CN107471372A - A kind of wood treatment process for making seamless pseudo-classic furniture - Google Patents

A kind of wood treatment process for making seamless pseudo-classic furniture Download PDF

Info

Publication number
CN107471372A
CN107471372A CN201710820358.2A CN201710820358A CN107471372A CN 107471372 A CN107471372 A CN 107471372A CN 201710820358 A CN201710820358 A CN 201710820358A CN 107471372 A CN107471372 A CN 107471372A
Authority
CN
China
Prior art keywords
timber
high temperature
shaping
furniture
wood
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710820358.2A
Other languages
Chinese (zh)
Inventor
曹运建
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANXI TANGRENJU ANCIENT HOUSEHOLD CULTURE Co Ltd
Original Assignee
SHANXI TANGRENJU ANCIENT HOUSEHOLD CULTURE Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANXI TANGRENJU ANCIENT HOUSEHOLD CULTURE Co Ltd filed Critical SHANXI TANGRENJU ANCIENT HOUSEHOLD CULTURE Co Ltd
Priority to CN201710820358.2A priority Critical patent/CN107471372A/en
Publication of CN107471372A publication Critical patent/CN107471372A/en
Pending legal-status Critical Current

Abstract

The present invention relates to furniture processing technology field, a kind of more particularly to wood treatment process for making seamless pseudo-classic furniture, technical problem to be solved is to be to provide a kind of wood treatment process for making seamless pseudo-classic furniture, make solid wood furniture overall appearance, safeguard simple, service life is grown, and the technical scheme used is comprises the following steps:Shaping is compressed to hardwood timber using high temperature, high pressure, vapor first, high temperature casting closing is then carried out again, is finally closed again with professional insulation rubber.

Description

A kind of wood treatment process for making seamless pseudo-classic furniture
Technical field
The present invention relates to furniture processing technology field, more particularly to a kind of wood-treating worker for making seamless pseudo-classic furniture Skill.
Background technology
Classic solid wood furniture, furniture panel generally have the not wide not narrow gap of bar, and this gap is referred to as expansion joint, this The expansion joint for seeming unremarkable is but very crucial, and its presence is mainly to contain the characteristic expanded with heat and contract with cold of solid wood, extends real The service life of wooden furniture, expansion joint are a kind of traditional handicrafts of Chinese classic furniture, are in order to when timber is by external environment Influence and be not to crack the frame of furniture when convergent-divergent, cause furniture components to loosen, can not normal use, especially It it is the heat supply in winter phase, temperature raises in family, protection of the solid wood furniture with greater need for this road expansion joint.
But expansion joint also brings many troubles, as maintenance, repair cost, desktop expansion joint health cleaning and Overall attractive in appearance of furniture, simultaneous retractable seam also has serious quality problems, such as loosens, shrinks, expands, is unfavorable for handed down from ancient times hundred Year, this just needs the research of seamless furniture, solves pseudo-classic furniture problem in thousand.
The content of the invention
Present invention solves the technical problem that being to provide a kind of wood treatment process for making seamless pseudo-classic furniture, make solid wood Furniture overall appearance, safeguard simple, service life length.
In order to solve the above-mentioned technical problem, the technical solution adopted in the present invention is:It is a kind of to make seamless pseudo-classic furniture Wood treatment process, comprise the following steps:Shaping is compressed to hardwood timber using high temperature, high pressure, vapor first, then High temperature casting closing is carried out again, is finally closed again with professional insulation rubber.
A kind of wood treatment process for making seamless pseudo-classic furniture, specifically includes following steps:
1. compression shaping:120 DEG C of -180 DEG C of thermophilic digestions of timber are handled 24 hours first;Make wood-fibred expansion softening, then Timber is placed in 120 DEG C of -180 DEG C of vapor heating platforms, carries out high temperature, pressurization, shaping, thickness is at below 40mm timber Manage 3-5 hours, thickness is 40mm-50mm treating of wood 6-10 hours, and thickness is more than 50mm treating of wood 24 hours;
2. high temperature casting:Timber high temperature casting at 80 DEG C -100 DEG C after shaping, with wax molecular replacement hydrone, continuous processing 7-15 days;Then timber is placed in 120 DEG C of -180 DEG C of vapor heating platforms again, to noted wax timber carry out high temperature, pressurization, Shaping, 3-24 hours are needed to handle completion according to the thickness difference of timber;
3. professional insulation rubber closing:Insulation rubber carries out continuous five closings.
The purpose of compression shaping as described above is that timber is handled by compression shaping, makes the density of timber shaping wood can obtain Redistribution, intensity, hardness are high, and anti-wear performance is good and can obtain the stability of timber simultaneously by processing.
As described above, the present invention has an advantageous effect in that compared with prior art:
1st, originality:Classic furniture generally has expansion joint, contains the characteristic expanded with heat and contract with cold of solid wood, and the present invention creates modelled after an antique The seamless process of furniture, had both accomplished seamless, while has also contained expanding with heat and contract with cold for solid wood, has solved pseudo-classic furniture problem in thousand.
2nd, overall aesthetics:The seamless process of pseudo-classic furniture of the present invention substantially increases the overall aesthetics of solid wood furniture, Solid wood furniture is set to turn into the more perfect art work and collectibles.
3rd, maintenance, repair cost is saved:The present invention pseudo-classic furniture seamless process make pseudo-classic furniture saved maintenance and Maintenance cost, without carrying out difficult hygienic cleaning to expansion joint.
4th, stability and wearability:The seamless process of the pseudo-classic furniture of the present invention, make timber shaping wooden by compression shaping Density can be redistributed, intensity, hardness are high, and anti-wear performance is good and can obtain the steady of timber simultaneously by processing It is qualitative.
5th, the life-span is extended:The seamless process of the pseudo-classic furniture of the present invention is isolated by compression shaping, high temperature casting and specialty Glue is closed, and is completely cut off with outside air, it is therefore prevented that oxidation of the air to furniture panel, make furniture sturdy and durable, life.
Embodiment
Below in conjunction with specific embodiment, the invention will be further described.
Embodiment 1
By taking rosewood as an example
Specifically include following steps:
1. compression shaping:120 DEG C of -180 DEG C of thermophilic digestions of rosewood material are handled 24 hours first;Make wood-fibred expansion softening, Then timber is placed in 120 DEG C of -180 DEG C of vapor heating platforms, carries out high temperature, pressurization, shaping, thickness 45mm, it is small to handle 8 When;
2. high temperature casting:Timber high temperature casting at 80 DEG C -100 DEG C after shaping, with wax molecular replacement hydrone, continuous processing 7-15 days;Then timber is placed in 120 DEG C of -180 DEG C of vapor heating platforms again, to noted wax timber carry out high temperature, pressurization, Shaping, handle 8 hours;
3. professional insulation rubber closing:Insulation rubber carries out continuous five closings.
Embodiment 2
By taking Door frame as an example
Specifically include following steps:
1. compression shaping:120 DEG C of -180 DEG C of thermophilic digestions of chicken wings timber are handled 24 hours first;Make wood-fibred expansion softening, Then timber is placed in 120 DEG C of -180 DEG C of vapor heating platforms, carries out high temperature, pressurization, shaping, thickness 38mm, it is small to handle 3 When;
2. high temperature casting:Timber high temperature casting at 80 DEG C -100 DEG C after shaping, with wax molecular replacement hydrone, continuous processing 7-15 days;Then timber is placed in 120 DEG C of -180 DEG C of vapor heating platforms again, to noted wax timber carry out high temperature, pressurization, Shaping, handle 3 hours;
3. professional insulation rubber closing:Insulation rubber carries out continuous five closings.
Embodiment 3
By taking sour branch wood as an example
Specifically include following steps:
1. compression shaping:Sour 120 DEG C of -180 DEG C of thermophilic digestions of branch timber are handled 24 hours first;Make wood-fibred expansion softening, Then timber is placed in 120 DEG C of -180 DEG C of vapor heating platforms, carries out high temperature, pressurization, shaping, thickness 47mm, it is small to handle 8 When;
2. high temperature casting:Timber high temperature casting at 80 DEG C -100 DEG C after shaping, with wax molecular replacement hydrone, continuous processing 7-15 days;Then timber is placed in 120 DEG C of -180 DEG C of vapor heating platforms again, to noted wax timber carry out high temperature, pressurization, Shaping, handle 8 hours;
3. professional insulation rubber closing:Insulation rubber carries out continuous five closings.
The present invention can be summarized with others without prejudice to the concrete form of the spirit or essential characteristics of the present invention.Therefore, nothing By from the point of view of which point, the embodiment above of the invention can only all be considered the description of the invention and can not limit invention, Claims indicate the scope of the present invention, and above-mentioned explanation does not point out the scope of the present invention, therefore, with the present invention The suitable implication and scope of claims in any change, be all considered as being included within the scope of the claims.

Claims (2)

1. a kind of wood treatment process for making seamless pseudo-classic furniture, it is characterised in that comprise the following steps:First using height Temperature, high pressure, vapor are compressed shaping to hardwood timber, then carry out high temperature casting closing again, are finally entered again with insulation rubber Row closing.
A kind of 2. wood treatment process for making seamless pseudo-classic furniture according to claim 1, it is characterised in that including with Lower step:
1. compression shaping:120 DEG C of -180 DEG C of thermophilic digestions of timber are handled 24 hours first;Then timber be placed in 120 DEG C- 180 DEG C of vapor heating platforms, high temperature, pressurization, shaping are carried out, thickness is below 40mm treating of wood 3-5 hours, and thickness is 40mm-50mm treating of wood 6-10 hours, the treating of wood that thickness is more than 50mm 24 hours;
2. high temperature casting:Timber high temperature casting at 80 DEG C -100 DEG C after shaping, continuous processing 7-15 days;Timber is placed in again 120 DEG C of -180 DEG C of vapor heating platforms, high temperature, pressurization, shaping are carried out to the timber for noting wax, it is different according to the thickness of timber 3-24 hours are needed to handle completion;
3. insulation rubber is closed:Insulation rubber carries out continuous five closings.
CN201710820358.2A 2017-09-13 2017-09-13 A kind of wood treatment process for making seamless pseudo-classic furniture Pending CN107471372A (en)