell internal memory contain sodium chlorite and Citric acid, the reative cell are reserved with hand-hole, and solvent can be injected into reative cell by hand-hole;The top of reative cell is provided with Adsorption chamber, the adsorption chamber is interior to be provided with adsorbent and is connected with the reative cell, and the adsorption chamber is provided with spout hole.
In this way, after using solvent is injected into reative cell in hand-hole, sodium chlorite and the generable chemistry of citric acid are anti- Chlorine dioxide and should be generated, chlorine dioxide escapes into the adsorbed agent of adsorption chamber and adsorbed, and adsorbent is slowly to interior Chlorine dioxide is discharged, continual elimination is carried out to indoor air pollutants, especially PARA FORMALDEHYDE PRILLS(91,95), toluene etc. can be effective Eliminate.Meanwhile can by control solvent injection rate and adsorbent and reactant between ratio control adsorbent release two Aoxidize the speed of chlorine body.
Described above is only the preferred embodiment of the present invention, it is noted that for the ordinary skill people of the art For member, under the premise without departing from the principles of the invention, some improvements and modifications can also be made, these improvements and modifications also should It is considered as protection scope of the present invention.

Claims (10)

1. a kind of assembled architecture indoor facing technique, comprises the following steps:
(1) the piece processing between building element;
(2) roller coat of waterproof priming paint:At least in one layer of waterproof priming paint of inner surface roller coat of inner wall of building;
(3) interior decoration:Including setting partition wall, furred ceiling, the installation of moulding and door and window cover, and ground construction;
(4) roller coat of wall clothing:At least in one layer of wall clothing of inner wall of building roller coat, and finishing interface is carried out at closing in using wall clothing Reason.
2. assembled architecture indoor facing technique according to claim 1, it is characterised in that after the completion of the step (1) The step of also including building element removing surface.
3. assembled architecture indoor facing technique according to claim 2, it is characterised in that used in the step (2) Waterproof priming paint be white polyurethane waterproof priming paint.
4. the assembled architecture indoor facing technique according to claims 1 to 3 any one, it is characterised in that the wall Clothing is made by purified cotton, wood fibre, cotton fiber, hydroxypropyl methyl cellulose, water-soluble plant glue and functional filler.
5. assembled architecture indoor facing technique according to claim 4, it is characterised in that the preparation method of the wall clothing It is as follows:Purified cotton, wood fibre and common cotton fiber are woven into a diameter of 1~2 μm of one-ply yarn respectively, and carried out on demand Dyeing;The fiber weaved is cut into the segment of fiber of 5mm~25mm varying length;By hydroxypropyl methyl cellulose and water-soluble Basic viscose glue is made in property natural plant gum mixing;Segment of fiber, functional filler and basic viscose glue are put into mixing equipment, it is fully mixed It is even.
6. assembled architecture indoor facing technique according to claim 5, it is characterised in that the functional filler includes Color filament, radium point and bright gold powder.
7. assembled architecture indoor facing technique according to claim 6, it is characterised in that the weight of the raw material of the wall clothing It is as follows to measure percentage:Purified cotton 40-60%, wood fibre 6-18%, cotton fiber 5-15%, color filament 7-12%, radium point With bright gold powder 5-10%, hydroxypropyl methyl cellulose 4-8% and water-soluble plant glue 10-15%.
8. assembled architecture indoor facing technique according to claim 4, it is characterised in that the step (3) it is specific Step is as follows:First interior architecture space is measured, obtains shape, the area size of each functional area;Then according to acquisition The position of each functional area, area size are set, and determine ceiling structure and size, kitchen and bath's integrated morphology and size, indoor partition Set location and its structure and size, moulding set location and its structure and size;Door and window cover and above-mentioned is carried out again The installation of associated component.
9. assembled architecture indoor facing technique according to claim 8, it is characterised in that also wrapped after the step (4) Include the step that indoor infrared heats preset time and room air is evacuated to outdoor.
10. assembled architecture indoor facing technique according to claim 8, it is characterised in that interior is provided with pollutant Absorption plant, the pollutant absorption plant, the pollutant absorption plant bottom are provided with reative cell, the reative cell memory storage There are sodium chlorite and citric acid, the reative cell is reserved with hand-hole, and solvent can be injected into reative cell by hand-hole;Reaction The top of room is provided with adsorption chamber, and adsorbent is provided with the adsorption chamber and is connected with the reative cell, the adsorption chamber is provided with Spout hole.
CN201710848356.4A 2017-09-19 2017-09-19 A kind of assembled architecture indoor facing technique Pending CN107620435A (en)